Hi Sham,
I agree with Carlo. I would also add that you should try different
k-weights, including multiple k-weights at once. Since the dependence
of S02 and ss on k is quite different, that can often reduce the
correlation between the two.
--Scott Calvin
Sarah Lawrence College
At 11:58 PM 12/19/2006, Shantanu Behera wrote:
>Hi Folks
>
>I have a small doubt. I work on the structural features of Y that are
>segregated to Alumina grain boundaries (very dilute amounts of Yttrium
>in polycrystalline alumina).
>
>In some of my fits, I find a correlation ~0.85 between SO2 and ss. If
>I restrain the ss, from 0.004 to 0.007, the CN changes by ~0.5 (not
>considering +/-0.3). I would appreciate if someone can explain me how
>to interpret the results from a structural point of view.