Hi
     I am fitting a copper foil whose data is taken at room temperature. So do I need to change the guess value of parameters enot, ss,amp, delr to some other value or I should take them as the default guess value. Also what should be the ideal fitting range in R for the copper foil.
                                             
                                                                                                                    With thanks