[Ifeffit] Self-Absorption Corrections
Francois Farges
farges at univ-mlv.fr
Wed Jul 30 03:28:12 CDT 2003
>On Tuesday 29 July 2003 04:07 am, Francois Farges wrote:
>> both spectra are normalized. Is there not any remaining
>> self-absorption in the fluo spectrum for Nb2O5, despite data
>> collected at 90° ?? (while TiO2 sounds fine, as Troeger predicted ?).
>>
>
>It's hard to know how to interpret your data unless you tell us how
>thick the samples are.
3 mu filters as made by the exafs company so it don't know their
thickness exactly. the angles were the same so that's not the
problem. I ve much more data that shows exactly the same. FF
--
Francois FARGES
Laboratoire des Géomatériaux
Université de Marne la Vallée
5 Bd Descartes-Champs S/Marne
77454 Marne la Vallée cedex 2
TEL: 01 49 32 90 57
from outside France: +33 1 49 32 90 57
FAX: 01 49 32 91 37
from outside France: +33 1 49 32 91 37