[Ifeffit] NiO data
Matt Newville
newville at cars.uchicago.edu
Mon Nov 14 09:43:57 CST 2005
Hi Scott,
I have some NiO data that is fairly old (~1992) and not very well
documented. There are spectra at 80K, 180K, and room temperature. I
believe the data was taken at X11-A, but I have no notes on sample
prep (the files indicate powder on tape). The data looks pretty good
until the Cu edge, but I'd be reluctant to put it in a database
without better notes.
The data is at http://cars9.uchicago.edu/iffwiki/XafsData
--Matt
More information about the Ifeffit
mailing list