i think you shoud first determine the accurate debyewaller factor the the cn number.

发自我的华为手机


-------- 原始邮件 --------
主题:Re: [Ifeffit] Making N (coordination number) a variable.
发件人:Anatoly Frenkel
收件人:XAFS Analysis using Ifeffit
抄送:


Make it 1 in the N window and make amp*N expression in the S02 window instead. Then use N as a coordination number (fix or vary it).
Anatoly

-------------------------------------------------------------------
Anatoly I. Frenkel
Professor
Department of Materials Science and Chemical Engineering
Stony Brook University
Stony Brook, NY 11794,
Ph: 631-632-2751
Email:  anatoly.frenkel@stonybrook.edu

Joint Appointment:
Chemistry Department, Brookhaven National Laboratory
Upton, NY 11973. Ph: 631-344-3013. Group: 631-344-3494
Email: frenkel@bnl.gov

https://www.bnl.gov/chemistry/bio/FrenkelAnatoly.asp

Spokesperson, Synchrotron Catalysis Consortium (SCC) at BNL
http://you.stonybrook.edu/scc2
-------------------------------------------------------------------

On Wed, Aug 1, 2018 at 11:07 AM, M Solo <sarsol89@gmail.com> wrote:
Hello
Is there a way in artemis to make N, coordination number, a variable to be used in GDS window? I do realize that N and ss are closely linked and do very similar things in the fit, but it seems i may need fractional (average) coordination number for one of the paths, and am fine fixing ss to see where N levels off. 

Thank you very much.

Alex Solov

_______________________________________________
Ifeffit mailing list
Ifeffit@millenia.cars.aps.anl.gov
http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit