Hi everyone, Does anyone have any experience modeling Mo2C in Artemis? I can't find any existing INP files for Mo2C. I was wondering if anyone had any experience with Mo2C or knowledge or where I can find some relevant information. Thanks! Marc
14 Aug
14 Aug
3:01 p.m.
Hi Marc, The Crystallography open database has a CIF file for Mo2C, which can then be read into Artemis: http://www.crystallography.net --Scott Calvin Sarah Lawrence College On Aug 14, 2012, at 10:30 AM, Marc Porosoff wrote:
Hi everyone,
Does anyone have any experience modeling Mo2C in Artemis? I can't find any existing INP files for Mo2C. I was wondering if anyone had any experience with Mo2C or knowledge or where I can find some relevant information.
Thanks! Marc