Hi,

All data measured on APS 20BM, In K-edge

files attached:
in2o3 (avg of 3 scans)
in foil ref measured after sample (avg of 3 scans, no shift detected)

I can provide a foil scan without the sample in place, but the transmission detectors were still
purging (changed gas for high energy) during those measurements.

cheers,
-R.

On 2023-05-16 7:29 p.m., Shuting Xiang wrote:
Dear all, 

I hope this email finds you well. I am writing to inquire if any of you might have the XAFS spectra of In oxide (In2O3) and In foil. We are in need of these spectra as references for our ongoing research. If anyone would be kind enough to share these spectra with us, we would greatly appreciate it. 

Please feel free to reach out to me if you are able to assist. Your support would be greatly appreciated. 

Thank you very much for your attention and consideration. 

Best,

Shuting Xiang
Department of Material Science and Engineering 
Stony Brook University 

_______________________________________________
Ifeffit mailing list
Ifeffit@millenia.cars.aps.anl.gov
http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit