Name : Fit 4 (fzexv) Description : fit to cu010k Figure of merit : 4 Time of fit : 2021-03-26T12:12:21 Environment : Demeter 0.9.26 with perl 5.030000 and using Larch X.xx on linux Interface : Artemis (Wx 0.9932) Prepared by : ava@ava-PC Contact : =*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*= Independent points : 25.401 Number of variables : 4 Chi-square : 0.0000000 Reduced chi-square : 0.0000000 R-factor : 0.0000000 Number of data sets : 1 Happiness = 100.00/100 color = #D8E796 ***** Note: happiness is a semantic parameter and should ***** ***** NEVER be reported in a publication -- NEVER! ***** guess parameters: ss_Cu1 = 0.00341875 # +/- 0.00003724 [0.00300] dr_Cu1 = -0.00471435 # +/- 0.00045738 [-0.00504] dE0 = 5.41536257 # +/- 0.14032983 [5.36177] amp = 0.89986572 # +/- 0.00826589 [0.90000] set parameters: N1 = 1.00000000 Correlations between variables: All other correlations below 0.4 ===== Data set >> cu010k << ==================================== : file = : name = cu010k : k-range = 3.000 - 22.950 : dk = 1 : k-window = Hanning : k-weight = 3 : R-range = 1 - 3 : dR = 0.0 : R-window = Hanning : fitting space = r : background function = no : phase correction = no : background removal = : user-supplied epsilon_k = 0 : epsilon_k by k-weight = 3 -> 2.602e-04 : epsilon_r by k-weight = 3 -> 3.592e-01 : R-factor by k-weight = 1 -> 0.00434, 2 -> 0.00233, 3 -> 0.00246 name N S02 sigma^2 e0 delr Reff R ================================================================================= [atoms] Cu.1 12.000 0.000 0.00000 0.000 0.00000 2.55270 2.55270 name ei third fourth ================================================= [atoms] Cu.1 0.00000 0.00000 0.00000 =*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=*=