Your feff inp has a Sn atom 2Ang away from your absorbing Sn. Should that be substituting for a Ge at ~2. 6Ang instead? 2Ang is too short a distance for Sn-Sn metallic/covalent. . . 2. 8 - 3. 0 would be more reasonable. * x y z ipot tag distance occupancy
ZjQcmQRYFpfptBannerStart
This Message Is From an External Sender
This message came from outside your organization.
 
ZjQcmQRYFpfptBannerEnd
Your feff inp has a Sn atom 2Ang away from your absorbing Sn.
Should that be substituting for a Ge at ~2.6Ang instead?

2Ang is too short a distance for Sn-Sn metallic/covalent...2.8 - 3.0 would be
more reasonable.

*   x          y          z     ipot   tag    distance   occupancy
 -0.000000   0.000000   0.000000 0  Sn(abs)    0.00000         *1
 -1.379100   1.447800   0.075150 1     Sn    2.00092         *1
  1.483650  -1.502850   1.483200 2     Ge    2.58063         *1
  1.528650   1.506600  -1.445400 2     Ge    2.58762         *1
 -1.487700  -1.531050  -1.488750 2     Ge    2.60264         *1
 -1.423050   1.539600   1.552350 2     Ge    2.60868         *1


On 2024-12-04 12:38 p.m., Anis Attiaoui via Ifeffit wrote:
Dear Matt and Community, I am having a problem related to a specific .inp file when I am trying to generate the inp file from its corresponding cif with feff8. I am attaching the .cif and feff. inp. The error I am getting is the following: ‘’
ZjQcmQRYFpfptBannerStart
This Message Is From an External Sender
This message came from outside your organization.
 
ZjQcmQRYFpfptBannerEnd

Dear Matt and Community,

 

I am having a problem related to a specific .inp file when I am trying to generate the inp file from its corresponding cif with feff8. I am attaching the .cif and feff.inp.

 

The error I am getting is the following:

‘’
Calculating potentials ...

    free atom potential and density for atom type    0

    free atom potential and density for atom type    1

    free atom potential and density for atom type    2

    initial state energy

    overlapped potential and density for unique potential    0

    overlapped potential and density for unique potential    1

    overlapped potential and density for unique potential    2

    muffin tin radii and interstitial parameters

    : ipot, Norman radius, Muffin tin radius, Overlap

         0  1.49498E+00  1.39776E+00  1.15000E+00

         1  1.20678E+00  8.53844E-01  1.15000E+00

         2  1.56883E+00  1.42805E+00  1.15000E+00

tell authors to INCREASE NOVP

‘’

 

I did try to run the same cif using ARTEMIS and it worked wo any issues using the feff6L instead of version 8.

Thus, I tried to use the new Larixite ciff2feffinp module and use the feff6L instead of version 8 but I noticed this is not installed yet.

 

I also found that a similar issue has previously been documented but I didn’t find any clear answers in there.

https://millenia.cars.aps.anl.gov/feff/feffusers/msg00255.html

 

Any suggestions will be tremendously appreciated.

Thank you very much.

Dr. Anis Attiaoui,

 

Stanford University, GLAM

Dept. Material Science and Engineering,

McCullough Building,

476 Lomita Mall, Stanford

California, USA, 94305

Office/shipping: McC-203

Tel: +1(650)485-0501

Web: https://mcintyre.stanford.edu

 

 

 


ifeffit mailing list:  https://millenia.cars.aps.anl.gov/mailman3/lists/ifeffit.millenia.cars.aps.anl.gov/
to unsubscribe, send mail to ifeffit-leave@millenia.cars.aps.anl.gov