Hi Paul,
Kel-f is good to a little over 200 C. I have mm thicknesses of it.
http://www.boedeker.com/pctfe_p.htm
Jeff
Jeff Terry
Biological, Chemical, and Physical Sciences
Illinois Institute of Technology
Chicago IL 60616
phone 630-252-9708
fax 630-252-0358
http://mrmac.mr.aps.anl.gov/~jterry/
On Apr 26, 2004, at 8:12 PM, Paul Fons wrote:
>
> OK, I admit this isn't an athena question (but it is about how to take
> the raw data for it!). I want to do biaxial strain measurements. The
> idea is to deposit a thin film of the material to be investigated on a
> substrate and then deform the plate with a form of cylindrical
> symmetry. One can then solve for the stress of a plate using
> elasticity theory. The twist is that I need a plate that is stiff and
> (surprise) x-ray transparent ... and heat resistant to about 250 C.
> Kapton would be a wonderful choice, but is only made in thicknesses up
> to 175 microns (hardly stiff enough). There must be someone out there
> in the collective iffeffit world who knows of an appropriate material.
> Doing some web surfing, I came across another product by DuPont
> called Vespar that *may* be available in thicker forms. The specs I
> am looking for are: a thin (semiconducting) film has to stick to the
> surface, heat resistant to <=250 C, thick enough to be elastically
> stiff, and x-ray transparent. Any suggestions? Thanks for any help
> that may come my way in advance!
>
>
>
>
>
>
>
>
>
> Dr. Paul Fons
> Senior Researcher
> National Institute for Advanced Industrial Science & Technology
> METI
> Center for Applied Near-Field Optics Research (CANFOR)
> AIST Central 4, Higashi 1-1-1
> Tsukuba, Ibaraki JAPAN 305-8568
>
> tel. +81-298-61-5636
> fax. +81-298-61-2939
>
> email: paul-fons at aist.go.jp
>
> The lines below are in a Japanese font
>
> 〒305−8568
> 茨城県つくば市東1−1−1
> つくば中央第4
> 近接場光応用工学センター
> ポール・フォンス主任研究官_______________________________________________
> Ifeffit mailing list
> Ifeffit at millenia.cars.aps.anl.gov
> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
-------------- next part --------------
A non-text attachment was scrubbed...
Name: not available
Type: text/enriched
Size: 2269 bytes
Desc: not available
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20040426/5a9509d7/attachment.bin>
More information about the Ifeffit
mailing list