Energy INTENSITY 11.4168 9.6723335e-05 11.4175 9.6308155e-05 11.4235 0.00010055632 11.429 0.00010177809 11.434 0.00010517327 11.439 0.00010839591 11.444 0.00010952767 11.449 0.00011518454 11.454 0.00011869337 11.459 0.00012080449 11.464 0.00012592273 11.469 0.00012939482 11.474 0.00013985642 11.479 0.00014285026 11.484 0.0001493879 11.489 0.00016023775 11.494 0.0001671419 11.499 0.00017522901 11.5037 0.00018965336 11.509 0.0002062602 11.514 0.00022381436 11.516 0.00023456637 11.518 0.0002467591 11.52 0.00025494036 11.522 0.0002670222 11.524 0.00027926086 11.526 0.00029781129 11.528 0.00031411511 11.53 0.00033150456 11.532 0.00035864284 11.534 0.00037354237 11.536 0.00040435418 11.538 0.0004364365 11.54 0.00047827273 11.542 0.00052546058 11.544 0.00058461586 11.5443 0.00058736786 11.5446 0.00060000003 11.5449 0.00061063695 11.5452 0.00061468687 11.5455 0.00062789459 11.5458 0.00063460227 11.5461 0.00065737974 11.5464 0.00066892902 11.5467 0.00068066188 11.547 0.00070017041 11.5473 0.000712779 11.5476 0.0007253075 11.5479 0.00074325444 11.5482 0.00076021801 11.5485 0.00077601417 11.5488 0.00079429417 11.5491 0.00080699904 11.5494 0.00083182845 11.5497 0.00085174432 11.55 0.00087290537 11.5503 0.00089843542 11.5506 0.00091890362 11.5509 0.00095465075 11.5512 0.00096270407 11.5515 0.00099883252 11.5518 0.0010240998 11.5521 0.0010561168 11.5524 0.0010889997 11.5527 0.0011170295 11.553 0.001163146 11.5533 0.0011883264 11.5536 0.0012169275 11.5539 0.0012569524 11.5542 0.0012985012 11.5545 0.0013399606 11.5548 0.001383865 11.5551 0.0014316675 11.5554 0.0014922896 11.5557 0.0015390585 11.556 0.0015943312 11.5563 0.0016500839 11.5566 0.0017343245 11.5569 0.001803488 11.5572 0.001898319 11.5575 0.0019685645 11.5578 0.0021026405 11.5581 0.0022292412 11.5584 0.0023468859 11.5587 0.0024757702 11.559 0.0026536756 11.5593 0.0027478095 11.5596 0.0029751207 11.5599 0.0031808163 11.5602 0.0033637458 11.5605 0.0036186329 11.5608 0.0038696723 11.5611 0.004215721 11.5614 0.0045515806 11.5617 0.0049103471 11.562 0.005350804 11.5623 0.00574141 11.5626 0.0062289331 11.5629 0.0067626471 11.5632 0.0073227105 11.5635 0.0078016547 11.5638 0.0083440328 11.5641 0.0089615285 11.5644 0.009571543 11.5647 0.010021884 11.565 0.010543477 11.5653 0.01104006 11.5656 0.011377083 11.5659 0.011764083 11.5662 0.012014689 11.5665 0.012172356 11.5668 0.012342677 11.5671 0.012411535 11.5674 0.012451035 11.5677 0.012385586 11.568 0.012281559 11.5683 0.012129555 11.5686 0.011988839 11.5689 0.011649692 11.5692 0.011373192 11.5695 0.011068569 11.5698 0.010818686 11.5701 0.010451589 11.5704 0.010152096 11.5707 0.009869609 11.571 0.00964115 11.5713 0.0093449904 11.5716 0.0091434941 11.5719 0.0089017786 11.5722 0.0087153018 11.5725 0.0085200537 11.5728 0.0083151022 11.5731 0.0081564691 11.5734 0.0080031408 11.5737 0.0079030069 11.574 0.007773607 11.5743 0.0076768603 11.5746 0.0076041562 11.5749 0.0075520845 11.5752 0.0074948287 11.5755 0.0074720341 11.5758 0.007421081 11.5761 0.0074186004 11.5764 0.0073976265 11.5767 0.0074100597 11.577 0.0073991856 11.5773 0.0073972689 11.5776 0.0074164886 11.5779 0.0074253054 11.5782 0.0074454141 11.5785 0.0074587758 11.5788 0.0074919732 11.5791 0.0074752886 11.5794 0.0074965023 11.5797 0.007538802 11.58 0.007516996 11.5803 0.0075214552 11.5806 0.0075300252 11.5809 0.0075615179 11.5812 0.0075615621 11.5815 0.0075740758 11.5818 0.0076169991 11.5821 0.0075960038 11.5824 0.0076257605 11.5827 0.0076639522 11.583 0.0076589705 11.5833 0.0076912073 11.5836 0.0077124247 11.5839 0.0077241343 11.584 0.0077258963 11.5849 0.0077857338 11.5858 0.007836259 11.5867 0.0078736059 11.5876 0.00790965 11.5886 0.0079629458 11.5896 0.0080508403 11.5906 0.0081296582 11.5916 0.0082556587 11.5926 0.0083649531 11.5937 0.0084553175 11.5948 0.0085193543 11.5958 0.0085329283 11.597 0.0085541848 11.5981 0.0085877869 11.5992 0.0085919369 11.6004 0.0086092595 11.6016 0.0086512398 11.6028 0.0086885877 11.604 0.008753079 11.6053 0.0088060349 11.6065 0.0088460203 11.6078 0.008893799 11.6091 0.008922847 11.6104 0.008962173 11.6118 0.009016335 11.6131 0.0090908101 11.6145 0.0091451667 11.6159 0.0091929194 11.6173 0.0092072533 11.6188 0.0091747371 11.6202 0.0091048852 11.6217 0.0090320744 11.6232 0.0089176977 11.6247 0.0088450126 11.6262 0.0087753851 11.6278 0.0086821858 11.6293 0.0086220875 11.6309 0.0085266465 11.6325 0.0084845573 11.6341 0.0084273368 11.6358 0.0083632693 11.6374 0.0083363149 11.6391 0.0083257593 11.6408 0.0083083911 11.6426 0.0083260331 11.6443 0.0083543304 11.6461 0.0083909472 11.6478 0.0084212441 11.6496 0.0084666423 11.6514 0.0085114352 11.6533 0.0085469093 11.6551 0.0085604247 11.657 0.0085732536 11.6589 0.0086042024 11.6608 0.0085970685 11.6627 0.0086227544 11.6647 0.0086036641 11.6666 0.0086391764 11.6686 0.0086628683 11.6706 0.0087019894 11.6727 0.0087205693 11.6747 0.0087670181 11.6768 0.0087890103 11.6789 0.0088273548 11.681 0.0088600153 11.6831 0.0088730883 11.6852 0.0088586295 11.6874 0.0088515766 11.6895 0.0088399081 11.6917 0.0088325329 11.694 0.0088193696 11.6962 0.0087969098 11.6984 0.0087614991 11.7007 0.0087307133 11.703 0.0087022437 11.7053 0.0086680455 11.7076 0.0086674755 11.71 0.0086399186 11.7124 0.0086397473 11.7148 0.0086278031 11.7172 0.0086261993 11.7196 0.0086472388 11.722 0.0086602271 11.7245 0.0086554252 11.727 0.0086851064 11.7295 0.0086717643 11.732 0.0087170154 11.7345 0.0087095145 11.7371 0.0087254122 11.7397 0.008742271 11.7423 0.0087545924 11.7449 0.0087451432 11.7475 0.0087813465 11.7502 0.0087700048 11.7528 0.0087846173 11.7555 0.0088062081 11.7582 0.0088152047 11.761 0.0088340333 11.7637 0.0088418424 11.7665 0.0088504357 11.7693 0.0088555226 11.7721 0.0088780485 11.7749 0.0088894973 11.7777 0.0088912863 11.7806 0.0089093642 11.7835 0.0089232996 11.7864 0.0089202859 11.7893 0.00889959 11.7922 0.0088790618 11.7952 0.0088629527 11.7982 0.008843096 11.8012 0.0088156834 11.8042 0.0088104922 11.8072 0.0088046649 11.8103 0.0087781046 11.8134 0.0087804142 11.8164 0.0087956591 11.8196 0.0087841805 11.8227 0.008802834 11.8258 0.0088119768 11.829 0.0088134501 11.8322 0.0088165496 11.8354 0.0088220146 11.8386 0.0088334708 11.8419 0.0088311527 11.8451 0.0088399835 11.8484 0.0088442378 11.8517 0.008866528 11.855 0.0088588297 11.8584 0.0088609401 11.8617 0.0088516437 11.8651 0.008852493 11.8685 0.0088415649 11.8719 0.0088737421 11.8753 0.0088498853 11.8788 0.0088533163 11.8823 0.0088708345 11.8858 0.0088730529 11.8893 0.0088783335 11.8928 0.0088880016 11.8963 0.0089042429 11.8999 0.0089195035 11.9035 0.0089449119 11.9071 0.0089525934 11.9107 0.0089541618 11.9144 0.0089631248 11.918 0.0089896526 11.9217 0.0089771934 11.9254 0.0089708306 11.9291 0.0089821387 11.9329 0.0089488402 11.9366 0.0089357514 11.9404 0.0089466432 11.9442 0.008940855 11.948 0.0089296307 11.9519 0.0089104045 11.9557 0.0089208093 11.9596 0.0089076199 11.9635 0.0089071635 11.9674 0.008926753 11.9713 0.0089131175 11.9753 0.0089197187 11.9792 0.0089358911 11.9832 0.0089534502 11.9872 0.0089517217 11.9912 0.0089566885 11.9953 0.0089763701 11.9993 0.0089875422 12.0034 0.0089795087 12.0075 0.0089971386 12.0116 0.0089826435 12.0158 0.0089847231 12.0199 0.0089945085 12.0241 0.008988481 12.0283 0.0089935455 12.0325 0.0089912396 12.0368 0.0089870328 12.041 0.0089986362 12.0453 0.0089924866 12.0496 0.0089919455 12.0539 0.0089875096 12.0582 0.0090119746 12.0626 0.009015834 12.0669 0.0090167578 12.0713 0.0090309903 12.0757 0.0090344418 12.0801 0.0090272948 12.0846 0.0090457248 12.089 0.0090485252 12.0935 0.0090352744 12.098 0.0090415515 12.1025 0.0090471916 12.1071 0.0090556145 12.1116 0.0090406295 12.1162 0.0090485457 12.1208 0.0090376996 12.1254 0.0090638828 12.1301 0.0090410504 12.1347 0.0090334462 12.1394 0.00903749 12.1441 0.0090288697 12.1488 0.0090425238 12.1535 0.0090460731 12.1583 0.0090395808 12.163 0.009037137 12.1678 0.0090407114 12.1726 0.009062022 12.1774 0.0090583693 12.1823 0.0090384502 12.1872 0.0090400316 12.192 0.0090356544 12.1969 0.0090403119 12.2019 0.0090283323 12.2068 0.0090293391 12.2117 0.0090240305 12.2167 0.0090361536 12.2217 0.009024512 12.2264 0.0090338979 12.2318 0.0090206964 12.2368 0.0090401405 12.2419 0.0090389214 12.247 0.0090283602 12.2521 0.0090545025 12.2572 0.0090407236 12.2624 0.0090526687 12.2675 0.0090492498 12.2727 0.0090570934 12.2779 0.0090803374 12.2831 0.0090902727 12.2884 0.0090871975 12.2937 0.0090801921 12.2989 0.0090935696 12.3042 0.0090888888 12.3096 0.0090947691 12.3149 0.0090863537