8.2316064E+3 1.2460149E-3 8.2366065E+3 1.4793792E-3 8.2416067E+3 1.6763827E-3 8.2466068E+3 1.6317915E-3 8.2516070E+3 1.7582957E-3 8.2566071E+3 1.6515803E-3 8.2616072E+3 2.0952501E-3 8.2666074E+3 2.1554625E-3 8.2716075E+3 2.3964267E-3 8.2766077E+3 2.7184428E-3 8.2816078E+3 2.9151296E-3 8.2866080E+3 3.3403745E-3 8.2916081E+3 4.0589194E-3 8.2966083E+3 3.4122299E-3 8.3016084E+3 4.1509290E-3 8.3066086E+3 5.5472506E-3 8.3116087E+3 7.0882989E-3 8.3121087E+3 6.7281363E-3 8.3126087E+3 6.6862830E-3 8.3131088E+3 6.7701557E-3 8.3136088E+3 6.9752720E-3 8.3141088E+3 7.0065226E-3 8.3146088E+3 7.4805818E-3 8.3151088E+3 8.5669886E-3 8.3156088E+3 8.3118100E-3 8.3161088E+3 7.9527824E-3 8.3166089E+3 7.9749572E-3 8.3171089E+3 8.2385041E-3 8.3176089E+3 8.2735361E-3 8.3181089E+3 8.7199093E-3 8.3186089E+3 9.1019289E-3 8.3191089E+3 9.1394568E-3 8.3196089E+3 9.5330423E-3 8.3201090E+3 9.7359248E-3 8.3206090E+3 1.0404152E-2 8.3211090E+3 1.1121663E-2 8.3216090E+3 1.1528490E-2 8.3221090E+3 1.1827616E-2 8.3226090E+3 1.2199642E-2 8.3231091E+3 1.2195658E-2 8.3236091E+3 1.3237446E-2 8.3241091E+3 1.3889887E-2 8.3246091E+3 1.5159374E-2 8.3251091E+3 1.5539870E-2 8.3256091E+3 1.6185819E-2 8.3261091E+3 1.6793515E-2 8.3266092E+3 1.7458003E-2 8.3271092E+3 1.8565124E-2 8.3276092E+3 1.9882821E-2 8.3281092E+3 2.1187953E-2 8.3286092E+3 2.1955502E-2 8.3291092E+3 2.3820709E-2 8.3296092E+3 2.6436867E-2 8.3301093E+3 2.9557773E-2 8.3306093E+3 3.4992527E-2 8.3311093E+3 4.2085814E-2 8.3316093E+3 4.8755423E-2 8.3321093E+3 4.9709093E-2 8.3326093E+3 4.7157604E-2 8.3331093E+3 4.6339530E-2 8.3336094E+3 4.8267792E-2 8.3341094E+3 5.2632993E-2 8.3346094E+3 5.9288549E-2 8.3351094E+3 6.9084534E-2 8.3356094E+3 8.2138766E-2 8.3361094E+3 9.5573015E-2 8.3366094E+3 1.0957398E-1 8.3371095E+3 1.2839516E-1 8.3376095E+3 1.4950528E-1 8.3381095E+3 1.8353240E-1 8.3386095E+3 2.2706347E-1 8.3391095E+3 2.7861999E-1 8.3396095E+3 3.3649083E-1 8.3401096E+3 3.8670135E-1 8.3406096E+3 4.3216611E-1 8.3411096E+3 4.8959628E-1 8.3416096E+3 5.4482993E-1 8.3421096E+3 6.1294780E-1 8.3426096E+3 6.8024796E-1 8.3431096E+3 7.6596771E-1 8.3436097E+3 8.7743535E-1 8.3441097E+3 9.8031974E-1 8.3446097E+3 1.0937161E+0 8.3451097E+3 1.1757946E+0 8.3456097E+3 1.2449745E+0 8.3461097E+3 1.3160904E+0 8.3466097E+3 1.3756815E+0 8.3471098E+3 1.4378302E+0 8.3476098E+3 1.5131641E+0 8.3481098E+3 1.5747498E+0 8.3486098E+3 1.6168092E+0 8.3491098E+3 1.6225129E+0 8.3496098E+3 1.6035003E+0 8.3501098E+3 1.5543196E+0 8.3506099E+3 1.4924833E+0 8.3511099E+3 1.4268707E+0 8.3516099E+3 1.3496396E+0 8.3521099E+3 1.2906728E+0 8.3526099E+3 1.2370054E+0 8.3531099E+3 1.1861179E+0 8.3536100E+3 1.1456613E+0 8.3541100E+3 1.1131266E+0 8.3546100E+3 1.0826292E+0 8.3551100E+3 1.0525643E+0 8.3556100E+3 1.0176343E+0 8.3561100E+3 9.8303504E-1 8.3566100E+3 9.4283622E-1 8.3571101E+3 9.0434480E-1 8.3576101E+3 8.7615715E-1 8.3581101E+3 8.5277118E-1 8.3586101E+3 8.3171509E-1 8.3591101E+3 8.1806563E-1 8.3596101E+3 8.0952729E-1 8.3601101E+3 8.0696072E-1 8.3606102E+3 8.1098476E-1 8.3611102E+3 8.1923333E-1 8.3616102E+3 8.3499585E-1 8.3636144E+3 9.1181020E-1 8.3656186E+3 9.3129595E-1 8.3676228E+3 8.9581575E-1 8.3696270E+3 8.6202100E-1 8.3716311E+3 8.3400214E-1 8.3736353E+3 8.0910329E-1 8.3756395E+3 7.9941294E-1 8.3776437E+3 8.1540374E-1 8.3796479E+3 8.4713954E-1 8.3816521E+3 8.8040787E-1 8.3836563E+3 9.0571371E-1 8.3856605E+3 9.3467944E-1 8.3876647E+3 9.7918478E-1 8.3896689E+3 1.0318247E+0 8.3916731E+3 1.0813841E+0 8.3936773E+3 1.1165049E+0 8.3956814E+3 1.1385288E+0 8.3976856E+3 1.1511347E+0 8.3996898E+3 1.1451416E+0 8.4016940E+3 1.1216301E+0 8.4036982E+3 1.0889921E+0 8.4057024E+3 1.0518465E+0 8.4077066E+3 1.0182888E+0 8.4097108E+3 9.8612572E-1 8.4117150E+3 9.5856413E-1 8.4137192E+3 9.3566774E-1 8.4157234E+3 9.1793551E-1 8.4177276E+3 9.0842961E-1 8.4197317E+3 9.0696703E-1 8.4217359E+3 9.1201954E-1 8.4237401E+3 9.2302266E-1 8.4257443E+3 9.3672374E-1 8.4277485E+3 9.4999103E-1 8.4297527E+3 9.5736984E-1 8.4317569E+3 9.6182422E-1 8.4337611E+3 9.6469121E-1 8.4357653E+3 9.6958905E-1 8.4377695E+3 9.7594345E-1 8.4397737E+3 9.8577045E-1 8.4417779E+3 9.9989791E-1 8.4437821E+3 1.0155560E+0 8.4457862E+3 1.0278709E+0 8.4477904E+3 1.0329944E+0 8.4497946E+3 1.0302152E+0 8.4520558E+3 1.0194594E+0 8.4543169E+3 1.0022746E+0 8.4565780E+3 9.8390803E-1 8.4588392E+3 9.6293263E-1 8.4611003E+3 9.4523433E-1 8.4633615E+3 9.3453140E-1 8.4656226E+3 9.3582555E-1 8.4678837E+3 9.4989428E-1 8.4701449E+3 9.7231235E-1 8.4724060E+3 9.9935940E-1 8.4746672E+3 1.0201046E+0 8.4769283E+3 1.0327100E+0 8.4791894E+3 1.0343250E+0 8.4814506E+3 1.0292013E+0 8.4837117E+3 1.0204819E+0 8.4859729E+3 1.0144707E+0 8.4882340E+3 1.0153284E+0 8.4904952E+3 1.0196892E+0 8.4927563E+3 1.0264258E+0 8.4950174E+3 1.0342815E+0 8.4972786E+3 1.0403690E+0 8.4995397E+3 1.0430828E+0 8.5018009E+3 1.0426297E+0 8.5040620E+3 1.0384375E+0 8.5063231E+3 1.0313037E+0 8.5085843E+3 1.0194884E+0 8.5108454E+3 1.0060790E+0 8.5131066E+3 9.9041690E-1 8.5153677E+3 9.7306642E-1 8.5176288E+3 9.5668750E-1 8.5198900E+3 9.4141100E-1 8.5221511E+3 9.2987528E-1 8.5244123E+3 9.2354597E-1 8.5266734E+3 9.2307026E-1 8.5289345E+3 9.3047381E-1 8.5311957E+3 9.4315648E-1 8.5334568E+3 9.6013024E-1 8.5357180E+3 9.7812615E-1 8.5379791E+3 9.9483888E-1 8.5404987E+3 1.0110561E+0 8.5430182E+3 1.0224487E+0 8.5455378E+3 1.0307371E+0 8.5480573E+3 1.0340081E+0 8.5505769E+3 1.0344115E+0 8.5530964E+3 1.0331541E+0 8.5556160E+3 1.0300672E+0 8.5581356E+3 1.0259220E+0 8.5606551E+3 1.0217437E+0 8.5631747E+3 1.0185599E+0 8.5656942E+3 1.0151457E+0 8.5682138E+3 1.0125115E+0 8.5707333E+3 1.0105728E+0 8.5732529E+3 1.0071155E+0 8.5757725E+3 1.0033821E+0 8.5782920E+3 1.0006339E+0 8.5808116E+3 9.9832820E-1 8.5833311E+3 9.9679062E-1 8.5858507E+3 9.9714413E-1 8.5883702E+3 9.9684617E-1 8.5908898E+3 9.9676189E-1 8.5934094E+3 9.9485380E-1 8.5959289E+3 9.9217873E-1 8.5984485E+3 9.8766356E-1 8.6009680E+3 9.8346472E-1 8.6034876E+3 9.8061687E-1 8.6060071E+3 9.7964311E-1 8.6085267E+3 9.7923731E-1 8.6110463E+3 9.8062782E-1 8.6135658E+3 9.8367080E-1 8.6160854E+3 9.8885792E-1 8.6186049E+3 9.9251778E-1 8.6211245E+3 9.9541023E-1 8.6236440E+3 1.0008445E+0 8.6261636E+3 1.0053323E+0 8.6290083E+3 1.0108198E+0 8.6318529E+3 1.0152371E+0 8.6346976E+3 1.0168119E+0 8.6375422E+3 1.0173977E+0 8.6403869E+3 1.0177455E+0 8.6432316E+3 1.0154347E+0 8.6460762E+3 1.0135769E+0 8.6489209E+3 1.0085603E+0 8.6517656E+3 1.0020884E+0 8.6546102E+3 9.9620968E-1 8.6574549E+3 9.9092214E-1 8.6602995E+3 9.8715195E-1 8.6631442E+3 9.8437928E-1 8.6659889E+3 9.8490380E-1 8.6688335E+3 9.8651367E-1 8.6716782E+3 9.8801610E-1 8.6745228E+3 9.8921549E-1 8.6773675E+3 9.9023489E-1 8.6802122E+3 9.9124598E-1 8.6830568E+3 9.9058247E-1 8.6859015E+3 9.9043213E-1 8.6887462E+3 9.9069630E-1 8.6915908E+3 9.9375980E-1 8.6944355E+3 9.9617939E-1 8.6972801E+3 9.9954656E-1 8.7001248E+3 1.0032708E+0 8.7029695E+3 1.0063592E+0 8.7058141E+3 1.0099597E+0 8.7086588E+3 1.0123900E+0 8.7115035E+3 1.0147777E+0 8.7143481E+3 1.0160414E+0 8.7173890E+3 1.0157375E+0 8.7204298E+3 1.0143761E+0 8.7234707E+3 1.0117998E+0 8.7265115E+3 1.0089594E+0 8.7295524E+3 1.0057434E+0 8.7325932E+3 1.0006195E+0 8.7356340E+3 9.9649888E-1 8.7386749E+3 9.9217778E-1 8.7417157E+3 9.8912265E-1 8.7447566E+3 9.8739565E-1 8.7477974E+3 9.8762911E-1 8.7508383E+3 9.8880623E-1 8.7538791E+3 9.9066705E-1 8.7569200E+3 9.9334953E-1 8.7599608E+3 9.9551743E-1 8.7630017E+3 9.9664035E-1 8.7660425E+3 9.9716375E-1 8.7690834E+3 9.9727026E-1 8.7721242E+3 9.9774591E-1 8.7751651E+3 9.9769279E-1 8.7782059E+3 9.9804948E-1 8.7812467E+3 9.9773316E-1 8.7842876E+3 9.9701346E-1 8.7873284E+3 9.9802731E-1 8.7903693E+3 9.9940054E-1 8.7934101E+3 1.0002061E+0 8.7964510E+3 1.0011316E+0 8.7994918E+3 1.0027635E+0 8.8025327E+3 1.0039248E+0 8.8059244E+3 1.0048820E+0 8.8093161E+3 1.0069235E+0 8.8127078E+3 1.0091062E+0 8.8160995E+3 1.0107551E+0 8.8194912E+3 1.0106834E+0 8.8228830E+3 1.0105649E+0 8.8262747E+3 1.0096880E+0 8.8296664E+3 1.0095806E+0 8.8330581E+3 1.0084990E+0 8.8364498E+3 1.0072841E+0 8.8398415E+3 1.0057034E+0 8.8432332E+3 1.0040360E+0 8.8466250E+3 1.0036670E+0 8.8500167E+3 1.0030774E+0 8.8534084E+3 1.0030081E+0 8.8568001E+3 1.0024990E+0 8.8601918E+3 1.0022452E+0 8.8635835E+3 1.0027207E+0 8.8669752E+3 1.0035254E+0 8.8703670E+3 1.0026064E+0 8.8737587E+3 1.0034891E+0 8.8771504E+3 1.0045430E+0 8.8805421E+3 1.0049623E+0 8.8839338E+3 1.0044841E+0 8.8873255E+3 1.0060078E+0 8.8907173E+3 1.0072633E+0 8.8943916E+3 1.0075458E+0 8.8980660E+3 1.0093169E+0 8.9017403E+3 1.0109209E+0 8.9054147E+3 1.0133200E+0 8.9090890E+3 1.0148400E+0 8.9127634E+3 1.0149890E+0 8.9164378E+3 1.0151294E+0 8.9201121E+3 1.0148043E+0 8.9237865E+3 1.0137022E+0 8.9274608E+3 1.0129851E+0 8.9311352E+3 1.0121241E+0 8.9348096E+3 1.0115116E+0 8.9384839E+3 1.0113599E+0 8.9421583E+3 1.0121646E+0 8.9458326E+3 1.0125751E+0 8.9495070E+3 1.0124518E+0 8.9531813E+3 1.0122118E+0 8.9568557E+3 1.0119550E+0 8.9605301E+3 1.0121961E+0 8.9642044E+3 1.0125556E+0 8.9678788E+3 1.0123913E+0 8.9715531E+3 1.0143750E+0 8.9752275E+3 1.0149052E+0 8.9789019E+3 1.0149266E+0 8.9827360E+3 1.0163669E+0 8.9865701E+3 1.0168249E+0 8.9904042E+3 1.0178274E+0 8.9942383E+3 1.0181719E+0 8.9980724E+3 1.0195063E+0 9.0019065E+3 1.0208873E+0 9.0057407E+3 1.0215341E+0 9.0095748E+3 1.0220925E+0 9.0134089E+3 1.0229333E+0 9.0172430E+3 1.0238930E+0 9.0210771E+3 1.0241327E+0 9.0249112E+3 1.0241039E+0 9.0287453E+3 1.0238570E+0 9.0325795E+3 1.0232697E+0 9.0364136E+3 1.0238954E+0 9.0402477E+3 1.0243265E+0 9.0440818E+3 1.0232058E+0 9.0479159E+3 1.0240996E+0 9.0517500E+3 1.0241860E+0 9.0555841E+3 1.0243291E+0 9.0594183E+3 1.0254229E+0 9.0632524E+3 1.0260072E+0