[Ifeffit] Fitting results
Abhijeet Gaur
abhijeetgaur9 at gmail.com
Thu Jan 21 01:28:27 CST 2010
Hello Sir,
I had done fitting of a Cu2O data taken at SSRL EXAFS
beamline in transmission mode, Stanford, by my research guide
Dr. B. D. Shrivastava.
I had used here the fiting procedure as discussed before in
this mailing list. The fitted curves are coming nice, but the
values of some fitting parameters are not reliable as shown *
bold* below.
*amp = 0.4898160 +/- 0.0469990 (1.0000)
* enot = 7.6843630 +/- 0.4828620 (0.0000)
alpha = 0.0022670 +/- 0.0030950 (0.0000)
* ss011 = 0.0003280 +/- 0.0013130 (0.0030)
* sscu11 = 0.0174780 +/- 0.0016220 (0.0030)
*sscu11o11 = 0.0470530 +/- 0.0655560 (0.0030)
* ss012 = 0.0070100 +/- 0.0044660 (0.0030)
sscu12 = 0.0186980 +/- 0.0093570 (0.0030)
* ss013cu11 = 0.0088980 +/- 0.0190580 (0.0030)
* sscu13 = 0.0196150 +/- 0.0062940 (0.0030)
sscu13012 = 0.0084870 +/- 0.0067030 (0.0030)
* sscu11cu11 = 0.0071110 +/- 0.0132390 (0.0030)
sscu12cu11 = 0.0111440 +/- 0.0139470 (0.0030)*
Def parameters (using "FEFF0: Path 1: [O1_1]"):
delr = 0.0041920
So, if someone can please tell me that where I had done wrong or what should
I do to make things right I will be very thankful. The Artemis project
file is attached herewith.
With regards
Abhijeet Gaur
Research Scholar
School of Studies in Physics
Vikram University, Ujjain (INDIA)
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20100121/51bb2aa0/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: Cu2O 13 fitting
Type: application/octet-stream
Size: 358385 bytes
Desc: not available
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20100121/51bb2aa0/attachment.obj>
More information about the Ifeffit
mailing list