[Ifeffit] Pd data
Kelly, Shelly D.
SKelly at anl.gov
Mon Dec 19 11:12:33 CST 2005
Hi Dave,
Thanks a bunch for the data file. Could I trouble you for a key for the
columns within the file?
Shelly
Shelly Kelly Bldg 203 RM E113
Skelly at anl.gov Argonne National Laboratory
630-252-7376 9700 S Cass Ave
www.mesg.anl.gov Argonne, IL 60439
> -----Original Message-----
> From: ifeffit-bounces at millenia.cars.aps.anl.gov [mailto:ifeffit-
> bounces at millenia.cars.aps.anl.gov] On Behalf Of Barton, David (DG)
> Sent: Monday, December 19, 2005 10:11 AM
> To: 'XAFS Analysis using Ifeffit'
> Subject: RE: [Ifeffit] Pd data
>
> Shelly,
>
> Attached is a Pd foil data set. It was only collected out to k=16A-1,
> otherwise the data looks great. Data was collected with Si111 mono at
> DND-CAT (APS-ANL).
>
> Dave
>
> -----Original Message-----
> From: ifeffit-bounces at millenia.cars.aps.anl.gov [mailto:ifeffit-
> bounces at millenia.cars.aps.anl.gov] On Behalf Of Kelly, Shelly D.
> Sent: Monday, December 19, 2005 10:38 AM
> To: XAFS Analysis using Ifeffit
> Subject: [Ifeffit] Pd data
>
>
> Hello friends,
>
> Does anyone have Pd foil data or know of an EXAFS study that models
the
> data beyond the first shell? I have some data but it doesn't seem to
> correspond to the crystallographic structure of Pd. I'm suspicious
that
> something about the foil sample caused the structure to become
non-ideal.
>
> Thanks
> Shelly
>
>
>
>
More information about the Ifeffit
mailing list