Hello everyone,
I am new to the mailing list. i am Fitting data of regular and distorted ( from irradiation) NBS glass doped with Hafnium. Literature available Hafnia (monoclinic) data is taken as standard model to fit the data (monoclinic) of regular glass.
Now i want to fit the distorted glass data with exafs result of regular glass data as standard model. or will it be ok , to also fit the distorted glass data with hafnia as standard model. .

thanks