Hi I am analyzing my data in ARTEMIS (ver 0.9.26). I used the Rietveld refined parameters of XRD data into ATOMS interface and used that for path calculation. But the paths were not at same distances as indicated by .CIF file (in Vesta). I am having FEFF9 with me. So, I want to run EXAFS in FEFF9 and import the paths in ARTEMIS for fitting. Is it possible? Manju Junior Research Fellow Department of Basic and Applied Sciences Punjabi University, Patiala- 147 002 Punjab, India.