title name: Arrojadite title formula: title sites1: Al1, Ca1, F, Fe1-7, K, Na1-4, O1-26, P1-7 title refer1: American Mineralogist 66 (1981) 1034-1049 title schoen: c_2h^4 title notes1: Moore P B, Araki T, Merlino S, Mellini M, Zanazzi P F title notes2: The arrojadite-dickinsonite series, KNa4Ca(Fe,Mn)14Al(OH)2(PO4)12: title notes3: Crystal structure and crystal chemistry title notes4: sample NP title notes5: American Mineralogist Crystal Structure Database title notes6: ftp://ftp.geo.arizona.edu/pub/xtal/data/066103401.amc space = A2/a a = 24.730000 b = 10.057000 c = 16.526000 beta = 105.78000 core = Al1 atoms # elem. x y z tag occ. Al 0.00000 0.50000 0.00000 Al1 1.000 Fe 0.47380 0.89570 0.22020 Fe1 0.327 Fe 0.26740 0.00780 0.21230 Fe2 0.654 Fe 0.13940 0.01420 0.10660 Fe3 0.654 Fe 0.40360 0.24960 0.02220 Fe4 0.654 Fe 0.40040 0.74340 0.03340 Fe5 0.654 Fe 0.35170 0.69920 0.20440 Fe6 0.654 Fe 0.34320 0.29450 0.21930 Fe7 0.654 Mn 0.47380 0.89570 0.22020 Mn1 0.173 Mn 0.26740 0.00780 0.21230 Mn2 0.346 Mn 0.13940 0.01420 0.10660 Mn3 0.346 Mn 0.40360 0.24960 0.02220 Mn4 0.346 Mn 0.40040 0.74340 0.03340 Mn5 0.346 Mn 0.35170 0.69920 0.20440 Mn6 0.346 Mn 0.34320 0.29450 0.21930 Mn7 0.346 Ca 0.48480 0.22230 0.23220 Ca1 0.500 Na 0.12020 0.51500 0.12890 Na1 1.000 Na 0.00000 0.00000 0.00000 Na2 1.000 Na 0.25000 0.14600 0.00000 Na3 0.500 Na 0.45670 0.94170 0.20770 Na4 0.500 Na 0.25000 0.91920 0.00000 Na5 0.500 K 0.25000 0.50430 0.00000 K1 1.000 P 0.36620 0.00850 0.11300 P1 0.500 P 0.33540 0.99480 0.07990 P2 0.500 P 0.42460 0.46700 0.13030 P3 1.000 P 0.03850 0.25180 0.12590 P4 1.000 P 0.04740 0.76730 0.10230 P5 1.000 P 0.21150 0.72410 0.13040 P6 1.000 P 0.20450 0.29720 0.14250 P7 1.000 O 0.36750 0.06140 0.02500 O1 1.000 O 0.36350 -0.14160 0.11200 O2 1.000 O 0.32200 0.07700 0.14260 O3 0.500 O 0.42220 0.04620 0.18070 O4 0.500 O 0.27200 0.96780 0.02340 O5 0.500 O 0.42220 0.04620 0.18070 O6 0.500 O 0.44500 0.44480 0.05010 O7 1.000 O 0.39240 0.58790 0.12130 O8 1.000 O 0.38710 0.34450 0.13010 O9 1.000 O 0.47330 0.46370 0.21030 O10 1.000 O 0.07510 0.16640 0.08420 O11 1.000 O 0.03600 0.39510 0.09410 O12 1.000 O -0.02060 0.18910 0.10780 O13 1.000 O 0.06230 0.25330 0.22240 O14 1.000 O 0.04820 0.64280 0.04670 O15 1.000 O 0.07940 0.87190 0.06520 O16 1.000 O -0.01260 -0.81390 0.09610 O17 1.000 O 0.07700 0.73570 0.19390 O18 1.000 O 0.17030 0.67850 0.04840 O19 1.000 O 0.27030 0.67810 0.13150 O20 1.000 O 0.20880 0.87730 0.13950 O21 1.000 O 0.19380 0.66040 0.20440 O22 1.000 O 0.16530 0.34020 0.05830 O23 1.000 O 0.26320 0.35090 0.15160 O24 1.000 O 0.20520 0.14470 0.14890 O25 1.000 O 0.18240 0.35410 0.21560 O26 1.000 O 0.13830 0.00130 0.23150 O27 0.500 F 0.13830 0.00130 0.23150 F 0.500