# E I0 It 8782.9478 159190 125360 8800.4368 158910 124840 8818.0011 159920 126810 8835.641 161220 129260 8853.3572 162450 131510 8871.15 163940 134060 8889.02 165220 136610 8906.9676 166340 138800 8924.9934 167600 141180 8943.0978 168890 143410 8961.2813 169510 144060 8961.9901 169090 143550 8962.6989 169110 143480 8963.4079 169670 143940 8964.117 169580 143810 8964.8263 169420 143340 8965.5356 169550 143370 8966.2451 169480 143150 8966.9547 169410 142980 8967.6644 169780 143070 8968.3742 169470 142450 8969.0841 169210 141930 8969.7942 169360 141500 8970.5044 169150 140600 8971.2147 168800 139630 8971.9252 168420 138350 8972.6357 168240 136360 8973.3464 167490 133550 8974.0572 166660 129200 8974.7681 165390 121700 8975.4791 163240 107580 8976.1903 159460 82537 8976.9016 151880 61009 8977.613 136640 48960 8978.3245 119090 41493 8979.0361 116320 41299 8979.7479 120730 44121 8980.4598 123790 45589 8981.1718 121680 43218 8981.8839 117250 39397 8982.5962 113760 36532 8983.3085 111300 34330 8984.021 109330 32133 8984.7336 106570 29584 8985.4464 102780 26525 8986.1592 98911 23610 8986.8722 94689 20708 8987.5853 89996 18138 8988.2985 84839 16054 8989.0119 79632 14300 8989.7253 75900 13192 8990.4389 73922 12716 8991.1526 72669 12581 8991.8665 71644 12713 8992.5804 70417 12865 8993.2945 69763 13148 8994.0087 70171 13503 8994.723 71490 13930 8995.4374 73225 14251 8996.152 74888 14409 8996.8667 76314 14287 8997.5815 77830 13981 8998.2964 79371 13701 8999.0115 80758 13475 8999.7266 81587 13329 9000.4419 82145 13530 9001.1573 82232 13778 9001.8729 82233 14188 9002.5885 82172 14557 9003.3043 82126 14926 9004.0202 81993 15186 9004.7362 81647 15351 9005.4524 81167 15576 9006.1687 80577 15759 9006.8851 80132 15947 9007.6016 80021 16068 9008.3182 79934 16154 9009.035 80173 16187 9009.7518 80461 16202 9010.4688 80556 16129 9011.186 80606 15999 9011.9032 80800 15975 9013.4406 81695 15665 9015.0811 83639 15413 9016.8248 85378 15098 9018.5693 86752 14776 9020.3144 88069 14525 9022.163 88905 14379 9024.0125 89202 14570 9025.8627 89278 15080 9027.8166 88934 15639 9029.7715 88102 16129 9031.8302 86986 16332 9033.8899 85730 16250 9036.0537 84461 15992 9038.2185 82970 15567 9040.3845 80013 15154 9042.6549 81460 15423 9044.9265 81114 15238 9047.3026 81684 15117 9049.68 82371 15136 9052.0589 82691 15168 9054.5425 83050 14944 9057.0276 83392 14700 9059.5142 83796 14538 9062.106 84119 14470 9064.8031 84058 14221 9067.3981 84091 14020 9070.2025 83900 13999 9072.9048 83772 14190 9075.7129 83881 14727 9078.5228 83978 15180 9081.4387 84150 15627 9084.3567 84671 15907 9087.381 85309 16164 9090.4075 86255 16750 9093.4361 83956 17261 9096.4669 87601 17461 9099.7091 88022 17162 9102.8491 88423 16774 9106.0961 88230 16313 9109.3457 88062 16125 9112.7027 87711 16019 9116.0624 87635 16002 9119.4247 87507 15640 9122.8948 87486 14960 9126.3678 87436 14514 9129.8437 87479 14489 9133.4278 87256 14596 9137.015 87208 14944 9140.7108 86640 15400 9144.4098 86692 16119 9148.112 88157 17166 9151.9233 88304 18074 9155.7381 87894 18411 9159.6624 89065 18341 9163.5902 89620 17695 9167.5217 90026 17095 9171.4568 90332 16878 9175.502 90359 16827 9179.6577 90233 16920 9183.7106 90410 17008 9187.8742 90528 17110 9192.1488 90750 17293 9196.4276 91068 17265 9200.7107 91526 16913 9204.9981 91977 16659 9209.3971 92282 16597 9213.8006 92445 16760 9218.3162 92820 17147 9222.8365 92935 17674 9227.3615 93216 18320 9231.9992 93584 18957 9236.6419 93740 19220 9241.2896 93888 19235 9246.0506 93926 19197 9250.8168 94143 19223 9255.5883 94377 19269 9260.4737 94540 19248 9265.3646 94776 19157 9270.261 95168 19115 9275.2719 95513 19060 9280.2886 95756 19122 9285.3112 96150 19173 9290.4489 96250 19160 9295.5927 96466 19282 9300.8523 96705 19459 9306.0084 97211 19870 9311.2805 97445 20266 9316.6691 97884 20677 9322.0643 98123 20781 9327.4663 98357 20897 9332.8749 98901 21287 9338.4008 98904 21559 9343.9336 99181 21778 9349.4735 99582 21887 9355.1315 99947 22016 9360.7967 100370 22065 9366.4693 100410 22025 9372.2606 100940 22217 9378.0596 100980 22178 9383.8663 101200 22272 9389.7925 101350 22334 9395.7267 101680 22523 9401.669 101830 22685 9407.6192 102240 23045 9413.69 102570 23384 9419.7692 102820 23640 9425.9696 103160 23886 9432.0657 103450 24010 9438.2833 103590 24221 9444.623 103710 24338 9450.8583 104260 24717 9457.216 104440 24817 9463.6966 104920 25242 9470.0727 105030 25315 9476.5721 105400 25512 9483.0811 105460 25506 9489.5995 105780 25601 9496.2421 106080 25744 9502.8947 106450 25851 9509.5571 106590 25997 9516.3447 106940 26284 9523.1426 107310 26611 9529.9508 107550 26893 9536.7694 107950 27159 9543.7143 108310 27408 9550.6699 108720 27719 9557.6363 108890 27870 9564.73 109210 28083 9571.7183 109540 28302 9578.8342 109850 28638 9586.0783 110030 28792 9593.2169 110300 28975 9600.4842 110670 29198 9607.7632 111020 29407 9615.1717 111160 29542 9622.4744 111390 29745 9629.907 111660 29936 9637.3518 112300 30272 9644.9273 112460 30493 9652.3969 112600 30707 9659.9976 113050 30976 9667.6111 113240 31246 9675.3565 113410 31465 9683.1152 113640 31699 9690.7674 113840 31908 9698.6723 114350 32255 9706.4708 114600 32545 9714.4029 114730 32703 9722.3487 114970 32981 9730.3084 115440 33277 9738.282 115670 33563 9746.3905 115920 33741 9754.5134 116430 34096 9762.6507 116360 34224 9770.8025 116850 34559 9779.0906 117180 34858 9787.2715 117160 35035 9795.5894 117550 35335 9804.0449 118050 35680 9812.3931 118420 36031 9820.8794 118500 36269 9829.3814 118730 36519 9837.8989 119020 36800 9846.4321 119240 37077 9855.1051 119890 37545 9863.67 119910 37768 9872.3752 120150 38047 9881.0967 120720 38517 9889.9595 120820 38741 9898.8391 121190 39059 9907.6102 121360 39368 9916.5235 121480 39644 9925.5797 121630 39947 9934.5273 121890 40335 9943.6183 121900 40533 9952.727 122340 40916 9961.8534 122280 41183