# created: Tue May 16 20:37:57 2023 # from file: in2o3.0002 # No: 288 [E0: 0,0,0,-1] #--------------------------------------------------------------------- # X Y 2.7690399648E+001 4.2361659692E-001 2.7702051151E+001 4.2363261461E-001 2.7712867133E+001 4.2327793887E-001 2.7721153845E+001 4.2333304464E-001 2.7731138317E+001 4.2320226231E-001 2.7743501970E+001 4.2301494294E-001 2.7751976606E+001 4.2306020429E-001 2.7760795735E+001 4.2290210455E-001 2.7773695344E+001 4.2296610376E-001 2.7783208013E+001 4.2282584882E-001 2.7791196903E+001 4.2287617800E-001 2.7801572334E+001 4.2290905712E-001 2.7813317843E+001 4.2292985225E-001 2.7820642542E+001 4.2300891436E-001 2.7828823519E+001 4.2306760840E-001 2.7840421498E+001 4.2344763678E-001 2.7850321552E+001 4.2365012450E-001 2.7858690894E+001 4.2395824724E-001 2.7870313850E+001 4.2488408437E-001 2.7881604255E+001 4.2573013549E-001 2.7888965061E+001 4.2687346824E-001 2.7900613361E+001 4.2942088461E-001 2.7911928396E+001 4.3423921951E-001 2.7913472068E+001 4.3513216227E-001 2.7914501278E+001 4.3580031725E-001 2.7915702119E+001 4.3667448958E-001 2.7916731494E+001 4.3740395289E-001 2.7918104112E+001 4.3874645772E-001 2.7918962067E+001 4.3939572897E-001 2.7919991683E+001 4.4034500621E-001 2.7921021375E+001 4.4157106815E-001 2.7921879510E+001 4.4249140840E-001 2.7922909342E+001 4.4380995433E-001 2.7923939249E+001 4.4509808756E-001 2.7924797564E+001 4.4678954465E-001 2.7925827611E+001 4.4866265783E-001 2.7927029430E+001 4.5126007387E-001 2.7927887935E+001 4.5350203705E-001 2.7929089931E+001 4.5735639234E-001 2.7930292031E+001 4.6217387122E-001 2.7931837740E+001 4.6984653384E-001 2.7932868308E+001 4.7703655701E-001 2.7934586091E+001 4.9181463003E-001 2.7935616863E+001 5.0399503345E-001 2.7937334984E+001 5.2784996109E-001 2.7938537796E+001 5.5344159927E-001 2.7940428138E+001 6.0443847579E-001 2.7941631216E+001 6.4220056443E-001 2.7943521978E+001 7.0613177731E-001 2.7944897239E+001 7.5998532773E-001 2.7946100703E+001 8.0891478915E-001 2.7947304271E+001 8.4468408654E-001 2.7948679905E+001 8.7606077441E-001 2.7949711720E+001 8.8803665093E-001 2.7951259585E+001 8.8844847317E-001 2.7951947580E+001 8.8223255617E-001 2.7953151653E+001 8.6698650641E-001 2.7954011769E+001 8.5432624687E-001 2.7954871938E+001 8.3735270504E-001 2.7955560112E+001 8.2513370080E-001 2.7956248319E+001 8.1295881891E-001 2.7957108626E+001 8.0013497553E-001 2.7957796910E+001 7.8992894592E-001 2.7958657313E+001 7.8041318785E-001 2.7959517768E+001 7.7218483970E-001 2.7960550385E+001 7.6296653343E-001 2.7961755202E+001 7.5466171880E-001 2.7962960122E+001 7.4737906638E-001 2.7964337301E+001 7.3824373128E-001 2.7965714617E+001 7.3147796763E-001 2.7967264259E+001 7.2365552638E-001 2.7968814074E+001 7.1833414663E-001 2.7970191832E+001 7.1365844505E-001 2.7972086471E+001 7.1037722062E-001 2.7973464551E+001 7.0952372798E-001 2.7975359635E+001 7.1122176490E-001 2.7977427292E+001 7.1770125685E-001 2.7978805901E+001 7.2457518771E-001 2.7980356998E+001 7.3392495154E-001 2.7982253018E+001 7.4579224513E-001 2.7984321697E+001 7.6102572474E-001 2.7985700986E+001 7.6946065389E-001 2.7987252850E+001 7.7596776134E-001 2.7989149807E+001 7.8247486913E-001 2.7990529574E+001 7.8516779717E-001 2.7992426976E+001 7.8619545696E-001 2.7994324636E+001 7.8481806261E-001 2.7996395105E+001 7.8242753090E-001 2.7998983623E+001 7.8030621352E-001 2.8001227393E+001 7.8028749168E-001 2.8003644165E+001 7.8019488994E-001 2.8006061354E+001 7.8025980693E-001 2.8009169784E+001 7.7841678584E-001 2.8011587930E+001 7.7501737674E-001 2.8014524813E+001 7.6977837227E-001 2.8017289502E+001 7.6436992446E-001 2.8019190543E+001 7.5973665775E-001 2.8021264701E+001 7.5548605648E-001 2.8023166283E+001 7.5244531263E-001 2.8025068124E+001 7.4917157131E-001 2.8026797294E+001 7.4722391629E-001 2.8028872582E+001 7.4546200316E-001 2.8031813099E+001 7.4409073624E-001 2.8035273324E+001 7.4352968584E-001 2.8038907481E+001 7.4595971712E-001 2.8042023225E+001 7.4960321256E-001 2.8045312820E+001 7.5648584339E-001 2.8047910414E+001 7.6230418068E-001 2.8050854938E+001 7.6815398702E-001 2.8053453562E+001 7.7145108666E-001 2.8056225960E+001 7.7298193713E-001 2.8058478937E+001 7.7369788489E-001 2.8060905626E+001 7.7264484806E-001 2.8063506118E+001 7.7122358010E-001 2.8066453925E+001 7.6918306229E-001 2.8069575810E+001 7.6657842284E-001 2.8072698391E+001 7.6580653724E-001 2.8076342283E+001 7.6638519005E-001 2.8080160710E+001 7.6697893915E-001 2.8083632912E+001 7.6791311371E-001 2.8087279650E+001 7.6787186731E-001 2.8090058754E+001 7.6654405380E-001 2.8092490923E+001 7.6593325725E-001 2.8094923514E+001 7.6428482130E-001 2.8097008928E+001 7.6310003529E-001 2.8100137631E+001 7.6074153351E-001 2.8103962551E+001 7.5849226557E-001 2.8108310317E+001 7.5610047814E-001 2.8112137467E+001 7.5415280468E-001 2.8115791631E+001 7.5312911215E-001 2.8119620824E+001 7.5275609566E-001 2.8122928696E+001 7.5296365258E-001 2.8126411509E+001 7.5452779068E-001 2.8129546780E+001 7.5596728645E-001 2.8132856994E+001 7.5777765662E-001 2.8137213728E+001 7.6143103941E-001 2.8141397466E+001 7.6271757177E-001 2.8146105662E+001 7.6269931219E-001 2.8150815437E+001 7.6108093356E-001 2.8154828715E+001 7.5920921373E-001 2.8159017706E+001 7.5764427890E-001 2.8161811061E+001 7.5653355931E-001 2.8164779609E+001 7.5536079853E-001 2.8168447506E+001 7.5471583981E-001 2.8173689020E+001 7.5473490564E-001 2.8178932490E+001 7.5575432189E-001 2.8183828161E+001 7.5704828966E-001 2.8188025807E+001 7.5759306086E-001 2.8191874752E+001 7.5784702656E-001 2.8195724750E+001 7.5749708484E-001 2.8199050596E+001 7.5631802563E-001 2.8203252790E+001 7.5443617472E-001 2.8207981760E+001 7.5228174233E-001 2.8212361853E+001 7.5069919125E-001 2.8217444469E+001 7.4893536772E-001 2.8222528922E+001 7.4825678115E-001 2.8227439791E+001 7.4769475767E-001 2.8231124068E+001 7.4738192428E-001 2.8234107284E+001 7.4702144773E-001 2.8238144406E+001 7.4724880409E-001 2.8243060726E+001 7.4717667332E-001 2.8248857163E+001 7.4731943591E-001 2.8253952972E+001 7.4920865304E-001 2.8258523195E+001 7.5064725847E-001 2.8263094900E+001 7.5135447587E-001 2.8266964424E+001 7.5126032228E-001 2.8271714838E+001 7.5069451735E-001 2.8278227264E+001 7.4893359022E-001 2.8283509818E+001 7.4699984618E-001 2.8289322913E+001 7.4552765474E-001 2.8294962142E+001 7.4462818021E-001 2.8299545675E+001 7.4457132467E-001 2.8303248846E+001 7.4437149664E-001 2.8308011494E+001 7.4424325371E-001 2.8314540696E+001 7.4322592242E-001 2.8321072918E+001 7.4238538447E-001 2.8326901503E+001 7.4189700333E-001 2.8331848856E+001 7.4117714249E-001 2.8336090823E+001 7.4139450727E-001 2.8340510893E+001 7.4160135068E-001 2.8346524407E+001 7.4208530200E-001 2.8352186522E+001 7.4189208388E-001 2.8358382058E+001 7.4154417121E-001 2.8364403178E+001 7.4109592986E-001 2.8369540864E+001 7.4030408259E-001 2.8373439665E+001 7.3940973247E-001 2.8377871424E+001 7.3869403099E-001 2.8384255595E+001 7.3751599940E-001 2.8390820106E+001 7.3696774145E-001 2.8396855043E+001 7.3650524986E-001 2.8402359728E+001 7.3638643187E-001 2.8406800549E+001 7.3628762135E-001 2.8412842299E+001 7.3635557852E-001 2.8420487027E+001 7.3665561806E-001 2.8427246266E+001 7.3756308875E-001 2.8433830728E+001 7.3782641399E-001 2.8439527864E+001 7.3760008943E-001 2.8443980345E+001 7.3724313447E-001 2.8450216165E+001 7.3596551249E-001 2.8457702769E+001 7.3457943837E-001 2.8465014931E+001 7.3360271803E-001 2.8471081533E+001 7.3254107123E-001 2.8476258036E+001 7.3203462331E-001 2.8481615025E+001 7.3146874045E-001 2.8488403446E+001 7.3110235169E-001 2.8495195111E+001 7.3125611845E-001 2.8502705466E+001 7.3125024184E-001 2.8509325020E+001 7.3134436064E-001 2.8513978443E+001 7.3179065847E-001 2.8518991524E+001 7.3210317834E-001 2.8525976976E+001 7.3212289483E-001 2.8533324356E+001 7.3229165127E-001 2.8540316848E+001 7.3149459050E-001 2.8546236257E+001 7.3058759793E-001 2.8551799156E+001 7.2966301017E-001 2.8560416966E+001 7.2869194143E-001 2.8568141517E+001 7.2739656609E-001 2.8575870258E+001 7.2700339837E-001 2.8582164189E+001 7.2696112153E-001 2.8587561199E+001 7.2718775625E-001 2.8594940418E+001 7.2698148659E-001 2.8603584357E+001 7.2715140149E-001 2.8611512571E+001 7.2739257138E-001 2.8617461624E+001 7.2715589426E-001 2.8622872005E+001 7.2700069061E-001 2.8630630463E+001 7.2622082245E-001 2.8638393138E+001 7.2577604046E-001 2.8646521387E+001 7.2513027110E-001 2.8653388845E+001 7.2433931754E-001 2.8659174527E+001 7.2373453271E-001 2.8665143466E+001 7.2308134608E-001 2.8673105929E+001 7.2260995492E-001 2.8681616187E+001 7.2248330967E-001 2.8688681735E+001 7.2234708214E-001 2.8694300430E+001 7.2207392106E-001 2.8703186093E+001 7.2223033511E-001 2.8712440297E+001 7.2202137458E-001 2.8720973979E+001 7.2178137599E-001 2.8727877270E+001 7.2171210498E-001 2.8733874933E+001 7.2163653920E-001 2.8742785185E+001 7.2081172721E-001 2.8752611065E+001 7.2015352145E-001 2.8759893838E+001 7.1954575276E-001 2.8766087102E+001 7.1898447883E-001 2.8773194434E+001 7.1857367134E-001 2.8782129151E+001 7.1821952410E-001 2.8791251944E+001 7.1783368354E-001 2.8799102184E+001 7.1744571164E-001 2.8805129697E+001 7.1722897834E-001 2.8812073603E+001 7.1705362197E-001 2.8821215437E+001 7.1672406747E-001 2.8829814064E+001 7.1660123592E-001 2.8836953000E+001 7.1620701261E-001 2.8844095481E+001 7.1610695172E-001 2.8854907516E+001 7.1552240322E-001 2.8864076620E+001 7.1495302028E-001 2.8872517356E+001 7.1438781837E-001 2.8879126602E+001 7.1394651847E-001 2.8888494893E+001 7.1325633492E-001 2.8898420904E+001 7.1274771890E-001 2.8907065776E+001 7.1247391662E-001 2.8913690887E+001 7.1227859621E-001 2.8922160738E+001 7.1183002560E-001 2.8931925649E+001 7.1173773632E-001 2.8942250473E+001 7.1129403738E-001 2.8949629872E+001 7.1088815151E-001 2.8956274556E+001 7.1061940556E-001 2.8965323623E+001 7.1026701242E-001 2.8975672359E+001 7.0963243749E-001 2.8983993680E+001 7.0925773485E-001 2.8991394433E+001 7.0894375703E-001 2.9002317461E+001 7.0833766418E-001 2.9012878055E+001 7.0772680965E-001 2.9021962623E+001 7.0728800413E-001 2.9028826179E+001 7.0713950326E-001 2.9039963190E+001 7.0645547739E-001 2.9050551286E+001 7.0602167206E-001 2.9059287645E+001 7.0550697325E-001 2.9066540963E+001 7.0526681261E-001 2.9076590013E+001 7.0487565640E-001 2.9087018609E+001 7.0453459623E-001 2.9096709021E+001 7.0400926103E-001 2.9103235059E+001 7.0373561067E-001 2.9112189826E+001 7.0332787802E-001 2.9123017542E+001 7.0285739643E-001 2.9132171388E+001 7.0238381554E-001 2.9140209108E+001 7.0206379731E-001 2.9151057728E+001 7.0139763656E-001