[Ifeffit] DW Factor follow up
Ian James Drake
idrake at uclink.berkeley.edu
Mon Feb 7 16:10:06 CST 2005
> Hi,
>
> Thank you for all this valuable information.
>
> Can I make a general statement in comparing the DW of metal and its crystalline oxide at a given
>temperature? For example, I find the DW for Al metal to be 0.015A in the first scattering path
>(Al-Al) at 25C (using correlated Debye model). However, the fitted value of the DW for Al oxide
>in the first path (Al-O) was 0.001 A. In both fits, the CN was set to a constant since it is
>known from other techniques. Can a general statement be made comparing relative magnitudes of
>metal-metal DW and metal-oxygen DW-factors?
>
> Is there a good general resource for the Debye temperatures of metal oxides, like zeolite or
>Al2O3?
>
> Thank you again for all your guidance.
>
> Ian Drake
More information about the Ifeffit
mailing list