Hello again, I have a follow up question about handling air sensitive sample. Some of you mentioned vacuum sealing like which used for food, this reminds me a aluminized mylar bags. Does anyone know a good source to get thine aluminized mylar
ZjQcmQRYFpfptBannerStart
This Message Is From an External Sender
This message came from outside your organization.
 
ZjQcmQRYFpfptBannerEnd
Hello again,
I have a follow up question about handling air sensitive sample. Some of you mentioned vacuum sealing like which used for food, this reminds me a aluminized mylar bags. Does anyone know a good source to get thine aluminized mylar bags. It seems that the standard thickness is about 0.1mm, just wondering if there is a well known source who makes bags thinner than that.
Thank you!

Best,
Helen

Mike Massey <mmassey@gmail.com> 於 2025年3月22日 週六 下午12:42寫道:
You can also use a cryostat with only vacuum and no cooling, if desired. Good luck! Mike On Mar 23, 2025, at 08: 16, Carlo Segre via Ifeffit <ifeffit@ millenia. cars. aps. anl. gov> wrote:  Hi Helen, We have had luck using a vacuum sealing
ZjQcmQRYFpfptBannerStart
This Message Is From an Untrusted Sender
You have not previously corresponded with this sender.
See https://itconnect.uw.edu/email-tags for additional information. Please contact the UW-IT Service Center, help@uw.edu 206.221.5000, for assistance.
 
ZjQcmQRYFpfptBannerEnd
You can also use a cryostat with only vacuum and no cooling, if desired.


Good luck!


Mike





On Mar 23, 2025, at 08:16, Carlo Segre via Ifeffit <ifeffit@millenia.cars.aps.anl.gov> wrote:


Hi Helen, We have had luck using a vacuum sealing system such as used for food. However the Polyethylene is subject to degradation under the beam so that wrapping with Kapton is helpful as well as double bagging it. Finally, if you keep it under
ZjQcmQRYFpfptBannerStart
This Message Is From an External Sender
This message came from outside your organization.
 
ZjQcmQRYFpfptBannerEnd
Hi Helen,

We have had luck using a vacuum sealing system such as used for food.  However the Polyethylene is subject to degradation under the beam so that wrapping with Kapton is helpful as well as double bagging it.  Finally, if you keep it under Argon when transporting it to the beamline and then in a helium filled chamber, you should avoid the oxidation.

Carlo


--
Carlo Segre, Duchossois Professor of Physics
Illinois Institute of Technology

From: Helen Chen via Ifeffit <ifeffit@millenia.cars.aps.anl.gov>
Sent: Tuesday, March 18, 2025 8:05 PM
To: ifeffit@millenia.cars.aps.anl.gov <ifeffit@millenia.cars.aps.anl.gov>
Cc: Helen Chen <helen86@uw.edu>
Subject: [Ext][Ifeffit] Question about Air sensitive sample holder
 
Hello, Our group (Jerry Seidler) just started a project involving doing VTC and HERFD on Yb doped CrX3 material. They are thin small crystal sheets and are very air sensitive. We have tried encapsulated them between a layer of laptop tape and
ZjQcmQRYFpfptBannerStart
This Message Is From an External Sender
This message came from outside your organization.
 
ZjQcmQRYFpfptBannerEnd
Hello,
Our group (Jerry Seidler) just started a project involving doing VTC and HERFD on Yb doped CrX3 material. They are thin small crystal sheets and are very air sensitive. We have tried encapsulated them between a layer of laptop tape and film, but after 12hr we see degradation due to air leaks. I am looking for some advice on air sensitive sample holder. What are some typical methods you use to deal with air sensitivity, especially for samples in thin sheets geometry?
Thank you

ifeffit mailing list:  https://millenia.cars.aps.anl.gov/mailman3/lists/ifeffit.millenia.cars.aps.anl.gov/
to unsubscribe, send mail to ifeffit-leave@millenia.cars.aps.anl.gov