7.0089965E+3 7.2044097E-4 7.0139965E+3 1.0369100E-3 7.0189965E+3 9.8733340E-4 7.0239965E+3 1.1813398E-3 7.0289965E+3 1.0074852E-3 7.0339965E+3 1.2094186E-3 7.0389965E+3 9.2689483E-4 7.0439965E+3 1.2496682E-3 7.0489964E+3 1.0718455E-3 7.0539964E+3 1.7727697E-3 7.0589964E+3 1.3862643E-3 7.0639964E+3 1.6755738E-3 7.0689964E+3 2.0695993E-3 7.0739964E+3 2.3149711E-3 7.0789964E+3 2.6163304E-3 7.0839964E+3 3.1848020E-3 7.0889964E+3 3.8758497E-3 7.0939964E+3 4.6214346E-3 7.0989964E+3 6.1192189E-3 7.1039964E+3 8.2504680E-3 7.1089964E+3 1.6200379E-2 7.1096985E+3 1.8666270E-2 7.1104006E+3 2.3044233E-2 7.1111028E+3 3.1297154E-2 7.1118049E+3 4.3788382E-2 7.1125070E+3 7.6466023E-2 7.1132091E+3 9.4008575E-2 7.1139113E+3 8.2571667E-2 7.1146134E+3 7.2726816E-2 7.1153155E+3 7.0747124E-2 7.1160177E+3 7.4727647E-2 7.1167198E+3 8.3828413E-2 7.1174219E+3 1.0027126E-1 7.1181240E+3 1.2905512E-1 7.1188262E+3 1.6620897E-1 7.1195283E+3 2.2323819E-1 7.1202304E+3 2.9610592E-1 7.1209325E+3 3.6819375E-1 7.1216347E+3 4.4186320E-1 7.1223368E+3 5.2140612E-1 7.1230389E+3 6.0226574E-1 7.1237410E+3 6.9339004E-1 7.1244432E+3 7.8978412E-1 7.1251453E+3 8.6489637E-1 7.1258474E+3 9.4431837E-1 7.1265496E+3 1.0231337E+0 7.1272517E+3 1.0953116E+0 7.1279538E+3 1.1913987E+0 7.1286559E+3 1.2813998E+0 7.1293581E+3 1.3567689E+0 7.1300602E+3 1.4026646E+0 7.1307623E+3 1.4165951E+0 7.1314644E+3 1.4028619E+0 7.1321666E+3 1.3732620E+0 7.1328687E+3 1.3283111E+0 7.1335708E+3 1.2765312E+0 7.1342730E+3 1.2294025E+0 7.1349751E+3 1.1997918E+0 7.1356772E+3 1.1809577E+0 7.1363793E+3 1.1680378E+0 7.1370815E+3 1.1579486E+0 7.1377836E+3 1.1419540E+0 7.1384857E+3 1.1276579E+0 7.1391878E+3 1.1102432E+0 7.1398900E+3 1.0930830E+0 7.1405921E+3 1.0813365E+0 7.1412942E+3 1.0709503E+0 7.1419963E+3 1.0657474E+0 7.1440142E+3 1.0739237E+0 7.1460321E+3 1.0692659E+0 7.1480499E+3 1.0132286E+0 7.1500678E+3 9.5081560E-1 7.1520856E+3 9.1518664E-1 7.1541035E+3 8.9053226E-1 7.1561213E+3 8.6795469E-1 7.1581392E+3 8.4899743E-1 7.1601570E+3 8.4446339E-1 7.1621749E+3 8.5240842E-1 7.1641928E+3 8.6422979E-1 7.1662106E+3 8.7915407E-1 7.1682285E+3 9.0362210E-1 7.1702463E+3 9.3290710E-1 7.1722642E+3 9.6413276E-1 7.1742820E+3 9.9230898E-1 7.1762999E+3 1.0122211E+0 7.1783177E+3 1.0369151E+0 7.1803356E+3 1.0587214E+0 7.1823534E+3 1.0700518E+0 7.1843713E+3 1.0713926E+0 7.1863892E+3 1.0680952E+0 7.1884070E+3 1.0634151E+0 7.1904249E+3 1.0571113E+0 7.1924427E+3 1.0471647E+0 7.1944606E+3 1.0365617E+0 7.1964784E+3 1.0242937E+0 7.1984963E+3 1.0101418E+0 7.2005141E+3 9.9827911E-1 7.2025320E+3 9.8497250E-1 7.2045499E+3 9.7576558E-1 7.2065677E+3 9.6993534E-1 7.2085856E+3 9.6497333E-1 7.2106034E+3 9.6740783E-1 7.2126213E+3 9.7084516E-1 7.2146391E+3 9.7523650E-1 7.2166570E+3 9.8384214E-1 7.2186748E+3 9.9152718E-1 7.2206927E+3 9.9913192E-1 7.2227105E+3 1.0086880E+0 7.2247284E+3 1.0146467E+0 7.2267463E+3 1.0175728E+0 7.2287641E+3 1.0166839E+0 7.2307820E+3 1.0116183E+0 7.2327998E+3 1.0056367E+0 7.2348177E+3 9.9853235E-1 7.2368355E+3 9.8856386E-1 7.2388534E+3 9.7938671E-1 7.2408712E+3 9.6699710E-1 7.2428891E+3 9.5570345E-1 7.2449070E+3 9.4935466E-1 7.2469248E+3 9.4729052E-1 7.2489427E+3 9.5071465E-1 7.2509605E+3 9.5530312E-1 7.2529784E+3 9.6423586E-1 7.2549962E+3 9.7505335E-1 7.2554962E+3 9.7718538E-1 7.2559962E+3 9.8024617E-1 7.2564962E+3 9.8348953E-1 7.2569962E+3 9.8630216E-1 7.2574962E+3 9.8833333E-1 7.2579962E+3 9.9166626E-1 7.2584962E+3 9.9487384E-1 7.2589962E+3 9.9772320E-1 7.2594962E+3 1.0005951E+0 7.2599962E+3 1.0022634E+0 7.2604962E+3 1.0039499E+0 7.2609962E+3 1.0079558E+0 7.2614962E+3 1.0109047E+0 7.2619962E+3 1.0120833E+0 7.2624962E+3 1.0150540E+0 7.2629962E+3 1.0183554E+0 7.2634962E+3 1.0201999E+0 7.2639962E+3 1.0209801E+0 7.2644962E+3 1.0211583E+0 7.2649962E+3 1.0237875E+0 7.2654962E+3 1.0248092E+0 7.2659962E+3 1.0264308E+0 7.2664962E+3 1.0280794E+0 7.2669962E+3 1.0284660E+0 7.2674962E+3 1.0300534E+0 7.2679962E+3 1.0317614E+0 7.2684962E+3 1.0314736E+0 7.2689962E+3 1.0320166E+0 7.2694962E+3 1.0331159E+0 7.2699962E+3 1.0339442E+0 7.2724173E+3 1.0340833E+0 7.2748383E+3 1.0341037E+0 7.2772594E+3 1.0330303E+0 7.2796804E+3 1.0304655E+0 7.2821015E+3 1.0275769E+0 7.2845225E+3 1.0211386E+0 7.2869436E+3 1.0156348E+0 7.2893646E+3 1.0083529E+0 7.2917857E+3 9.9931305E-1 7.2942067E+3 9.9208824E-1 7.2966278E+3 9.8909345E-1 7.2990488E+3 9.8644273E-1 7.3014699E+3 9.8334005E-1 7.3038909E+3 9.8007232E-1 7.3063120E+3 9.7961175E-1 7.3087330E+3 9.7824571E-1 7.3111541E+3 9.7812771E-1 7.3135751E+3 9.8181105E-1 7.3159962E+3 9.8577086E-1 7.3184172E+3 9.9189692E-1 7.3208383E+3 9.9716879E-1 7.3232593E+3 1.0044390E+0 7.3256804E+3 1.0088603E+0 7.3281014E+3 1.0136281E+0 7.3305225E+3 1.0126273E+0 7.3329435E+3 1.0121463E+0 7.3353646E+3 1.0103163E+0 7.3377856E+3 1.0065401E+0 7.3402067E+3 1.0041875E+0 7.3426277E+3 1.0017288E+0 7.3450488E+3 9.9852072E-1 7.3474698E+3 9.9403917E-1 7.3498909E+3 9.9131926E-1 7.3523119E+3 9.8900675E-1 7.3547330E+3 9.8896266E-1 7.3571540E+3 9.8950437E-1 7.3595751E+3 9.8924959E-1 7.3619961E+3 9.9019648E-1 7.3648166E+3 9.9121814E-1 7.3676371E+3 9.9432837E-1 7.3704576E+3 9.9589151E-1 7.3732782E+3 9.9824625E-1 7.3760987E+3 9.9897812E-1 7.3789192E+3 1.0000317E+0 7.3817397E+3 9.9918826E-1 7.3845602E+3 9.9849171E-1 7.3873807E+3 9.9939121E-1 7.3902012E+3 1.0008791E+0 7.3930217E+3 1.0024226E+0 7.3958422E+3 1.0044447E+0 7.3986627E+3 1.0047276E+0 7.4014832E+3 1.0057345E+0 7.4043038E+3 1.0033947E+0 7.4071243E+3 1.0027957E+0 7.4099448E+3 1.0023960E+0 7.4127653E+3 1.0002453E+0 7.4155858E+3 9.9867140E-1 7.4184063E+3 9.9696098E-1 7.4212268E+3 9.9583644E-1 7.4240473E+3 9.9544437E-1 7.4268678E+3 9.9553933E-1 7.4296883E+3 9.9405263E-1 7.4325089E+3 9.9381979E-1 7.4353294E+3 9.9459338E-1 7.4381499E+3 9.9440023E-1 7.4409704E+3 9.9391889E-1 7.4437909E+3 9.9563322E-1 7.4466114E+3 9.9824560E-1 7.4494319E+3 9.9858789E-1 7.4522524E+3 1.0004185E+0 7.4550729E+3 1.0015981E+0 7.4578934E+3 1.0009451E+0 7.4607140E+3 1.0000748E+0 7.4635345E+3 9.9846529E-1 7.4663550E+3 9.9820601E-1 7.4691755E+3 9.9649958E-1 7.4719960E+3 9.9677044E-1 7.4753293E+3 9.9551566E-1 7.4786626E+3 9.9608056E-1 7.4819960E+3 9.9681073E-1 7.4853293E+3 9.9700455E-1 7.4886626E+3 9.9648719E-1 7.4919960E+3 9.9727042E-1 7.4953293E+3 9.9633958E-1 7.4986626E+3 9.9821462E-1 7.5019960E+3 9.9768949E-1 7.5053293E+3 9.9911683E-1 7.5086626E+3 9.9834697E-1 7.5119959E+3 9.9876900E-1 7.5153293E+3 9.9938804E-1 7.5186626E+3 9.9878157E-1 7.5219959E+3 9.9931101E-1 7.5253293E+3 9.9975541E-1 7.5286626E+3 1.0003978E+0 7.5319959E+3 1.0006670E+0 7.5353293E+3 1.0002330E+0 7.5386626E+3 1.0003173E+0 7.5419959E+3 1.0004343E+0 7.5453292E+3 1.0008437E+0 7.5486626E+3 9.9928146E-1 7.5519959E+3 9.9917168E-1 7.5553292E+3 9.9851145E-1 7.5586626E+3 9.9829987E-1 7.5619959E+3 9.9824001E-1 7.5653292E+3 9.9906704E-1 7.5686625E+3 9.9961439E-1 7.5719959E+3 9.9860486E-1 7.5753292E+3 9.9950948E-1 7.5786625E+3 9.9984315E-1 7.5819959E+3 9.9994482E-1 7.5857459E+3 1.0017179E+0 7.5894959E+3 1.0021797E+0 7.5932459E+3 1.0020303E+0 7.5969958E+3 1.0028791E+0 7.6007458E+3 1.0035326E+0 7.6044958E+3 1.0036090E+0 7.6082458E+3 1.0042966E+0 7.6119958E+3 1.0037053E+0 7.6157458E+3 1.0039636E+0 7.6194958E+3 1.0034844E+0 7.6232458E+3 1.0028421E+0 7.6269958E+3 1.0021879E+0 7.6307458E+3 1.0027943E+0 7.6344958E+3 1.0011936E+0 7.6382458E+3 1.0010858E+0 7.6419958E+3 1.0008913E+0 7.6460984E+3 1.0002634E+0 7.6502009E+3 9.9965208E-1 7.6543035E+3 1.0001022E+0 7.6584060E+3 9.9955955E-1 7.6625086E+3 9.9986989E-1 7.6666112E+3 9.9961125E-1 7.6707137E+3 1.0003307E+0 7.6748163E+3 9.9983645E-1 7.6789188E+3 1.0008706E+0 7.6830214E+3 1.0013612E+0 7.6871240E+3 1.0013228E+0 7.6912265E+3 1.0018616E+0 7.6953291E+3 1.0014526E+0 7.6994316E+3 1.0017525E+0 7.7035342E+3 1.0024602E+0 7.7076367E+3 1.0013441E+0 7.7117393E+3 1.0010393E+0 7.7158419E+3 1.0010459E+0 7.7199444E+3 1.0018967E+0 7.7240470E+3 1.0010229E+0 7.7281495E+3 1.0013851E+0 7.7322521E+3 1.0005963E+0 7.7363547E+3 1.0007761E+0 7.7404572E+3 1.0002414E+0 7.7445598E+3 1.0002000E+0 7.7486623E+3 1.0003981E+0 7.7527649E+3 1.0005839E+0 7.7568675E+3 9.9959341E-1 7.7609700E+3 9.9959989E-1 7.7650726E+3 1.0009049E+0 7.7691751E+3 1.0002561E+0 7.7732777E+3 1.0008681E+0 7.7773803E+3 1.0004078E+0 7.7814828E+3 1.0011717E+0 7.7855854E+3 1.0015000E+0 7.7896879E+3 1.0013722E+0 7.7937905E+3 1.0010713E+0 7.7978931E+3 1.0008159E+0 7.8019956E+3 1.0005693E+0 7.8067782E+3 1.0015864E+0 7.8115608E+3 1.0016180E+0 7.8163434E+3 1.0018587E+0 7.8211260E+3 1.0001345E+0 7.8259086E+3 1.0008462E+0 7.8306912E+3 1.0005346E+0 7.8354738E+3 9.9929929E-1 7.8402564E+3 9.9954273E-1 7.8450390E+3 1.0001869E+0 7.8498216E+3 9.9947812E-1 7.8546042E+3 9.9968531E-1 7.8593869E+3 9.9816563E-1 7.8641695E+3 9.9830503E-1 7.8689521E+3 9.9791356E-1 7.8737347E+3 9.9852910E-1 7.8785173E+3 9.9875942E-1 7.8832999E+3 9.9931237E-1 7.8880825E+3 9.9904457E-1 7.8928651E+3 9.9831050E-1 7.8976477E+3 9.9767258E-1 7.9024303E+3 9.9723159E-1 7.9072129E+3 9.9737597E-1 7.9119955E+3 9.9831108E-1