[Ifeffit] Re: Artemis Fit Questions
Scott Calvin
scalvin at slc.edu
Tue Aug 17 12:17:16 CDT 2004
Dan Carter wrote:
>Ok, I'll put it on the mailing list from now on, but I used a different
model
>from the ICSD and it worked muc better. I used the hexagonal model and
this is
>the results:
>
>Reduced Chi-square = 382.556284248
>R-factor = 0.015036203
>Do you use these to determine if the fit "doesn't work"?
>
>About separation of the three paths they are here:
>
># degen reff amp fs scattering path
> 0001 6 2.414 100.00 : [+] S_1 [+]
> 0002 6 3.150 59.25 : [+] Mo_1 [+]
> 0003 6 3.968 21.22 : [+] S_3 [+]
>
>What is fitting a third cumulant?
>The two e0's really seems to improve the reduced chi-square.
>The two ss's increased the reduced chi-square.
>
> Thanks, Dan
>
More information about the Ifeffit
mailing list