[Ifeffit] debye function
Bruce Ravel
bravel at bnl.gov
Tue Aug 24 12:23:05 CDT 2010
On Tuesday 24 August 2010 12:23:18 pm Kleber Daum Machado wrote:
> Hi,
>
> I'd like to know the explicit mathematical expressions that are
> represented by the functions debye(temp,thetad) and eins(temp,thetae).
> Are they given in some documentation file or article?
See
"Extended x-ray absorption fine structure Debye-Waller
factors. I. Monatomic crystals"
E. Sevillano, H. Meuth, J. J. Rehr
Phys. Rev. B 20, 4908–4911 (1979)
http://link.aps.org/doi/10.1103/PhysRevB.20.4908
B
--
Bruce Ravel ------------------------------------ bravel at bnl.gov
National Institute of Standards and Technology
Synchrotron Methods Group at NSLS --- Beamlines U7A, X24A, X23A2
Building 535A
Upton NY, 11973
My homepage: http://xafs.org/BruceRavel
EXAFS software: http://cars9.uchicago.edu/~ravel/software/exafs/
More information about the Ifeffit
mailing list