Am 19.06.2009 um 16:44 schrieb Zajac, Dariusz A.:

Hi Scott,
I am afraid that E0 jumps over the edge - see bmp's in the attachment
(files with enot_12 means E0=12...). Hovewer 12 eV is still less than
k=3 (the starting k value). Can it influence? I did also once more fit
with R from 1.7 to 4A. Fits of first 2 peaks are identical - you can see
in the attachment too...
I hope you and anyone from the mailing list don't mind that I am
attaching so many files...

cheers
darek

-----Original Message-----
From: ifeffit-bounces@millenia.cars.aps.anl.gov
[mailto:ifeffit-bounces@millenia.cars.aps.anl.gov] On Behalf
Of Scott Calvin
Sent: Friday, June 19, 2009 2:49 PM
To: XAFS Analysis using Ifeffit
Subject: Re: [Ifeffit] problem with E0 (enot) parameters


Hi Darek,

OK, so if the K, H, and O don't affect the fit much for the C and N,  
and the K, H, and O are returning nonsensical values, then a logical  
possibility is that the E0's for C and N are correct. If you
add 12 eV  
to the E0 you chose in Athena, where in the spectrum does it fall? Is  
it still before the white line? If so, it seems to me you
don't have a  
problem. If not, then we have to ponder further.

--Scott Calvin
Sarah Lawrence College

On Jun 19, 2009, at 8:28 AM, Zajac, Dariusz A. wrote:

Hi Scott,
look also at H and O,
but for me and for this fit important are only W-C and W-C-N
bondings.
This sample is an reference sample for other cyano-brigded networks.
So
you suggest to focuse on K ions? how can it help with first
2 peaks? K
is at ~5A.
I have analysed in larger R space only to see how the
spectrum behave.
contribution from K, O etc. at k highers than 5A is for me too low to
analyse it resonable for such compound.
I have attached in the previus post the last version of results.  
Anyway,
enots for C and N do not change if I am enlarging R region (when I am
including next paths, also for K).
about material I am quite sure ;) and crystal structure is from
literature

in the attachment you will find bmp file of the fit: data, fit, bkg
and
K path.
fitting ranges k(3-15) R(1.7-6) dk 2 dr 0.5, phase correction -  
first C

cheers
darek


_______________________________________________
Ifeffit mailing list
Ifeffit@millenia.cars.aps.anl.gov
http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit

<K4W(CN)8_enot_12.bmp><K4W(CN)8_enot_0.bmp><K4WCN8_b.apj><K4W(CN)8_2.bmp><K4W(CN)8_2q.bmp><mime-attachment.txt>

--
Dr. Stefan Mangold
Institut für Synchrotronstrahlung
Forschungszentrum Karlsruhe
Tel.: +49-7247-826073