Joyti,

The coordination number of Rh-C bonds is defined as the total number of Rh-C bonds in the sample divided by the total number of Rh atoms in the sample.
Anatoly
-------------------------------------------------------------------
Anatoly I. Frenkel
Professor
Department of Materials Science and Chemical Engineering (primary appointment)
Department of Chemistry (affiliate appointment)
Stony Brook University
Stony Brook, NY 11794

Email:  anatoly.frenkel@stonybrook.edu
Co-Director and Spokesperson, Synchrotron Catalysis Consortium (SCC) at BNL
http://you.stonybrook.edu/scc2

Joint Appointment:
Senior Chemist
Chemistry Division, Brookhaven National Laboratory
Upton, NY 11973. Ph: 631-344-3013. Group: 631-344-3494
Email: frenkel@bnl.gov

https://www.bnl.gov/staff/frenkel
-------------------------------------------------------------------


On Mon, Apr 24, 2023 at 12:25 PM Jyoti Pandey <jyotipandey51092@gmail.com> wrote:
Hello everyone,

I have a cluster of 13 Rh atoms above the graphene sheet. The first coordination number that I am getting is around 1.65 (which is obtained by choosing a Rh-C) path. I am curious to know whether this value is the "exact" or the "average" coordination number w.r.t all the Rh atoms.

Thanks

With Best Regards

Dr. Jyoti Pandey, Ph.D.
Postdoctoral Researcher
Department of Physics
Central Michigan University, MI, USA
Mobile No. +1-928-265-0599
.....................................

_______________________________________________
Ifeffit mailing list
Ifeffit@millenia.cars.aps.anl.gov
http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit