>Shelly wrote:
>
>I was hoping that you could help me put together a list of EXAFS papers
>that fit the R-space data out to at least 5 Angstroms.
Hi Shelly,
You can add to Scott's list the following entry:
Mutiple-scattering EXAFS and EXELFS of titanium alloys
T. Sikora, G. Hug, M. Jaouen, and J.J. Rehr, PRB 32, n°3, 1723 (2000)
Best regards,
M. Jaouen
--