I try multiple k-weights refinments with ARTEMIS of Al K EXAFS of ternary
aluminium and titanium nitrides films.
This system is rather disordered and textured with large grain boundaries
that contribute to EXAFS. Consequently only few parameters can be varied
simultaneously.
I think that the k**3 weighting plays the major role in the multiple
k-weights calculation.
There is no great dfference between the results of k**3 weight and
multiple k-weights fits.
Best regards
Marie-Hélène Tuilier
Laboratoire MMPF (Mécanique, matériaux et Procédés de Fabrication)
Pôle STIC-SPI-Maths, Université de Haute Alsace,
IUT de Mulhouse, 61 rue Albert Camus,
F-68093 Mulhouse Cedex
Tel : 33 (0)3 89 33 75 16
Fax : 33 (0)3 89 33 75 05
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20070413/a9c28298/attachment.html>
More information about the Ifeffit
mailing list