Calculations of EXAFS averaged over an atomic configuration which may include up to a few tens of thousands atoms was implemented into the PMCProfile code for reverse
http://www.nist.gov/mml/ceramics/structure_determination/rmcprofile-utilities.cfm
Victor Krayzman
Ceramics Division. MML. NIST