Ref. XAS Data for Fe K-edge (Fe3C Iron Carbide)
5 Dec
2023
5 Dec
'23
10:29 a.m.
Dear All, Does anyone by chance have the Fe K-edge XAS data for Iron Carbide (Fe3C)? Best regards, Esmael
5 Dec
5 Dec
11:58 a.m.
I found it online: https://xaslib.xrayabsorption.org/spectrum/105/ Thanks @Matt Best, Esmael On 12/5/2023 11:29 AM, Esmael Balaghi wrote:
Dear All,
Does anyone by chance have the Fe K-edge XAS data for Iron Carbide (Fe3C)?
Best regards,
Esmael
_______________________________________________ Ifeffit mailing list Ifeffit@millenia.cars.aps.anl.gov http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit Unsubscribe:http://millenia.cars.aps.anl.gov/mailman/options/ifeffit