[Ifeffit] Cementite EXAFS - thanks
Scott Calvin
SCalvin at slc.edu
Thu Sep 24 17:08:29 CDT 2009
One thing I can say is that the EXAFS data in Matt's archive is
reasonably well fit by a cementite structure. Since there's a lot of
variation in cementite-like materials, that doesn't tell us exactly
what it is, but at least it's in the right family.
--Scott Calvin
Sarah Lawrence College
On Sep 24, 2009, at 5:49 PM, Bhoopesh Mishra wrote:
> Hi Matt,
> I imagined you might not remember about the data or how was
> it prepared, so I decided not to bother you asking about it. But
> sounds like you do have an amazing memory.
>
> Yes, I would be happy to characterize the sample by running
> both EXAFS and XRD on it if you still have it. I would of course
> share the information with the mailing list, once I characterize it.
> I will collect the sample from you sometime soon. Thanks again for
> offering.
>
>
> Regards,
> Bhoopesh
>
More information about the Ifeffit