Hi JA,
You are correct.
Anatoly
-----Original Message-----
From: ifeffit-bounces at millenia.cars.aps.anl.gov
[mailto:ifeffit-bounces at millenia.cars.aps.anl.gov] On Behalf Of Juan
Antonio Maciá Agulló
Sent: Thursday, October 20, 2005 12:13 PM
To: XAFS Analysis using Ifeffit
Subject: [Ifeffit] S02
Hi people,
I fitted several supported platinum based catalysts by Artemis. I
obtained good R-factors < 0.02 but stranges values of SO2 (<0.30) and I
do not know if these low values of SO2 are related with a low
coordination number for Pt. I know that particle sizes of these
catalysts are very small and then the coordination number is smaller
than 12.
Thank you very much.
JA