# XDI/1.0 Demeter/0.9.18 # Athena.element: Pt # Athena.edge: l3 # Athena.e0: 11564.5 # Athena.eshift: 0 # Athena.rbkg: 1.0 # Athena.standard: None # Athena.bkg_kweight: 2 # Athena.edge_step: 0.2951816 # Athena.fixed_step: no # Athena.flatten: yes # Athena.pre_edge_range: -150.000 -30.000 # Athena.pre_edge_line: 2.948236 - 0.000220084 * E # Athena.normalization_range: 150.000 1679.900 # Athena.post_edge_polynomial: 6.725490 - 0.000743354 * E + 1.92114e-08 * E^2 + 0 * E^3 # Athena.spline_range_energy: 0.000 1666.788 # Athena.clamps: 0/24 # Athena.spline_range_k: 0.000 20.916 # Athena.kweight: 2 # Athena.window: hanning # Athena.phase_correction: 0 # Athena.k_range: 3.000 19.614 # Athena.dk: 1 # Athena.r_range: 1 3 # Athena.dr: 0.0 # Athena.window: hanning # Athena.plot_multiplier: 1 # Athena.y_offset: 0 # /// # NPTS NS CUEDGE CUHITE DSPACE STPDEG STEPMM START STOP SCALE # 974 4 84294. 200000. 1.92017 4000. 3150. 66000. 55000. 10.000 # DELTA: 20. 6. 13. 4. 10. # DELEND: 65137. 64561. 56530. 56097. 55000. # SEC: 2.000 2.000 2.000 2.000 2.000 # OFFSET: 1868. 1950. 927. 1537. 4. 6. 137. 4. 6. 18. 641. 3. 2. 5. 61. 20. 93. 232. 0. 0. 0. 0. 0. 0. # PTO2 AT RT 7 9 6-13-83 #------------------------ # e xmu bkg pre_edge post_edge der sec i0 11367.400 0.45119140 0.45119140 0.44644965 0.75793470 -0.39628800E-03 0.21106019E-04 98177.500 11370.800 0.44984402 0.44984402 0.44570137 0.75689252 -0.32452753E-03 0.24751171E-04 97888.500 11374.100 0.44901706 0.44901706 0.44497509 0.75588142 -0.23045515E-03 0.12299131E-04 97547.500 11377.500 0.44829997 0.44829997 0.44422680 0.75484012 -0.24212336E-03 -0.12497928E-04 97207.500 11380.800 0.44739484 0.44739484 0.44350052 0.75382987 -0.31419127E-03 -0.11745171E-04 96929.500 11384.200 0.44619489 0.44619489 0.44275224 0.75278945 -0.32081600E-03 0.47661230E-05 96575.000 11387.500 0.44524537 0.44524537 0.44202596 0.75178005 -0.28225824E-03 0.10044517E-04 96333.500 11390.900 0.44430376 0.44430376 0.44127767 0.75074050 -0.25351774E-03 0.18482634E-05 96017.500 11394.300 0.44352145 0.44352145 0.44052938 0.74970139 -0.26969005E-03 -0.89616142E-06 95697.000 11397.600 0.44249683 0.44249683 0.43980311 0.74869327 -0.25952202E-03 0.16601138E-06 95351.500 11401.000 0.44178265 0.44178265 0.43905482 0.74765504 -0.26857778E-03 -0.17952170E-04 94914.000 11404.400 0.44067050 0.44067050 0.43830653 0.74661726 -0.38159677E-03 -0.11724451E-04 94570.000 11407.700 0.43922595 0.43922595 0.43758025 0.74561042 -0.34713160E-03 0.19508711E-04 94343.500 11411.100 0.43834472 0.43834472 0.43683197 0.74457351 -0.25088841E-03 0.12221753E-04 94279.000 11414.500 0.43751991 0.43751991 0.43608368 0.74353704 -0.26402368E-03 -0.55964786E-05 94058.000 11417.900 0.43654936 0.43654936 0.43533539 0.74250102 -0.28894447E-03 -0.62386322E-05 93721.500 11421.300 0.43555509 0.43555509 0.43458711 0.74146544 -0.30644638E-03 0.57273953E-05 93253.500 11424.600 0.43449617 0.43449617 0.43386083 0.74046075 -0.25057092E-03 0.26995368E-04 92917.000 11428.000 0.43387626 0.43387626 0.43311254 0.73942604 -0.12557741E-03 0.71262888E-05 92487.500 11431.400 0.43364224 0.43364224 0.43236425 0.73839178 -0.20211215E-03 -0.30931707E-04 92219.000 11434.800 0.43250190 0.43250190 0.43161597 0.73735797 -0.33591302E-03 -0.18139697E-04 91949.000 11438.200 0.43135803 0.43135803 0.43086768 0.73632460 -0.32546209E-03 0.10362710E-04 91780.000 11441.600 0.43028876 0.43028876 0.43011939 0.73529167 -0.26544660E-03 0.63489092E-05 91430.500 11445.000 0.42955300 0.42955300 0.42937111 0.73425919 -0.28228951E-03 -0.31917345E-05 91132.000 11448.400 0.42836919 0.42836919 0.42862282 0.73322715 -0.28715039E-03 0.52644626E-05 90828.500 11451.800 0.42760038 0.42760038 0.42787453 0.73219556 -0.24649116E-03 0.54195411E-05 90567.000 11455.200 0.42669305 0.42669305 0.42712625 0.73116441 -0.25029751E-03 0.10344794E-05 90170.000 11458.600 0.42589835 0.42589835 0.42637796 0.73013370 -0.23945670E-03 -0.25081559E-06 89907.000 11462.000 0.42506474 0.42506474 0.42562967 0.72910344 -0.25200306E-03 -0.31190752E-05 89531.500 11465.400 0.42418473 0.42418473 0.42488139 0.72807362 -0.26066641E-03 -0.16523756E-05 89089.000 11468.800 0.42329221 0.42329221 0.42413310 0.72704425 -0.26323921E-03 0.14056045E-05 88838.500 11472.200 0.42239470 0.42239470 0.42338481 0.72601532 -0.25110830E-03 0.45221434E-05 88502.500 11475.600 0.42158468 0.42158468 0.42263653 0.72498684 -0.23248864E-03 0.37541565E-05 88222.000 11479.100 0.42079053 0.42079053 0.42186623 0.72392857 -0.22520462E-03 0.48608188E-05 87792.500 11482.500 0.42003076 0.42003076 0.42111795 0.72290098 -0.19894899E-03 0.20795329E-06 87496.000 11485.900 0.41943768 0.41943768 0.42036966 0.72187384 -0.22379054E-03 -0.11893254E-04 87165.000 11489.300 0.41850899 0.41850899 0.41962137 0.72084715 -0.27982312E-03 -0.36886846E-05 86826.500 11492.700 0.41753488 0.41753488 0.41887309 0.71982090 -0.24887359E-03 0.76485723E-05 86557.500 11496.200 0.41679176 0.41679176 0.41810279 0.71876493 -0.22704797E-03 0.21258279E-05 86098.000 11499.600 0.41596825 0.41596825 0.41735450 0.71773958 -0.23420538E-03 0.44096436E-05 85847.500 11503.000 0.41519916 0.41519916 0.41660622 0.71671467 -0.19706239E-03 0.12921151E-04 85497.500 11506.500 0.41460852 0.41460852 0.41583592 0.71566009 -0.14504944E-03 0.60843725E-05 85198.000 11509.900 0.41419832 0.41419832 0.41508764 0.71463608 -0.15508022E-03 -0.71532406E-05 84782.500 11513.300 0.41355398 0.41355398 0.41433935 0.71361252 -0.19369148E-03 0.18384000E-05 84493.500 11516.800 0.41286185 0.41286185 0.41356905 0.71255932 -0.14239526E-03 0.23629277E-04 84022.500 11517.800 0.41291320 0.41291320 0.41334897 0.71225849 -0.87359731E-04 -0.62257058E-04 83816.000 11518.800 0.41268713 0.41268713 0.41312888 0.71195770 -0.26690938E-03 -0.61716026E-04 83859.000 11519.900 0.41235269 0.41235269 0.41288679 0.71162688 -0.21696339E-03 0.69983446E-04 83837.000 11520.900 0.41223151 0.41223151 0.41266671 0.71132617 -0.11994414E-03 0.38407259E-04 83405.500 11521.900 0.41211280 0.41211280 0.41244662 0.71102550 -0.14014887E-03 0.24702974E-04 83531.500 11523.000 0.41193720 0.41193720 0.41220453 0.71069481 -0.68067894E-04 0.38857529E-04 83736.500 11524.000 0.41196986 0.41196986 0.41198445 0.71039422 -0.58548058E-04 0.40961962E-04 83703.000 11525.000 0.41182010 0.41182010 0.41176436 0.71009367 0.13856031E-04 0.53091749E-04 83538.000 11526.100 0.41199895 0.41199895 0.41152227 0.70976310 0.52944614E-04 -0.16922531E-04 83485.000 11527.100 0.41193128 0.41193128 0.41130218 0.70946263 -0.21681285E-04 -0.18114934E-04 83231.000 11528.200 0.41195342 0.41195342 0.41106009 0.70913216 0.14903252E-04 0.52513373E-04 83218.500 11529.200 0.41196258 0.41196258 0.41084001 0.70883177 0.88596798E-04 0.35310070E-04 83063.000 11530.200 0.41213062 0.41213062 0.41061992 0.70853142 0.85523393E-04 -0.17991449E-04 82895.000 11531.300 0.41214218 0.41214218 0.41037783 0.70820108 0.50814755E-04 0.10456781E-04 82789.500 11532.300 0.41223733 0.41223733 0.41015775 0.70790081 0.10748263E-03 -0.75258625E-04 82815.500 11533.300 0.41235714 0.41235714 0.40993766 0.70760057 -0.99702494E-04 -0.11069456E-03 82691.000 11534.400 0.41202795 0.41202795 0.40969557 0.70727036 -0.12497595E-03 0.83690348E-04 83499.500 11535.400 0.41209470 0.41209470 0.40947549 0.70697021 0.76047237E-04 0.19604939E-03 83380.500 11536.400 0.41218005 0.41218005 0.40925540 0.70667010 0.26712282E-03 0.80510649E-04 83146.000 11537.500 0.41265565 0.41265565 0.40901331 0.70634002 0.24511960E-03 0.32168749E-04 83178.000 11538.500 0.41269480 0.41269480 0.40879322 0.70603998 0.33467719E-03 0.90540638E-04 83111.000 11539.500 0.41332501 0.41332501 0.40857314 0.70573999 0.42620088E-03 0.67787696E-04 82921.500 11540.600 0.41358982 0.41358982 0.40833105 0.70541004 0.47703136E-03 0.62614535E-04 83010.000 11541.600 0.41432677 0.41432677 0.40811096 0.70511013 0.55769140E-03 0.62611437E-04 82765.500 11542.700 0.41476097 0.41476097 0.40786887 0.70478027 0.60851537E-03 0.23700082E-03 82888.500 11543.700 0.41560466 0.41560466 0.40764879 0.70448043 0.10553931E-02 0.17716539E-03 82714.500 11544.700 0.41687176 0.41687176 0.40742870 0.70418064 0.96284614E-03 0.37129821E-04 82588.000 11545.800 0.41762663 0.41762663 0.40718661 0.70385091 0.11333657E-02 0.24494993E-03 82620.000 11546.800 0.41925183 0.41925183 0.40696652 0.70355120 0.14772410E-02 0.27629708E-03 82343.000 11547.800 0.42058111 0.42058111 0.40674644 0.70325152 0.16859599E-02 0.27480414E-03 82500.500 11548.900 0.42279234 0.42279234 0.40650435 0.70292192 0.20543297E-02 0.38970916E-03 82239.000 11549.900 0.42489521 0.42489521 0.40628426 0.70262233 0.25043491E-02 0.49300174E-03 82263.000 11551.000 0.42805148 0.42805148 0.40604217 0.70229282 0.30896334E-02 0.70349134E-03 81994.500 11552.000 0.43138344 0.43138344 0.40582209 0.70199330 0.39816810E-02 0.78719048E-03 81812.500 11553.000 0.43601484 0.43601484 0.40560200 0.70169383 0.46640143E-02 0.95803633E-03 81717.500 11554.100 0.44117787 0.44117787 0.40535991 0.70136445 0.59935573E-02 0.16062207E-02 82311.500 11555.100 0.44860131 0.44860131 0.40513982 0.70106505 0.80370777E-02 0.19507629E-02 82088.500 11556.200 0.45805573 0.45805573 0.40489773 0.70073576 0.10090159E-01 0.31336998E-02 81901.500 11557.200 0.46979064 0.46979064 0.40467765 0.70043645 0.14617847E-01 0.43386269E-02 81780.500 11558.200 0.48729142 0.48729142 0.40445756 0.70013718 0.18767413E-01 0.57277663E-02 81677.000 11559.300 0.50920221 0.50920221 0.40421547 0.69980802 0.26646156E-01 0.90712237E-02 82270.000 11560.300 0.54324835 0.54324835 0.40399539 0.69950882 0.37816983E-01 0.14619217E-01 82041.000 11561.400 0.58861788 0.58861788 0.40375329 0.69917975 0.57346511E-01 0.21715144E-01 82372.000 11562.400 0.66367603 0.66367603 0.40353321 0.69888064 0.83418785E-01 0.25379916E-01 82194.000 11563.400 0.75545545 0.75545545 0.40331312 0.69858156 0.10810634 0.16343234E-01 82153.000 11564.500 0.89069935 0.83518390 0.40307103 0.69825262 0.11773958 -0.16223828E-01 81958.500 11565.500 1.0027086 0.93229948 0.40285095 0.69795363 0.74036304E-01 -0.58567861E-01 82070.000 11566.600 1.0461756 0.86572236 0.40260885 0.69762478 -0.52529323E-02 -0.74141333E-01 81787.500 11567.600 0.99167740 0.81396268 0.40238877 0.69732586 -0.81660496E-01 -0.44467422E-01 81866.500 11568.600 0.88285459 0.76994769 0.40216869 0.69702699 -0.94187776E-01 -0.44799593E-03 81702.500 11569.700 0.79388307 0.72977994 0.40192659 0.69669827 -0.82601287E-01 0.15349262E-01 81511.500 11570.700 0.70939189 0.70012960 0.40170651 0.69639947 -0.61954326E-01 0.23030398E-01 81708.000 11571.800 0.66377898 0.67434776 0.40146442 0.69607084 -0.34237450E-01 0.19518959E-01 81429.500 11572.800 0.63749325 0.65648899 0.40124433 0.69577213 -0.20964512E-01 0.10193849E-01 81640.000 11573.900 0.61975351 0.64226268 0.40100224 0.69544358 -0.12830368E-01 0.75450990E-02 81307.500 11574.900 0.61054947 0.63362238 0.40078215 0.69514495 -0.51198046E-02 0.60217588E-02 81945.500 11575.900 0.60951390 0.62846746 0.40056207 0.69484635 -0.78685059E-03 0.54330488E-03 81238.000 11577.000 0.60889709 0.62612629 0.40031998 0.69451794 -0.39788643E-02 0.10246451E-02 81403.000 11578.000 0.60115828 0.62639149 0.40009989 0.69421943 0.13649041E-02 0.54187207E-02 83074.000 11579.100 0.61176339 0.62859725 0.39985780 0.69389111 0.74004491E-02 0.83158144E-03 81326.000 11580.100 0.61669923 0.63170947 0.39963772 0.69359267 0.31112251E-02 -0.29090849E-02 80651.000 11581.200 0.61829696 0.63563177 0.39939562 0.69326444 0.12913709E-02 -0.10489298E-02 80824.500 11582.200 0.61941111 0.63912363 0.39917554 0.69296609 0.90847259E-03 0.25419765E-03 80452.000 11583.300 0.62020475 0.64276674 0.39893345 0.69263794 0.18251859E-02 0.15714830E-02 80316.000 11584.300 0.62324400 0.64590276 0.39871336 0.69233967 0.42085868E-02 0.18992308E-02 80346.000 11585.300 0.62862192 0.64887506 0.39849328 0.69204143 0.56236475E-02 0.14181661E-02 80100.500 11586.400 0.63505366 0.65195994 0.39825118 0.69171342 0.71867356E-02 0.81362639E-03 80155.000 11587.400 0.64371407 0.65460051 0.39803110 0.69141527 0.73322630E-02 -0.74718448E-03 79889.000 11588.500 0.65045141 0.65732947 0.39778901 0.69108734 0.56176482E-02 -0.17793620E-02 79926.000 11589.500 0.65551113 0.65965466 0.39756892 0.69078927 0.35956029E-02 -0.19427811E-02 79599.500 11590.600 0.65800217 0.66204568 0.39732683 0.69046143 0.15378078E-02 -0.14809007E-02 79449.500 11591.600 0.65874053 0.66407182 0.39710675 0.69016344 0.48571129E-03 -0.85064871E-03 79013.500 11592.700 0.65902217 0.66614287 0.39686465 0.68983569 -0.24855451E-03 -0.45092778E-03 78841.500 11593.700 0.65821856 0.66788629 0.39664457 0.68953778 -0.46123704E-03 0.79695424E-04 78487.500 11594.800 0.65805357 0.66965534 0.39640248 0.68921012 -0.81194124E-04 0.43151358E-03 78266.000 11595.800 0.65804805 0.67113239 0.39618239 0.68891229 0.44494148E-03 0.59907039E-03 78183.500 11596.900 0.65898795 0.67261740 0.39594030 0.68858472 0.11768537E-02 0.76195948E-03 78200.000 11597.900 0.66051945 0.67384441 0.39572021 0.68828697 0.20450564E-02 0.80930613E-03 78617.000 11599.000 0.66328257 0.67506337 0.39547812 0.68795949 0.28763966E-02 0.92617618E-03 78753.000 11600.000 0.66655988 0.67605668 0.39525804 0.68766182 0.39900264E-02 0.67906042E-03 79068.000 11601.000 0.67126262 0.67694444 0.39503795 0.68736419 0.42345174E-02 0.15928453E-03 79269.500 11602.100 0.67545237 0.67780350 0.39479586 0.68703684 0.43245239E-02 0.43729864E-04 79564.000 11603.100 0.68034412 0.67848168 0.39457578 0.68673929 0.43263501E-02 0.75275065E-05 79501.000 11604.200 0.68453770 0.67911918 0.39433368 0.68641203 0.43403316E-02 0.28488013E-03 79672.500 11605.200 0.68945881 0.67960411 0.39411360 0.68611456 0.49245984E-02 0.69565448E-03 79265.500 11606.300 0.69487936 0.68003802 0.39387151 0.68578739 0.58012061E-02 0.69235799E-03 79217.500 11607.300 0.70164135 0.68034604 0.39365142 0.68549000 0.63785502E-02 0.18286622E-04 78988.500 11608.400 0.70827431 0.68059434 0.39340933 0.68516291 0.58396080E-02 -0.54877173E-03 78803.500 11609.400 0.71390452 0.68074179 0.39318924 0.68486560 0.52261295E-02 -0.68041191E-03 78838.000 11610.500 0.71924919 0.68082245 0.39294715 0.68453861 0.44107430E-02 -0.11647415E-02 78504.000 11611.500 0.72316708 0.68082566 0.39272707 0.68424138 0.27801723E-02 -0.17731709E-02 78586.500 11612.600 0.72508755 0.68075665 0.39248498 0.68391448 0.68708397E-03 -0.20653873E-02 78385.500 11613.600 0.72460996 0.68063197 0.39226489 0.68361733 -0.15571410E-02 -0.22530653E-02 78378.000 11614.700 0.72181755 0.68043125 0.39202280 0.68329051 -0.40443533E-02 -0.10885594E-02 78161.500 11617.000 0.71085916 0.67981762 0.39151660 0.68260732 -0.52582428E-02 -0.39880109E-03 78041.500 11619.200 0.69815546 0.67901936 0.39103242 0.68195401 -0.58389582E-02 -0.13289703E-04 77786.000 11621.500 0.68458385 0.67800736 0.39052622 0.68127122 -0.53180465E-02 0.32000963E-03 77720.000 11623.800 0.67369244 0.67685838 0.39002003 0.68058862 -0.43669139E-02 0.40892107E-03 77342.000 11626.100 0.66449604 0.67561750 0.38951384 0.67990623 -0.34370095E-02 0.46252894E-03 77081.000 11628.400 0.65788220 0.67432978 0.38900764 0.67922404 -0.22392807E-02 0.51180854E-03 76778.500 11630.700 0.65419535 0.67304031 0.38850145 0.67854206 -0.10826902E-02 0.39780113E-03 76394.000 11632.900 0.65301010 0.67184366 0.38801726 0.67788992 -0.44917563E-03 0.18173804E-03 76059.500 11635.200 0.65217406 0.67064318 0.38751107 0.67720833 -0.26486905E-03 0.89127864E-04 75588.000 11637.500 0.65179170 0.66949281 0.38700488 0.67652695 -0.39187459E-04 0.18734820E-03 75265.500 11639.800 0.65199380 0.66839087 0.38649868 0.67584577 0.59693269E-03 0.17913059E-03 74595.500 11642.100 0.65453759 0.66733570 0.38599249 0.67516479 0.78481325E-03 -0.51491510E-04 75420.500 11644.400 0.65560394 0.66632559 0.38548629 0.67448401 0.36007174E-03 -0.13565701E-03 75382.500 11646.700 0.65619392 0.66535888 0.38498010 0.67380344 0.16079099E-03 -0.11328612E-03 75161.000 11648.900 0.65632750 0.66447326 0.38449591 0.67315265 -0.14971579E-03 -0.10173989E-03 74945.500 11651.200 0.65552020 0.66358660 0.38398972 0.67247248 -0.29703852E-03 -0.14392767E-04 74703.000 11653.500 0.65496112 0.66273836 0.38348353 0.67179251 -0.21592252E-03 0.15873765E-04 74385.000 11655.800 0.65452695 0.66192688 0.38297733 0.67111274 -0.22401920E-03 0.44115510E-04 74193.000 11658.100 0.65393063 0.66115046 0.38247114 0.67043318 -0.12991174E-04 0.19259033E-03 73830.500 11660.400 0.65446719 0.66040743 0.38196494 0.66975382 0.66189632E-03 0.86793336E-04 72998.500 11662.700 0.65697536 0.65969611 0.38145875 0.66907467 0.38625817E-03 -0.10030744E-03 73543.500 11665.000 0.65624398 0.65901481 0.38095256 0.66839571 0.20048211E-03 0.10205560E-04 73655.500 11667.300 0.65789758 0.65836187 0.38044636 0.66771696 0.43320375E-03 0.13174730E-03 73454.000 11669.600 0.65823672 0.65773559 0.37994017 0.66703841 0.80651969E-03 0.13413522E-03 73659.500 11671.900 0.66160757 0.65713431 0.37943397 0.66636007 0.10502258E-02 0.39613992E-04 72885.000 11674.200 0.66306776 0.65655633 0.37892778 0.66568193 0.98874405E-03 0.26552315E-04 73008.000 11676.500 0.66615579 0.65599999 0.37842159 0.66500399 0.11723664E-02 -0.65190759E-04 72532.000 11678.800 0.66846064 0.65546359 0.37791539 0.66432626 0.68886656E-03 -0.23040206E-03 72274.000 11681.100 0.66932458 0.65494546 0.37740920 0.66364873 0.11251694E-03 -0.20882052E-03 72024.000 11683.400 0.66897822 0.65444392 0.37690300 0.66297140 -0.27170782E-03 -0.14189159E-03 71817.500 11685.700 0.66807472 0.65395729 0.37639681 0.66229428 -0.54018437E-03 -0.10967015E-03 71581.000 11688.000 0.66649337 0.65348389 0.37589062 0.66161736 -0.77619052E-03 -0.91682426E-04 71445.500 11690.300 0.66450424 0.65302204 0.37538442 0.66094064 -0.96192353E-03 -0.57453493E-04 71184.000 11692.600 0.66206852 0.65257006 0.37487823 0.66026413 -0.10404766E-02 -0.13649678E-04 70989.500 11694.900 0.65971805 0.65212627 0.37437204 0.65958781 -0.10247120E-02 0.14953372E-04 70744.500 11697.300 0.65725238 0.65167010 0.37384383 0.65888232 -0.97019574E-03 0.29595845E-04 70578.000 11699.600 0.65515813 0.65123783 0.37333764 0.65820642 -0.88561158E-03 0.26419844E-04 70336.000 11701.900 0.65317856 0.65080862 0.37283144 0.65753073 -0.84866446E-03 0.27911747E-04 70170.000 11704.200 0.65125427 0.65038082 0.37232525 0.65685524 -0.75721754E-03 0.42477306E-04 69944.000 11706.500 0.64969536 0.64995274 0.37181906 0.65617995 -0.65326885E-03 0.31040177E-04 69656.000 11708.800 0.64824924 0.64952269 0.37131286 0.65550487 -0.61443273E-03 0.13059069E-04 69541.000 11711.100 0.64686897 0.64908900 0.37080667 0.65482999 -0.59319714E-03 0.12706469E-04 69109.000 11713.500 0.64546121 0.64863075 0.37027847 0.65412598 -0.55471232E-03 0.45070912E-06 69017.500 11715.800 0.64426183 0.64818444 0.36977227 0.65345152 -0.59107881E-03 -0.18128919E-04 68780.500 11718.100 0.64274225 0.64773040 0.36926608 0.65277726 -0.63810534E-03 0.18758230E-04 68493.500 11720.400 0.64132654 0.64726876 0.36875988 0.65210320 -0.50479095E-03 0.61094076E-04 68210.500 11722.700 0.64042021 0.64679969 0.36825369 0.65142935 -0.35707259E-03 0.51542363E-04 68014.000 11725.100 0.63964830 0.64630250 0.36772549 0.65072641 -0.26254184E-03 0.35902196E-04 67834.500 11727.400 0.63918626 0.64581878 0.36721929 0.65005297 -0.18833228E-03 0.69433867E-05 67734.000 11729.700 0.63878197 0.64532814 0.36671310 0.64937974 -0.23060226E-03 -0.77375467E-05 67583.500 11732.000 0.63812549 0.64483076 0.36620691 0.64870670 -0.22392499E-03 0.15156755E-04 67418.000 11734.400 0.63772952 0.64430475 0.36567870 0.64800463 -0.15936551E-03 0.34293728E-04 67309.000 11736.700 0.63737647 0.64379410 0.36517251 0.64733201 -0.62744467E-04 0.42039678E-04 67071.500 11739.000 0.63744090 0.64327722 0.36466632 0.64665960 0.34017008E-04 0.31383192E-04 66854.500 11741.300 0.63753295 0.64275428 0.36416012 0.64598739 0.81618214E-04 0.12675175E-04 66688.500 11743.700 0.63782450 0.64220231 0.36363192 0.64528617 0.93590330E-04 0.12907348E-04 66434.500 11746.000 0.63797283 0.64166749 0.36312573 0.64461437 0.14228275E-03 0.27485066E-04 66265.500 11748.300 0.63847901 0.64112711 0.36261953 0.64394278 0.22002164E-03 0.25556075E-04 66033.000 11750.700 0.63900693 0.64055750 0.36209133 0.64324220 0.26239630E-03 0.17105457E-04 65724.000 11753.000 0.63971227 0.64000630 0.36158514 0.64257103 0.30041728E-03 0.91095391E-05 65595.000 11755.300 0.64038885 0.63945006 0.36107894 0.64190005 0.30430018E-03 -0.16975077E-04 65397.500 11757.700 0.64114248 0.63886444 0.36055074 0.64120012 0.22063442E-03 -0.31325586E-04 65171.500 11760.000 0.64142583 0.63829841 0.36004455 0.64052957 0.15706993E-03 -0.13817783E-04 65001.000 11762.300 0.64186500 0.63772786 0.35953835 0.63985921 0.15707262E-03 -0.32465904E-04 64783.500 11764.700 0.64216407 0.63712785 0.35901015 0.63915993 0.44801801E-05 -0.56045896E-04 64552.000 11767.000 0.64188606 0.63654856 0.35850396 0.63848999 -0.10634310E-03 -0.28793511E-04 64345.000 11769.300 0.64167489 0.63596525 0.35799776 0.63782025 -0.12796997E-03 -0.42999801E-04 64131.000 11771.700 0.64128460 0.63535248 0.35746956 0.63712161 -0.30844216E-03 -0.62512643E-04 63974.000 11774.000 0.64022522 0.63476148 0.35696337 0.63645229 -0.42177939E-03 -0.43827590E-04 63791.500 11776.400 0.63930224 0.63414106 0.35643516 0.63575409 -0.51443183E-03 -0.39642742E-04 63536.500 11778.700 0.63780739 0.63354308 0.35592897 0.63508518 -0.60810028E-03 -0.19096032E-04 63329.000 11781.100 0.63644416 0.63291573 0.35540077 0.63438741 -0.60418318E-03 -0.35492816E-05 63109.500 11783.400 0.63496772 0.63231146 0.35489457 0.63371892 -0.62478190E-03 -0.11876628E-04 62964.500 11785.800 0.63350769 0.63167792 0.35436637 0.63302158 -0.66000334E-03 0.53001391E-05 62704.000 11788.100 0.63186571 0.63106808 0.35386018 0.63235351 -0.59987125E-03 0.40828451E-04 62524.000 11790.400 0.63074828 0.63045576 0.35335398 0.63168564 -0.47219246E-03 0.33832702E-04 62402.500 11792.800 0.62964640 0.62981436 0.35282578 0.63098894 -0.44085755E-03 0.58020307E-05 62246.500 11795.100 0.62867625 0.62919751 0.35231959 0.63032149 -0.44492292E-03 0.40129577E-05 61955.500 11797.500 0.62755527 0.62855175 0.35179138 0.62962523 -0.42199665E-03 0.14869038E-04 61791.500 11799.900 0.62665067 0.62790404 0.35126318 0.62892919 -0.37355154E-03 0.12691619E-04 61737.500 11802.200 0.62579957 0.62728167 0.35075699 0.62826236 -0.36234604E-03 0.13719400E-04 61455.000 11804.600 0.62494764 0.62663070 0.35022878 0.62756676 -0.30907036E-03 0.12604644E-04 61192.500 11806.900 0.62434694 0.62600556 0.34972259 0.62690034 -0.30310421E-03 -0.26797708E-05 61054.000 11809.300 0.62352305 0.62535207 0.34919439 0.62620517 -0.32166528E-03 0.20565198E-04 60875.000 11811.600 0.62283512 0.62472486 0.34868819 0.62553917 -0.20644778E-03 0.45103472E-04 60684.000 11814.000 0.62255275 0.62406958 0.34815999 0.62484444 -0.10967896E-03 0.92458500E-05 60521.500 11816.300 0.62231963 0.62344101 0.34765380 0.62417885 -0.16299228E-03 -0.19228071E-04 60322.000 11818.700 0.62178668 0.62278467 0.34712560 0.62348455 -0.20005089E-03 0.18714448E-05 60132.500 11821.100 0.62135938 0.62212807 0.34659739 0.62279047 -0.15400935E-03 0.12886719E-04 60003.500 11823.400 0.62106284 0.62149877 0.34609120 0.62212551 -0.13948332E-03 -0.35797798E-05 59741.000 11825.800 0.62070381 0.62084223 0.34556300 0.62143186 -0.17083431E-03 -0.15960160E-04 59600.500 11828.200 0.62024283 0.62018599 0.34503479 0.62073843 -0.21609209E-03 -0.27405778E-04 59309.000 11830.500 0.61968818 0.61955756 0.34452860 0.62007411 -0.29964147E-03 -0.20615016E-04 59212.000 11832.900 0.61883452 0.61890247 0.34400040 0.61938111 -0.31298266E-03 -0.14024324E-04 59038.000 11835.300 0.61818586 0.61824810 0.34347220 0.61868834 -0.36695823E-03 -0.36253330E-04 58835.500 11837.600 0.61710981 0.61762167 0.34296600 0.61802464 -0.48337331E-03 -0.19713383E-04 58629.500 11840.000 0.61591401 0.61696867 0.34243780 0.61733230 -0.45961113E-03 -0.47549695E-05 58446.500 11842.400 0.61490368 0.61631634 0.34190960 0.61664018 -0.50619717E-03 -0.13674524E-04 58227.500 11844.700 0.61353488 0.61569179 0.34140340 0.61597710 -0.52388139E-03 0.19213296E-04 58043.500 11847.100 0.61244144 0.61504070 0.34087520 0.61528542 -0.41589468E-03 0.28131299E-04 57850.000 11849.500 0.61153858 0.61439020 0.34034700 0.61459396 -0.38885115E-03 0.19562322E-04 57666.000 11851.900 0.61057495 0.61374029 0.33981880 0.61390271 -0.32199553E-03 0.18312795E-04 57563.500 11854.200 0.61002521 0.61311797 0.33931260 0.61324048 -0.30278102E-03 0.23273248E-04 57288.000 11856.600 0.60915188 0.61246912 0.33878440 0.61254967 -0.21261127E-03 0.55123968E-04 57158.000 11859.000 0.60900467 0.61182079 0.33825620 0.61185908 -0.38185973E-04 0.29132556E-04 56974.000 11861.400 0.60896859 0.61117294 0.33772800 0.61116871 -0.72774999E-04 -0.10781448E-04 56726.500 11863.700 0.60866263 0.61055253 0.33722180 0.61050732 -0.88858779E-04 0.42109577E-05 56552.000 11866.100 0.60855095 0.60990558 0.33669360 0.60981739 -0.52983497E-04 0.34100312E-05 56434.500 11868.500 0.60840831 0.60925905 0.33616540 0.60912768 -0.72490629E-04 -0.64484692E-05 56228.000 11870.900 0.60820300 0.60861293 0.33563719 0.60843819 -0.83936149E-04 -0.11253344E-04 56035.500 11873.300 0.60800542 0.60796719 0.33510899 0.60774892 -0.12650668E-03 -0.98673861E-05 55973.000 11875.700 0.60759577 0.60732181 0.33458079 0.60705987 -0.13129960E-03 0.21853082E-05 55727.000 11878.000 0.60738831 0.60670363 0.33407460 0.60639974 -0.11623573E-03 -0.47559250E-05 55497.000 11880.400 0.60704946 0.60605889 0.33354639 0.60571112 -0.15365245E-03 0.84820405E-06 55352.500 11882.800 0.60665078 0.60541444 0.33301819 0.60502273 -0.11216435E-03 0.18226677E-04 55130.500 11885.200 0.60651107 0.60477026 0.33248999 0.60433456 -0.66164400E-04 -0.12155380E-05 54993.500 11887.600 0.60633319 0.60412634 0.33196179 0.60364661 -0.11799893E-03 -0.15587608E-04 54721.500 11890.000 0.60594467 0.60348264 0.33143358 0.60295888 -0.14098492E-03 0.37926400E-05 54670.000 11892.400 0.60565646 0.60283914 0.33090538 0.60227137 -0.99794260E-04 0.99334106E-05 54471.000 11894.800 0.60546566 0.60219583 0.33037718 0.60158408 -0.93304547E-04 -0.22240805E-04 54249.000 11897.200 0.60520860 0.60155268 0.32984898 0.60089702 -0.20655012E-03 -0.31823464E-04 54116.000 11899.500 0.60449488 0.60093646 0.32934278 0.60023879 -0.24287483E-03 -0.18960866E-05 53909.000 11901.900 0.60406708 0.60029357 0.32881458 0.59955215 -0.21546173E-03 -0.11214480E-04 53697.500 11904.300 0.60346066 0.59965077 0.32828638 0.59886574 -0.29670433E-03 -0.38903783E-04 53520.500 11906.700 0.60264290 0.59900804 0.32775818 0.59817955 -0.40219989E-03 -0.28271957E-04 53358.000 11909.100 0.60153010 0.59836537 0.32722997 0.59749359 -0.43240973E-03 -0.63951508E-05 53170.000 11911.500 0.60056734 0.59772272 0.32670177 0.59680784 -0.43289662E-03 -0.50070883E-05 53029.500 11913.900 0.59945220 0.59708009 0.32617357 0.59612231 -0.45644375E-03 -0.16925453E-04 52893.000 11916.300 0.59837641 0.59643744 0.32564537 0.59543701 -0.51413879E-03 -0.24537534E-04 52681.500 11918.700 0.59698433 0.59579475 0.32511716 0.59475193 -0.57422391E-03 0.57096818E-05 52486.500 11921.100 0.59562013 0.59515201 0.32458896 0.59406707 -0.48673232E-03 0.25189613E-04 52370.500 11923.500 0.59464802 0.59450919 0.32406076 0.59338243 -0.45331377E-03 0.47565578E-05 52142.000 11925.900 0.59344423 0.59386626 0.32353256 0.59269801 -0.46390084E-03 0.11597280E-04 51996.000 11928.400 0.59237490 0.59319641 0.32298235 0.59198531 -0.39648710E-03 0.13176415E-04 51803.000 11930.800 0.59150144 0.59255321 0.32245414 0.59130134 -0.39933641E-03 0.61224104E-05 51657.500 11933.200 0.59045809 0.59190984 0.32192594 0.59061759 -0.36709953E-03 0.22833639E-04 51517.000 11935.600 0.58973936 0.59126628 0.32139774 0.58993407 -0.28973494E-03 0.19515711E-04 51333.000 11938.000 0.58906736 0.59062250 0.32086954 0.58925077 -0.27342412E-03 -0.14754380E-04 51130.000 11940.400 0.58842693 0.58997849 0.32034133 0.58856768 -0.36055596E-03 -0.14059135E-04 50995.500 11942.800 0.58733669 0.58933422 0.31981313 0.58788482 -0.34090796E-03 0.29368289E-04 50791.500 11945.200 0.58679057 0.58868967 0.31928493 0.58720218 -0.21958818E-03 0.26428212E-04 50632.500 11947.600 0.58628267 0.58804483 0.31875673 0.58651977 -0.21405255E-03 0.87507194E-05 50401.000 11950.100 0.58574171 0.58737276 0.31820652 0.58580915 -0.17670965E-03 0.37410952E-05 50248.000 11952.500 0.58541679 0.58672723 0.31767831 0.58512718 -0.19572118E-03 -0.12586921E-04 50053.000 11954.900 0.58480225 0.58608133 0.31715011 0.58444544 -0.23712687E-03 0.27750841E-05 49972.000 11957.300 0.58427858 0.58543504 0.31662191 0.58376392 -0.18240078E-03 0.14440431E-04 49757.500 11959.700 0.58392673 0.58478833 0.31609371 0.58308261 -0.16781280E-03 -0.18923573E-04 49532.000 11962.100 0.58347308 0.58414119 0.31556550 0.58240153 -0.27323393E-03 -0.12373214E-04 49402.000 11964.600 0.58258788 0.58346660 0.31501529 0.58169231 -0.22844155E-03 0.42968896E-04 49241.000 11967.000 0.58235372 0.58281851 0.31448709 0.58101168 -0.62686338E-04 0.30224516E-04 49114.000 11969.400 0.58228698 0.58216991 0.31395889 0.58033127 -0.83363876E-04 -0.29959197E-04 48933.500 11971.800 0.58195357 0.58152079 0.31343069 0.57965109 -0.20649048E-03 -0.38185205E-04 48812.500 11974.300 0.58127518 0.58084404 0.31288047 0.57894279 -0.27047138E-03 -0.73995551E-05 48580.000 11976.700 0.58062826 0.58019379 0.31235227 0.57826306 -0.24274830E-03 0.91478373E-05 48490.500 11979.100 0.58010999 0.57954294 0.31182407 0.57758355 -0.22656176E-03 -0.12692591E-04 48280.500 11981.500 0.57954076 0.57889148 0.31129587 0.57690425 -0.30367274E-03 -0.27777222E-04 48087.000 11984.000 0.57862199 0.57821220 0.31074566 0.57619689 -0.36267015E-03 -0.31694954E-05 47938.500 11986.400 0.57776368 0.57755946 0.31021745 0.57551805 -0.31920327E-03 0.13409817E-04 47626.500 11988.800 0.57708982 0.57690611 0.30968925 0.57483944 -0.29830303E-03 -0.95866523E-05 47642.500 11991.300 0.57630199 0.57622489 0.30913904 0.57413278 -0.36617787E-03 -0.20578069E-04 47447.500 11993.700 0.57529555 0.57557032 0.30861084 0.57345461 -0.39913557E-03 0.37528008E-05 47294.000 11996.100 0.57438614 0.57491515 0.30808264 0.57277666 -0.34816442E-03 0.17394855E-04 47148.000 11998.600 0.57358954 0.57423208 0.30753243 0.57207071 -0.31390077E-03 0.39522320E-05 47023.500 12001.000 0.57284803 0.57357575 0.30700422 0.57139321 -0.32879849E-03 0.38158213E-06 46825.500 12003.400 0.57201131 0.57291887 0.30647602 0.57071594 -0.31206918E-03 0.12099493E-04 46688.000 12005.900 0.57131889 0.57223403 0.30592581 0.57001068 -0.26951097E-03 -0.86413995E-05 46468.000 12008.300 0.57069070 0.57157604 0.30539761 0.56933386 -0.35441204E-03 -0.18625982E-04 46364.500 12010.800 0.56958227 0.57089007 0.30484740 0.56862908 -0.36077829E-03 0.22819069E-04 46135.500 12013.200 0.56892289 0.57023100 0.30431919 0.56795271 -0.24259860E-03 0.43036435E-04 46041.500 12015.600 0.56841780 0.56957143 0.30379099 0.56727656 -0.15420340E-03 0.13365898E-04 45847.000 12018.100 0.56816729 0.56888385 0.30324078 0.56657248 -0.17710570E-03 -0.17804425E-04 45745.500 12020.500 0.56754998 0.56822327 0.30271258 0.56589678 -0.24144508E-03 -0.82295387E-05 45525.000 12023.000 0.56698421 0.56753465 0.30216237 0.56519317 -0.21743044E-03 0.92562699E-05 45397.000 12025.400 0.56648457 0.56687309 0.30163417 0.56451792 -0.19608936E-03 0.34437553E-06 45217.500 12027.900 0.56602337 0.56618348 0.30108395 0.56381478 -0.21574300E-03 -0.50854676E-05 45153.500 12030.300 0.56542743 0.56552100 0.30055575 0.56313999 -0.22100815E-03 0.51709146E-05 44958.500 12032.800 0.56494043 0.56483044 0.30000554 0.56243732 -0.19040552E-03 0.18731269E-04 44751.000 12035.200 0.56449444 0.56416706 0.29947734 0.56176298 -0.12922493E-03 -0.26086888E-04 44567.500 12037.700 0.56430723 0.56347559 0.29892713 0.56106078 -0.31823127E-03 -0.36148051E-04 44258.500 12040.100 0.56293511 0.56281135 0.29839893 0.56038689 -0.30635038E-03 0.40073460E-04 44329.500 12042.600 0.56280612 0.56211901 0.29784872 0.55968516 -0.12187131E-03 0.30619543E-04 44117.500 12045.000 0.56233794 0.56145396 0.29732051 0.55901172 -0.15631462E-03 -0.18637029E-04 44060.000 12047.500 0.56204017 0.56076079 0.29677030 0.55831046 -0.21319275E-03 -0.21500479E-04 43889.000 12050.000 0.56127198 0.56006721 0.29622009 0.55760944 -0.26381701E-03 0.94469812E-06 43751.000 12052.400 0.56074747 0.55940100 0.29569189 0.55693668 -0.20856373E-03 0.88976403E-05 43566.000 12054.900 0.56025002 0.55870665 0.29514168 0.55623613 -0.22021857E-03 -0.66420793E-05 43413.000 12057.300 0.55966840 0.55803972 0.29461348 0.55556383 -0.24110992E-03 -0.21365508E-04 43242.500 12059.800 0.55906858 0.55734465 0.29406326 0.55486375 -0.32490956E-03 -0.91517625E-05 43116.000 12062.300 0.55804385 0.55664922 0.29351305 0.55416391 -0.28686873E-03 0.11726903E-04 42970.500 12064.700 0.55766292 0.55598128 0.29298485 0.55349230 -0.26744774E-03 -0.89851800E-05 42831.000 12067.200 0.55673336 0.55528519 0.29243464 0.55279293 -0.33089612E-03 -0.98135807E-05 42645.500 12069.700 0.55600844 0.55458877 0.29188443 0.55209380 -0.31651564E-03 -0.69759187E-05 42503.000 12072.100 0.55518243 0.55391991 0.29135623 0.55142286 -0.36507812E-03 -0.16169652E-04 42362.500 12074.600 0.55421956 0.55322288 0.29080602 0.55072420 -0.39574694E-03 -0.11606334E-04 42202.500 12077.100 0.55320370 0.55252556 0.29025581 0.55002579 -0.42310979E-03 0.33044664E-06 42027.500 12079.500 0.55214632 0.55185587 0.28972760 0.54935553 -0.39412775E-03 0.98301233E-05 41911.000 12082.000 0.55127247 0.55115801 0.28917739 0.54865759 -0.37494218E-03 0.51546316E-05 41772.000 12084.500 0.55027161 0.55045989 0.28862718 0.54795988 -0.36835459E-03 0.25349477E-05 41673.000 12086.900 0.54946753 0.54978945 0.28809898 0.54729031 -0.36252094E-03 0.30728629E-05 41591.000 12089.400 0.54849526 0.54909085 0.28754877 0.54659307 -0.35329756E-03 -0.23482565E-05 41345.500 12091.900 0.54770105 0.54839201 0.28699856 0.54589607 -0.37426222E-03 -0.90679906E-05 41160.500 12094.400 0.54662394 0.54769296 0.28644835 0.54519932 -0.39863752E-03 0.47886695E-05 41016.000 12096.800 0.54574772 0.54702167 0.28592014 0.54453066 -0.35079774E-03 0.26375686E-04 40905.000 12099.300 0.54490504 0.54632221 0.28536993 0.54383438 -0.26939666E-03 0.24389668E-04 40814.500 12101.800 0.54440074 0.54562257 0.28481972 0.54313833 -0.22884940E-03 -0.65868729E-07 40609.500 12104.300 0.54376079 0.54492274 0.28426951 0.54244253 -0.26972600E-03 -0.12927714E-04 40444.000 12106.800 0.54305211 0.54422275 0.28371930 0.54174696 -0.29348797E-03 0.39898236E-05 40294.000 12109.200 0.54232270 0.54355062 0.28319110 0.54107945 -0.25017586E-03 0.78652116E-05 40164.000 12111.700 0.54182625 0.54285033 0.28264089 0.54038435 -0.25494843E-03 -0.39169426E-04 39994.500 12114.200 0.54104796 0.54214991 0.28209068 0.53968950 -0.44602299E-03 -0.25793551E-04 39810.500 12116.700 0.53959613 0.54144936 0.28154047 0.53899488 -0.38391619E-03 0.65089478E-04 39703.000 12119.200 0.53912837 0.54074870 0.28099026 0.53830051 -0.12057561E-03 0.49693586E-04 39651.000 12121.700 0.53899325 0.54004793 0.28044005 0.53760638 -0.13544826E-03 -0.29053084E-04 39592.500 12124.200 0.53845113 0.53934707 0.27988983 0.53691248 -0.26584103E-03 -0.24293781E-04 39386.000 12126.700 0.53766405 0.53864612 0.27933962 0.53621883 -0.25691716E-03 0.12502534E-04 39310.500 12129.100 0.53719224 0.53797315 0.27881142 0.53555315 -0.20457861E-03 0.63465975E-05 39031.000 12131.600 0.53666161 0.53727207 0.27826121 0.53485997 -0.22581884E-03 -0.95587271E-05 38953.000 12134.100 0.53606314 0.53657094 0.27771100 0.53416703 -0.25237225E-03 0.12231313E-05 38801.500 12136.600 0.53539975 0.53586977 0.27716079 0.53347432 -0.21970318E-03 0.16203764E-04 38751.000 12139.100 0.53496463 0.53516857 0.27661058 0.53278186 -0.17135343E-03 -0.12195952E-04 38539.500 12141.600 0.53454298 0.53446735 0.27606037 0.53208964 -0.28068294E-03 0.16263919E-04 38356.000 12144.100 0.53356121 0.53376612 0.27551016 0.53139766 -0.90033834E-04 0.34576322E-04 38109.500 12146.600 0.53409282 0.53306489 0.27495995 0.53070592 -0.10780133E-03 -0.35661714E-04 38154.500 12149.100 0.53302221 0.53236367 0.27440973 0.53001442 -0.26834240E-03 -0.12346983E-04 38083.000 12151.600 0.53275110 0.53166248 0.27385952 0.52932316 -0.16953624E-03 0.10238395E-04 37918.500 12154.100 0.53217453 0.53096131 0.27330931 0.52863213 -0.21715043E-03 -0.11915136E-04 37771.500 12156.600 0.53166535 0.53026019 0.27275910 0.52794135 -0.22911193E-03 -0.12212226E-04 37634.000 12159.100 0.53102897 0.52955913 0.27220889 0.52725081 -0.27821156E-03 -0.42286030E-05 37465.500 12161.600 0.53027429 0.52885813 0.27165868 0.52656051 -0.25025494E-03 -0.15707954E-05 37399.000 12164.100 0.52977769 0.52815720 0.27110847 0.52587045 -0.28606554E-03 -0.21713863E-04 37242.000 12166.600 0.52884397 0.52745636 0.27055826 0.52518063 -0.35882426E-03 -0.67093363E-05 37091.000 12169.100 0.52798357 0.52675560 0.27000805 0.52449105 -0.31961222E-03 0.84807465E-05 36965.000 12171.700 0.52721394 0.52602691 0.26943583 0.52377414 -0.31557245E-03 -0.36483454E-05 36881.500 12174.200 0.52637415 0.52532634 0.26888562 0.52308505 -0.33821878E-03 -0.92932185E-05 36707.500 12176.700 0.52552285 0.52462585 0.26833541 0.52239620 -0.36203854E-03 -0.90757059E-05 36532.500 12179.200 0.52456396 0.52392545 0.26778520 0.52170759 -0.38359731E-03 0.27607572E-05 36413.000 12181.700 0.52360486 0.52322513 0.26723499 0.52101922 -0.34823476E-03 0.13178644E-04 36292.000 12184.200 0.52282278 0.52252490 0.26668477 0.52033109 -0.31770409E-03 -0.93354990E-05 36197.000 12186.700 0.52201634 0.52182475 0.26613456 0.51964320 -0.39491225E-03 -0.16551177E-04 36124.000 12189.200 0.52084822 0.52112469 0.26558435 0.51895555 -0.40045997E-03 0.14033375E-04 35932.000 12191.800 0.51997400 0.52039671 0.26501213 0.51824065 -0.32334204E-03 0.16953874E-04 35798.000 12194.300 0.51919918 0.51969682 0.26446192 0.51755349 -0.31399521E-03 0.20218427E-05 35637.500 12196.800 0.51840402 0.51899701 0.26391171 0.51686658 -0.31323282E-03 -0.58286384E-05 35542.000 12199.300 0.51763301 0.51829728 0.26336150 0.51617990 -0.34313840E-03 0.32090546E-05 35400.500 12201.800 0.51668833 0.51759763 0.26281129 0.51549346 -0.29718755E-03 0.17596297E-04 35326.000 12204.400 0.51611736 0.51687009 0.26223907 0.51477981 -0.25339729E-03 0.95075678E-05 35147.500 12206.900 0.51539600 0.51617061 0.26168886 0.51409387 -0.24869895E-03 -0.17945845E-05 35015.000 12209.400 0.51487386 0.51547121 0.26113865 0.51340816 -0.26237021E-03 -0.51395289E-05 34900.500 12211.900 0.51408415 0.51477189 0.26058844 0.51272269 -0.27439660E-03 0.84139382E-05 34786.000 12214.500 0.51347444 0.51404468 0.26001622 0.51201005 -0.21945913E-03 -0.61838690E-05 34715.500 12217.000 0.51296491 0.51334552 0.25946601 0.51132508 -0.30593433E-03 -0.24947852E-04 34550.000 12219.500 0.51194477 0.51264644 0.25891580 0.51064034 -0.34419839E-03 0.38357454E-05 34420.500 12222.100 0.51120950 0.51191948 0.25834358 0.50992846 -0.28637203E-03 0.12719230E-04 34306.000 12224.600 0.51048427 0.51122056 0.25779337 0.50924421 -0.27933032E-03 0.36855803E-05 34172.000 12227.100 0.50981285 0.51052171 0.25724316 0.50856021 -0.26794413E-03 0.94680022E-05 34047.500 12229.700 0.50911776 0.50979500 0.25667094 0.50784909 -0.23104351E-03 0.11168890E-04 33931.500 12232.200 0.50863452 0.50909631 0.25612073 0.50716557 -0.21098279E-03 -0.32172113E-05 33812.000 12234.700 0.50806284 0.50839769 0.25557052 0.50648229 -0.24712956E-03 -0.79676949E-05 33675.500 12237.300 0.50737416 0.50767122 0.25499830 0.50577194 -0.25161803E-03 0.10292752E-04 33551.000 12239.800 0.50677959 0.50697275 0.25444809 0.50508915 -0.19463653E-03 0.13157513E-04 33463.000 12242.300 0.50640098 0.50627437 0.25389788 0.50440660 -0.18583047E-03 -0.10342065E-04 33337.500 12244.900 0.50583186 0.50554812 0.25332566 0.50369700 -0.24738106E-03 -0.12654775E-04 33158.500 12247.400 0.50513934 0.50484989 0.25277545 0.50301495 -0.25036982E-03 0.31297535E-05 33085.000 12250.000 0.50455497 0.50412380 0.25220323 0.50230586 -0.23141931E-03 0.13254979E-04 33013.500 12252.500 0.50395910 0.50342571 0.25165302 0.50162429 -0.18276943E-03 0.10779922E-04 32873.000 12255.100 0.50362285 0.50269977 0.25108080 0.50091571 -0.17644171E-03 -0.17423209E-04 32739.500 12257.600 0.50305925 0.50200183 0.25053059 0.50023463 -0.27162779E-03 -0.22826275E-04 32621.000 12260.200 0.50223754 0.50127604 0.24995837 0.49952657 -0.29285571E-03 0.31212468E-06 32521.500 12262.700 0.50156568 0.50057824 0.24940816 0.49884598 -0.27003596E-03 0.37834829E-05 32427.000 12265.300 0.50086036 0.49985261 0.24883594 0.49813842 -0.27355995E-03 0.26801488E-06 32268.000 12267.800 0.50017053 0.49915495 0.24828573 0.49745832 -0.26866908E-03 -0.47206327E-05 32160.000 12270.400 0.49949015 0.49842946 0.24771351 0.49675127 -0.29763518E-03 -0.16189001E-04 32061.500 12272.900 0.49865259 0.49773194 0.24716330 0.49607166 -0.35123298E-03 -0.11116312E-04 31979.500 12275.500 0.49769886 0.49700659 0.24659108 0.49536512 -0.35432837E-03 -0.50876276E-05 31824.000 12278.000 0.49684551 0.49630921 0.24604087 0.49468600 -0.37717988E-03 -0.27888618E-05 31715.500 12280.600 0.49577524 0.49558401 0.24546865 0.49397997 -0.36855156E-03 0.10283266E-04 31631.500 12283.100 0.49496590 0.49488676 0.24491844 0.49330134 -0.32473522E-03 0.62056488E-05 31496.000 12285.700 0.49411909 0.49416170 0.24434622 0.49259582 -0.33690276E-03 -0.70018420E-05 31400.500 12288.200 0.49324770 0.49346459 0.24379600 0.49191768 -0.36044462E-03 -0.36665978E-05 31297.000 12290.800 0.49228083 0.49273967 0.24322379 0.49121267 -0.35560240E-03 0.52077278E-06 31173.500 12293.400 0.49139856 0.49201481 0.24265157 0.49050792 -0.35773660E-03 0.18184703E-05 31070.000 12295.900 0.49045637 0.49131790 0.24210136 0.48983052 -0.34632821E-03 0.96219966E-05 30979.500 12298.500 0.48963229 0.49059318 0.24152914 0.48912628 -0.30866442E-03 0.14261706E-04 30867.500 12301.100 0.48885131 0.48986852 0.24095692 0.48842230 -0.27216733E-03 0.92440793E-05 30741.500 12303.600 0.48824424 0.48917181 0.24040671 0.48774564 -0.26151961E-03 -0.38831035E-05 30643.000 12306.200 0.48751756 0.48844729 0.23983449 0.48704217 -0.29197116E-03 -0.24261848E-04 30532.000 12308.800 0.48672599 0.48772283 0.23926227 0.48633896 -0.38768122E-03 0.47480423E-06 30433.000 12311.300 0.48554039 0.48702630 0.23871206 0.48566303 -0.28954966E-03 0.39076412E-04 30316.500 12313.900 0.48524928 0.48630198 0.23813984 0.48496033 -0.18839152E-03 0.14047307E-05 30263.000 12316.500 0.48456075 0.48557772 0.23756762 0.48425789 -0.28224506E-03 -0.21803111E-04 30092.000 12319.000 0.48380983 0.48488137 0.23701741 0.48358271 -0.29958739E-03 0.15340296E-04 30017.500 12321.600 0.48303286 0.48415724 0.23644519 0.48288077 -0.20400955E-03 0.17562056E-04 29918.000 12324.200 0.48274898 0.48343317 0.23587297 0.48217910 -0.20826469E-03 -0.16878511E-04 29822.000 12326.800 0.48194988 0.48270916 0.23530075 0.48147769 -0.29177781E-03 0.52328181E-06 29690.500 12329.300 0.48126092 0.48201306 0.23475054 0.48080349 -0.20559596E-03 0.26328349E-04 29594.000 12331.900 0.48090134 0.48128917 0.23417832 0.48010259 -0.15750323E-03 0.22911998E-05 29485.500 12334.500 0.48044190 0.48056534 0.23360610 0.47940194 -0.19368172E-03 -0.25262177E-04 29389.500 12337.100 0.47989420 0.47984158 0.23303388 0.47870156 -0.28886655E-03 -0.28391821E-04 29301.500 12339.700 0.47893979 0.47911788 0.23246166 0.47800143 -0.34131919E-03 0.36359641E-05 29167.000 12342.200 0.47815347 0.47842206 0.23191145 0.47732848 -0.27032313E-03 0.24757265E-04 29061.000 12344.800 0.47756115 0.47769847 0.23133923 0.47662886 -0.21505714E-03 0.90722270E-05 28978.500 12347.400 0.47703517 0.47697494 0.23076701 0.47592951 -0.22314755E-03 -0.17701045E-05 28854.500 12350.000 0.47640078 0.47625147 0.23019479 0.47523041 -0.22426168E-03 -0.51601501E-05 28742.000 12352.600 0.47586901 0.47552806 0.22962257 0.47453157 -0.24998033E-03 0.30922613E-05 28672.000 12355.200 0.47510088 0.47480470 0.22905036 0.47383300 -0.20818192E-03 0.11943637E-04 28535.000 12357.800 0.47478647 0.47408140 0.22847814 0.47313468 -0.18787341E-03 -0.97508443E-05 28436.000 12360.400 0.47412394 0.47335816 0.22790592 0.47243662 -0.25888631E-03 -0.65514722E-05 28328.000 12362.900 0.47346615 0.47266278 0.22735571 0.47176566 -0.22128592E-03 0.11987488E-04 28288.500 12365.500 0.47299538 0.47193965 0.22678349 0.47106811 -0.19775013E-03 0.89028900E-05 28146.000 12368.100 0.47243784 0.47121656 0.22621127 0.47037082 -0.17499089E-03 -0.13500049E-04 28002.000 12370.700 0.47208543 0.47049353 0.22563905 0.46967379 -0.26795038E-03 -0.38825979E-04 27928.000 12373.300 0.47104450 0.46977056 0.22506683 0.46897702 -0.37688598E-03 -0.45457974E-05 27856.500 12375.900 0.47012562 0.46904764 0.22449461 0.46828051 -0.29158853E-03 0.30044454E-04 27708.500 12378.500 0.46952824 0.46832477 0.22392239 0.46758427 -0.22065482E-03 -0.30095497E-05 27592.000 12381.100 0.46897822 0.46760195 0.22335017 0.46688828 -0.30723819E-03 -0.17384756E-04 27506.500 12383.700 0.46793060 0.46687918 0.22277795 0.46619255 -0.31105555E-03 -0.34763283E-05 27429.000 12386.300 0.46736073 0.46615647 0.22220573 0.46549708 -0.32531509E-03 -0.12948445E-04 27365.500 12388.900 0.46623897 0.46543382 0.22163351 0.46480187 -0.37838747E-03 0.28304992E-05 27287.000 12391.500 0.46539311 0.46471123 0.22106129 0.46410691 -0.31059650E-03 0.94535003E-05 27162.000 12394.100 0.46462386 0.46398872 0.22048907 0.46341222 -0.32922927E-03 -0.26304153E-05 27069.500 12396.700 0.46368112 0.46326628 0.21991686 0.46271779 -0.32427466E-03 0.12820958E-06 26995.500 12399.300 0.46293764 0.46254392 0.21934464 0.46202362 -0.32856258E-03 -0.28246284E-05 26896.000 12402.000 0.46193974 0.46179386 0.21875041 0.46130303 -0.33924519E-03 0.38712148E-05 26779.500 12404.600 0.46113964 0.46107168 0.21817819 0.46060938 -0.30804514E-03 0.16074851E-04 26655.000 12407.200 0.46033790 0.46034960 0.21760597 0.45991600 -0.25565596E-03 0.23983003E-05 26617.000 12409.800 0.45981022 0.45962761 0.21703375 0.45922288 -0.29557398E-03 -0.21293012E-04 26452.500 12412.400 0.45880092 0.45890573 0.21646153 0.45853002 -0.36637962E-03 -0.79711129E-05 26400.500 12415.000 0.45790505 0.45818396 0.21588931 0.45783741 -0.33702376E-03 -0.16155612E-06 26316.000 12417.600 0.45704840 0.45746230 0.21531709 0.45714507 -0.36721972E-03 -0.11282478E-04 26229.500 12420.200 0.45599551 0.45674077 0.21474487 0.45645299 -0.39569265E-03 0.75883287E-05 26102.500 12422.900 0.45495122 0.45599162 0.21415065 0.45573456 -0.32700157E-03 0.29212993E-04 26013.000 12425.500 0.45426240 0.45527035 0.21357843 0.45504300 -0.24086379E-03 0.17729470E-04 25956.500 12428.100 0.45369873 0.45454921 0.21300621 0.45435171 -0.23480833E-03 -0.84468822E-05 25849.000 12430.700 0.45304140 0.45382821 0.21243399 0.45366067 -0.28478758E-03 -0.12749612E-04 25751.000 12433.300 0.45221784 0.45310736 0.21186177 0.45296990 -0.30110631E-03 0.42326014E-05 25663.000 12436.000 0.45144553 0.45235894 0.21126754 0.45225283 -0.26235479E-03 0.10717313E-04 25594.500 12438.600 0.45082736 0.45163840 0.21069532 0.45156259 -0.24430455E-03 -0.10531304E-04 25490.000 12441.200 0.45017515 0.45091803 0.21012310 0.45087260 -0.31711757E-03 -0.24118861E-04 25407.500 12443.800 0.44917835 0.45019781 0.20955088 0.45018287 -0.36972263E-03 -0.59541670E-05 25296.000 12446.500 0.44821562 0.44945008 0.20895666 0.44946689 -0.34867465E-03 0.13679489E-04 25238.000 12449.100 0.44733037 0.44873022 0.20838444 0.44877770 -0.29722134E-03 0.27879602E-04 25144.500 12451.700 0.44667007 0.44801055 0.20781222 0.44808876 -0.20370072E-03 0.17258879E-04 25056.000 12454.400 0.44625076 0.44726339 0.20721799 0.44737360 -0.20574928E-03 0.99247759E-05 24933.000 12457.000 0.44557960 0.44654409 0.20664577 0.44668519 -0.15109941E-03 0.15552947E-04 24858.500 12459.600 0.44546504 0.44582499 0.20607355 0.44599705 -0.12487396E-03 -0.11307888E-04 24737.000 12462.300 0.44491777 0.44507845 0.20547932 0.44528271 -0.21103121E-03 -0.26673395E-04 24698.500 12464.900 0.44434657 0.44435977 0.20490710 0.44459509 -0.26624295E-03 -0.90048955E-05 24615.000 12467.500 0.44353330 0.44364130 0.20433489 0.44390773 -0.25785667E-03 0.48414223E-05 24568.500 12470.200 0.44297993 0.44289543 0.20374066 0.44319421 -0.24058342E-03 -0.20845154E-05 24489.500 12472.800 0.44225821 0.44217740 0.20316844 0.44250738 -0.26890460E-03 0.27785865E-05 24345.000 12475.500 0.44155474 0.44143200 0.20257421 0.44179441 -0.22585691E-03 0.83507647E-05 24296.000 12478.100 0.44106117 0.44071445 0.20200199 0.44110811 -0.22464555E-03 0.17232628E-05 24226.500 12480.700 0.44038658 0.43999713 0.20142977 0.44042207 -0.21689594E-03 -0.98720239E-06 24169.000 12483.400 0.43991162 0.43925247 0.20083554 0.43970992 -0.22987772E-03 -0.73465646E-05 24083.000 12486.000 0.43916823 0.43853565 0.20026333 0.43902441 -0.25583273E-03 0.78206930E-05 23979.000 12488.700 0.43855571 0.43779153 0.19966910 0.43831281 -0.18842805E-03 -0.82543214E-05 23908.500 12491.300 0.43816956 0.43707522 0.19909688 0.43762783 -0.29958064E-03 -0.25615534E-04 23836.500 12494.000 0.43696793 0.43633165 0.19850265 0.43691678 -0.32419038E-03 0.83793330E-05 23691.000 12496.600 0.43645135 0.43561588 0.19793043 0.43623233 -0.25517017E-03 0.32892360E-05 23645.500 12499.300 0.43561553 0.43487288 0.19733620 0.43552182 -0.30675743E-03 -0.25137178E-05 23567.000 12501.900 0.43482554 0.43415768 0.19676398 0.43483790 -0.26849288E-03 0.17110007E-04 23509.000 12504.600 0.43419251 0.43341527 0.19616976 0.43412795 -0.21607439E-03 0.19675472E-05 23401.500 12507.200 0.43368034 0.43270065 0.19559754 0.43344456 -0.25806488E-03 -0.26327577E-04 23317.000 12509.900 0.43282477 0.43195885 0.19500331 0.43273516 -0.35561055E-03 -0.12417034E-04 23211.500 12512.600 0.43176005 0.43121737 0.19440908 0.43202603 -0.32511686E-03 0.17322259E-04 23156.000 12515.200 0.43110165 0.43050367 0.19383686 0.43134344 -0.26380258E-03 0.94851136E-05 23051.500 12517.900 0.43036189 0.42976284 0.19324264 0.43063487 -0.27484576E-03 -0.36001947E-05 23016.000 12520.500 0.42964497 0.42904977 0.19267042 0.42995281 -0.28288361E-03 0.79875294E-06 22936.500 12523.200 0.42886261 0.42830961 0.19207619 0.42924478 -0.27061237E-03 -0.13498672E-05 22851.000 12525.900 0.42818366 0.42756980 0.19148196 0.42853704 -0.29017289E-03 -0.18548171E-04 22758.000 12528.500 0.42732469 0.42685772 0.19090974 0.42785578 -0.36891767E-03 -0.12098305E-04 22682.500 12531.200 0.42622840 0.42611861 0.19031551 0.42714859 -0.35429391E-03 0.15955910E-04 22614.000 12533.900 0.42541151 0.42537987 0.18972129 0.42644167 -0.28275576E-03 0.96322127E-05 22530.500 12536.500 0.42472979 0.42466883 0.18914907 0.42576121 -0.30324318E-03 -0.86531380E-05 22507.500 12539.200 0.42380432 0.42393082 0.18855484 0.42505485 -0.32861739E-03 -0.82493220E-05 22380.500 12541.900 0.42295526 0.42319319 0.18796061 0.42434876 -0.34778952E-03 0.19157307E-05 22303.500 12544.500 0.42196103 0.42248325 0.18738839 0.42366910 -0.31846402E-03 0.51344215E-05 22245.500 12547.200 0.42126740 0.42174639 0.18679416 0.42296357 -0.32057709E-03 0.51710217E-05 22161.500 12549.900 0.42022992 0.42100993 0.18619994 0.42225831 -0.29054050E-03 0.57665814E-05 22086.000 12552.500 0.41972753 0.42030112 0.18562772 0.42157945 -0.29001421E-03 -0.68415704E-05 22028.500 12555.200 0.41869284 0.41956546 0.18503349 0.42087474 -0.32680082E-03 0.71622145E-05 21951.000 12557.900 0.41796281 0.41883021 0.18443926 0.42017032 -0.25133825E-03 0.66536215E-05 21856.000 12560.600 0.41733561 0.41809538 0.18384503 0.41946618 -0.29087127E-03 -0.14145961E-04 21796.000 12563.300 0.41639211 0.41736098 0.18325081 0.41876232 -0.32772644E-03 0.84498196E-05 21734.500 12565.900 0.41559866 0.41665418 0.18267859 0.41808479 -0.24608722E-03 0.22659467E-04 21666.500 12568.600 0.41508784 0.41592063 0.18208436 0.41738148 -0.20763126E-03 0.11011495E-04 21610.000 12571.300 0.41447746 0.41518753 0.18149013 0.41667844 -0.18662515E-03 -0.61905195E-05 21534.000 12574.000 0.41408007 0.41445487 0.18089590 0.41597569 -0.24106007E-03 -0.13764596E-04 21444.500 12576.700 0.41317573 0.41372267 0.18030168 0.41527322 -0.26095397E-03 0.74373044E-05 21377.500 12579.400 0.41267092 0.41299092 0.17970745 0.41457103 -0.20089862E-03 0.23624488E-05 21302.500 12582.000 0.41211097 0.41228672 0.17913523 0.41389511 -0.24843299E-03 -0.13991886E-04 21241.500 12584.700 0.41135422 0.41155590 0.17854100 0.41319347 -0.27505562E-03 -0.64751685E-05 21194.500 12587.400 0.41062567 0.41082555 0.17794677 0.41249211 -0.28339890E-03 0.71992707E-05 21118.000 12590.100 0.40982387 0.41009569 0.17735255 0.41179102 -0.23617956E-03 0.16364911E-04 21026.500 12592.800 0.40935030 0.40936631 0.17675832 0.41109022 -0.19502838E-03 0.45577807E-05 20940.500 12595.500 0.40877071 0.40863742 0.17616409 0.41038970 -0.21156754E-03 0.53197068E-05 20893.000 12598.200 0.40820783 0.40790904 0.17556986 0.40968946 -0.16630197E-03 0.59818423E-05 20792.500 12600.900 0.40787268 0.40718116 0.17497564 0.40898950 -0.17926559E-03 -0.21027572E-04 20772.000 12603.600 0.40723980 0.40645378 0.17438141 0.40828982 -0.27985085E-03 -0.24827213E-04 20698.000 12606.300 0.40636149 0.40572693 0.17378718 0.40759042 -0.31333254E-03 0.71666231E-05 20592.000 12609.000 0.40554780 0.40500059 0.17319295 0.40689129 -0.24115109E-03 0.14746345E-04 20558.000 12611.700 0.40505927 0.40427479 0.17259873 0.40619245 -0.23370228E-03 -0.52378655E-07 20447.500 12614.400 0.40428581 0.40354951 0.17200450 0.40549389 -0.24143393E-03 0.45381073E-05 20381.500 12617.100 0.40375553 0.40282477 0.17141027 0.40479561 -0.20919650E-03 -0.11690398E-04 20338.500 12619.800 0.40315615 0.40210058 0.17081604 0.40409761 -0.30456208E-03 -0.25908340E-04 20245.500 12622.500 0.40211089 0.40137694 0.17022182 0.40339989 -0.34910153E-03 0.11645258E-04 20179.500 12625.200 0.40127100 0.40065385 0.16962759 0.40270245 -0.24167769E-03 0.23434749E-04 20117.000 12627.900 0.40080583 0.39993132 0.16903336 0.40200529 -0.22255389E-03 -0.14070287E-05 20031.500 12630.600 0.40006921 0.39920936 0.16843913 0.40130841 -0.24927564E-03 -0.11761108E-04 19970.500 12633.300 0.39945975 0.39848796 0.16784490 0.40061181 -0.28606387E-03 -0.17491591E-04 19889.000 12636.100 0.39849586 0.39774047 0.16722867 0.39988971 -0.34547939E-03 -0.95401956E-05 19811.000 12638.800 0.39755961 0.39702026 0.16663444 0.39919368 -0.33853495E-03 -0.38886775E-06 19756.000 12641.500 0.39666777 0.39630065 0.16604021 0.39849793 -0.34757928E-03 0.48705656E-06 19697.500 12644.200 0.39568268 0.39558165 0.16544599 0.39780246 -0.33590484E-03 0.27525981E-04 19638.000 12646.900 0.39485389 0.39486325 0.16485176 0.39710727 -0.19893898E-03 0.20604083E-04 19596.500 12649.600 0.39460841 0.39414547 0.16425753 0.39641236 -0.22464280E-03 -0.18192867E-04 19517.500 12652.300 0.39364081 0.39342832 0.16366330 0.39571773 -0.29718047E-03 -0.63647322E-05 19446.000 12655.100 0.39297392 0.39268528 0.16304707 0.39499767 -0.25964883E-03 -0.43354787E-05 19416.000 12657.800 0.39221275 0.39196942 0.16245284 0.39430361 -0.32102560E-03 -0.30417553E-04 19362.000 12660.500 0.39124038 0.39125422 0.16185861 0.39360983 -0.42390361E-03 -0.16318101E-04 19321.000 12663.200 0.38992367 0.39053968 0.16126438 0.39291633 -0.40914334E-03 0.22823675E-04 19284.500 12666.000 0.38899009 0.38979937 0.16064815 0.39219745 -0.29837340E-03 0.21016409E-04 19176.500 12668.700 0.38828261 0.38908619 0.16005392 0.39150452 -0.29355309E-03 0.78683852E-05 19130.500 12671.400 0.38740491 0.38837369 0.15945969 0.39081187 -0.25588412E-03 0.96478472E-05 19057.000 12674.100 0.38690084 0.38766188 0.15886546 0.39011950 -0.24145472E-03 0.14132940E-05 18988.500 12676.900 0.38607690 0.38692444 0.15824923 0.38940179 -0.24811100E-03 -0.54825998E-05 18953.000 12679.600 0.38553623 0.38621406 0.15765500 0.38870999 -0.27160902E-03 -0.10857298E-04 18868.500 12682.300 0.38461022 0.38550439 0.15706077 0.38801848 -0.30674041E-03 -0.27344904E-05 18829.000 12685.100 0.38384916 0.38476920 0.15644454 0.38730164 -0.28664871E-03 0.27665662E-05 18765.500 12687.800 0.38303365 0.38406101 0.15585031 0.38661070 -0.29152430E-03 0.10190394E-04 18682.000 12690.500 0.38227492 0.38335356 0.15525608 0.38592003 -0.23162059E-03 0.10459495E-04 18618.000 12693.300 0.38175973 0.38262069 0.15463984 0.38520408 -0.23399708E-03 -0.40516342E-04 18563.000 12696.000 0.38098794 0.38191476 0.15404562 0.38451398 -0.45446047E-03 -0.31455185E-04 18455.000 12698.800 0.37926020 0.38118349 0.15342938 0.38379863 -0.40700059E-03 0.38325992E-04 18372.000 12701.500 0.37874944 0.38047912 0.15283515 0.38310910 -0.24366751E-03 0.25717411E-04 18367.000 12704.200 0.37794440 0.37977553 0.15224093 0.38241986 -0.26812658E-03 0.42896387E-04 18270.500 12707.000 0.37727474 0.37904671 0.15162469 0.38170538 -0.77373847E-05 0.68374720E-04 18171.500 12709.700 0.37790184 0.37834472 0.15103046 0.38101671 0.10793438E-03 -0.37247393E-04 18143.500 12712.500 0.37786838 0.37761759 0.15041423 0.38030282 -0.21259805E-03 -0.10190935E-03 18148.000 12715.200 0.37673255 0.37691724 0.14982000 0.37961472 -0.45256706E-03 -0.20557373E-04 18132.500 12718.000 0.37537926 0.37619182 0.14920376 0.37890142 -0.32566360E-03 0.46160177E-04 18140.000 12720.700 0.37494140 0.37549315 0.14860953 0.37821389 -0.19868608E-03 0.23484501E-04 18077.500 12723.500 0.37428649 0.37476948 0.14799330 0.37750119 -0.19649884E-03 0.31329885E-05 18023.500 12726.200 0.37386066 0.37407251 0.14739907 0.37681423 -0.18145465E-03 -0.25624120E-05 17971.500 12729.000 0.37328849 0.37335062 0.14678283 0.37610212 -0.21059211E-03 -0.52175887E-05 17891.500 12731.700 0.37270240 0.37265539 0.14618861 0.37541572 -0.21015138E-03 0.89366927E-06 17844.000 12734.500 0.37213265 0.37193532 0.14557237 0.37470421 -0.20567693E-03 -0.26045160E-05 17770.000 12737.200 0.37157118 0.37124186 0.14497814 0.37401839 -0.22447622E-03 -0.31285474E-05 17710.000 12740.000 0.37089804 0.37052365 0.14436191 0.37330746 -0.22288394E-03 -0.69768309E-05 17672.000 12742.800 0.37032303 0.36980639 0.14374567 0.37259683 -0.26354648E-03 -0.11479227E-04 17594.500 12745.500 0.36944853 0.36911566 0.14315144 0.37191187 -0.28601969E-03 0.52300200E-05 17541.500 12748.300 0.36874992 0.36840031 0.14253521 0.37120184 -0.23478137E-03 0.11854143E-04 17502.500 12751.000 0.36815723 0.36771143 0.14194098 0.37051745 -0.22082190E-03 0.14998031E-04 17449.500 12753.800 0.36753540 0.36699801 0.14132474 0.36980801 -0.15229219E-03 0.17520804E-04 17365.000 12756.600 0.36730440 0.36628559 0.14070851 0.36909887 -0.12270540E-03 -0.12848046E-04 17335.000 12759.300 0.36686052 0.36559957 0.14011428 0.36841534 -0.22295645E-03 -0.21211163E-04 17297.000 12762.100 0.36607814 0.36488914 0.13949804 0.36770679 -0.23936680E-03 -0.44422608E-05 17233.000 12764.900 0.36552007 0.36417974 0.13888181 0.36699854 -0.24783311E-03 -0.68488802E-05 17171.500 12767.600 0.36471505 0.36349665 0.13828758 0.36631588 -0.27703564E-03 -0.49904850E-05 17126.000 12770.400 0.36399637 0.36278928 0.13767134 0.36560822 -0.27528077E-03 0.34556148E-05 17077.000 12773.200 0.36317348 0.36208296 0.13705511 0.36490087 -0.25768419E-03 0.96214533E-05 17004.000 12776.000 0.36255334 0.36137771 0.13643887 0.36419381 -0.22140063E-03 0.42377338E-05 16964.000 12778.700 0.36195578 0.36069865 0.13584464 0.36351230 -0.23437666E-03 -0.25511633E-04 16911.500 12781.500 0.36126427 0.35999550 0.13522841 0.36280583 -0.36171461E-03 -0.31001708E-04 16879.000 12784.300 0.35993018 0.35929344 0.13461217 0.36209967 -0.40798622E-03 0.11143603E-04 16813.500 12787.100 0.35897954 0.35859248 0.13399594 0.36139382 -0.29931044E-03 0.26228910E-04 16756.000 12789.800 0.35828397 0.35791759 0.13340171 0.36071345 -0.26372722E-03 0.48304181E-05 16705.000 12792.600 0.35752905 0.35721879 0.13278547 0.36000818 -0.27274314E-03 0.92733119E-05 16649.500 12795.400 0.35675661 0.35652112 0.13216924 0.35930322 -0.21179667E-03 0.68025277E-05 16619.500 12798.200 0.35634298 0.35582458 0.13155300 0.35859855 -0.23464898E-03 -0.14950082E-04 16565.500 12801.000 0.35544257 0.35512918 0.13093676 0.35789419 -0.29551713E-03 -0.17515177E-04 16508.500 12803.800 0.35468809 0.35443492 0.13032053 0.35719013 -0.33273398E-03 -0.74475603E-05 16449.000 12806.600 0.35357926 0.35374182 0.12970429 0.35648636 -0.33722347E-03 0.16897962E-04 16403.000 12809.300 0.35283336 0.35307457 0.12911006 0.35580802 -0.23979518E-03 0.27914004E-04 16368.000 12812.100 0.35226039 0.35238377 0.12849383 0.35510485 -0.18369645E-03 -0.14282397E-04 16306.000 12814.900 0.35180466 0.35169414 0.12787759 0.35440199 -0.31977661E-03 -0.37314257E-04 16254.500 12817.700 0.35046964 0.35100571 0.12726135 0.35369942 -0.39265629E-03 0.11931530E-04 16203.000 12820.500 0.34960578 0.35031847 0.12664512 0.35299715 -0.25296004E-03 0.28377678E-04 16150.000 12823.300 0.34905306 0.34963244 0.12602888 0.35229519 -0.23374130E-03 -0.10920539E-05 16095.000 12826.100 0.34829683 0.34894763 0.12541265 0.35159352 -0.25907554E-03 -0.51709979E-05 16054.500 12828.900 0.34760224 0.34826405 0.12479641 0.35089216 -0.26269888E-03 -0.32561794E-05 16011.500 12831.700 0.34682572 0.34758169 0.12418017 0.35019110 -0.27731015E-03 0.13633004E-04 15963.000 12834.500 0.34604930 0.34690059 0.12356394 0.34949034 -0.18635406E-03 0.24265043E-04 15907.500 12837.300 0.34578214 0.34622073 0.12294770 0.34878988 -0.14142590E-03 0.95888330E-06 15887.000 12840.100 0.34525732 0.34554213 0.12233147 0.34808973 -0.18098431E-03 -0.22389702E-05 15837.000 12842.900 0.34476862 0.34486480 0.12171523 0.34738987 -0.15396414E-03 0.94071682E-06 15797.500 12845.700 0.34439512 0.34418875 0.12109899 0.34669032 -0.17571630E-03 -0.82119147E-05 15753.500 12848.500 0.34378461 0.34351399 0.12048276 0.34599106 -0.19995086E-03 -0.24593582E-04 15691.000 12851.300 0.34327539 0.34284052 0.11986652 0.34529211 -0.31344035E-03 -0.19165908E-04 15784.500 12854.100 0.34202935 0.34216836 0.11925029 0.34459346 -0.30727994E-03 0.59983236E-05 15594.500 12857.000 0.34152390 0.34147357 0.11861204 0.34387017 -0.27924991E-03 0.13775768E-04 15543.000 12859.800 0.34043762 0.34080409 0.11799580 0.34317214 -0.22875806E-03 0.25007187E-04 15494.500 12862.600 0.34024285 0.34013594 0.11737957 0.34247440 -0.13920966E-03 -0.35079258E-06 15443.000 12865.400 0.33965805 0.33946913 0.11676333 0.34177696 -0.23072250E-03 -0.17517921E-04 15411.500 12868.200 0.33895081 0.33880366 0.11614710 0.34107983 -0.23731002E-03 0.83837504E-06 15358.500 12871.000 0.33832911 0.33813956 0.11553086 0.34038300 -0.22602760E-03 0.56581203E-05 15319.500 12873.800 0.33768505 0.33747681 0.11491462 0.33968647 -0.20562455E-03 0.34029824E-06 15279.500 12876.700 0.33715705 0.33679185 0.11427638 0.33896538 -0.22408790E-03 -0.18054078E-04 15221.000 12879.500 0.33640775 0.33613192 0.11366014 0.33826946 -0.30853279E-03 -0.76979571E-05 15197.000 12882.300 0.33542927 0.33547338 0.11304391 0.33757384 -0.26719646E-03 0.14846001E-04 15122.000 12885.100 0.33491145 0.33481624 0.11242767 0.33687852 -0.22539518E-03 0.15293327E-04 15096.000 12888.000 0.33414452 0.33413712 0.11178943 0.33615869 -0.18002450E-03 -0.18197962E-04 15053.000 12890.800 0.33388531 0.33348285 0.11117319 0.33546399 -0.32912357E-03 -0.28437877E-04 15010.000 12893.600 0.33230142 0.33283002 0.11055695 0.33476959 -0.33927661E-03 0.28490192E-04 14973.000 12896.400 0.33198536 0.33217862 0.10994072 0.33407549 -0.16957849E-03 0.14966986E-04 14939.000 12899.300 0.33133483 0.33150549 0.10930247 0.33335692 -0.25396479E-03 -0.17325093E-04 14887.500 12902.100 0.33053776 0.33085704 0.10868624 0.33266343 -0.26833152E-03 -0.86900781E-05 14848.500 12904.900 0.32983217 0.33021006 0.10807000 0.33197024 -0.30262923E-03 0.84059222E-05 14797.000 12907.800 0.32881278 0.32954152 0.10743176 0.33125262 -0.22041777E-03 0.51839216E-04 14759.000 12910.600 0.32857579 0.32889754 0.10681552 0.33056005 -0.71456991E-05 0.25992508E-04 14718.000 12913.400 0.32877276 0.32825506 0.10619928 0.32986777 -0.74859721E-04 -0.50641993E-04 14682.000 12916.300 0.32814909 0.32759120 0.10556104 0.32915110 -0.29580506E-03 -0.16515099E-04 14630.500 12919.100 0.32708667 0.32695174 0.10494480 0.32845944 -0.16899578E-03 0.20774250E-04 14590.000 12921.900 0.32720271 0.32631371 0.10432857 0.32776808 -0.17946926E-03 -0.23608566E-04 14548.000 12924.800 0.32606370 0.32565434 0.10369032 0.32705235 -0.30356461E-03 -0.11880773E-04 14506.500 12927.600 0.32547239 0.32501904 0.10307409 0.32636161 -0.24718967E-03 0.27759050E-05 14464.000 12930.500 0.32465472 0.32436239 0.10243584 0.32564651 -0.28774195E-03 -0.82301831E-05 14433.500 12933.300 0.32383226 0.32372961 0.10181961 0.32495638 -0.29410171E-03 0.23435953E-04 14385.000 12936.200 0.32297834 0.32307544 0.10118136 0.32424192 -0.15415701E-03 0.74075497E-05 14337.500 12939.000 0.32295357 0.32244495 0.10056513 0.32355240 -0.25187868E-03 -0.35029002E-04 14458.000 12941.900 0.32154263 0.32179303 0.99926882E-01 0.32283858 -0.35382233E-03 0.27611596E-05 14299.000 12944.700 0.32093678 0.32116461 0.99310645E-01 0.32214968 -0.23614007E-03 0.79226105E-05 14229.000 12947.600 0.32019663 0.32051472 0.98672401E-01 0.32143649 -0.30866345E-03 0.70118244E-06 14198.500 12950.400 0.31917740 0.31988813 0.98056165E-01 0.32074819 -0.23214333E-03 0.23750784E-04 14134.500 12953.300 0.31887341 0.31924003 0.97417920E-01 0.32003564 -0.17328398E-03 -0.42211144E-05 14091.000 12956.100 0.31818968 0.31861506 0.96801684E-01 0.31934796 -0.25620368E-03 -0.24705085E-04 14058.000 12959.000 0.31741305 0.31796852 0.96163440E-01 0.31863604 -0.31410297E-03 -0.97062450E-05 14010.000 12961.800 0.31639929 0.31734495 0.95547203E-01 0.31794898 -0.31152928E-03 0.20077035E-04 13961.500 12964.700 0.31563734 0.31669973 0.94908959E-01 0.31723769 -0.19966387E-03 0.21902676E-04 13925.500 12967.600 0.31524124 0.31605511 0.94270714E-01 0.31652673 -0.18449376E-03 -0.14794884E-04 13896.000 12970.400 0.31458572 0.31543321 0.93654478E-01 0.31584059 -0.28399471E-03 -0.33593065E-05 13859.500 12973.300 0.31362247 0.31478956 0.93016234E-01 0.31513027 -0.20364180E-03 0.13816081E-04 13801.000 12976.200 0.31340460 0.31414632 0.92377989E-01 0.31442026 -0.20386144E-03 -0.29719160E-04 13772.000 12979.000 0.31246046 0.31352559 0.91761753E-01 0.31373505 -0.37304101E-03 0.33781706E-04 13718.000 12981.900 0.31127826 0.31288298 0.91123509E-01 0.31302568 -0.11305715E-04 0.79254964E-04 13603.500 12984.800 0.31239489 0.31224060 0.90485264E-01 0.31231664 0.86637780E-04 -0.36943412E-04 13692.500 12987.600 0.31177210 0.31162053 0.89869028E-01 0.31163235 -0.22188317E-03 -0.40406470E-04 13615.000 12990.500 0.31113016 0.31097843 0.89230783E-01 0.31092394 -0.14367910E-03 -0.13467331E-04 13616.500 12993.400 0.31093876 0.31033637 0.88592539E-01 0.31021585 -0.29999369E-03 -0.33601531E-04 13575.000 12996.200 0.30942019 0.30971645 0.87976303E-01 0.30953249 -0.33520783E-03 0.14835775E-04 13543.500 12999.100 0.30902808 0.30907433 0.87338058E-01 0.30882504 -0.21542977E-03 0.16143661E-04 13505.500 13002.000 0.30817070 0.30843208 0.86699814E-01 0.30811791 -0.24157459E-03 0.19639206E-04 13456.500 13004.900 0.30762694 0.30778964 0.86061569E-01 0.30741110 -0.10152238E-03 0.41461452E-05 13414.500 13007.800 0.30758187 0.30714696 0.85423324E-01 0.30670462 -0.21752695E-03 -0.32016414E-04 13461.500 13010.600 0.30638704 0.30652615 0.84807088E-01 0.30602281 -0.28401593E-03 -0.47511319E-05 13377.500 13013.500 0.30596298 0.30588281 0.84168844E-01 0.30531696 -0.24460840E-03 0.58815174E-05 13298.500 13016.400 0.30496831 0.30523905 0.83530599E-01 0.30461143 -0.24990313E-03 0.14680320E-04 13269.000 13019.300 0.30451354 0.30459480 0.82892355E-01 0.30390623 -0.15946255E-03 0.16456757E-04 13225.000 13022.200 0.30404343 0.30395001 0.82254110E-01 0.30320136 -0.15445394E-03 -0.28168049E-06 13191.000 13025.100 0.30361771 0.30330462 0.81615866E-01 0.30249680 -0.16109629E-03 -0.19166202E-04 13161.000 13027.900 0.30312518 0.30268085 0.80999630E-01 0.30181685 -0.26370130E-03 0.14790403E-04 13131.500 13030.800 0.30211461 0.30203409 0.80361385E-01 0.30111293 -0.76790998E-04 0.24471646E-04 13125.000 13033.700 0.30267979 0.30138655 0.79723140E-01 0.30040933 -0.12176575E-03 -0.50811042E-04 13406.500 13036.600 0.30140837 0.30073817 0.79084896E-01 0.29970606 -0.37149504E-03 -0.23834772E-04 13013.000 13039.500 0.30052512 0.30008889 0.78446651E-01 0.29900311 -0.26000743E-03 0.26705807E-04 12974.500 13042.400 0.29990033 0.29943865 0.77808407E-01 0.29830048 -0.21660136E-03 0.14972416E-04 12947.500 13045.300 0.29926883 0.29878738 0.77170162E-01 0.29759818 -0.17316741E-03 -0.16411273E-05 12911.000 13048.200 0.29889596 0.29813503 0.76531918E-01 0.29689620 -0.22611990E-03 -0.14829653E-04 12874.500 13051.100 0.29795734 0.29748154 0.75893673E-01 0.29619454 -0.25917940E-03 -0.31695173E-05 12837.500 13054.000 0.29739272 0.29682685 0.75255429E-01 0.29549321 -0.24450310E-03 0.10961909E-04 12804.000 13056.900 0.29653922 0.29617090 0.74617184E-01 0.29479220 -0.19560033E-03 0.22186294E-04 12765.500 13059.800 0.29625823 0.29551362 0.73978940E-01 0.29409151 -0.11582260E-03 -0.79549874E-05 12733.000 13062.700 0.29586745 0.29485497 0.73340695E-01 0.29339114 -0.24173925E-03 -0.24197311E-04 12704.500 13065.600 0.29485615 0.29419487 0.72702450E-01 0.29269110 -0.25616700E-03 -0.10291164E-05 12669.500 13068.500 0.29438168 0.29353327 0.72064206E-01 0.29199138 -0.24770813E-03 -0.49471055E-05 12640.000 13071.400 0.29341944 0.29287010 0.71425961E-01 0.29129199 -0.28486021E-03 0.53304952E-05 12597.000 13074.300 0.29272949 0.29220532 0.70787717E-01 0.29059291 -0.21679126E-03 0.25304207E-04 12559.500 13077.200 0.29216205 0.29153885 0.70149472E-01 0.28989417 -0.13809581E-03 0.94598390E-05 12543.000 13080.200 0.29191473 0.29084757 0.69489219E-01 0.28917166 -0.16097821E-03 -0.21635967E-04 12564.000 13083.100 0.29121228 0.29017749 0.68850975E-01 0.28847357 -0.26574802E-03 -0.12919894E-04 12457.500 13086.000 0.29037339 0.28950555 0.68212730E-01 0.28777580 -0.23591359E-03 0.89615880E-05 12427.000 13088.900 0.28984398 0.28883169 0.67574486E-01 0.28707835 -0.21377081E-03 -0.10551446E-04 12379.000 13091.800 0.28913352 0.28815584 0.66936241E-01 0.28638123 -0.29711198E-03 -0.10161045E-04 12341.500 13094.700 0.28812073 0.28747795 0.66297997E-01 0.28568443 -0.27270487E-03 0.77878426E-05 12313.000 13097.700 0.28752456 0.28677446 0.65637744E-01 0.28496395 -0.25116371E-03 -0.36335073E-05 12273.000 13100.600 0.28663886 0.28609223 0.64999499E-01 0.28426780 -0.29414257E-03 -0.17400402E-04 12231.500 13103.500 0.28581853 0.28540776 0.64361255E-01 0.28357199 -0.35208604E-03 -0.27812150E-04 12205.500 13106.400 0.28459676 0.28472101 0.63723010E-01 0.28287649 -0.45545304E-03 -0.24420536E-05 12168.000 13109.400 0.28313136 0.28400811 0.63062757E-01 0.28215735 -0.36649416E-03 0.41565670E-04 12117.000 13112.300 0.28243445 0.28331653 0.62424512E-01 0.28146251 -0.21021558E-03 0.24643564E-04 12088.000 13115.200 0.28191211 0.28262247 0.61786268E-01 0.28076800 -0.22356148E-03 -0.17902968E-04 12056.500 13118.100 0.28113779 0.28192589 0.61148023E-01 0.28007381 -0.31405280E-03 -0.63479954E-05 12022.000 13121.100 0.28005920 0.28120256 0.60487770E-01 0.27935602 -0.26101466E-03 0.14041558E-04 11992.500 13124.000 0.27959781 0.28050064 0.59849526E-01 0.27866248 -0.23120760E-03 0.26050246E-06 11962.500 13126.900 0.27871819 0.27979602 0.59211281E-01 0.27796927 -0.25950374E-03 -0.39482526E-05 11931.500 13129.900 0.27806673 0.27906418 0.58551028E-01 0.27725250 -0.25450229E-03 -0.23601424E-05 11947.500 13132.800 0.27721663 0.27835386 0.57912784E-01 0.27655994 -0.27342858E-03 0.83217353E-05 11859.500 13135.700 0.27648085 0.27764064 0.57274539E-01 0.27586771 -0.20623623E-03 0.89164271E-05 11831.000 13138.700 0.27599983 0.27689972 0.56614286E-01 0.27515195 -0.22082166E-03 -0.10396374E-04 11795.000 13141.600 0.27517800 0.27618043 0.55976042E-01 0.27446038 -0.26757483E-03 0.71402735E-05 11757.000 13144.600 0.27442114 0.27543310 0.55315789E-01 0.27374530 -0.17869405E-03 0.13572646E-04 11731.000 13147.500 0.27412371 0.27470749 0.54677544E-01 0.27305438 -0.18749622E-03 -0.16767066E-04 11679.500 13150.500 0.27331492 0.27395350 0.54017291E-01 0.27233998 -0.27761974E-03 0.25055280E-05 11651.000 13153.400 0.27248575 0.27322133 0.53379047E-01 0.27164972 -0.17271361E-03 0.45122306E-05 11642.000 13156.400 0.27229590 0.27246041 0.52718794E-01 0.27093600 -0.25099758E-03 -0.16813135E-04 11615.500 13159.300 0.27100486 0.27172142 0.52080549E-01 0.27024640 -0.27191111E-03 0.19426335E-04 11581.500 13162.300 0.27069163 0.27095332 0.51420296E-01 0.26953336 -0.13638220E-03 -0.10299738E-05 11551.000 13165.200 0.27020021 0.27020726 0.50782052E-01 0.26884441 -0.27798795E-03 -0.49364645E-04 11516.500 13168.200 0.26905150 0.26943173 0.50121799E-01 0.26813205 -0.42763361E-03 -0.13363908E-04 11491.500 13171.100 0.26767717 0.26867836 0.49483554E-01 0.26744377 -0.35683501E-03 0.23116535E-04 11453.500 13174.100 0.26694617 0.26789514 0.48823301E-01 0.26673209 -0.29124605E-03 0.25926068E-04 11427.500 13177.000 0.26595882 0.26713421 0.48185057E-01 0.26604446 -0.20387120E-03 0.15515571E-04 11396.000 13180.000 0.26574333 0.26634303 0.47524804E-01 0.26533346 -0.19970418E-03 -0.75777725E-05 11365.500 13182.900 0.26478056 0.26557429 0.46886559E-01 0.26464649 -0.24858006E-03 0.86048467E-05 11328.500 13185.900 0.26427671 0.26477490 0.46226306E-01 0.26393617 -0.14893559E-03 0.85243026E-05 11300.000 13188.900 0.26388695 0.26397125 0.45566053E-01 0.26322619 -0.19743425E-03 -0.23530785E-04 11265.000 13191.800 0.26311185 0.26319025 0.44927809E-01 0.26254021 -0.28776722E-03 -0.18912349E-04 11227.000 13194.800 0.26218912 0.26237800 0.44267556E-01 0.26183092 -0.30901710E-03 0.54934156E-05 11190.000 13197.800 0.26125775 0.26156128 0.43607303E-01 0.26112197 -0.25480673E-03 0.23426100E-04 11164.000 13200.700 0.26068576 0.26076747 0.42969058E-01 0.26043698 -0.17080311E-03 0.18452868E-04 11137.500 13203.700 0.26025001 0.25994177 0.42308805E-01 0.25972871 -0.14593481E-03 -0.27620633E-05 11108.000 13206.700 0.25981015 0.25911140 0.41648552E-01 0.25902079 -0.18737549E-03 0.12479239E-04 11089.500 13209.600 0.25914449 0.25830421 0.41010308E-01 0.25833679 -0.72307296E-04 0.14429124E-04 11057.500 13212.600 0.25938354 0.25746447 0.40350055E-01 0.25762955 -0.10224366E-03 -0.22017208E-04 11024.500 13215.600 0.25853103 0.25661986 0.39689802E-01 0.25692266 -0.20441055E-03 -0.15239003E-04 10990.500 13218.600 0.25815708 0.25577033 0.39029549E-01 0.25621610 -0.19367768E-03 -0.31789697E-05 10960.500 13221.500 0.25738833 0.25494436 0.38391304E-01 0.25553343 -0.22316647E-03 -0.75992043E-05 10927.500 13224.500 0.25684040 0.25408494 0.37731051E-01 0.25482756 -0.23851299E-03 0.75517963E-04 10906.000 13225.400 0.25645813 0.25382611 0.37532975E-01 0.25461587 0.71353586E-04 0.75816135E-04 10865.000 13226.400 0.25697597 0.25353799 0.37312891E-01 0.25438069 -0.94462330E-04 -0.24562350E-03 10848.000 13227.300 0.25627865 0.25327819 0.37114815E-01 0.25416906 -0.39533105E-03 -0.31177944E-03 10838.500 13228.200 0.25626437 0.25301792 0.36916739E-01 0.25395747 -0.65566532E-03 -0.31944425E-03 10739.500 13229.100 0.25509846 0.25275718 0.36718663E-01 0.25374590 -0.97033071E-03 0.27457832E-03 10560.500 13230.000 0.25451778 0.25249597 0.36520587E-01 0.25353436 -0.16142435E-03 0.82409641E-03 10550.500 13230.900 0.25480789 0.25223428 0.36322512E-01 0.25332286 0.51304282E-03 0.18156745E-03 10515.500 13231.900 0.25549256 0.25549256 0.36102427E-01 0.25308789 0.18355381E-03 -0.42259679E-03 10508.500 13232.800 0.25515664 0.25515664 0.35904351E-01 0.25287646 -0.28989107E-03 -0.76749493E-04 10494.000 13233.700 0.25497075 0.25497075 0.35706275E-01 0.25266505 0.45404722E-04 0.17451960E-03 10478.500 13234.600 0.25523837 0.25523837 0.35508200E-01 0.25245367 0.24244197E-04 -0.25159969E-03 10440.000 13235.500 0.25501439 0.25501439 0.35310124E-01 0.25224233 -0.40747473E-03 -0.33657625E-03 10432.500 13236.500 0.25446417 0.25446417 0.35090039E-01 0.25200754 -0.61525067E-03 0.12442422E-03 10434.500 13237.400 0.25384542 0.25384542 0.34891963E-01 0.25179626 -0.17106871E-03 0.49551822E-03 10410.000 13238.300 0.25415625 0.25415625 0.34693888E-01 0.25158501 0.27668213E-03 0.20484199E-03 10405.500 13239.200 0.25434345 0.25434345 0.34495812E-01 0.25137379 0.19764687E-03 -0.40367140E-03 10401.000 13240.100 0.25451201 0.25451201 0.34297736E-01 0.25116261 -0.44992639E-03 -0.37464695E-03 10390.500 13241.000 0.25353358 0.25353358 0.34099660E-01 0.25095146 -0.47671764E-03 0.26466739E-03 10356.500 13242.000 0.25360625 0.25360625 0.33879576E-01 0.25071688 0.52941650E-04 0.13823334E-03 10340.500 13242.900 0.25363417 0.25363417 0.33681500E-01 0.25050579 -0.21407430E-03 -0.22098880E-03 10339.500 13243.800 0.25322091 0.25322091 0.33483424E-01 0.25029473 -0.34483818E-03 0.10016671E-03 10365.500 13244.700 0.25301346 0.25301346 0.33285348E-01 0.25008370 -0.33774231E-04 0.22480009E-03 10283.500 13245.600 0.25316012 0.25316012 0.33087272E-01 0.24987271 0.59801988E-04 0.49582456E-05 10280.500 13246.600 0.25312708 0.25312708 0.32867188E-01 0.24963830 -0.24353564E-04 -0.14427754E-03 10270.500 13247.500 0.25311385 0.25311385 0.32669112E-01 0.24942738 -0.21432535E-03 -0.77918981E-04 10266.500 13248.400 0.25274130 0.25274130 0.32471036E-01 0.24921648 -0.16460773E-03 0.63618131E-04 10239.500 13249.300 0.25281756 0.25281756 0.32272960E-01 0.24900561 -0.99812711E-04 -0.24303979E-04 10243.500 13250.200 0.25256163 0.25256163 0.32074884E-01 0.24879477 -0.20835489E-03 -0.92291938E-04 10223.500 13251.200 0.25242168 0.25242168 0.31854800E-01 0.24856055 -0.27516739E-03 -0.76049838E-04 10224.000 13252.100 0.25203882 0.25203882 0.31656724E-01 0.24834978 -0.35284958E-03 0.31908668E-03 10199.500 13253.000 0.25178655 0.25178655 0.31458648E-01 0.24813904 0.29918863E-03 0.35454111E-03 10199.500 13253.900 0.25257736 0.25257736 0.31260572E-01 0.24792833 0.28532442E-03 -0.11156368E-03 10209.500 13254.800 0.25230014 0.25230014 0.31062496E-01 0.24771765 0.98374002E-04 0.71588003E-04 10179.000 13255.800 0.25276427 0.25276427 0.30842412E-01 0.24748360 0.42134163E-03 0.24850429E-04 10176.000 13256.700 0.25310068 0.25310068 0.30644336E-01 0.24727299 0.14558982E-03 -0.11485104E-03 10182.000 13257.600 0.25302633 0.25302633 0.30446260E-01 0.24706241 0.21460976E-03 0.84546663E-04 10164.500 13258.500 0.25348698 0.25348698 0.30248184E-01 0.24685186 0.29777381E-03 -0.25029548E-04 10150.500 13259.500 0.25359210 0.25359210 0.30028100E-01 0.24661795 0.16705362E-03 0.56964285E-04 10153.500 13260.400 0.25380438 0.25380438 0.29830024E-01 0.24640747 0.40600595E-03 0.33879066E-03 10150.500 13261.300 0.25432291 0.25432291 0.29631948E-01 0.24619702 0.77687681E-03 0.21160728E-03 10139.000 13262.200 0.25520276 0.25520276 0.29433872E-01 0.24598660 0.78689906E-03 0.16644014E-03 10130.500 13263.100 0.25573933 0.25573933 0.29235796E-01 0.24577621 0.10764691E-02 0.43493425E-03 10134.000 13264.100 0.25724805 0.25724805 0.29015712E-01 0.24554248 0.16132741E-02 0.63414784E-03 10110.500 13265.000 0.25880455 0.25880455 0.28817636E-01 0.24533215 0.22813500E-02 0.20516613E-03 10112.000 13265.900 0.26135448 0.26135448 0.28619560E-01 0.24512186 0.19825732E-02 0.24781100E-03 10106.000 13266.800 0.26237318 0.26237318 0.28421484E-01 0.24491160 0.27274098E-02 0.12838959E-02 10095.500 13267.800 0.26653656 0.26653656 0.28201400E-01 0.24467801 0.44219754E-02 0.15348451E-02 10073.000 13268.700 0.27077493 0.27077493 0.28003324E-01 0.24446781 0.56436155E-02 0.20373906E-02 10064.000 13269.600 0.27669507 0.27669507 0.27805248E-01 0.24425765 0.80892784E-02 0.36275716E-02 10056.500 13270.500 0.28533563 0.28533563 0.27607172E-01 0.24404751 0.12173244E-01 0.51797704E-02 10046.000 13271.400 0.29860691 0.29860691 0.27409096E-01 0.24383741 0.17412865E-01 0.65289397E-02 10038.000 13272.400 0.31842008 0.31842008 0.27189012E-01 0.24360400 0.24578230E-01 0.78160574E-02 10028.500 13273.300 0.34530555 0.34530555 0.26990936E-01 0.24339396 0.32263374E-01 0.60569984E-02 10020.000 13274.200 0.37649415 0.37649415 0.26792860E-01 0.24318396 0.35480827E-01 -0.29581325E-02 9995.0000 13275.100 0.40917104 0.40917104 0.26594784E-01 0.24297398 0.26938736E-01 -0.14588830E-01 9989.0000 13276.100 0.42767775 0.42767775 0.26374700E-01 0.24274071 0.77620507E-02 -0.21612688E-01 9955.5000 13277.000 0.42391893 0.42391893 0.26176624E-01 0.24253080 -0.14125371E-01 -0.19104731E-01 9951.0000 13277.900 0.40225208 0.40225208 0.25978548E-01 0.24232092 -0.26626466E-01 -0.74528253E-02 9959.0000 13278.800 0.37599129 0.37599129 0.25780472E-01 0.24211108 -0.27540457E-01 0.26378312E-02 9939.0000 13279.800 0.34992521 0.34992521 0.25560388E-01 0.24187795 -0.21614586E-01 0.68679415E-02 9924.5000 13280.700 0.33492358 0.33492358 0.25362312E-01 0.24166817 -0.14491368E-01 0.61865898E-02 9923.5000 13281.600 0.32384075 0.32384075 0.25164236E-01 0.24145842 -0.10478725E-01 0.50464932E-02 9918.5000 13282.500 0.31606188 0.31606188 0.24966160E-01 0.24124870 -0.54076800E-02 0.43830311E-02 9902.0000 13283.500 0.31356616 0.31356616 0.24746076E-01 0.24101571 -0.21509656E-02 0.22662185E-02 9904.0000 13284.400 0.31197504 0.31197504 0.24548000E-01 0.24080606 -0.11018649E-02 0.15249080E-02 9898.5000 13285.300 0.31158280 0.31158280 0.24349924E-01 0.24059644 0.59386889E-03 0.18822390E-02 9875.5000 13286.200 0.31304401 0.31304401 0.24151848E-01 0.24038685 0.22861654E-02 0.13082564E-02 9879.0000 13287.200 0.31592652 0.31592652 0.23931764E-01 0.24015400 0.30795561E-02 0.73901080E-03 9865.0000 13288.100 0.31889516 0.31889516 0.23733688E-01 0.23994448 0.36902859E-02 0.67345534E-03 9856.5000 13289.000 0.32256903 0.32256903 0.23535612E-01 0.23973498 0.42917757E-02 -0.18930263E-03 9855.5000 13289.900 0.32662036 0.32662036 0.23337536E-01 0.23952552 0.33495412E-02 -0.11545627E-02 9856.0000 13290.900 0.32893316 0.32893316 0.23117452E-01 0.23929282 0.20981066E-02 -0.90297105E-03 9842.0000 13291.800 0.33060676 0.33060676 0.22919376E-01 0.23908342 0.16338962E-02 -0.14864992E-03 9839.0000 13292.700 0.33187417 0.33187417 0.22721300E-01 0.23887405 0.18305368E-02 0.30128590E-03 9825.0000 13293.700 0.33408478 0.33408478 0.22501216E-01 0.23864146 0.22063394E-02 0.46786552E-03 9823.0000 13294.600 0.33606622 0.33606622 0.22303140E-01 0.23843216 0.27194813E-02 0.98016710E-03 9800.5000 13295.500 0.33897985 0.33897985 0.22105064E-01 0.23822289 0.39706401E-02 0.96729279E-03 9790.5000 13296.400 0.34321337 0.34321337 0.21906988E-01 0.23801365 0.44606083E-02 -0.33465250E-03 9782.0000 13297.400 0.34745500 0.34745500 0.21686904E-01 0.23778120 0.33348004E-02 -0.10444926E-02 9770.5000 13298.300 0.34954949 0.34954949 0.21488828E-01 0.23757203 0.24760724E-02 -0.74869939E-03 9769.0000 13299.200 0.35191193 0.35191193 0.21290752E-01 0.23736289 0.19871415E-02 -0.98101979E-03 9739.5000 13300.100 0.35312634 0.35312634 0.21092676E-01 0.23715378 0.71023676E-03 -0.20929307E-02 9725.0000 13301.100 0.35326138 0.35326138 0.20872592E-01 0.23692147 -0.19894268E-02 -0.15358023E-02 9713.5000 13302.000 0.34934643 0.34934643 0.20674516E-01 0.23671242 -0.22077875E-02 0.13309188E-02 9711.0000 13302.900 0.34928736 0.34928736 0.20476440E-01 0.23650341 0.40622708E-03 0.15850057E-02 9700.5000 13303.900 0.35011827 0.35011827 0.20256356E-01 0.23627121 0.80372323E-03 0.82595098E-04 9696.5000 13304.800 0.35081444 0.35081444 0.20058280E-01 0.23606226 0.56315776E-03 0.16321428E-03 9685.5000 13305.700 0.35113195 0.35113195 0.19860204E-01 0.23585334 0.10975089E-02 0.19619418E-02 9676.5000 13306.600 0.35278996 0.35278996 0.19662128E-01 0.23564446 0.40946531E-02 0.15889693E-02 9670.5000 13307.600 0.35891179 0.35891179 0.19442044E-01 0.23541240 0.41165506E-02 -0.11063811E-02 9622.5000 13308.500 0.36061140 0.36061140 0.19243968E-01 0.23520358 0.19925290E-02 -0.13228049E-02 9636.0000 13309.400 0.36249834 0.36249834 0.19045892E-01 0.23499479 0.17355018E-02 -0.41213763E-03 9607.5000 13310.400 0.36390885 0.36390885 0.18825808E-01 0.23476284 0.12094675E-02 -0.28852448E-03 9622.5000 13311.300 0.36479633 0.36479633 0.18627732E-01 0.23455411 0.11873053E-02 0.10811534E-03 9608.0000 13312.200 0.36604600 0.36604600 0.18429656E-01 0.23434542 0.14040752E-02 0.31617318E-03 9595.5000 13313.100 0.36732367 0.36732367 0.18231580E-01 0.23413676 0.17564170E-02 0.53777495E-03 9582.5000 13314.100 0.36938320 0.36938320 0.18011496E-01 0.23390495 0.24258476E-02 0.46230053E-03 9582.0000 13315.000 0.37193278 0.37193278 0.17813420E-01 0.23369636 0.26347880E-02 0.40570225E-03 9576.0000 13315.900 0.37412582 0.37412582 0.17615344E-01 0.23348779 0.31561116E-02 -0.86410454E-04 9558.5000 13316.900 0.37792939 0.37792939 0.17395260E-01 0.23325609 0.24706082E-02 -0.64070075E-03 10138.500 13317.800 0.37881997 0.37881997 0.17197184E-01 0.23304759 0.19387802E-02 -0.98186283E-04 9565.5000 13318.700 0.38141919 0.38141919 0.16999108E-01 0.23283912 0.22938729E-02 -0.10643656E-03 9545.0000 13319.700 0.38317833 0.38317833 0.16779023E-01 0.23260753 0.17365507E-02 -0.61278747E-03 9531.0000 13320.600 0.38471864 0.38471864 0.16580948E-01 0.23239913 0.11295767E-02 -0.80694314E-03 9531.0000 13321.500 0.38521157 0.38521157 0.16382872E-01 0.23219076 0.28405306E-03 -0.86565355E-03 9521.0000 13322.400 0.38522993 0.38522993 0.16184796E-01 0.23198242 -0.42859972E-03 -0.10912411E-02 9517.5000 13323.400 0.38439723 0.38439723 0.15964711E-01 0.23175097 -0.17893051E-02 -0.64018731E-03 9501.5000 13325.700 0.37932523 0.37932523 0.15458517E-01 0.23121877 -0.25412178E-02 -0.21553708E-03 9498.0000 13328.000 0.37270763 0.37270763 0.14952324E-01 0.23068678 -0.27807756E-02 -0.33434414E-04 9476.0000 13330.400 0.36625558 0.36625558 0.14424121E-01 0.23013188 -0.26983596E-02 0.40240976E-04 9454.0000 13332.700 0.36002534 0.36002534 0.13917927E-01 0.22960030 -0.25916430E-02 0.14468520E-03 9439.0000 13335.000 0.35433402 0.35433402 0.13411733E-01 0.22906893 -0.20328077E-02 0.26733704E-03 9417.5000 13337.400 0.35047114 0.35047114 0.12883531E-01 0.22851467 -0.13351589E-02 0.28676760E-03 9389.0000 13339.700 0.34805878 0.34805878 0.12377337E-01 0.22798372 -0.68499993E-03 0.29412985E-03 9377.0000 13342.000 0.34732014 0.34732014 0.11871143E-01 0.22745297 0.17838391E-04 0.21865942E-03 9363.0000 13344.400 0.34814262 0.34814262 0.11342941E-01 0.22689935 0.34269936E-03 0.13535874E-03 9344.5000