[Ifeffit] in situ liquid cell
Scott Calvin
SCalvin at slc.edu
Sun Mar 25 09:05:33 CDT 2007
Hi Renato,
I don't have a photo, but I have an article. The reference is:
"Automated system for x-ray absorption spectroscopy of nanoparticle
nucleation and growth," S. Calvin, E. E. Carpenter, V. Cestone, L. K.
Kurihara, V. G. Harris, and E. C. Brown, Rev. Sci. Instrum. 76, 016103 (2005).
This article has a design I used, and also references to some other
designs. If you don't have access to that journal, let me know, and
I'll send you a copy of the article.
--Scott Calvin
Sarah Lawrence College
At 05:49 AM 3/25/2007, you wrote:
>Dear Colleagues,
>
>I need to perform XAFS measurements microemulsions (liquid).
>As I do not have a liquid cell for the in situ XAFS measurements, I would
>like to know more about liquid cells.
>Could anyone shoot its cell and send me the photo?
>I am designing a cell where you optimize the edge
>jump by modifying the optical path.
>Thank you very much for your kind attention
>Renato Canha Ambrosio
More information about the Ifeffit
mailing list