I guess the problem lies in the different "end line character" for Linux and Windows.

Before you load "dos style"(Windows use it) apj file, you should translate it into "Linux style".
It is easy in Linux system by using "dos2unix".

On 5/30/07, ifeffit-request@millenia.cars.aps.anl.gov <ifeffit-request@millenia.cars.aps.anl.gov> wrote:
Send Ifeffit mailing list submissions to
        ifeffit@millenia.cars.aps.anl.gov

To subscribe or unsubscribe via the World Wide Web, visit
         http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
or, via email, send a message with subject or body 'help' to
        ifeffit-request@millenia.cars.aps.anl.gov

You can reach the person managing the list at
        ifeffit-owner@millenia.cars.aps.anl.gov

When replying, please edit your Subject line so it is more specific
than "Re: Contents of Ifeffit digest..."


Today's Topics:

   1. Using windows apj files on linux (joshua jason kas)


----------------------------------------------------------------------

Message: 1
Date: Tue, 29 May 2007 10:13:06 -0700 (PDT)
From: joshua jason kas <hebhop@u.washington.edu>
Subject: [Ifeffit] Using windows apj files on linux
To: ifeffit@millenia.cars.aps.anl.gov
Message-ID:
        <Pine.LNX.4.64.0705290956010.21265@dante01.u.washington.edu >
Content-Type: text/plain; charset="us-ascii"

Hi,
I recently updated to redhat 4. I am running:
        artemis 0.8.009
        IFEFFIT 1.2.9
        Tk-804.027
        perl 5.8.5

I have an artemis project file that I
started on my win xp machine and would like to use on the linux machine.
When I open the apj file on linux, some of the information about the fits
seems to be scrambled. Here are some of the symptoms.

        1) The raw logs seem to have aquired the following
            escape character at the end of each line: \x{d}
           This shows up as a carriage return or end of line on this screen.

        2) Quick summary of selected fits gives 0 for all reported values
           (chisq, rfactor, nidp, etc) and does not report any guessed
            parameters.

Here is one of the quick summaries. Note that the \x{d} do not show up
here, but they do in the artemis message palette. I am also attatching the
project file.
Thanks for any help,
Josh Kas

Project title   : Fitting pt1_amine_165_he_573.chi

Comment         : fer dw, constant delr, ei=0, kw=1, kmin=2.0, rmin=1.2

Figure of merit : 17


Fitting statistics
   Number of independent points : 0
   Number of variables          : 0
   Chi-square                   : 0
   Reduced chi-square           : 0
   R-factor                     : 0
   Measurement uncertainty (k)  : 0
   Measurement uncertainty (R)  : 0

Guess parameters

=*==*==*==*==*==*==*==*==*==*==*==*==*==*==*==*==*==*==*==*=


-------------- next part --------------
A non-text attachment was scrubbed...
Name: ptTemp.apj
Type: application/zip
Size: 1634557 bytes
Desc:
Url : http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20070529/05efdf8d/attachment.zip

------------------------------

_______________________________________________
Ifeffit mailing list
Ifeffit@millenia.cars.aps.anl.gov
http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit


End of Ifeffit Digest, Vol 51, Issue 26
***************************************



--
Shanghai Institute of Applied Physics, Chinese Academy of Sciences
No. 2019, Baojia Road,
Jiading District, Shanghai,China 201800