4916.30 0.909 4916.34 0.909 4916.38 0.909 4916.42 0.908 4916.46 0.908 4916.50 0.908 4916.54 0.908 4916.58 0.908 4916.62 0.908 4916.65 0.908 4916.69 0.908 4916.73 0.908 4916.77 0.907 4916.81 0.907 4916.85 0.907 4916.89 0.907 4916.93 0.907 4916.97 0.907 4917.01 0.906 4917.05 0.906 4917.08 0.906 4917.12 0.906 4917.16 0.906 4917.20 0.906 4917.24 0.906 4917.28 0.906 4917.32 0.906 4917.36 0.906 4917.40 0.905 4917.44 0.906 4917.47 0.905 4917.51 0.905 4917.55 0.905 4917.59 0.905 4917.63 0.905 4917.67 0.905 4917.71 0.904 4917.75 0.904 4917.79 0.904 4917.83 0.904 4917.87 0.904 4917.90 0.904 4917.94 0.903 4917.98 0.903 4918.02 0.903 4918.06 0.903 4918.10 0.903 4918.14 0.903 4918.18 0.903 4918.22 0.902 4918.26 0.902 4918.30 0.902 4918.33 0.902 4918.37 0.902 4918.41 0.902 4918.45 0.902 4918.49 0.902 4918.53 0.901 4918.57 0.901 4918.61 0.901 4918.65 0.901 4918.69 0.901 4918.73 0.901 4918.76 0.901 4918.80 0.901 4918.84 0.901 4918.88 0.901 4918.92 0.900 4918.96 0.900 4919.00 0.900 4919.04 0.900 4919.08 0.900 4919.12 0.900 4919.16 0.899 4919.19 0.900 4919.23 0.899 4919.27 0.899 4919.31 0.899 4919.35 0.899 4919.39 0.899 4919.43 0.899 4919.47 0.899 4919.51 0.899 4919.55 0.899 4919.59 0.898 4919.63 0.898 4919.66 0.898 4919.70 0.898 4919.74 0.898 4919.78 0.898 4919.82 0.898 4919.86 0.898 4919.90 0.898 4919.94 0.898 4919.98 0.898 4920.02 0.898 4920.06 0.897 4920.09 0.897 4920.13 0.897 4920.17 0.897 4920.21 0.897 4920.25 0.897 4920.29 0.897 4920.33 0.896 4920.37 0.896 4920.41 0.896 4920.45 0.896 4920.49 0.896 4920.52 0.896 4920.56 0.896 4920.60 0.896 4920.64 0.895 4920.68 0.896 4920.72 0.896 4920.76 0.896 4920.80 0.895 4920.84 0.895 4920.88 0.895 4920.92 0.895 4920.96 0.895 4920.99 0.895 4921.03 0.894 4921.07 0.894 4921.11 0.894 4921.15 0.894 4921.19 0.894 4921.23 0.894 4921.27 0.894 4921.31 0.894 4921.35 0.894 4921.39 0.894 4921.43 0.893 4921.46 0.893 4921.50 0.893 4921.54 0.893 4921.58 0.894 4921.62 0.894 4921.66 0.894 4921.70 0.894 4921.74 0.895 4921.78 0.895 4921.82 0.895 4921.86 0.895 4921.89 0.895 4921.93 0.895 4921.97 0.894 4922.01 0.894 4922.05 0.894 4922.09 0.894 4922.13 0.894 4922.17 0.894 4922.21 0.894 4922.25 0.894 4922.29 0.894 4922.33 0.893 4922.36 0.893 4922.40 0.893 4922.44 0.893 4922.48 0.893 4922.52 0.893 4922.56 0.893 4922.60 0.893 4922.64 0.892 4922.68 0.893 4922.72 0.892 4922.76 0.892 4922.80 0.892 4922.83 0.892 4922.87 0.892 4922.91 0.892 4922.95 0.892 4922.99 0.892 4923.03 0.891 4923.07 0.891 4923.11 0.891 4923.15 0.891 4923.19 0.891 4923.23 0.891 4923.27 0.890 4923.30 0.890 4923.34 0.890 4923.38 0.890 4923.42 0.890 4923.46 0.890 4923.50 0.889 4923.54 0.889 4923.58 0.889 4923.62 0.889 4923.66 0.889 4923.70 0.889 4923.74 0.889 4923.78 0.889 4923.81 0.889 4923.85 0.889 4923.89 0.888 4923.93 0.888 4923.97 0.888 4924.01 0.888 4924.05 0.887 4924.09 0.887 4924.13 0.886 4924.17 0.886 4924.21 0.885 4924.25 0.885 4924.28 0.884 4924.32 0.884 4924.36 0.883 4924.40 0.883 4924.44 0.883 4924.48 0.883 4924.52 0.883 4924.56 0.883 4924.60 0.883 4924.64 0.882 4924.68 0.882 4924.72 0.883 4924.75 0.883 4924.79 0.882 4924.83 0.882 4924.87 0.882 4924.91 0.882 4924.95 0.882 4924.99 0.882 4925.03 0.882 4925.07 0.882 4925.11 0.882 4925.15 0.881 4925.19 0.881 4925.23 0.881 4925.26 0.881 4925.30 0.881 4925.34 0.881 4925.38 0.881 4925.42 0.880 4925.46 0.880 4925.50 0.880 4925.54 0.880 4925.58 0.880 4925.62 0.880 4925.66 0.880 4925.70 0.880 4925.74 0.880 4925.77 0.880 4925.81 0.880 4925.85 0.880 4925.89 0.880 4925.93 0.879 4925.97 0.879 4926.01 0.879 4926.05 0.879 4926.09 0.879 4926.13 0.879 4926.17 0.879 4926.21 0.879 4926.25 0.878 4926.28 0.878 4926.32 0.878 4926.36 0.878 4926.40 0.878 4926.44 0.878 4926.48 0.878 4926.52 0.878 4926.56 0.878 4926.60 0.878 4926.64 0.878 4926.68 0.878 4926.72 0.878 4926.76 0.877 4926.79 0.877 4926.83 0.877 4926.87 0.877 4926.91 0.877 4926.95 0.876 4926.99 0.876 4927.03 0.876 4927.07 0.876 4927.11 0.876 4927.15 0.876 4927.19 0.876 4927.23 0.876 4927.27 0.876 4927.30 0.875 4927.34 0.875 4927.38 0.875 4927.42 0.875 4927.46 0.875 4927.50 0.875 4927.54 0.875 4927.58 0.875 4927.62 0.875 4927.66 0.875 4927.70 0.874 4927.74 0.874 4927.78 0.874 4927.81 0.874 4927.85 0.874 4927.89 0.874 4927.93 0.873 4927.97 0.873 4928.01 0.873 4928.05 0.873 4928.09 0.873 4928.13 0.873 4928.17 0.873 4928.21 0.873 4928.25 0.873 4928.29 0.873 4928.33 0.873 4928.36 0.872 4928.40 0.872 4928.44 0.872 4928.48 0.872 4928.52 0.872 4928.56 0.872 4928.60 0.872 4928.64 0.871 4928.68 0.871 4928.72 0.871 4928.76 0.871 4928.80 0.871 4928.84 0.871 4928.87 0.871 4928.91 0.871 4928.95 0.871 4928.99 0.870 4929.03 0.870 4929.07 0.870 4929.11 0.870 4929.15 0.870 4929.19 0.870 4929.23 0.870 4929.27 0.870 4929.31 0.870 4929.35 0.870 4929.39 0.869 4929.42 0.869 4929.46 0.869 4929.50 0.869 4929.54 0.869 4929.58 0.868 4929.62 0.868 4929.66 0.868 4929.70 0.868 4929.74 0.868 4929.78 0.868 4929.82 0.868 4929.86 0.868 4929.90 0.868 4929.94 0.868 4929.97 0.868 4930.01 0.867 4930.05 0.867 4930.09 0.867 4930.13 0.867 4930.17 0.867 4930.21 0.867 4930.25 0.867 4930.29 0.867 4930.33 0.867 4930.37 0.867 4930.41 0.867 4930.45 0.867 4930.49 0.867 4930.53 0.866 4930.56 0.866 4930.60 0.866 4930.64 0.866 4930.68 0.866 4930.72 0.865 4930.76 0.865 4930.80 0.865 4930.84 0.865 4930.88 0.865 4930.92 0.865 4930.96 0.865 4931.00 0.865 4931.04 0.864 4931.08 0.864 4931.11 0.864 4931.15 0.864 4931.19 0.864 4931.23 0.864 4931.27 0.864 4931.31 0.864 4931.35 0.864 4931.39 0.863 4931.43 0.863 4931.47 0.863 4931.51 0.863 4931.55 0.863 4931.59 0.863 4931.63 0.863 4931.67 0.863 4931.70 0.863 4931.74 0.863 4931.78 0.862 4931.82 0.862 4931.86 0.862 4931.90 0.862 4931.94 0.862 4931.98 0.861 4932.02 0.861 4932.06 0.861 4932.10 0.861 4932.14 0.861 4932.18 0.861 4932.22 0.861 4932.26 0.861 4932.29 0.861 4932.33 0.861 4932.37 0.861 4932.41 0.861 4932.45 0.861 4932.49 0.860 4932.53 0.860 4932.57 0.861 4932.61 0.860 4932.65 0.860 4932.69 0.860 4932.73 0.860 4932.77 0.860 4932.81 0.860 4932.85 0.860 4932.88 0.860 4932.92 0.859 4932.96 0.859 4933.00 0.859 4933.04 0.859 4933.08 0.859 4933.12 0.859 4933.16 0.859 4933.20 0.859 4933.24 0.858 4933.28 0.858 4933.32 0.858 4933.36 0.858 4933.40 0.858 4933.44 0.858 4933.47 0.858 4933.51 0.858 4933.55 0.857 4933.59 0.857 4933.63 0.857 4933.67 0.858 4933.71 0.858 4933.75 0.857 4933.79 0.857 4933.83 0.857 4933.87 0.857 4933.91 0.857 4933.95 0.856 4933.99 0.856 4934.03 0.856 4934.07 0.856 4934.10 0.856 4934.14 0.856 4934.18 0.856 4934.22 0.856 4934.26 0.855 4934.30 0.855 4934.34 0.855 4934.38 0.855 4934.42 0.855 4934.46 0.855 4934.50 0.855 4934.54 0.855 4934.58 0.855 4934.62 0.855 4934.66 0.855 4934.70 0.855 4934.73 0.854 4934.77 0.854 4934.81 0.854 4934.85 0.854 4934.89 0.854 4934.93 0.854 4934.97 0.854 4935.01 0.854 4935.05 0.854 4935.09 0.854 4935.13 0.854 4935.17 0.853 4935.21 0.853 4935.25 0.853 4935.29 0.853 4935.33 0.853 4935.36 0.853 4935.40 0.853 4935.44 0.852 4935.48 0.852 4935.52 0.853 4935.56 0.852 4935.60 0.852 4935.64 0.852 4935.68 0.852 4935.72 0.852 4935.76 0.852 4935.80 0.851 4935.84 0.851 4935.88 0.851 4935.92 0.851 4935.96 0.851 4935.99 0.851 4936.03 0.850 4936.07 0.850 4936.11 0.850 4936.15 0.850 4936.19 0.850 4936.23 0.850 4936.27 0.850 4936.31 0.850 4936.35 0.850 4936.39 0.850 4936.43 0.850 4936.47 0.850 4936.51 0.850 4936.55 0.849 4936.59 0.849 4936.63 0.849 4936.66 0.849 4936.70 0.849 4936.74 0.849 4936.78 0.849 4936.82 0.848 4936.86 0.848 4936.90 0.848 4936.94 0.848 4936.98 0.847 4937.02 0.847 4937.06 0.848 4937.10 0.848 4937.14 0.847 4937.18 0.847 4937.22 0.847 4937.26 0.847 4937.30 0.847 4937.33 0.847 4937.37 0.847 4937.41 0.847 4937.45 0.846 4937.49 0.846 4937.53 0.846 4937.57 0.846 4937.61 0.846 4937.65 0.846 4937.69 0.846 4937.73 0.846 4937.77 0.846 4937.81 0.845 4937.85 0.845 4937.89 0.845 4937.93 0.845 4937.97 0.845 4938.01 0.845 4938.04 0.844 4938.08 0.844 4938.12 0.844 4938.16 0.844 4938.20 0.844 4938.24 0.844 4938.28 0.844 4938.32 0.844 4938.36 0.844 4938.40 0.844 4938.44 0.844 4938.48 0.844 4938.52 0.844 4938.56 0.843 4938.60 0.843 4938.64 0.843 4938.68 0.843 4938.72 0.843 4938.75 0.842 4938.79 0.842 4938.83 0.842 4938.87 0.842 4938.91 0.842 4938.95 0.842 4938.99 0.842 4939.03 0.842 4939.07 0.842 4939.11 0.842 4939.15 0.842 4939.19 0.842 4939.23 0.841 4939.27 0.841 4939.31 0.841 4939.35 0.841 4939.39 0.841 4939.43 0.841 4939.46 0.841 4939.50 0.840 4939.54 0.840 4939.58 0.840 4939.62 0.840 4939.66 0.840 4939.70 0.840 4939.74 0.840 4939.78 0.840 4939.82 0.840 4939.86 0.840 4939.90 0.840 4939.94 0.839 4939.98 0.839 4940.02 0.839 4940.06 0.839 4940.10 0.839 4940.14 0.839 4940.18 0.839 4940.21 0.839 4940.25 0.839 4940.29 0.838 4940.33 0.838 4940.37 0.838 4940.41 0.838 4940.45 0.838 4940.49 0.838 4940.53 0.838 4940.57 0.837 4940.61 0.837 4940.65 0.837 4940.69 0.837 4940.73 0.837 4940.77 0.837 4940.81 0.837 4940.85 0.837 4940.89 0.836 4940.93 0.836 4940.96 0.836 4941.00 0.836 4941.04 0.836 4941.08 0.836 4941.12 0.836 4941.16 0.836 4941.20 0.835 4941.24 0.835 4941.28 0.835 4941.32 0.835 4941.36 0.835 4941.40 0.835 4941.44 0.835 4941.48 0.835 4941.52 0.835 4941.56 0.834 4941.60 0.834 4941.64 0.834 4941.68 0.834 4941.72 0.834 4941.75 0.834 4941.79 0.834 4941.83 0.834 4941.87 0.834 4941.91 0.833 4941.95 0.833 4941.99 0.833 4942.03 0.833 4942.07 0.833 4942.11 0.833 4942.15 0.833 4942.19 0.833 4942.23 0.833 4942.27 0.833 4942.31 0.833 4942.35 0.833 4942.39 0.832 4942.43 0.832 4942.47 0.832 4942.51 0.832 4942.54 0.832 4942.58 0.831 4942.62 0.831 4942.66 0.831 4942.70 0.831 4942.74 0.831 4942.78 0.831 4942.82 0.831 4942.86 0.831 4942.90 0.831 4942.94 0.831 4942.98 0.831 4943.02 0.831 4943.06 0.830 4943.10 0.830 4943.14 0.830 4943.18 0.830 4943.22 0.830 4943.26 0.830 4943.30 0.830 4943.34 0.830 4943.37 0.829 4943.41 0.829 4943.45 0.829 4943.49 0.829 4943.53 0.829 4943.57 0.829 4943.61 0.829 4943.65 0.829 4943.69 0.829 4943.73 0.828 4943.77 0.828 4943.81 0.828 4943.85 0.828 4943.89 0.828 4943.93 0.828 4943.97 0.828 4944.01 0.828 4944.05 0.828 4944.09 0.828 4944.13 0.828 4944.17 0.828 4944.20 0.827 4944.24 0.827 4944.28 0.827 4944.32 0.827 4944.36 0.827 4944.40 0.827 4944.44 0.827 4944.48 0.827 4944.52 0.827 4944.56 0.826 4944.60 0.826 4944.64 0.826 4944.68 0.826 4944.72 0.826 4944.76 0.826 4944.80 0.825 4944.84 0.825 4944.88 0.825 4944.92 0.825 4944.96 0.825 4945.00 0.825 4945.04 0.825 4945.08 0.825 4945.11 0.824 4945.15 0.824 4945.19 0.824 4945.23 0.824 4945.27 0.824 4945.31 0.824 4945.35 0.824 4945.39 0.824 4945.43 0.823 4945.47 0.824 4945.51 0.824 4945.55 0.823 4945.59 0.823 4945.63 0.823 4945.67 0.823 4945.71 0.823 4945.75 0.823 4945.79 0.823 4945.83 0.823 4945.87 0.823 4945.91 0.823 4945.95 0.822 4945.99 0.822 4946.02 0.822 4946.06 0.822 4946.10 0.822 4946.14 0.822 4946.18 0.822 4946.22 0.822 4946.26 0.822 4946.30 0.821 4946.34 0.821 4946.38 0.821 4946.42 0.821 4946.46 0.821 4946.50 0.821 4946.54 0.821 4946.58 0.821 4946.62 0.821 4946.66 0.820 4946.70 0.820 4946.74 0.820 4946.78 0.820 4946.82 0.820 4946.86 0.820 4946.90 0.820 4946.94 0.820 4946.97 0.820 4947.01 0.820 4947.05 0.819 4947.09 0.819 4947.13 0.819 4947.17 0.819 4947.21 0.819 4947.25 0.819 4947.29 0.819 4947.33 0.819 4947.37 0.819 4947.41 0.819 4947.45 0.819 4947.49 0.818 4947.53 0.818 4947.57 0.818 4947.61 0.818 4947.65 0.818 4947.69 0.817 4947.73 0.817 4947.77 0.817 4947.81 0.817 4947.85 0.817 4947.89 0.817 4947.93 0.817 4947.96 0.817 4948.00 0.817 4948.04 0.817 4948.08 0.817 4948.12 0.817 4948.16 0.816 4948.20 0.816 4948.24 0.816 4948.28 0.816 4948.32 0.816 4948.36 0.816 4948.40 0.815 4948.44 0.815 4948.48 0.815 4948.52 0.815 4948.56 0.815 4948.60 0.815 4948.64 0.815 4948.68 0.815 4948.72 0.815 4948.76 0.815 4948.80 0.814 4948.84 0.814 4948.88 0.814 4948.92 0.814 4948.96 0.814 4948.99 0.814 4949.03 0.814 4949.07 0.813 4949.11 0.813 4949.15 0.813 4949.19 0.813 4949.23 0.813 4949.27 0.813 4949.31 0.813 4949.35 0.813 4949.39 0.813 4949.43 0.813 4949.47 0.812 4949.51 0.812 4949.55 0.812 4949.59 0.812 4949.63 0.812 4949.67 0.812 4949.71 0.812 4949.75 0.812 4949.79 0.812 4949.83 0.812 4949.87 0.812 4949.91 0.812 4949.95 0.812 4949.99 0.812 4950.03 0.812 4950.06 0.812 4950.10 0.811 4950.14 0.811 4950.18 0.811 4950.22 0.811 4950.26 0.810 4950.30 0.810 4950.34 0.810 4950.38 0.810 4950.42 0.810 4950.46 0.810 4950.50 0.810 4950.54 0.810 4950.58 0.810 4950.62 0.810 4950.66 0.809 4950.70 0.809 4950.74 0.809 4950.78 0.809 4950.82 0.809 4950.86 0.809 4950.90 0.809 4950.94 0.809 4950.98 0.809 4951.02 0.809 4951.06 0.808 4951.10 0.808 4951.14 0.808 4951.18 0.808 4951.21 0.808 4951.25 0.808 4951.29 0.807 4951.33 0.807 4951.37 0.807 4951.41 0.807 4951.45 0.807 4951.49 0.807 4951.53 0.807 4951.57 0.807 4951.61 0.807 4951.65 0.806 4951.69 0.806 4951.73 0.806 4951.77 0.806 4951.81 0.806 4951.85 0.806 4951.89 0.806 4951.93 0.806 4951.97 0.806 4952.01 0.806 4952.05 0.806 4952.09 0.806 4952.13 0.806 4952.17 0.805 4952.21 0.805 4952.25 0.805 4952.29 0.805 4952.33 0.805 4952.37 0.805 4952.41 0.804 4952.44 0.804 4952.48 0.804 4952.52 0.804 4952.56 0.804 4952.60 0.804 4952.64 0.803 4952.68 0.803 4952.72 0.803 4952.76 0.803 4952.80 0.803 4952.84 0.803 4952.88 0.803 4952.92 0.803 4952.96 0.803 4953.00 0.803 4953.04 0.803 4953.08 0.802 4953.12 0.802 4953.16 0.802 4953.20 0.802 4953.24 0.802 4953.28 0.802 4953.32 0.802 4953.36 0.802 4953.40 0.802 4953.44 0.802 4953.48 0.802 4953.52 0.801 4953.56 0.801 4953.60 0.801 4953.64 0.801 4953.68 0.801 4953.72 0.800 4953.75 0.800 4953.79 0.800 4953.83 0.800 4953.87 0.800 4953.91 0.800 4953.95 0.800 4953.99 0.800 4954.03 0.800 4954.07 0.800 4954.11 0.800 4954.15 0.800 4954.19 0.800 4954.23 0.800 4954.27 0.799 4954.31 0.799 4954.35 0.799 4954.39 0.799 4954.43 0.799 4954.47 0.799 4954.51 0.799 4954.55 0.799 4954.59 0.799 4954.63 0.798 4954.67 0.798 4954.71 0.798 4954.75 0.798 4954.79 0.798 4954.83 0.797 4954.87 0.797 4954.91 0.797 4954.95 0.797 4954.99 0.797 4955.03 0.797 4955.07 0.797 4955.11 0.797 4955.15 0.797 4955.18 0.797 4955.22 0.797 4955.26 0.797 4955.30 0.797 4955.34 0.797 4955.38 0.797 4955.42 0.796 4955.46 0.796 4955.50 0.796 4955.54 0.796 4955.58 0.796 4955.62 0.796 4955.66 0.796 4955.70 0.796 4955.74 0.796 4955.78 0.796 4955.82 0.796 4955.86 0.796 4955.90 0.796 4955.94 0.795 4955.98 0.795 4956.02 0.795 4956.06 0.795 4956.10 0.795 4956.14 0.795 4956.18 0.795 4956.22 0.795 4956.26 0.795 4956.30 0.794 4956.34 0.794 4956.38 0.794 4956.42 0.794 4956.46 0.793 4956.50 0.793 4956.54 0.793 4956.58 0.793 4956.62 0.793 4956.66 0.793 4956.70 0.793 4956.74 0.793 4956.77 0.793 4956.81 0.792 4956.85 0.792 4956.89 0.792 4956.93 0.792 4956.97 0.792 4957.01 0.792 4957.05 0.792 4957.09 0.792 4957.13 0.791 4957.17 0.791 4957.21 0.791 4957.25 0.791 4957.29 0.791 4957.33 0.791 4957.37 0.791 4957.41 0.791 4957.45 0.790 4957.49 0.790 4957.53 0.790 4957.57 0.790 4957.61 0.790 4957.65 0.790 4957.69 0.790 4957.73 0.790 4957.77 0.790 4957.81 0.790 4957.85 0.790 4957.89 0.790 4957.93 0.790 4957.97 0.790 4958.01 0.790 4958.05 0.790 4958.09 0.789 4958.13 0.789 4958.17 0.789 4958.21 0.789 4958.25 0.789 4958.29 0.788 4958.33 0.788 4958.37 0.788 4958.41 0.788 4958.45 0.788 4958.49 0.788 4958.53 0.788 4958.57 0.788 4958.60 0.788 4958.64 0.788 4958.68 0.787 4958.72 0.787 4958.76 0.787 4958.80 0.787 4958.84 0.787 4958.88 0.787 4958.92 0.787 4958.96 0.787 4959.00 0.787 4959.04 0.786 4959.08 0.786 4959.12 0.787 4959.16 0.786 4959.20 0.786 4959.24 0.786 4959.28 0.786 4959.32 0.786 4959.36 0.786 4959.40 0.786 4959.44 0.786 4959.48 0.785 4959.52 0.785 4959.56 0.785 4959.60 0.785 4959.64 0.785 4959.68 0.785 4959.72 0.785 4959.76 0.785 4959.80 0.785 4959.84 0.785 4959.88 0.785 4959.92 0.785 4959.96 0.784 4960.00 0.784 4960.04 0.784 4960.08 0.784 4960.12 0.784 4960.16 0.784 4960.20 0.784 4960.24 0.784 4960.28 0.783 4960.32 0.783 4960.36 0.783 4960.40 0.783 4960.44 0.783 4960.48 0.783 4960.52 0.783 4960.56 0.783 4960.60 0.783 4960.64 0.783 4960.68 0.783 4960.71 0.782 4960.75 0.782 4960.79 0.782 4960.83 0.782 4960.87 0.782 4960.91 0.782 4960.95 0.782 4960.99 0.782 4961.03 0.782 4961.07 0.782 4961.11 0.782 4961.15 0.782 4961.19 0.782 4961.23 0.782 4961.27 0.782 4961.31 0.782 4961.35 0.782 4961.39 0.782 4961.43 0.782 4961.47 0.782 4961.51 0.781 4961.55 0.781 4961.59 0.781 4961.63 0.781 4961.67 0.781 4961.71 0.780 4961.75 0.780 4961.79 0.780 4961.83 0.780 4961.87 0.780 4961.91 0.780 4961.95 0.780 4961.99 0.779 4962.03 0.779 4962.07 0.779 4962.11 0.779 4962.15 0.779 4962.19 0.779 4962.23 0.779 4962.27 0.779 4962.31 0.779 4962.35 0.779 4962.39 0.779 4962.43 0.779 4962.47 0.779 4962.51 0.779 4962.55 0.779 4962.59 0.779 4962.63 0.779 4962.67 0.779 4962.71 0.779 4962.75 0.779 4962.79 0.778 4962.83 0.778 4962.87 0.778 4962.91 0.778 4962.95 0.778 4962.99 0.778 4963.03 0.778 4963.07 0.777 4963.11 0.778 4963.15 0.778 4963.19 0.778 4963.23 0.778 4963.27 0.777 4963.31 0.777 4963.35 0.777 4963.39 0.777 4963.43 0.777 4963.47 0.776 4963.50 0.776 4963.54 0.776 4963.58 0.776 4963.62 0.776 4963.66 0.776 4963.70 0.776 4963.74 0.776 4963.78 0.776 4963.82 0.776 4963.86 0.776 4963.90 0.776 4963.94 0.776 4963.98 0.776 4964.02 0.776 4964.06 0.776 4964.10 0.776 4964.14 0.776 4964.18 0.776 4964.22 0.776 4964.26 0.775 4964.30 0.775 4964.34 0.775 4964.38 0.775 4964.42 0.775 4964.46 0.775 4964.50 0.775 4964.54 0.775 4964.58 0.775 4964.62 0.775 4964.66 0.775 4964.70 0.774 4964.74 0.774 4964.78 0.774 4964.82 0.774 4964.86 0.774 4964.90 0.774 4964.94 0.774 4964.98 0.774 4965.02 0.774 4965.06 0.774 4965.10 0.774 4965.14 0.774 4965.18 0.774 4965.22 0.774 4965.26 0.774 4965.30 0.774 4965.34 0.774 4965.38 0.774 4965.42 0.774 4965.46 0.774 4965.50 0.774 4965.54 0.774 4965.58 0.774 4965.62 0.774 4965.66 0.774 4965.70 0.774 4965.74 0.774 4965.78 0.774 4965.82 0.774 4965.86 0.774 4965.90 0.774 4965.94 0.774 4965.98 0.774 4966.02 0.774 4966.06 0.774 4966.10 0.774 4966.14 0.774 4966.18 0.774 4966.22 0.774 4966.26 0.774 4966.30 0.774 4966.34 0.774 4966.38 0.774 4966.42 0.774 4966.46 0.774 4966.50 0.774 4966.54 0.774 4966.58 0.774 4966.62 0.774 4966.66 0.775 4966.70 0.775 4966.74 0.775 4966.78 0.775 4966.82 0.776 4966.86 0.776 4966.90 0.776 4966.94 0.776 4966.98 0.777 4967.02 0.777 4967.06 0.777 4967.10 0.778 4967.14 0.778 4967.18 0.778 4967.22 0.779 4967.26 0.779 4967.30 0.780 4967.34 0.780 4967.38 0.781 4967.42 0.782 4967.46 0.783 4967.50 0.783 4967.54 0.785 4967.58 0.786 4967.62 0.787 4967.66 0.788 4967.70 0.790 4967.74 0.791 4967.78 0.793 4967.82 0.794 4967.86 0.796 4967.90 0.798 4967.94 0.800 4967.98 0.802 4968.02 0.804 4968.06 0.806 4968.10 0.808 4968.14 0.810 4968.18 0.812 4968.22 0.814 4968.26 0.816 4968.30 0.818 4968.34 0.820 4968.38 0.822 4968.42 0.824 4968.46 0.825 4968.50 0.826 4968.54 0.827 4968.58 0.827 4968.62 0.828 4968.66 0.828 4968.70 0.827 4968.74 0.827 4968.78 0.826 4968.82 0.825 4968.86 0.824 4968.90 0.822 4968.94 0.821 4968.98 0.819 4969.02 0.818 4969.06 0.816 4969.10 0.815 4969.14 0.814 4969.18 0.812 4969.22 0.811 4969.26 0.810 4969.30 0.810 4969.34 0.809 4969.38 0.809 4969.42 0.809 4969.46 0.809 4969.50 0.809 4969.54 0.809 4969.58 0.810 4969.62 0.811 4969.66 0.811 4969.70 0.813 4969.74 0.814 4969.78 0.815 4969.82 0.817 4969.86 0.819 4969.90 0.820 4969.94 0.822 4969.98 0.824 4970.02 0.826 4970.05 0.828 4970.09 0.830 4970.13 0.832 4970.17 0.834 4970.21 0.836 4970.25 0.838 4970.29 0.840 4970.33 0.842 4970.37 0.843 4970.41 0.845 4970.46 0.847 4970.50 0.848 4970.54 0.850 4970.58 0.851 4970.62 0.853 4970.66 0.854 4970.70 0.856 4970.74 0.857 4970.78 0.859 4970.82 0.860 4970.86 0.861 4970.90 0.863 4970.94 0.864 4970.98 0.865 4971.02 0.867 4971.06 0.868 4971.10 0.870 4971.14 0.871 4971.18 0.872 4971.22 0.874 4971.26 0.875 4971.30 0.876 4971.34 0.877 4971.38 0.878 4971.42 0.879 4971.46 0.879 4971.50 0.880 4971.54 0.880 4971.58 0.881 4971.62 0.881 4971.66 0.881 4971.70 0.880 4971.74 0.880 4971.78 0.879 4971.82 0.879 4971.86 0.878 4971.90 0.877 4971.94 0.876 4971.98 0.875 4972.02 0.874 4972.06 0.872 4972.10 0.871 4972.14 0.869 4972.18 0.868 4972.22 0.866 4972.26 0.864 4972.30 0.863 4972.34 0.861 4972.38 0.860 4972.42 0.858 4972.46 0.857 4972.50 0.855 4972.54 0.854 4972.58 0.853 4972.62 0.852 4972.66 0.851 4972.70 0.850 4972.74 0.850 4972.78 0.849 4972.82 0.849 4972.86 0.849 4972.90 0.849 4972.94 0.849 4972.98 0.849 4973.02 0.849 4973.06 0.850 4973.10 0.850 4973.14 0.851 4973.18 0.852 4973.22 0.852 4973.26 0.853 4973.30 0.855 4973.34 0.856 4973.38 0.857 4973.42 0.858 4973.46 0.859 4973.50 0.860 4973.54 0.862 4973.58 0.863 4973.62 0.864 4973.66 0.865 4973.70 0.866 4973.74 0.866 4973.78 0.867 4973.82 0.868 4973.86 0.868 4973.90 0.869 4973.94 0.869 4973.98 0.869 4974.02 0.870 4974.06 0.870 4974.10 0.870 4974.14 0.870 4974.18 0.869 4974.22 0.869 4974.26 0.869 4974.30 0.868 4974.34 0.868 4974.38 0.867 4974.42 0.867 4974.46 0.866 4974.50 0.865 4974.54 0.865 4974.58 0.864 4974.62 0.863 4974.66 0.862 4974.70 0.861 4974.74 0.860 4974.78 0.859 4974.82 0.857 4974.86 0.856 4974.90 0.855 4974.94 0.854 4974.98 0.853 4975.02 0.852 4975.06 0.851 4975.10 0.850 4975.14 0.849 4975.18 0.848 4975.22 0.847 4975.26 0.846 4975.30 0.845 4975.34 0.844 4975.38 0.843 4975.42 0.842 4975.46 0.841 4975.50 0.840 4975.54 0.840 4975.58 0.839 4975.62 0.838 4975.66 0.838 4975.70 0.837 4975.74 0.837 4975.78 0.836 4975.82 0.836 4975.86 0.836 4975.90 0.835 4975.94 0.835 4975.98 0.835 4976.02 0.835 4976.06 0.835 4976.10 0.835 4976.14 0.835 4976.18 0.835 4976.22 0.836 4976.26 0.836 4976.30 0.836 4976.34 0.837 4976.38 0.838 4976.42 0.838 4976.46 0.839 4976.50 0.840 4976.54 0.841 4976.58 0.841 4976.62 0.842 4976.66 0.843 4976.70 0.844 4976.74 0.845 4976.78 0.847 4976.82 0.848 4976.86 0.849 4976.90 0.851 4976.94 0.852 4976.99 0.854 4977.03 0.855 4977.07 0.857 4977.11 0.858 4977.15 0.860 4977.19 0.862 4977.23 0.863 4977.27 0.865 4977.31 0.867 4977.35 0.869 4977.39 0.871 4977.43 0.873 4977.47 0.875 4977.51 0.876 4977.55 0.879 4977.59 0.881 4977.63 0.883 4977.67 0.885 4977.71 0.887 4977.75 0.889 4977.79 0.892 4977.83 0.894 4977.87 0.896 4977.91 0.899 4977.95 0.901 4977.99 0.904 4978.03 0.906 4978.07 0.909 4978.11 0.912 4978.15 0.914 4978.19 0.917 4978.23 0.919 4978.27 0.922 4978.31 0.924 4978.35 0.927 4978.39 0.930 4978.43 0.933 4978.47 0.936 4978.51 0.938 4978.55 0.941 4978.59 0.944 4978.63 0.947 4978.67 0.950 4978.71 0.953 4978.75 0.956 4978.79 0.959 4978.83 0.962 4978.87 0.965 4978.91 0.968 4978.95 0.971 4978.99 0.974 4979.03 0.978 4979.07 0.981 4979.11 0.984 4979.15 0.987 4979.19 0.990 4979.23 0.993 4979.27 0.996 4979.31 0.999 4979.35 1.002 4979.39 1.005 4979.43 1.008 4979.47 1.011 4979.51 1.013 4979.55 1.016 4979.59 1.018 4979.63 1.021 4979.67 1.023 4979.71 1.025 4979.75 1.028 4979.80 1.030 4979.84 1.032 4979.88 1.034 4979.92 1.036 4979.96 1.038 4980.00 1.040 4980.04 1.042 4980.08 1.044 4980.12 1.045 4980.16 1.047 4980.20 1.049 4980.24 1.050 4980.28 1.051 4980.32 1.052 4980.36 1.053 4980.40 1.054 4980.44 1.055 4980.48 1.056 4980.52 1.057 4980.56 1.058 4980.60 1.059 4980.64 1.060 4980.68 1.061 4980.72 1.062 4980.76 1.063 4980.80 1.064 4980.84 1.065 4980.88 1.066 4980.92 1.067 4980.96 1.068 4981.00 1.070 4981.04 1.071 4981.08 1.073 4981.12 1.074 4981.16 1.076 4981.20 1.078 4981.24 1.080 4981.28 1.082 4981.32 1.085 4981.36 1.087 4981.40 1.089 4981.44 1.092 4981.48 1.095 4981.52 1.098 4981.56 1.101 4981.60 1.104 4981.64 1.107 4981.68 1.111 4981.72 1.114 4981.76 1.118 4981.80 1.122 4981.84 1.126 4981.88 1.131 4981.93 1.135 4981.97 1.139 4982.01 1.144 4982.05 1.148 4982.09 1.153 4982.13 1.158 4982.17 1.162 4982.21 1.167 4982.25 1.172 4982.29 1.177 4982.33 1.182 4982.37 1.188 4982.41 1.193 4982.45 1.198 4982.49 1.203 4982.53 1.208 4982.57 1.214 4982.61 1.219 4982.65 1.224 4982.69 1.229 4982.73 1.234 4982.77 1.239 4982.81 1.244 4982.85 1.249 4982.89 1.254 4982.93 1.259 4982.97 1.264 4983.01 1.269 4983.05 1.273 4983.09 1.278 4983.13 1.283 4983.17 1.288 4983.21 1.292 4983.25 1.297 4983.29 1.301 4983.33 1.306 4983.37 1.310 4983.41 1.315 4983.45 1.320 4983.49 1.324 4983.53 1.329 4983.57 1.333 4983.61 1.338 4983.65 1.342 4983.69 1.347 4983.74 1.352 4983.78 1.357 4983.82 1.362 4983.86 1.367 4983.90 1.372 4983.94 1.377 4983.98 1.382 4984.02 1.387 4984.06 1.393 4984.10 1.398 4984.14 1.404 4984.18 1.409 4984.22 1.415 4984.26 1.421 4984.30 1.426 4984.34 1.432 4984.38 1.438 4984.42 1.443 4984.46 1.449 4984.50 1.455 4984.54 1.461 4984.58 1.467 4984.62 1.473 4984.66 1.478 4984.70 1.484 4984.74 1.490 4984.78 1.496 4984.82 1.501 4984.86 1.507 4984.90 1.513 4984.94 1.519 4984.98 1.524 4985.02 1.530 4985.06 1.535 4985.10 1.541 4985.14 1.546 4985.18 1.552 4985.22 1.557 4985.26 1.562 4985.30 1.567 4985.35 1.572 4985.39 1.577 4985.43 1.582 4985.47 1.587 4985.51 1.591 4985.55 1.596 4985.59 1.600 4985.63 1.605 4985.67 1.610 4985.71 1.614 4985.75 1.619 4985.79 1.623 4985.83 1.627 4985.87 1.630 4985.91 1.634 4985.95 1.638 4985.99 1.641 4986.03 1.645 4986.07 1.648 4986.11 1.651 4986.15 1.654 4986.19 1.657 4986.23 1.660 4986.27 1.662 4986.31 1.665 4986.35 1.667 4986.39 1.669 4986.43 1.671 4986.47 1.673 4986.51 1.675 4986.55 1.676 4986.59 1.678 4986.63 1.679 4986.67 1.680 4986.71 1.681 4986.75 1.681 4986.80 1.682 4986.84 1.682 4986.88 1.682 4986.92 1.682 4986.96 1.682 4987.00 1.682 4987.04 1.682 4987.08 1.681 4987.12 1.680 4987.16 1.679 4987.20 1.679 4987.24 1.677 4987.28 1.676 4987.32 1.675 4987.36 1.674 4987.40 1.672 4987.44 1.670 4987.48 1.669 4987.52 1.667 4987.56 1.665 4987.60 1.663 4987.64 1.661 4987.68 1.659 4987.72 1.658 4987.76 1.656 4987.80 1.654 4987.84 1.652 4987.88 1.650 4987.92 1.648 4987.96 1.647 4988.00 1.645 4988.04 1.643 4988.08 1.641 4988.13 1.640 4988.17 1.638 4988.21 1.636 4988.25 1.635 4988.29 1.633 4988.33 1.632 4988.37 1.631 4988.41 1.629 4988.45 1.628 4988.49 1.627 4988.53 1.626 4988.57 1.624 4988.61 1.623 4988.65 1.622 4988.69 1.621 4988.73 1.621 4988.77 1.620 4988.81 1.619 4988.85 1.618 4988.89 1.618 4988.93 1.617 4988.97 1.616 4989.01 1.615 4989.05 1.615 4989.09 1.614 4989.13 1.613 4989.17 1.613 4989.21 1.612 4989.25 1.611 4989.29 1.611 4989.34 1.610 4989.38 1.610 4989.42 1.610 4989.46 1.609 4989.50 1.609 4989.54 1.609 4989.58 1.608 4989.62 1.608 4989.66 1.608 4989.70 1.608 4989.74 1.607 4989.78 1.607 4989.82 1.607 4989.86 1.607 4989.90 1.607 4989.94 1.607 4989.98 1.606 4990.02 1.606 4990.06 1.606 4990.10 1.606 4990.14 1.606 4990.18 1.606 4990.22 1.605 4990.26 1.605 4990.30 1.605 4990.34 1.605 4990.38 1.604 4990.42 1.604 4990.46 1.604 4990.51 1.604 4990.55 1.604 4990.59 1.604 4990.63 1.604 4990.67 1.603 4990.71 1.603 4990.75 1.603 4990.79 1.603 4990.83 1.602 4990.87 1.602 4990.91 1.602 4990.95 1.602 4990.99 1.601 4991.03 1.601 4991.07 1.601 4991.11 1.600 4991.15 1.600 4991.19 1.599 4991.23 1.599 4991.27 1.598 4991.31 1.598 4991.35 1.597 4991.39 1.597 4991.43 1.596 4991.47 1.595 4991.51 1.595 4991.55 1.594 4991.60 1.593 4991.64 1.593 4991.68 1.592 4991.72 1.592 4991.76 1.591 4991.80 1.590 4991.84 1.589 4991.88 1.588 4991.92 1.587 4991.96 1.586 4992.00 1.586 4992.04 1.585 4992.08 1.584 4992.12 1.584 4992.16 1.583 4992.20 1.582 4992.24 1.581 4992.28 1.581 4992.32 1.580 4992.36 1.579 4992.40 1.578 4992.44 1.578 4992.48 1.577 4992.52 1.576 4992.56 1.576 4992.60 1.575 4992.65 1.575 4992.69 1.575 4992.73 1.574 4992.77 1.574 4992.81 1.573 4992.85 1.572 4992.89 1.572 4992.93 1.572 4992.97 1.571 4993.01 1.571 4993.05 1.570 4993.09 1.570 4993.13 1.570 4993.17 1.570 4993.21 1.570 4993.25 1.570 4993.29 1.570 4993.33 1.570 4993.37 1.570 4993.41 1.571 4993.45 1.571 4993.49 1.571 4993.53 1.571 4993.57 1.572 4993.61 1.572 4993.66 1.572 4993.70 1.572 4993.74 1.572 4993.78 1.572 4993.82 1.572 4993.86 1.573 4993.90 1.573 4993.94 1.573 4993.98 1.573 4994.02 1.574 4994.06 1.574 4994.10 1.574 4994.14 1.575 4994.18 1.575 4994.22 1.575 4994.26 1.575 4994.30 1.576 4994.34 1.576 4994.38 1.577 4994.42 1.577 4994.46 1.577 4994.50 1.578 4994.54 1.578 4994.58 1.579 4994.63 1.579 4994.67 1.579 4994.71 1.580 4994.75 1.580 4994.79 1.580 4994.83 1.580 4994.87 1.580 4994.91 1.580 4994.95 1.580 4994.99 1.579 4995.03 1.579 4995.07 1.579 4995.11 1.579 4995.15 1.579 4995.19 1.579 4995.23 1.578 4995.27 1.578 4995.31 1.578 4995.35 1.578 4995.39 1.578 4995.43 1.577 4995.47 1.577 4995.51 1.576 4995.56 1.576 4995.60 1.575 4995.64 1.575 4995.68 1.574 4995.72 1.574 4995.76 1.573 4995.80 1.573 4995.84 1.572 4995.88 1.571 4995.92 1.571 4995.96 1.570 4996.00 1.570 4996.04 1.569 4996.08 1.568 4996.12 1.568 4996.16 1.567 4996.20 1.567 4996.24 1.566 4996.28 1.566 4996.32 1.566 4996.36 1.566 4996.40 1.565 4996.45 1.565 4996.49 1.565 4996.53 1.565 4996.57 1.564 4996.61 1.564 4996.65 1.564 4996.69 1.564 4996.73 1.564 4996.77 1.564 4996.81 1.564 4996.85 1.564 4996.89 1.564 4996.93 1.564 4996.97 1.564 4997.01 1.564 4997.05 1.565 4997.09 1.565 4997.13 1.565 4997.17 1.566 4997.21 1.566 4997.25 1.566 4997.30 1.567 4997.34 1.567 4997.38 1.567 4997.42 1.568 4997.46 1.568 4997.50 1.568 4997.54 1.569 4997.58 1.569 4997.62 1.569 4997.66 1.570 4997.70 1.570 4997.74 1.571 4997.78 1.572 4997.82 1.572 4997.86 1.573 4997.90 1.573 4997.94 1.574 4997.98 1.575 4998.02 1.575 4998.06 1.576 4998.10 1.577 4998.15 1.577 4998.19 1.578 4998.23 1.579 4998.27 1.579 4998.31 1.580 4998.35 1.581 4998.39 1.581 4998.43 1.582 4998.47 1.582 4998.51 1.583 4998.55 1.584 4998.59 1.584 4998.63 1.585 4998.67 1.585 4998.71 1.586 4998.75 1.587 4998.79 1.587 4998.83 1.588 4998.87 1.589 4998.91 1.589 4998.96 1.590 4999.00 1.590 4999.04 1.591 4999.08 1.591 4999.12 1.592 4999.16 1.592 4999.20 1.593 4999.24 1.593 4999.28 1.593 4999.32 1.594 4999.36 1.594 4999.40 1.594 4999.44 1.594 4999.48 1.595 4999.52 1.595 4999.56 1.595 4999.60 1.596 4999.64 1.596 4999.68 1.596 4999.73 1.596 4999.77 1.597 4999.81 1.597 4999.85 1.597 4999.89 1.597 4999.93 1.598 4999.97 1.598 5000.01 1.597 5000.05 1.597 5000.09 1.597 5000.13 1.597 5000.17 1.597 5000.21 1.598 5000.25 1.598 5000.29 1.598 5000.33 1.598 5000.37 1.598 5000.41 1.598 5000.45 1.598 5000.50 1.598 5000.54 1.597 5000.58 1.598 5000.62 1.598 5000.66 1.598 5000.70 1.598 5000.74 1.598 5000.78 1.598 5000.82 1.598 5000.86 1.598 5000.90 1.598 5000.94 1.599 5000.98 1.599 5001.02 1.599 5001.06 1.598 5001.10 1.599 5001.14 1.598 5001.18 1.598 5001.23 1.598 5001.27 1.599 5001.31 1.599 5001.35 1.599 5001.39 1.599 5001.43 1.600 5001.47 1.600 5001.51 1.600 5001.55 1.600 5001.59 1.600 5001.63 1.600 5001.67 1.601 5001.71 1.601 5001.75 1.602 5001.79 1.602 5001.83 1.602 5001.87 1.603 5001.91 1.603 5001.95 1.603 5002.00 1.604 5002.04 1.604 5002.08 1.604 5002.12 1.605 5002.16 1.605 5002.20 1.606 5002.24 1.606 5002.28 1.606 5002.32 1.606 5002.36 1.606 5002.40 1.607 5002.44 1.607 5002.48 1.607 5002.52 1.608 5002.56 1.608 5002.60 1.609 5002.64 1.609 5002.69 1.609 5002.73 1.609 5002.77 1.610 5002.81 1.610 5002.85 1.611 5002.89 1.611 5002.93 1.611 5002.97 1.612 5003.01 1.612 5003.05 1.612 5003.09 1.612 5003.13 1.612 5003.17 1.613 5003.21 1.613 5003.25 1.613 5003.29 1.613 5003.33 1.613 5003.38 1.613 5003.42 1.613 5003.46 1.613 5003.50 1.612 5003.54 1.612 5003.58 1.612 5003.62 1.612 5003.66 1.612 5003.70 1.612 5003.74 1.611 5003.78 1.611 5003.82 1.611 5003.86 1.610 5003.90 1.610 5003.94 1.610 5003.98 1.609 5004.02 1.609 5004.07 1.608 5004.11 1.608 5004.15 1.607 5004.19 1.607 5004.23 1.606 5004.27 1.605 5004.31 1.605 5004.35 1.604 5004.39 1.603 5004.43 1.603 5004.47 1.602 5004.51 1.601 5004.55 1.600 5004.59 1.600 5004.63 1.599 5004.67 1.598 5004.71 1.597 5004.76 1.596 5004.80 1.595 5004.84 1.594 5004.88 1.593 5004.92 1.592 5004.96 1.591 5005.00 1.590 5005.04 1.589 5005.08 1.587 5005.12 1.586 5005.16 1.585 5005.20 1.584 5005.24 1.583 5005.28 1.581 5005.32 1.580 5005.36 1.579 5005.41 1.578 5005.45 1.576 5005.49 1.575 5005.53 1.574 5005.57 1.572 5005.61 1.571 5005.65 1.570 5005.69 1.569 5005.73 1.567 5005.77 1.566 5005.81 1.564 5005.85 1.563 5005.89 1.562 5005.93 1.561 5005.97 1.559 5006.01 1.558 5006.06 1.557 5006.10 1.555 5006.14 1.554 5006.18 1.553 5006.22 1.551 5006.26 1.550 5006.30 1.549 5006.34 1.547 5006.38 1.546 5006.42 1.544 5006.46 1.543 5006.50 1.542 5006.54 1.540 5006.58 1.539 5006.62 1.537 5006.66 1.536 5006.71 1.534 5006.75 1.533 5006.79 1.531 5006.83 1.529 5006.87 1.527 5006.91 1.525 5006.95 1.523 5006.99 1.521 5007.03 1.518 5007.07 1.516 5007.11 1.514 5007.15 1.511 5007.19 1.509 5007.23 1.506 5007.27 1.504 5007.32 1.502 5007.36 1.500 5007.40 1.498 5007.44 1.496 5007.48 1.495 5007.52 1.493 5007.56 1.492 5007.60 1.490 5007.64 1.489 5007.68 1.488 5007.72 1.486 5007.76 1.485 5007.80 1.484 5007.84 1.482 5007.88 1.481 5007.93 1.480 5007.97 1.479 5008.01 1.478 5008.05 1.476 5008.09 1.475 5008.13 1.474 5008.17 1.473 5008.21 1.471 5008.25 1.470 5008.29 1.469 5008.33 1.468 5008.37 1.467 5008.41 1.466 5008.45 1.464 5008.49 1.463 5008.54 1.462 5008.58 1.461 5008.62 1.460 5008.66 1.458 5008.70 1.457 5008.74 1.456 5008.78 1.455 5008.82 1.454 5008.86 1.453 5008.90 1.452 5008.94 1.451 5008.98 1.450 5009.02 1.449 5009.06 1.447 5009.10 1.446 5009.15 1.445 5009.19 1.444 5009.23 1.443 5009.27 1.442 5009.31 1.441 5009.35 1.440 5009.39 1.439 5009.43 1.438 5009.47 1.437 5009.51 1.436 5009.55 1.434 5009.59 1.433 5009.63 1.432 5009.67 1.431 5009.72 1.430 5009.76 1.429 5009.80 1.428 5009.84 1.427 5009.88 1.426 5009.92 1.425 5009.96 1.423 5010.00 1.422 5010.04 1.421 5010.08 1.420 5010.12 1.419 5010.16 1.417 5010.20 1.416 5010.24 1.415 5010.28 1.415 5010.33 1.414 5010.37 1.413 5010.41 1.412 5010.45 1.412 5010.49 1.411 5010.53 1.410 5010.57 1.410 5010.61 1.409 5010.65 1.408 5010.69 1.407 5010.73 1.406 5010.77 1.405 5010.81 1.404 5010.85 1.403 5010.90 1.402 5010.94 1.401 5010.98 1.400 5011.02 1.399 5011.06 1.398 5011.10 1.397 5011.14 1.395 5011.18 1.394 5011.22 1.393 5011.26 1.392 5011.30 1.390 5011.34 1.389 5011.38 1.388 5011.43 1.386 5011.47 1.385 5011.51 1.384 5011.55 1.382 5011.59 1.381 5011.63 1.380 5011.67 1.379 5011.71 1.378 5011.75 1.377 5011.79 1.376 5011.83 1.375 5011.87 1.373 5011.91 1.372 5011.95 1.371 5012.00 1.370 5012.04 1.369 5012.08 1.368 5012.12 1.366 5012.16 1.365 5012.20 1.364 5012.24 1.363 5012.28 1.362 5012.32 1.362 5012.36 1.361 5012.40 1.360 5012.44 1.359 5012.48 1.358 5012.53 1.357 5012.57 1.356 5012.61 1.355 5012.65 1.354 5012.69 1.353 5012.73 1.352 5012.77 1.351 5012.81 1.350 5012.85 1.349 5012.89 1.348 5012.93 1.348 5012.97 1.347 5013.01 1.346 5013.05 1.345 5013.10 1.344 5013.14 1.343 5013.18 1.343 5013.22 1.342 5013.26 1.341 5013.30 1.340 5013.34 1.340 5013.38 1.339 5013.42 1.338 5013.46 1.338 5013.50 1.337 5013.54 1.336 5013.58 1.336 5013.63 1.335 5013.67 1.335 5013.71 1.334 5013.75 1.334 5013.79 1.333 5013.83 1.333 5013.87 1.332 5013.91 1.332 5013.95 1.331 5013.99 1.331 5014.03 1.330 5014.07 1.330 5014.11 1.329 5014.16 1.329 5014.20 1.329 5014.24 1.328 5014.28 1.328 5014.32 1.328 5014.36 1.327 5014.40 1.327 5014.44 1.326 5014.48 1.326 5014.52 1.326 5014.56 1.326 5014.60 1.325 5014.64 1.325 5014.69 1.325 5014.73 1.325 5014.77 1.325 5014.81 1.325 5014.85 1.325 5014.89 1.325 5014.93 1.325 5014.97 1.324 5015.01 1.324 5015.05 1.324 5015.09 1.324 5015.13 1.324 5015.18 1.324 5015.22 1.324 5015.26 1.324 5015.30 1.324 5015.34 1.323 5015.38 1.323 5015.42 1.323 5015.46 1.323 5015.50 1.323 5015.54 1.323 5015.58 1.323 5015.62 1.323 5015.66 1.323 5015.71 1.323 5015.75 1.323 5015.79 1.323 5015.83 1.323 5015.87 1.323 5015.91 1.323 5015.95 1.323 5015.99 1.323 5016.03 1.323 5016.07 1.323 5016.11 1.323 5016.15 1.323 5016.20 1.323 5016.24 1.323 5016.28 1.323 5016.32 1.323 5016.36 1.323 5016.40 1.323 5016.44 1.323 5016.48 1.323 5016.52 1.323 5016.56 1.323 5016.60 1.323 5016.64 1.323 5016.69 1.324 5016.73 1.324 5016.77 1.324 5016.81 1.324 5016.85 1.324 5016.89 1.324 5016.93 1.324 5016.97 1.324 5017.01 1.324 5017.05 1.324 5017.09 1.324 5017.13 1.324 5017.18 1.325 5017.22 1.325 5017.26 1.325 5017.30 1.325 5017.34 1.325 5017.38 1.325 5017.42 1.325 5017.46 1.325 5017.50 1.325 5017.54 1.325 5017.58 1.325 5017.62 1.324 5017.67 1.324 5017.71 1.324 5017.75 1.324 5017.79 1.324 5017.83 1.324 5017.87 1.324 5017.91 1.324 5017.95 1.324 5017.99 1.324 5018.03 1.324 5018.07 1.324 5018.11 1.324 5018.16 1.324 5018.20 1.324 5018.24 1.324 5018.28 1.324 5018.32 1.324 5018.36 1.324 5018.40 1.324 5018.44 1.323 5018.48 1.323 5018.52 1.323 5018.56 1.323 5018.60 1.323 5018.65 1.323 5018.69 1.323 5018.73 1.323 5018.77 1.323 5018.81 1.323 5018.85 1.323 5018.89 1.323 5018.93 1.323 5018.97 1.323 5019.01 1.323 5019.05 1.323 5019.09 1.323 5019.14 1.323 5019.18 1.322 5019.22 1.322 5019.26 1.322 5019.30 1.322 5019.34 1.322 5019.38 1.321 5019.42 1.321 5019.46 1.321 5019.50 1.321 5019.54 1.320 5019.59 1.320 5019.63 1.320 5019.67 1.320 5019.71 1.320 5019.75 1.320 5019.79 1.319 5019.83 1.319 5019.87 1.319 5019.91 1.319 5019.95 1.318 5019.99 1.318 5020.03 1.318 5020.08 1.318 5020.12 1.317 5020.16 1.317 5020.20 1.317 5020.24 1.316 5020.28 1.316 5020.32 1.316 5020.36 1.315 5020.40 1.315 5020.44 1.315 5020.48 1.315 5020.53 1.314 5020.57 1.314 5020.61 1.314 5020.65 1.314 5020.69 1.313 5020.73 1.313 5020.77 1.313 5020.81 1.312 5020.85 1.312 5020.89 1.312 5020.93 1.312 5020.98 1.311 5021.02 1.311 5021.06 1.311 5021.10 1.311 5021.14 1.310 5021.18 1.310 5021.22 1.310 5021.26 1.309 5021.30 1.309 5021.34 1.309 5021.38 1.309 5021.43 1.308 5021.47 1.308 5021.51 1.308 5021.55 1.307 5021.59 1.307 5021.63 1.307 5021.67 1.306 5021.71 1.306 5021.75 1.306 5021.79 1.305 5021.83 1.305 5021.88 1.304 5021.92 1.304 5021.96 1.304 5022.00 1.304 5022.04 1.303 5022.08 1.303 5022.12 1.303 5022.16 1.303 5022.20 1.302 5022.24 1.302 5022.28 1.301 5022.33 1.301 5022.37 1.300 5022.41 1.300 5022.45 1.300 5022.49 1.299 5022.53 1.299 5022.57 1.299 5022.61 1.299 5022.65 1.298 5022.69 1.298 5022.73 1.298 5022.78 1.298 5022.82 1.297 5022.86 1.297 5022.90 1.297 5022.94 1.297 5022.98 1.297 5023.02 1.296 5023.06 1.296 5023.10 1.296 5023.14 1.296 5023.18 1.295 5023.23 1.295 5023.27 1.295 5023.31 1.295 5023.35 1.294 5023.39 1.294 5023.43 1.294 5023.47 1.294 5023.51 1.293 5023.55 1.293 5023.59 1.293 5023.64 1.293 5023.68 1.293 5023.72 1.293 5023.76 1.293 5023.80 1.293 5023.84 1.293 5023.88 1.292 5023.92 1.292 5023.96 1.292 5024.00 1.292 5024.04 1.291 5024.09 1.291 5024.13 1.291 5024.17 1.291 5024.21 1.291 5024.25 1.291 5024.29 1.291 5024.33 1.290 5024.37 1.290 5024.41 1.290 5024.45 1.290 5024.50 1.290 5024.54 1.290 5024.58 1.290 5024.62 1.289 5024.66 1.289 5024.70 1.289 5024.74 1.289 5024.78 1.289 5024.82 1.289 5024.86 1.289 5024.90 1.289 5024.95 1.289 5024.99 1.288 5025.03 1.288 5025.07 1.288 5025.11 1.288 5025.15 1.288 5025.19 1.288 5025.23 1.288 5025.27 1.288 5025.31 1.287 5025.36 1.287 5025.40 1.287 5025.44 1.287 5025.48 1.287 5025.52 1.287 5025.56 1.287 5025.60 1.287 5025.64 1.287 5025.68 1.287 5025.72 1.287 5025.77 1.287 5025.81 1.287 5025.85 1.288 5025.89 1.288 5025.93 1.288 5025.97 1.288 5026.01 1.288 5026.05 1.288 5026.09 1.287 5026.13 1.287 5026.18 1.288 5026.22 1.288 5026.26 1.288 5026.30 1.288 5026.34 1.288 5026.38 1.288 5026.42 1.287 5026.46 1.287 5026.50 1.287 5026.54 1.287 5026.59 1.287 5026.63 1.287 5026.67 1.287 5026.71 1.287 5026.75 1.287 5026.79 1.287 5026.83 1.287 5026.87 1.287 5026.91 1.287 5026.95 1.287 5027.00 1.287 5027.04 1.287 5027.08 1.287 5027.12 1.287 5027.16 1.287 5027.20 1.288 5027.24 1.288 5027.28 1.288 5027.32 1.288 5027.36 1.288 5027.41 1.288 5027.45 1.288 5027.49 1.288 5027.53 1.288 5027.57 1.288 5027.61 1.288 5027.65 1.288 5027.69 1.288 5027.73 1.288 5027.77 1.288 5027.82 1.288 5027.86 1.288 5027.90 1.288 5027.94 1.288 5027.98 1.288 5028.02 1.288 5028.06 1.288 5028.10 1.288 5028.14 1.288 5028.18 1.288 5028.23 1.288 5028.27 1.288 5028.31 1.288 5028.35 1.288 5028.39 1.288 5028.43 1.289 5028.47 1.289 5028.51 1.289 5028.55 1.289 5028.60 1.289 5028.64 1.289 5028.68 1.289 5028.72 1.289 5028.76 1.289 5028.80 1.289 5028.84 1.289 5028.88 1.289 5028.92 1.289 5028.96 1.289 5029.01 1.289 5029.05 1.289 5029.09 1.289 5029.13 1.289 5029.17 1.289 5029.21 1.289 5029.25 1.289 5029.29 1.289 5029.33 1.289 5029.37 1.289 5029.42 1.289 5029.46 1.289 5029.50 1.289 5029.54 1.289 5029.58 1.289 5029.62 1.289 5029.66 1.289 5029.70 1.289 5029.74 1.289 5029.79 1.289 5029.83 1.289 5029.87 1.289 5029.91 1.290 5029.95 1.289 5029.99 1.289 5030.03 1.289 5030.07 1.289 5030.11 1.289 5030.15 1.289 5030.20 1.289 5030.24 1.289 5030.28 1.289 5030.32 1.289 5030.36 1.289 5030.40 1.290 5030.44 1.290 5030.48 1.290 5030.52 1.290 5030.57 1.290 5030.61 1.290 5030.65 1.290 5030.69 1.290 5030.73 1.290 5030.77 1.290 5030.81 1.290 5030.85 1.290 5030.89 1.290 5030.94 1.290 5030.98 1.290 5031.02 1.290 5031.06 1.290 5031.10 1.290 5031.14 1.290 5031.18 1.290 5031.22 1.290 5031.26 1.290 5031.30 1.290 5031.35 1.290 5031.39 1.290 5031.43 1.290 5031.47 1.290 5031.51 1.290 5031.55 1.290 5031.59 1.290 5031.63 1.290 5031.67 1.290 5031.72 1.289 5031.76 1.289 5031.80 1.289 5031.84 1.288 5031.88 1.288 5031.92 1.287 5031.96 1.286 5032.00 1.285 5032.04 1.284 5032.09 1.282 5032.13 1.281 5032.17 1.280 5032.21 1.279 5032.25 1.278 5032.29 1.277 5032.33 1.277 5032.37 1.276 5032.41 1.276 5032.46 1.275 5032.50 1.275 5032.54 1.275 5032.58 1.275 5032.62 1.275 5032.66 1.275 5032.70 1.275 5032.74 1.275 5032.78 1.275 5032.83 1.275 5032.87 1.276 5032.91 1.276 5032.95 1.276 5032.99 1.276 5033.03 1.277 5033.07 1.277 5033.11 1.277 5033.15 1.277 5033.20 1.278 5033.24 1.278 5033.28 1.278 5033.32 1.278 5033.36 1.278 5033.40 1.279 5033.44 1.279 5033.48 1.279 5033.52 1.280 5033.57 1.280 5033.61 1.281 5033.65 1.281 5033.69 1.282 5033.73 1.283 5033.77 1.284 5033.81 1.285 5033.85 1.286 5033.89 1.287 5033.94 1.288 5033.98 1.289 5034.02 1.290 5034.06 1.291 5034.10 1.291 5034.14 1.292 5034.18 1.292 5034.22 1.293 5034.26 1.293 5034.31 1.293 5034.35 1.293 5034.39 1.294 5034.43 1.294 5034.47 1.294 5034.51 1.294 5034.55 1.294 5034.59 1.294 5034.63 1.294 5034.68 1.294 5034.72 1.294 5034.76 1.294 5034.80 1.294 5034.84 1.294 5034.88 1.294 5034.92 1.294 5034.96 1.294 5035.01 1.293 5035.05 1.293 5035.09 1.293 5035.13 1.293 5035.17 1.293 5035.21 1.293 5035.25 1.293 5035.29 1.293 5035.33 1.293 5035.38 1.293 5035.42 1.293 5035.46 1.292 5035.50 1.292 5035.54 1.292 5035.58 1.292 5035.62 1.292 5035.66 1.292 5035.70 1.292 5035.75 1.292 5035.79 1.292 5035.83 1.292 5035.87 1.292 5035.91 1.292 5035.95 1.292 5035.99 1.292 5036.03 1.292 5036.08 1.291 5036.12 1.291 5036.16 1.291 5036.20 1.291 5036.24 1.291 5036.28 1.291 5036.32 1.291 5036.36 1.291 5036.40 1.291 5036.45 1.291 5036.49 1.291 5036.53 1.291 5036.57 1.291 5036.61 1.291 5036.65 1.291 5036.69 1.290 5036.73 1.290 5036.78 1.290 5036.82 1.290 5036.86 1.290 5036.90 1.290 5036.94 1.290 5036.98 1.290 5037.02 1.290 5037.06 1.290 5037.10 1.290 5037.15 1.290 5037.19 1.290 5037.23 1.290 5037.27 1.290 5037.31 1.290 5037.35 1.290 5037.39 1.290 5037.43 1.290 5037.48 1.290 5037.52 1.290 5037.56 1.289 5037.60 1.289 5037.64 1.289 5037.68 1.289 5037.72 1.289 5037.76 1.289 5037.80 1.289 5037.85 1.289 5037.89 1.289 5037.93 1.289 5037.97 1.289 5038.01 1.289 5038.05 1.290 5038.09 1.290 5038.13 1.290 5038.18 1.290 5038.22 1.290 5038.26 1.290 5038.30 1.290 5038.34 1.290 5038.38 1.290 5038.42 1.290 5038.46 1.290 5038.51 1.290 5038.55 1.290 5038.59 1.290 5038.63 1.290 5038.67 1.290 5038.71 1.290 5038.75 1.290 5038.79 1.290 5038.84 1.290 5038.88 1.290 5038.92 1.290 5038.96 1.290 5039.00 1.290 5039.04 1.290 5039.08 1.290 5039.12 1.290 5039.16 1.291 5039.21 1.291 5039.25 1.291 5039.29 1.291 5039.33 1.291 5039.37 1.291 5039.41 1.291 5039.45 1.291 5039.49 1.292 5039.54 1.292 5039.58 1.292 5039.62 1.292 5039.66 1.292 5039.70 1.292 5039.74 1.292 5039.78 1.293 5039.82 1.293 5039.87 1.293 5039.91 1.293 5039.95 1.293 5039.99 1.293 5040.03 1.294 5040.07 1.294 5040.11 1.294 5040.15 1.294 5040.20 1.294 5040.24 1.294 5040.28 1.294 5040.32 1.295 5040.36 1.295 5040.40 1.295 5040.44 1.295 5040.48 1.295 5040.53 1.296 5040.57 1.296 5040.61 1.296 5040.65 1.296 5040.69 1.297 5040.73 1.297 5040.77 1.297 5040.81 1.297 5040.86 1.298 5040.90 1.298 5040.94 1.298 5040.98 1.298 5041.02 1.299 5041.06 1.299 5041.10 1.299 5041.14 1.299 5041.19 1.300 5041.23 1.300 5041.27 1.300 5041.31 1.300 5041.35 1.300 5041.39 1.301 5041.43 1.301 5041.47 1.301 5041.52 1.301 5041.56 1.301 5041.60 1.302 5041.64 1.302 5041.68 1.302 5041.72 1.302 5041.76 1.302 5041.80 1.303 5041.85 1.303 5041.89 1.303 5041.93 1.304 5041.97 1.304 5042.01 1.304 5042.05 1.304 5042.09 1.304 5042.13 1.305 5042.18 1.305 5042.22 1.305 5042.26 1.306 5042.30 1.306 5042.34 1.306 5042.38 1.306 5042.42 1.307 5042.47 1.307 5042.51 1.307 5042.55 1.307 5042.59 1.307 5042.63 1.308 5042.67 1.308 5042.71 1.308 5042.75 1.308 5042.80 1.309 5042.84 1.309 5042.88 1.309 5042.92 1.310 5042.96 1.310 5043.00 1.310 5043.04 1.310 5043.08 1.310 5043.13 1.310 5043.17 1.310 5043.21 1.310 5043.25 1.310 5043.29 1.311 5043.33 1.311 5043.37 1.311 5043.41 1.311 5043.46 1.311 5043.50 1.311 5043.54 1.311 5043.58 1.312 5043.62 1.312 5043.66 1.312 5043.70 1.312 5043.75 1.312 5043.79 1.312 5043.83 1.312 5043.87 1.312 5043.91 1.313 5043.95 1.313 5043.99 1.313 5044.03 1.313 5044.08 1.313 5044.12 1.313 5044.16 1.313 5044.20 1.313 5044.24 1.313 5044.28 1.313 5044.32 1.313 5044.36 1.313 5044.41 1.313 5044.45 1.314 5044.49 1.314 5044.53 1.314 5044.57 1.314 5044.61 1.314 5044.65 1.314 5044.70 1.314 5044.74 1.314 5044.78 1.314 5044.82 1.314 5044.86 1.314 5044.90 1.314 5044.94 1.314 5044.98 1.314 5045.03 1.314 5045.07 1.314 5045.11 1.314 5045.15 1.314 5045.19 1.314 5045.23 1.314 5045.27 1.314 5045.32 1.314 5045.36 1.314 5045.40 1.314 5045.44 1.314 5045.48 1.314 5045.52 1.314 5045.56 1.314 5045.60 1.314 5045.65 1.314 5045.69 1.314 5045.73 1.313 5045.77 1.313 5045.81 1.313 5045.85 1.313 5045.89 1.313 5045.94 1.313 5045.98 1.313 5046.02 1.313 5046.06 1.313 5046.10 1.313 5046.14 1.313 5046.18 1.313 5046.22 1.313 5046.27 1.312 5046.31 1.312 5046.35 1.312 5046.39 1.312 5046.43 1.312 5046.47 1.312 5046.51 1.312 5046.56 1.312 5046.60 1.312 5046.64 1.312 5046.68 1.312 5046.72 1.312 5046.76 1.312 5046.80 1.312 5046.84 1.312 5046.89 1.312 5046.93 1.312 5046.97 1.312 5047.01 1.312 5047.05 1.311 5047.09 1.311 5047.13 1.311 5047.18 1.311 5047.22 1.311 5047.26 1.311 5047.30 1.311 5047.34 1.311 5047.38 1.311 5047.42 1.311 5047.47 1.311 5047.51 1.311 5047.55 1.311 5047.59 1.311 5047.63 1.311 5047.67 1.311 5047.71 1.311 5047.76 1.310 5047.80 1.310 5047.84 1.310 5047.88 1.310 5047.92 1.310 5047.96 1.310 5048.00 1.310 5048.04 1.310 5048.09 1.310 5048.13 1.310 5048.17 1.310 5048.21 1.310 5048.25 1.310 5048.29 1.310 5048.33 1.310 5048.38 1.309 5048.42 1.309 5048.46 1.309 5048.50 1.309 5048.54 1.309 5048.58 1.309 5048.62 1.309 5048.67 1.309 5048.71 1.309 5048.75 1.309 5048.79 1.309 5048.83 1.309 5048.87 1.309 5048.91 1.309 5048.96 1.309 5049.00 1.309 5049.04 1.309 5049.08 1.309 5049.12 1.309 5049.16 1.309 5049.20 1.309 5049.25 1.309 5049.29 1.309 5049.33 1.309 5049.37 1.309 5049.41 1.309 5049.45 1.309 5049.49 1.309 5049.53 1.309 5049.58 1.308 5049.62 1.308 5049.66 1.308 5049.70 1.308 5049.74 1.308 5049.78 1.308 5049.82 1.308 5049.87 1.308 5049.91 1.308 5049.95 1.308 5049.99 1.307 5050.03 1.307 5050.07 1.307 5050.11 1.307 5050.16 1.307 5050.20 1.307 5050.24 1.307 5050.28 1.307 5050.32 1.307 5050.36 1.307 5050.40 1.307 5050.45 1.307 5050.49 1.306 5050.53 1.306 5050.57 1.306 5050.61 1.306 5050.65 1.306 5050.69 1.306 5050.74 1.306 5050.78 1.306 5050.82 1.305 5050.86 1.305 5050.90 1.305 5050.94 1.305 5050.98 1.305 5051.03 1.305 5051.07 1.305 5051.11 1.305 5051.15 1.304 5051.19 1.304 5051.23 1.304 5051.27 1.304 5051.32 1.304 5051.36 1.304 5051.40 1.304 5051.44 1.304 5051.48 1.304 5051.52 1.304 5051.56 1.304 5051.61 1.304 5051.65 1.304 5051.69 1.304 5051.73 1.304 5051.77 1.304 5051.81 1.304 5051.85 1.304 5051.90 1.304 5051.94 1.304 5051.98 1.304 5052.02 1.304 5052.06 1.304 5052.10 1.304 5052.15 1.304 5052.19 1.304 5052.23 1.304 5052.27 1.303 5052.31 1.303 5052.35 1.303 5052.39 1.303 5052.44 1.303 5052.48 1.303 5052.52 1.303 5052.56 1.303 5052.60 1.303 5052.64 1.302 5052.68 1.302 5052.73 1.302 5052.77 1.302 5052.81 1.302 5052.85 1.302 5052.89 1.302 5052.93 1.302 5052.97 1.302 5053.02 1.302 5053.06 1.302 5053.10 1.302 5053.14 1.302 5053.18 1.302 5053.22 1.302 5053.26 1.302 5053.31 1.302 5053.35 1.302 5053.39 1.302 5053.43 1.302 5053.47 1.302 5053.51 1.302 5053.55 1.302 5053.60 1.302 5053.64 1.302 5053.68 1.302 5053.72 1.302 5053.76 1.302 5053.80 1.302 5053.85 1.302 5053.89 1.302 5053.93 1.302 5053.97 1.302 5054.01 1.302 5054.05 1.302 5054.09 1.302 5054.14 1.302 5054.18 1.302 5054.22 1.302 5054.26 1.302 5054.30 1.302 5054.34 1.302 5054.38 1.302 5054.43 1.302 5054.47 1.302 5054.51 1.302 5054.55 1.302 5054.59 1.303 5054.63 1.303 5054.68 1.303 5054.72 1.303 5054.76 1.303 5054.80 1.302 5054.84 1.302 5054.88 1.302 5054.92 1.302 5054.97 1.302 5055.01 1.302 5055.05 1.302 5055.09 1.302 5055.13 1.303 5055.17 1.303 5055.21 1.303 5055.26 1.303 5055.30 1.303 5055.34 1.302 5055.38 1.302 5055.42 1.301 5055.46 1.301 5055.51 1.300 5055.55 1.300 5055.59 1.300 5055.63 1.299 5055.67 1.299 5055.71 1.300 5055.75 1.300 5055.80 1.300 5055.84 1.300 5055.88 1.301 5055.92 1.301 5055.96 1.301 5056.00 1.302 5056.05 1.302 5056.09 1.302 5056.13 1.303 5056.17 1.303 5056.21 1.304 5056.25 1.304 5056.29 1.304 5056.34 1.304 5056.38 1.304 5056.42 1.305 5056.46 1.305 5056.50 1.305 5056.54 1.305 5056.58 1.306 5056.63 1.306 5056.67 1.306 5056.71 1.306 5056.75 1.306 5056.79 1.306 5056.83 1.306 5056.88 1.306 5056.92 1.307 5056.96 1.307 5057.00 1.307 5057.04 1.307 5057.08 1.307 5057.12 1.307 5057.17 1.307 5057.21 1.307 5057.25 1.307 5057.29 1.307 5057.33 1.307 5057.37 1.307 5057.42 1.307 5057.46 1.307 5057.50 1.307 5057.54 1.307 5057.58 1.308 5057.62 1.308 5057.67 1.308 5057.71 1.308 5057.75 1.308 5057.79 1.308 5057.83 1.308 5057.87 1.308 5057.91 1.308 5057.96 1.309 5058.00 1.309 5058.04 1.309 5058.08 1.309 5058.12 1.309 5058.16 1.309 5058.21 1.309 5058.25 1.310 5058.29 1.310 5058.33 1.310 5058.37 1.310 5058.41 1.310 5058.45 1.310 5058.50 1.310 5058.54 1.310 5058.58 1.310 5058.62 1.310 5058.66 1.310 5058.70 1.310 5058.75 1.310 5058.79 1.310 5058.83 1.310 5058.87 1.310 5058.91 1.310 5058.95 1.310 5059.00 1.310 5059.04 1.310 5059.08 1.310 5059.12 1.310 5059.16 1.311 5059.20 1.311 5059.24 1.311 5059.29 1.311 5059.33 1.311 5059.37 1.311 5059.41 1.311 5059.45 1.311 5059.49 1.311 5059.54 1.311 5059.58 1.311 5059.62 1.311 5059.66 1.311 5059.70 1.311 5059.74 1.311 5059.79 1.311 5059.83 1.311 5059.87 1.311 5059.91 1.311 5059.95 1.311 5059.99 1.311 5060.03 1.311 5060.08 1.311 5060.12 1.311 5060.16 1.311 5060.20 1.311 5060.24 1.311 5060.28 1.311 5060.33 1.311 5060.37 1.311 5060.41 1.311 5060.45 1.311 5060.49 1.311 5060.53 1.311 5060.58 1.311 5060.62 1.311 5060.66 1.311 5060.70 1.311 5060.74 1.311 5060.78 1.311 5060.83 1.311 5060.87 1.311 5060.91 1.311 5060.95 1.311 5060.99 1.311 5061.03 1.311 5061.07 1.311 5061.12 1.311 5061.16 1.311 5061.20 1.311 5061.24 1.311 5061.28 1.311 5061.32 1.311 5061.37 1.311 5061.41 1.311 5061.45 1.311 5061.49 1.311 5061.53 1.311 5061.57 1.311 5061.62 1.311 5061.66 1.311 5061.70 1.311 5061.74 1.311 5061.78 1.311 5061.82 1.311 5061.87 1.310 5061.91 1.310 5061.95 1.310 5061.99 1.310 5062.03 1.310 5062.07 1.310 5062.12 1.310 5062.16 1.310 5062.20 1.310 5062.24 1.310 5062.28 1.310 5062.32 1.310 5062.37 1.310 5062.41 1.310 5062.45 1.310 5062.49 1.310 5062.53 1.310 5062.57 1.309 5062.62 1.309 5062.66 1.309 5062.70 1.309 5062.74 1.309 5062.78 1.309 5062.82 1.309 5062.86 1.309 5062.91 1.308 5062.95 1.308 5062.99 1.308 5063.03 1.308 5063.07 1.308 5063.11 1.308 5063.16 1.308 5063.20 1.308 5063.24 1.308 5063.28 1.308 5063.32 1.307 5063.36 1.307 5063.41 1.307 5063.45 1.307 5063.49 1.307 5063.53 1.307 5063.57 1.307 5063.61 1.307 5063.66 1.306 5063.70 1.306 5063.74 1.306 5063.78 1.306 5063.82 1.306 5063.86 1.305 5063.91 1.305 5063.95 1.305 5063.99 1.305 5064.03 1.305 5064.07 1.305 5064.11 1.305 5064.16 1.305 5064.20 1.305 5064.24 1.304 5064.28 1.304 5064.32 1.304 5064.36 1.304 5064.41 1.304 5064.45 1.304 5064.49 1.304 5064.53 1.303 5064.57 1.303 5064.61 1.303 5064.66 1.303 5064.70 1.303 5064.74 1.303 5064.78 1.303 5064.82 1.303 5064.86 1.302 5064.91 1.302 5064.95 1.302 5064.99 1.302 5065.03 1.302 5065.07 1.302 5065.11 1.302 5065.16 1.302 5065.20 1.301 5065.24 1.301 5065.28 1.301 5065.32 1.301 5065.37 1.300 5065.41 1.300 5065.45 1.300 5065.49 1.300 5065.53 1.300 5065.57 1.300 5065.62 1.299 5065.66 1.299 5065.70 1.299 5065.74 1.299 5065.78 1.299 5065.82 1.299 5065.87 1.299 5065.91 1.298 5065.95 1.298 5065.99 1.298 5066.03 1.298 5066.07 1.298 5066.12 1.297 5066.16 1.297 5066.20 1.297 5066.24 1.296 5066.28 1.296 5066.32 1.296 5066.37 1.296 5066.41 1.296 5066.45 1.295 5066.49 1.295 5066.53 1.295 5066.57 1.295 5066.62 1.295 5066.66 1.295 5066.70 1.294 5066.74 1.294 5066.78 1.294 5066.82 1.294 5066.87 1.294 5066.91 1.294 5066.95 1.294 5066.99 1.293 5067.03 1.293 5067.08 1.293 5067.12 1.293 5067.16 1.293 5067.20 1.293 5067.24 1.292 5067.28 1.292 5067.33 1.292 5067.37 1.291 5067.41 1.291 5067.45 1.291 5067.49 1.291 5067.53 1.291 5067.58 1.290 5067.62 1.290 5067.66 1.290 5067.70 1.290 5067.74 1.289 5067.78 1.289 5067.83 1.289 5067.87 1.289 5067.91 1.289 5067.95 1.289 5067.99 1.288 5068.03 1.288 5068.08 1.288 5068.12 1.287 5068.16 1.287 5068.20 1.287 5068.24 1.286 5068.29 1.286 5068.33 1.286 5068.37 1.286 5068.41 1.285 5068.45 1.285 5068.49 1.285 5068.54 1.285 5068.58 1.284 5068.62 1.284 5068.66 1.284 5068.70 1.284 5068.74 1.283 5068.79 1.283 5068.83 1.283 5068.87 1.283 5068.91 1.283 5068.95 1.282 5069.00 1.282 5069.04 1.282 5069.08 1.282 5069.12 1.282 5069.16 1.281 5069.20 1.281 5069.25 1.281 5069.29 1.281 5069.33 1.280 5069.37 1.280 5069.41 1.280 5069.45 1.280 5069.50 1.279 5069.54 1.279 5069.58 1.279 5069.62 1.279 5069.66 1.279 5069.70 1.278 5069.75 1.278 5069.79 1.278 5069.83 1.278 5069.87 1.278 5069.91 1.277 5069.96 1.277 5070.00 1.277 5070.04 1.277 5070.08 1.276 5070.12 1.276 5070.16 1.276 5070.21 1.275 5070.25 1.275 5070.29 1.275 5070.33 1.274 5070.37 1.274 5070.42 1.274 5070.46 1.273 5070.50 1.273 5070.54 1.273 5070.58 1.273 5070.62 1.272 5070.67 1.272 5070.71 1.272 5070.75 1.272 5070.79 1.271 5070.83 1.271 5070.87 1.271 5070.92 1.270 5070.96 1.270 5071.00 1.270 5071.04 1.270 5071.08 1.270 5071.13 1.269 5071.17 1.269 5071.21 1.269 5071.25 1.269 5071.29 1.268 5071.33 1.268 5071.38 1.268 5071.42 1.267 5071.46 1.267 5071.50 1.267 5071.54 1.267 5071.59 1.267 5071.63 1.267 5071.67 1.266 5071.71 1.266 5071.75 1.266 5071.79 1.265 5071.84 1.265 5071.88 1.265 5071.92 1.265 5071.96 1.264 5072.00 1.264 5072.05 1.264 5072.09 1.263 5072.13 1.263 5072.17 1.263 5072.21 1.262 5072.25 1.262 5072.30 1.262 5072.34 1.262 5072.38 1.262 5072.42 1.261 5072.46 1.261 5072.51 1.261 5072.55 1.261 5072.59 1.260 5072.63 1.260 5072.67 1.260 5072.71 1.259 5072.76 1.259 5072.80 1.259 5072.84 1.259 5072.88 1.258 5072.92 1.258 5072.97 1.258 5073.01 1.258 5073.05 1.257 5073.09 1.257 5073.13 1.257 5073.17 1.257 5073.22 1.256 5073.26 1.256 5073.30 1.256 5073.34 1.256 5073.38 1.255 5073.43 1.255 5073.47 1.255 5073.51 1.254 5073.55 1.254 5073.59 1.254 5073.63 1.253 5073.68 1.253 5073.72 1.253 5073.76 1.252 5073.80 1.252 5073.84 1.252 5073.89 1.251 5073.93 1.251 5073.97 1.251 5074.01 1.251 5074.05 1.250 5074.09 1.250 5074.14 1.250 5074.18 1.250 5074.22 1.249 5074.26 1.249 5074.30 1.249 5074.35 1.248 5074.39 1.248 5074.43 1.248 5074.47 1.247 5074.51 1.247 5074.56 1.247 5074.60 1.246 5074.64 1.246 5074.68 1.245 5074.72 1.245 5074.76 1.244 5074.81 1.244 5074.85 1.243 5074.89 1.242 5074.93 1.242 5074.97 1.241 5075.02 1.240 5075.06 1.239 5075.10 1.238 5075.14 1.237 5075.18 1.235 5075.23 1.234 5075.27 1.233 5075.31 1.232 5075.35 1.230 5075.39 1.229 5075.43 1.227 5075.48 1.225 5075.52 1.224 5075.56 1.222 5075.60 1.220 5075.64 1.219 5075.69 1.217 5075.73 1.215 5075.77 1.214 5075.81 1.212 5075.85 1.211 5075.90 1.210 5075.94 1.209 5075.98 1.208 5076.02 1.207 5076.06 1.207 5076.10 1.206 5076.15 1.206 5076.19 1.206 5076.23 1.206 5076.27 1.206 5076.31 1.207 5076.36 1.207 5076.40 1.208 5076.44 1.208 5076.48 1.209 5076.52 1.210 5076.57 1.211 5076.61 1.212 5076.65 1.214 5076.69 1.215 5076.73 1.216 5076.77 1.217 5076.82 1.218 5076.86 1.219 5076.90 1.221 5076.94 1.222 5076.98 1.223 5077.03 1.223 5077.07 1.224 5077.11 1.225 5077.15 1.226 5077.19 1.227 5077.24 1.227 5077.28 1.228 5077.32 1.229 5077.36 1.229 5077.40 1.229 5077.45 1.230 5077.49 1.230 5077.53 1.230 5077.57 1.230 5077.61 1.231 5077.65 1.231 5077.70 1.231 5077.74 1.231 5077.78 1.231 5077.82 1.231 5077.86 1.231 5077.91 1.231 5077.95 1.231 5077.99 1.231 5078.03 1.231 5078.07 1.231 5078.12 1.231 5078.16 1.231 5078.20 1.231 5078.24 1.231 5078.28 1.231 5078.33 1.231 5078.37 1.231 5078.41 1.231 5078.45 1.231 5078.49 1.231 5078.53 1.231 5078.58 1.231 5078.62 1.231 5078.66 1.231 5078.70 1.230 5078.74 1.230 5078.79 1.230 5078.83 1.230 5078.87 1.230 5078.91 1.230 5078.95 1.230 5079.00 1.230 5079.04 1.230 5079.08 1.230 5079.12 1.230 5079.16 1.230 5079.21 1.229 5079.25 1.229 5079.29 1.229 5079.33 1.229 5079.37 1.229 5079.42 1.229 5079.46 1.229 5079.50 1.229 5079.54 1.229 5079.58 1.229 5079.63 1.229 5079.67 1.229 5079.71 1.229 5079.75 1.229 5079.79 1.229 5079.84 1.229 5079.88 1.229 5079.92 1.228 5079.96 1.228 5080.00 1.228 5080.04 1.228 5080.09 1.228 5080.13 1.228 5080.17 1.228 5080.21 1.228 5080.25 1.228 5080.30 1.228 5080.34 1.228 5080.38 1.227 5080.42 1.227 5080.46 1.227 5080.51 1.227 5080.55 1.227 5080.59 1.227 5080.63 1.226 5080.67 1.226 5080.72 1.226 5080.76 1.226 5080.80 1.226 5080.84 1.226 5080.88 1.226 5080.93 1.226 5080.97 1.226 5081.01 1.226 5081.05 1.225 5081.09 1.225 5081.14 1.225 5081.18 1.225 5081.22 1.225 5081.26 1.225 5081.30 1.225 5081.35 1.224 5081.39 1.224 5081.43 1.224 5081.47 1.224 5081.51 1.224 5081.56 1.224 5081.60 1.224 5081.64 1.224 5081.68 1.224 5081.72 1.224 5081.77 1.223 5081.81 1.223 5081.85 1.223 5081.89 1.223 5081.93 1.223 5081.98 1.223 5082.02 1.223 5082.06 1.223 5082.10 1.223 5082.14 1.223 5082.19 1.223 5082.23 1.222 5082.27 1.222 5082.31 1.222 5082.35 1.222 5082.40 1.222 5082.44 1.222 5082.48 1.222 5082.52 1.222 5082.56 1.221 5082.61 1.221 5082.65 1.221 5082.69 1.221 5082.73 1.221 5082.77 1.221 5082.82 1.221 5082.86 1.221 5082.90 1.221 5082.94 1.220 5082.98 1.220 5083.03 1.220 5083.07 1.220 5083.11 1.220 5083.15 1.220 5083.19 1.220 5083.24 1.219 5083.28 1.219 5083.32 1.219 5083.36 1.219 5083.40 1.219 5083.45 1.219 5083.49 1.219 5083.53 1.219 5083.57 1.219 5083.61 1.219 5083.66 1.218 5083.70 1.218 5083.74 1.218 5083.78 1.218 5083.82 1.218 5083.87 1.217 5083.91 1.217 5083.95 1.217 5083.99 1.217 5084.03 1.216 5084.08 1.216 5084.12 1.216 5084.16 1.216 5084.20 1.216 5084.24 1.216 5084.29 1.215 5084.33 1.215 5084.37 1.215 5084.41 1.215 5084.45 1.215 5084.50 1.214 5084.54 1.214 5084.58 1.214 5084.62 1.214 5084.66 1.213 5084.71 1.213 5084.75 1.213 5084.79 1.213 5084.83 1.212 5084.87 1.212 5084.92 1.212 5084.96 1.212 5085.00 1.212 5085.04 1.211 5085.08 1.211 5085.13 1.211 5085.17 1.211 5085.21 1.210 5085.25 1.210 5085.30 1.210 5085.34 1.210 5085.38 1.210 5085.42 1.209 5085.46 1.209 5085.51 1.209 5085.55 1.209 5085.59 1.209 5085.63 1.208 5085.67 1.208 5085.72 1.208 5085.76 1.208 5085.80 1.208 5085.84 1.207 5085.88 1.207 5085.93 1.207 5085.97 1.207 5086.01 1.207 5086.05 1.206 5086.09 1.206 5086.14 1.206 5086.18 1.206 5086.22 1.205 5086.26 1.205 5086.30 1.205 5086.35 1.204 5086.39 1.204 5086.43 1.204 5086.47 1.203 5086.51 1.203 5086.56 1.203 5086.60 1.202 5086.64 1.202 5086.68 1.202 5086.73 1.202 5086.77 1.201 5086.81 1.201 5086.85 1.201 5086.89 1.201 5086.94 1.200 5086.98 1.200 5087.02 1.200 5087.06 1.199 5087.10 1.199 5087.15 1.199 5087.19 1.198 5087.23 1.198 5087.27 1.198 5087.31 1.198 5087.36 1.197 5087.40 1.197 5087.44 1.197 5087.48 1.196 5087.52 1.196 5087.57 1.196 5087.61 1.195 5087.65 1.195 5087.69 1.195 5087.74 1.194 5087.78 1.194 5087.82 1.194 5087.86 1.193 5087.90 1.193 5087.95 1.193 5087.99 1.192 5088.03 1.192 5088.07 1.192 5088.11 1.191 5088.16 1.191 5088.20 1.190 5088.24 1.190 5088.28 1.190 5088.32 1.189 5088.37 1.188 5088.41 1.188 5088.45 1.187 5088.49 1.186 5088.54 1.186 5088.58 1.185 5088.62 1.184 5088.66 1.184 5088.70 1.183 5088.75 1.182 5088.79 1.182 5088.83 1.181 5088.87 1.180 5088.91 1.180 5088.96 1.179 5089.00 1.179 5089.04 1.178 5089.08 1.178 5089.12 1.178 5089.17 1.177 5089.21 1.177 5089.25 1.176 5089.29 1.176 5089.34 1.176 5089.38 1.175 5089.42 1.175 5089.46 1.175 5089.50 1.174 5089.55 1.174 5089.59 1.174 5089.63 1.173 5089.67 1.173 5089.71 1.172 5089.76 1.172 5089.80 1.172 5089.84 1.171 5089.88 1.171 5089.93 1.171 5089.97 1.170 5090.01 1.170 5090.05 1.170 5090.09 1.169 5090.14 1.169 5090.18 1.169 5090.22 1.168 5090.26 1.168 5090.30 1.168 5090.35 1.168 5090.39 1.167 5090.43 1.167 5090.47 1.167 5090.52 1.167 5090.56 1.167 5090.60 1.167 5090.64 1.167 5090.68 1.167 5090.73 1.167 5090.77 1.167 5090.81 1.167 5090.85 1.167 5090.89 1.167 5090.94 1.167 5090.98 1.167 5091.02 1.167 5091.06 1.167 5091.11 1.167 5091.15 1.167 5091.19 1.166 5091.23 1.166 5091.27 1.166 5091.32 1.166 5091.36 1.165 5091.40 1.165 5091.44 1.165 5091.48 1.164 5091.53 1.164 5091.57 1.164 5091.61 1.164 5091.65 1.164 5091.70 1.163 5091.74 1.163 5091.78 1.163 5091.82 1.163 5091.86 1.162 5091.91 1.162 5091.95 1.162 5091.99 1.161 5092.03 1.161 5092.07 1.161 5092.12 1.160 5092.16 1.160 5092.20 1.160 5092.24 1.159 5092.29 1.159 5092.33 1.159 5092.37 1.158 5092.41 1.158 5092.45 1.158 5092.50 1.157 5092.54 1.157 5092.58 1.157 5092.62 1.156 5092.67 1.156 5092.71 1.156 5092.75 1.155 5092.79 1.155 5092.83 1.155 5092.88 1.154 5092.92 1.154 5092.96 1.154 5093.00 1.154 5093.04 1.153 5093.09 1.153 5093.13 1.153 5093.17 1.153 5093.21 1.153 5093.26 1.152 5093.30 1.152 5093.34 1.152 5093.38 1.152 5093.42 1.152 5093.47 1.151 5093.51 1.151 5093.55 1.151 5093.59 1.151 5093.64 1.151 5093.68 1.151 5093.72 1.150 5093.76 1.150 5093.80 1.150 5093.85 1.150 5093.89 1.149 5093.93 1.149 5093.97 1.149 5094.02 1.148 5094.06 1.148 5094.10 1.148 5094.14 1.148 5094.18 1.147 5094.23 1.147 5094.27 1.147 5094.31 1.147 5094.35 1.146 5094.40 1.146 5094.44 1.146 5094.48 1.146 5094.52 1.146 5094.56 1.145 5094.61 1.145 5094.65 1.145 5094.69 1.145 5094.73 1.145 5094.78 1.144 5094.82 1.144 5094.86 1.144 5094.90 1.144 5094.94 1.144 5094.99 1.143 5095.03 1.143 5095.07 1.143 5095.11 1.143 5095.16 1.143 5095.20 1.142 5095.24 1.142 5095.28 1.142 5095.32 1.142 5095.37 1.141 5095.41 1.141 5095.45 1.141 5095.49 1.141 5095.54 1.140 5095.58 1.140 5095.62 1.140 5095.66 1.139 5095.70 1.139 5095.75 1.139 5095.79 1.139 5095.83 1.138 5095.87 1.138 5095.92 1.138 5095.96 1.138 5096.00 1.138 5096.04 1.137 5096.08 1.137 5096.13 1.137 5096.17 1.137 5096.21 1.137 5096.25 1.136 5096.30 1.136 5096.34 1.136 5096.38 1.136 5096.42 1.136 5096.46 1.136 5096.51 1.136 5096.55 1.135 5096.59 1.135 5096.63 1.135 5096.68 1.135 5096.72 1.135 5096.76 1.134 5096.80 1.134 5096.85 1.134 5096.89 1.134 5096.93 1.134 5096.97 1.133 5097.01 1.133 5097.06 1.133 5097.10 1.133 5097.14 1.132 5097.18 1.132 5097.23 1.132 5097.27 1.132 5097.31 1.132 5097.35 1.132 5097.39 1.131 5097.44 1.131 5097.48 1.131 5097.52 1.131 5097.56 1.131 5097.61 1.130 5097.65 1.130 5097.69 1.130 5097.73 1.130 5097.77 1.130 5097.82 1.129 5097.86 1.129 5097.90 1.129 5097.94 1.129 5097.99 1.129 5098.03 1.128 5098.07 1.128 5098.11 1.128 5098.16 1.128 5098.20 1.128 5098.24 1.128 5098.28 1.128 5098.32 1.127 5098.37 1.127 5098.41 1.127 5098.45 1.127 5098.49 1.127 5098.54 1.127 5098.58 1.127 5098.62 1.126 5098.66 1.126 5098.71 1.126 5098.75 1.126 5098.79 1.126 5098.83 1.126 5098.87 1.126 5098.92 1.125 5098.96 1.125 5099.00 1.125 5099.04 1.125 5099.09 1.125 5099.13 1.125 5099.17 1.125 5099.21 1.125 5099.25 1.125 5099.30 1.124 5099.34 1.124 5099.38 1.124 5099.42 1.124 5099.47 1.124 5099.51 1.123 5099.55 1.123 5099.59 1.123 5099.64 1.123 5099.68 1.123 5099.72 1.123 5099.76 1.123 5099.80 1.122 5099.85 1.122 5099.89 1.122 5099.93 1.122 5099.97 1.122 5100.02 1.122 5100.06 1.122 5100.10 1.122 5100.14 1.122 5100.19 1.122 5100.23 1.122 5100.27 1.121 5100.31 1.121 5100.36 1.121 5100.40 1.121 5100.44 1.121 5100.48 1.121 5100.52 1.121 5100.57 1.120 5100.61 1.120 5100.65 1.120 5100.69 1.120 5100.74 1.120 5100.78 1.120 5100.82 1.120 5100.86 1.119 5100.91 1.119 5100.95 1.119 5100.99 1.119 5101.03 1.119 5101.07 1.119 5101.12 1.119 5101.16 1.119 5101.20 1.118 5101.24 1.118 5101.29 1.118 5101.33 1.118 5101.37 1.118 5101.41 1.118 5101.46 1.118 5101.50 1.118 5101.54 1.117 5101.58 1.117 5101.63 1.117 5101.67 1.117 5101.71 1.117 5101.75 1.117 5101.79 1.117 5101.84 1.117 5101.88 1.117 5101.92 1.117 5101.96 1.117 5102.01 1.117 5102.05 1.116 5102.09 1.116 5102.13 1.116 5102.18 1.116 5102.22 1.116 5102.26 1.116 5102.30 1.116 5102.35 1.116 5102.39 1.116 5102.43 1.115 5102.47 1.115 5102.51 1.115 5102.56 1.115 5102.60 1.115 5102.64 1.115 5102.68 1.115 5102.73 1.115 5102.77 1.115 5102.81 1.115 5102.85 1.115 5102.90 1.114 5102.94 1.114 5102.98 1.114 5103.02 1.114 5103.07 1.114 5103.11 1.114 5103.15 1.114 5103.19 1.114 5103.23 1.114 5103.28 1.114 5103.32 1.114 5103.36 1.114 5103.40 1.113 5103.45 1.113 5103.49 1.113 5103.53 1.113 5103.57 1.113 5103.62 1.113 5103.66 1.113 5103.70 1.113 5103.74 1.113 5103.79 1.113 5103.83 1.113 5103.87 1.113 5103.91 1.113 5103.96 1.112 5104.00 1.112 5104.04 1.112 5104.08 1.112 5104.12 1.112 5104.17 1.112 5104.21 1.111 5104.25 1.111 5104.29 1.111 5104.34 1.111 5104.38 1.111 5104.42 1.111 5104.46 1.111 5104.51 1.111 5104.55 1.110 5104.59 1.110 5104.63 1.110 5104.68 1.110 5104.72 1.110 5104.76 1.110 5104.80 1.110 5104.85 1.110 5104.89 1.110 5104.93 1.110 5104.97 1.110 5105.02 1.109 5105.06 1.109 5105.10 1.109 5105.14 1.109 5105.18 1.109 5105.23 1.109 5105.27 1.108 5105.31 1.108 5105.35 1.108 5105.40 1.108 5105.44 1.108 5105.48 1.107 5105.52 1.107 5105.57 1.107 5105.61 1.107 5105.65 1.107 5105.69 1.107 5105.74 1.107 5105.78 1.106 5105.82 1.106 5105.86 1.106 5105.91 1.106 5105.95 1.105 5105.99 1.105 5106.03 1.105 5106.08 1.105 5106.12 1.105 5106.16 1.105 5106.20 1.105 5106.25 1.105 5106.29 1.104 5106.33 1.104 5106.37 1.104 5106.41 1.104 5106.46 1.104 5106.50 1.104 5106.54 1.104 5106.58 1.104 5106.63 1.104 5106.67 1.103 5106.71 1.103 5106.75 1.103 5106.80 1.103 5106.84 1.103 5106.88 1.103 5106.92 1.103 5106.97 1.102 5107.01 1.102 5107.05 1.102 5107.09 1.102 5107.14 1.102 5107.18 1.102 5107.22 1.102 5107.26 1.101 5107.31 1.101 5107.35 1.101 5107.39 1.101 5107.43 1.101 5107.48 1.100 5107.52 1.100 5107.56 1.100 5107.60 1.100 5107.65 1.100 5107.69 1.100 5107.73 1.099 5107.77 1.099 5107.82 1.099 5107.86 1.099 5107.90 1.099 5107.94 1.098 5107.99 1.098 5108.03 1.098 5108.07 1.098 5108.11 1.097 5108.16 1.097 5108.20 1.097 5108.24 1.097 5108.28 1.097 5108.32 1.097 5108.37 1.096 5108.41 1.096 5108.45 1.096 5108.49 1.096 5108.54 1.095 5108.58 1.095 5108.62 1.095 5108.66 1.095 5108.71 1.095 5108.75 1.095 5108.79 1.094 5108.83 1.094 5108.88 1.094 5108.92 1.094 5108.96 1.094 5109.00 1.094 5109.05 1.094 5109.09 1.094 5109.13 1.094 5109.17 1.094 5109.22 1.094 5109.26 1.094 5109.30 1.094 5109.34 1.093 5109.39 1.093 5109.43 1.093 5109.47 1.093 5109.51 1.092 5109.56 1.092 5109.60 1.092 5109.64 1.092 5109.68 1.091 5109.73 1.091 5109.77 1.091 5109.81 1.091 5109.85 1.090 5109.90 1.090 5109.94 1.090 5109.98 1.090 5110.02 1.090 5110.07 1.089 5110.11 1.089 5110.15 1.089 5110.19 1.089 5110.24 1.089 5110.28 1.089 5110.32 1.089 5110.36 1.088 5110.41 1.088 5110.45 1.088 5110.49 1.088 5110.53 1.088 5110.58 1.088 5110.62 1.088 5110.66 1.087 5110.70 1.087 5110.75 1.087 5110.79 1.087 5110.83 1.087 5110.87 1.087 5110.92 1.087 5110.96 1.087 5111.00 1.086 5111.04 1.086 5111.09 1.086 5111.13 1.086 5111.17 1.086 5111.21 1.086 5111.26 1.086 5111.30 1.085 5111.34 1.085 5111.38 1.085 5111.43 1.085 5111.47 1.085 5111.51 1.085 5111.55 1.085 5111.60 1.084 5111.64 1.084 5111.68 1.084 5111.72 1.084 5111.77 1.084 5111.81 1.084 5111.85 1.083 5111.89 1.083 5111.94 1.083 5111.98 1.083 5112.02 1.083 5112.06 1.083 5112.11 1.082 5112.15 1.082 5112.19 1.082 5112.23 1.082 5112.28 1.082 5112.32 1.082 5112.36 1.081 5112.41 1.081 5112.45 1.081 5112.49 1.081 5112.53 1.081 5112.58 1.081 5112.62 1.081 5112.66 1.080 5112.70 1.080 5112.75 1.080 5112.79 1.080 5112.83 1.080 5112.87 1.079 5112.92 1.079 5112.96 1.079 5113.00 1.079 5113.04 1.079 5113.09 1.079 5113.13 1.078 5113.17 1.078 5113.21 1.078 5113.26 1.078 5113.30 1.078 5113.34 1.078 5113.38 1.078 5113.43 1.078 5113.47 1.077 5113.51 1.077 5113.55 1.077 5113.60 1.077 5113.64 1.077 5113.68 1.077 5113.72 1.077 5113.77 1.077 5113.81 1.077 5113.85 1.077 5113.89 1.077 5113.94 1.077 5113.98 1.077 5114.02 1.077 5114.06 1.077 5114.11 1.076 5114.15 1.076 5114.19 1.076 5114.23 1.076 5114.28 1.076 5114.32 1.076 5114.36 1.076 5114.41 1.076 5114.45 1.076 5114.49 1.075 5114.53 1.075 5114.58 1.075 5114.62 1.075 5114.66 1.075 5114.70 1.075 5114.75 1.075 5114.79 1.075 5114.83 1.074 5114.87 1.074 5114.92 1.074 5114.96 1.074 5115.00 1.074 5115.04 1.074 5115.09 1.074 5115.13 1.074 5115.17 1.074 5115.21 1.074 5115.26 1.074 5115.30 1.074 5115.34 1.073 5115.38 1.073 5115.43 1.073 5115.47 1.073 5115.51 1.073 5115.56 1.073 5115.60 1.073 5115.64 1.073 5115.68 1.072 5115.73 1.072 5115.77 1.072 5115.81 1.072 5115.85 1.072 5115.90 1.072 5115.94 1.072 5115.98 1.072 5116.02 1.072 5116.07 1.072 5116.11 1.072 5116.15 1.071 5116.19 1.071 5116.24 1.071 5116.28 1.071 5116.32 1.071 5116.36 1.071 5116.41 1.071 5116.45 1.071 5116.49 1.071 5116.54 1.071 5116.58 1.070 5116.62 1.070 5116.66 1.070 5116.71 1.070 5116.75 1.070 5116.79 1.070 5116.83 1.070 5116.88 1.070 5116.92 1.070 5116.96 1.070 5117.00 1.070 5117.05 1.069 5117.09 1.069 5117.13 1.069 5117.17 1.069 5117.22 1.069 5117.26 1.069 5117.30 1.069 5117.34 1.069 5117.39 1.069 5117.43 1.069 5117.47 1.069 5117.52 1.069 5117.56 1.069 5117.60 1.069 5117.64 1.069 5117.69 1.069 5117.73 1.069 5117.77 1.069 5117.81 1.069 5117.86 1.069 5117.90 1.068 5117.94 1.068 5117.98 1.068 5118.03 1.068 5118.07 1.068 5118.11 1.068 5118.15 1.068 5118.20 1.067 5118.24 1.067 5118.28 1.067 5118.33 1.067 5118.37 1.067 5118.41 1.067 5118.45 1.067 5118.50 1.066 5118.54 1.066 5118.58 1.066 5118.62 1.066 5118.67 1.066 5118.71 1.066 5118.75 1.066 5118.79 1.066 5118.84 1.066 5118.88 1.066 5118.92 1.066 5118.97 1.066 5119.01 1.066 5119.05 1.066 5119.09 1.065 5119.14 1.065 5119.18 1.065 5119.22 1.065 5119.26 1.065 5119.31 1.065 5119.35 1.065 5119.39 1.065 5119.43 1.065 5119.48 1.065 5119.52 1.065 5119.56 1.065 5119.61 1.065 5119.65 1.065 5119.69 1.065 5119.73 1.065 5119.78 1.065 5119.82 1.065 5119.86 1.065 5119.90 1.065 5119.95 1.065 5119.99 1.065 5120.03 1.064 5120.07 1.064 5120.12 1.064 5120.16 1.064 5120.20 1.064 5120.25 1.064 5120.29 1.064 5120.33 1.064 5120.37 1.064 5120.42 1.064 5120.46 1.064 5120.50 1.064 5120.54 1.064 5120.59 1.064 5120.63 1.064 5120.67 1.064 5120.71 1.064 5120.76 1.064 5120.80 1.064 5120.84 1.064 5120.89 1.064 5120.93 1.063 5120.97 1.063 5121.01 1.063 5121.06 1.063 5121.10 1.063 5121.14 1.063 5121.18 1.063 5121.23 1.063 5121.27 1.063 5121.31 1.063 5121.36 1.063 5121.40 1.063 5121.44 1.063 5121.48 1.063 5121.53 1.063 5121.57 1.063 5121.61 1.063 5121.65 1.063 5121.70 1.063 5121.74 1.063 5121.78 1.063 5121.83 1.063 5121.87 1.062 5121.91 1.062 5121.95 1.062 5122.00 1.062 5122.04 1.062 5122.08 1.062 5122.12 1.062 5122.17 1.062 5122.21 1.062 5122.25 1.062 5122.29 1.062 5122.34 1.062 5122.38 1.062 5122.42 1.062 5122.47 1.062 5122.51 1.062 5122.55 1.062 5122.59 1.062 5122.64 1.062 5122.68 1.062 5122.72 1.062 5122.76 1.062 5122.81 1.062 5122.85 1.061 5122.89 1.061 5122.94 1.061 5122.98 1.061 5123.02 1.061 5123.06 1.061 5123.11 1.061 5123.15 1.061 5123.19 1.061 5123.23 1.061 5123.28 1.061 5123.32 1.061 5123.36 1.061 5123.41 1.061 5123.45 1.061 5123.49 1.061 5123.53 1.061 5123.58 1.061 5123.62 1.061 5123.66 1.061 5123.71 1.061 5123.75 1.061 5123.79 1.061 5123.83 1.061 5123.88 1.061 5123.92 1.061 5123.96 1.061 5124.00 1.061 5124.05 1.061 5124.09 1.061 5124.13 1.061 5124.18 1.061 5124.22 1.061 5124.26 1.061 5124.30 1.061 5124.35 1.060 5124.39 1.060 5124.43 1.060 5124.47 1.060 5124.52 1.060 5124.56 1.060 5124.60 1.059 5124.65 1.059 5124.69 1.059 5124.73 1.059 5124.77 1.059 5124.82 1.059 5124.86 1.059 5124.90 1.059 5124.94 1.059 5124.99 1.059 5125.03 1.059 5125.07 1.059 5125.12 1.059 5125.16 1.059 5125.20 1.059 5125.24 1.060 5125.29 1.060 5125.33 1.060 5125.37 1.060 5125.42 1.060 5125.46 1.060 5125.50 1.059 5125.54 1.059 5125.59 1.059 5125.63 1.059 5125.67 1.059 5125.71 1.059 5125.76 1.059 5125.80 1.059 5125.84 1.059 5125.89 1.059 5125.93 1.059 5125.97 1.059 5126.01 1.059 5126.06 1.059 5126.10 1.059 5126.14 1.059 5126.19 1.059 5126.23 1.059 5126.27 1.059 5126.31 1.059 5126.36 1.059 5126.40 1.059 5126.44 1.059 5126.48 1.059 5126.53 1.059 5126.57 1.059 5126.61 1.059 5126.66 1.059 5126.70 1.059 5126.74 1.059 5126.78 1.058 5126.83 1.058 5126.87 1.058 5126.91 1.058 5126.96 1.058 5127.00 1.058 5127.04 1.058 5127.08 1.058 5127.13 1.058 5127.17 1.058 5127.21 1.058 5127.26 1.058 5127.30 1.058 5127.34 1.058 5127.38 1.058 5127.43 1.058 5127.47 1.058 5127.51 1.058 5127.56 1.057 5127.60 1.057 5127.64 1.057 5127.68 1.057 5127.73 1.057 5127.77 1.057 5127.81 1.057 5127.85 1.057 5127.90 1.057 5127.94 1.057 5127.98 1.057 5128.03 1.057 5128.07 1.057 5128.11 1.057 5128.15 1.056 5128.20 1.056 5128.24 1.056 5128.28 1.056 5128.33 1.056 5128.37 1.056 5128.41 1.056 5128.45 1.056 5128.50 1.056 5128.54 1.056 5128.58 1.056 5128.63 1.056 5128.67 1.056 5128.71 1.057 5128.75 1.057 5128.80 1.057 5128.84 1.057 5128.88 1.057 5128.93 1.057 5128.97 1.056 5129.01 1.056 5129.05 1.056 5129.10 1.056 5129.14 1.056 5129.18 1.056 5129.23 1.056 5129.27 1.056 5129.31 1.056 5129.35 1.056 5129.40 1.056 5129.44 1.055 5129.48 1.055 5129.53 1.055 5129.57 1.055 5129.61 1.055 5129.65 1.055 5129.70 1.055 5129.74 1.055 5129.78 1.055 5129.83 1.055 5129.87 1.055 5129.91 1.055 5129.95 1.055 5130.00 1.055 5130.04 1.055 5130.08 1.055 5130.13 1.055 5130.17 1.055 5130.21 1.055 5130.25 1.055 5130.30 1.055 5130.34 1.055 5130.38 1.055 5130.43 1.054 5130.47 1.054 5130.51 1.054 5130.55 1.054 5130.60 1.054 5130.64 1.054 5130.68 1.054 5130.73 1.054 5130.77 1.054 5130.81 1.054 5130.85 1.054 5130.90 1.054 5130.94 1.053 5130.98 1.053 5131.03 1.054 5131.07 1.054 5131.11 1.054 5131.15 1.054 5131.20 1.054 5131.24 1.054 5131.28 1.054 5131.33 1.054 5131.37 1.054 5131.41 1.054 5131.45 1.054 5131.50 1.054 5131.54 1.054 5131.58 1.054 5131.63 1.054 5131.67 1.054 5131.71 1.054 5131.75 1.054 5131.80 1.054 5131.84 1.054 5131.88 1.054 5131.93 1.054 5131.97 1.054 5132.01 1.054 5132.05 1.054 5132.10 1.054 5132.14 1.054 5132.18 1.054 5132.23 1.054 5132.27 1.054 5132.31 1.054 5132.36 1.054 5132.40 1.054 5132.44 1.054 5132.48 1.054 5132.53 1.054 5132.57 1.054 5132.61 1.054 5132.66 1.054 5132.70 1.054 5132.74 1.054 5132.78 1.054 5132.83 1.054 5132.87 1.054 5132.91 1.054 5132.96 1.054 5133.00 1.054 5133.04 1.054 5133.08 1.054 5133.13 1.054 5133.17 1.054 5133.21 1.054 5133.26 1.054 5133.30 1.054 5133.34 1.054 5133.38 1.054 5133.43 1.054 5133.47 1.054 5133.51 1.054 5133.56 1.054 5133.60 1.054 5133.64 1.054 5133.69 1.054 5133.73 1.053 5133.77 1.053 5133.81 1.053 5133.86 1.053 5133.90 1.053 5133.94 1.053 5133.99 1.053 5134.03 1.053 5134.07 1.053 5134.11 1.053 5134.16 1.053 5134.20 1.053 5134.24 1.053 5134.29 1.053 5134.33 1.053 5134.37 1.053 5134.42 1.053 5134.46 1.053 5134.50 1.053 5134.54 1.053 5134.59 1.053 5134.63 1.053 5134.67 1.053 5134.72 1.053 5134.76 1.053 5134.80 1.053 5134.84 1.053 5134.89 1.053 5134.93 1.053 5134.97 1.053 5135.02 1.053 5135.06 1.053 5135.10 1.053 5135.15 1.053 5135.19 1.053 5135.23 1.053 5135.27 1.053 5135.32 1.053 5135.36 1.053 5135.40 1.053 5135.45 1.053 5135.49 1.053 5135.53 1.053 5135.57 1.053 5135.62 1.052 5135.66 1.052 5135.70 1.052 5135.75 1.052 5135.79 1.052 5135.83 1.052 5135.88 1.052 5135.92 1.052 5135.96 1.052 5136.00 1.052 5136.05 1.052 5136.09 1.052 5136.13 1.052 5136.18 1.052 5136.22 1.052 5136.26 1.053 5136.31 1.052 5136.35 1.053 5136.39 1.053 5136.43 1.053 5136.48 1.053 5136.52 1.053 5136.56 1.053 5136.61 1.053 5136.65 1.053 5136.69 1.053 5136.73 1.053 5136.78 1.053 5136.82 1.053 5136.86 1.053 5136.91 1.053 5136.95 1.053 5136.99 1.052 5137.04 1.052 5137.08 1.052 5137.12 1.052 5137.16 1.052 5137.21 1.052 5137.25 1.052 5137.29 1.052 5137.34 1.052 5137.38 1.052 5137.42 1.052 5137.47 1.052 5137.51 1.052 5137.55 1.052 5137.59 1.052 5137.64 1.052 5137.68 1.052 5137.72 1.052 5137.77 1.052 5137.81 1.052 5137.85 1.052 5137.90 1.052 5137.94 1.052 5137.98 1.052 5138.02 1.052 5138.07 1.052 5138.11 1.052 5138.15 1.052 5138.20 1.051 5138.24 1.051 5138.28 1.051 5138.33 1.051 5138.37 1.051 5138.41 1.051 5138.45 1.051 5138.50 1.051 5138.54 1.051 5138.58 1.051 5138.63 1.051 5138.67 1.051 5138.71 1.051 5138.76 1.051 5138.80 1.051 5138.84 1.051 5138.88 1.051 5138.93 1.051 5138.97 1.051 5139.01 1.051 5139.06 1.051 5139.10 1.051 5139.14 1.050 5139.19 1.050 5139.23 1.050 5139.27 1.050 5139.32 1.050 5139.36 1.050 5139.40 1.050 5139.44 1.050 5139.49 1.049 5139.53 1.049 5139.57 1.049 5139.62 1.049 5139.66 1.049 5139.70 1.049 5139.75 1.050 5139.79 1.050 5139.83 1.050 5139.87 1.050 5139.92 1.050 5139.96 1.050 5140.00 1.050 5140.05 1.050 5140.09 1.050 5140.13 1.049 5140.18 1.049 5140.22 1.049 5140.26 1.049 5140.31 1.049 5140.35 1.049 5140.39 1.049 5140.43 1.049 5140.48 1.049 5140.52 1.049 5140.56 1.049 5140.61 1.049 5140.65 1.049 5140.69 1.049 5140.74 1.049 5140.78 1.049 5140.82 1.049 5140.86 1.049 5140.91 1.049 5140.95 1.049 5140.99 1.049 5141.04 1.049 5141.08 1.049 5141.12 1.049 5141.17 1.049 5141.21 1.048 5141.25 1.048 5141.30 1.048 5141.34 1.048 5141.38 1.048 5141.42 1.048 5141.47 1.048 5141.51 1.048 5141.55 1.048 5141.60 1.048 5141.64 1.048 5141.68 1.048 5141.73 1.048 5141.77 1.048 5141.81 1.048 5141.86 1.048 5141.90 1.047 5141.94 1.047 5141.98 1.047 5142.03 1.047 5142.07 1.047 5142.11 1.047 5142.16 1.047 5142.20 1.047 5142.24 1.047 5142.29 1.047 5142.33 1.047 5142.37 1.047 5142.42 1.047 5142.46 1.047 5142.50 1.047 5142.54 1.047 5142.59 1.047 5142.63 1.047 5142.67 1.047 5142.72 1.047 5142.76 1.046 5142.80 1.046 5142.85 1.046 5142.89 1.046 5142.93 1.046 5142.98 1.046 5143.02 1.046 5143.06 1.046 5143.10 1.046 5143.15 1.046 5143.19 1.046 5143.23 1.045 5143.28 1.045 5143.32 1.045 5143.36 1.045 5143.41 1.045 5143.45 1.045 5143.49 1.045 5143.54 1.044 5143.58 1.044 5143.62 1.044 5143.66 1.044 5143.71 1.044 5143.75 1.044 5143.79 1.044 5143.84 1.044 5143.88 1.044 5143.92 1.044 5143.97 1.044 5144.01 1.044 5144.05 1.044 5144.10 1.043 5144.14 1.043 5144.18 1.043 5144.23 1.043 5144.27 1.043 5144.31 1.043 5144.35 1.043 5144.40 1.043 5144.44 1.043 5144.48 1.042 5144.53 1.042 5144.57 1.042 5144.61 1.042 5144.66 1.042 5144.70 1.042 5144.74 1.042 5144.79 1.041 5144.83 1.041 5144.87 1.041 5144.92 1.041 5144.96 1.041 5145.00 1.041 5145.04 1.041 5145.09 1.041 5145.13 1.041 5145.17 1.040 5145.22 1.040 5145.26 1.040 5145.30 1.040 5145.35 1.040 5145.39 1.040 5145.43 1.040 5145.48 1.039 5145.52 1.039 5145.56 1.039 5145.61 1.039 5145.65 1.039 5145.69 1.039 5145.73 1.039 5145.78 1.038 5145.82 1.038 5145.86 1.038 5145.91 1.038 5145.95 1.038 5145.99 1.037 5146.04 1.037 5146.08 1.037 5146.12 1.037 5146.17 1.037 5146.21 1.037 5146.25 1.037 5146.30 1.037 5146.34 1.036 5146.38 1.036 5146.43 1.036 5146.47 1.036 5146.51 1.036 5146.55 1.036 5146.60 1.035 5146.64 1.035 5146.68 1.035 5146.73 1.035 5146.77 1.035 5146.81 1.034 5146.86 1.034 5146.90 1.034 5146.94 1.034 5146.99 1.034 5147.03 1.034 5147.07 1.033 5147.12 1.033 5147.16 1.033 5147.20 1.033 5147.25 1.033 5147.29 1.032 5147.33 1.032 5147.38 1.032 5147.42 1.032 5147.46 1.032 5147.50 1.031 5147.55 1.031 5147.59 1.031 5147.63 1.031 5147.68 1.031 5147.72 1.030 5147.76 1.030 5147.81 1.030 5147.85 1.030 5147.89 1.030 5147.94 1.030 5147.98 1.030 5148.02 1.029 5148.07 1.029 5148.11 1.029 5148.15 1.029 5148.20 1.029 5148.24 1.029 5148.28 1.028 5148.33 1.028 5148.37 1.028 5148.41 1.028 5148.45 1.028 5148.50 1.028 5148.54 1.027 5148.58 1.027 5148.63 1.027 5148.67 1.027 5148.71 1.027 5148.76 1.026 5148.80 1.026 5148.84 1.026 5148.89 1.026 5148.93 1.025 5148.97 1.025 5149.02 1.025 5149.06 1.025 5149.10 1.025 5149.15 1.024 5149.19 1.024 5149.23 1.024 5149.28 1.024 5149.32 1.023 5149.36 1.023 5149.41 1.023 5149.45 1.023 5149.49 1.023 5149.53 1.022 5149.58 1.022 5149.62 1.022 5149.66 1.022 5149.71 1.022 5149.75 1.021 5149.79 1.021 5149.84 1.021 5149.88 1.021 5149.92 1.021 5149.97 1.020 5150.01 1.020 5150.05 1.020 5150.10 1.020 5150.14 1.020 5150.18 1.020 5150.23 1.020 5150.27 1.019 5150.31 1.019 5150.36 1.019 5150.40 1.019 5150.44 1.019 5150.49 1.018 5150.53 1.018 5150.57 1.018 5150.62 1.018 5150.66 1.018 5150.70 1.017 5150.75 1.017 5150.79 1.017 5150.83 1.017 5150.87 1.017 5150.92 1.017 5150.96 1.016 5151.00 1.016 5151.05 1.016 5151.09 1.016 5151.13 1.016 5151.18 1.015 5151.22 1.015 5151.26 1.015 5151.31 1.015 5151.35 1.014 5151.39 1.014 5151.44 1.014 5151.48 1.014 5151.52 1.013 5151.57 1.013 5151.61 1.013 5151.65 1.013 5151.70 1.012 5151.74 1.012 5151.78 1.012 5151.83 1.012 5151.87 1.012 5151.91 1.012 5151.96 1.011 5152.00 1.011 5152.04 1.011 5152.09 1.011 5152.13 1.011 5152.17 1.011 5152.22 1.010 5152.26 1.010 5152.30 1.010 5152.35 1.009 5152.39 1.009 5152.43 1.009 5152.48 1.009 5152.52 1.008 5152.56 1.008 5152.60 1.008 5152.65 1.008 5152.69 1.007 5152.73 1.007 5152.78 1.007 5152.82 1.007 5152.86 1.007 5152.91 1.006 5152.95 1.006 5152.99 1.006 5153.04 1.006 5153.08 1.006 5153.12 1.005 5153.17 1.005 5153.21 1.005 5153.25 1.005 5153.30 1.005 5153.34 1.004 5153.38 1.004 5153.43 1.004 5153.47 1.004 5153.51 1.003 5153.56 1.003 5153.60 1.003 5153.64 1.003 5153.69 1.003 5153.73 1.002 5153.77 1.002 5153.82 1.002 5153.86 1.002 5153.90 1.002 5153.95 1.001 5153.99 1.001 5154.03 1.001 5154.08 1.001 5154.12 1.001 5154.16 1.000 5154.21 1.000 5154.25 1.000 5154.29 1.000 5154.34 0.999 5154.38 0.999 5154.42 0.999 5154.47 0.999 5154.51 0.998 5154.55 0.998 5154.60 0.998 5154.64 0.998 5154.68 0.998 5154.73 0.997 5154.77 0.997 5154.81 0.997 5154.86 0.997 5154.90 0.997 5154.94 0.997 5154.99 0.996 5155.03 0.996 5155.07 0.996 5155.12 0.996 5155.16 0.996 5155.20 0.996 5155.25 0.995 5155.29 0.995 5155.33 0.995 5155.38 0.995 5155.42 0.995 5155.46 0.995 5155.51 0.994 5155.55 0.994 5155.59 0.994 5155.64 0.994 5155.68 0.993 5155.72 0.993 5155.77 0.993 5155.81 0.993 5155.85 0.993 5155.90 0.992 5155.94 0.992 5155.98 0.992 5156.03 0.992 5156.07 0.991 5156.11 0.991 5156.16 0.991 5156.20 0.991 5156.24 0.990 5156.29 0.990 5156.33 0.990 5156.37 0.990 5156.42 0.989 5156.46 0.989 5156.50 0.989 5156.55 0.988 5156.59 0.988 5156.63 0.988 5156.68 0.988 5156.72 0.987 5156.76 0.987 5156.81 0.987 5156.85 0.987 5156.89 0.987 5156.94 0.986 5156.98 0.986 5157.02 0.986 5157.07 0.986 5157.11 0.985 5157.15 0.985 5157.20 0.985 5157.24 0.985 5157.28 0.985 5157.33 0.985 5157.37 0.984 5157.41 0.984 5157.46 0.984 5157.50 0.984 5157.54 0.984 5157.59 0.984 5157.63 0.984 5157.67 0.984 5157.72 0.984 5157.76 0.984 5157.80 0.984 5157.85 0.984 5157.89 0.984 5157.93 0.984 5157.98 0.984 5158.02 0.983 5158.06 0.983 5158.11 0.983 5158.15 0.982 5158.19 0.982 5158.24 0.982 5158.28 0.981 5158.32 0.981 5158.37 0.980 5158.41 0.980 5158.45 0.980 5158.50 0.979 5158.54 0.979 5158.58 0.979 5158.63 0.979 5158.67 0.978 5158.71 0.978 5158.76 0.978 5158.80 0.977 5158.84 0.977 5158.89 0.977 5158.93 0.977 5158.97 0.976 5159.02 0.976 5159.06 0.976 5159.10 0.976 5159.15 0.975 5159.19 0.975 5159.23 0.975 5159.28 0.975 5159.32 0.975 5159.36 0.974 5159.41 0.974 5159.45 0.974 5159.49 0.973 5159.54 0.973 5159.58 0.973 5159.62 0.973 5159.67 0.972 5159.71 0.972 5159.76 0.972 5159.80 0.972 5159.84 0.971 5159.89 0.971 5159.93 0.971 5159.97 0.971 5160.02 0.970 5160.06 0.970 5160.10 0.970 5160.15 0.970 5160.19 0.969 5160.23 0.969 5160.28 0.969 5160.32 0.968 5160.36 0.968 5160.41 0.968 5160.45 0.968 5160.49 0.968 5160.54 0.967 5160.58 0.967 5160.62 0.967 5160.67 0.967 5160.71 0.967 5160.75 0.966 5160.80 0.966 5160.84 0.966 5160.88 0.966 5160.93 0.965 5160.97 0.965 5161.01 0.965 5161.06 0.965 5161.10 0.965 5161.14 0.964 5161.19 0.964 5161.23 0.964 5161.27 0.964 5161.32 0.963 5161.36 0.963 5161.40 0.963 5161.45 0.963 5161.49 0.963 5161.54 0.963 5161.58 0.963 5161.62 0.963 5161.67 0.963 5161.71 0.963 5161.75 0.963 5161.80 0.963 5161.84 0.962 5161.88 0.962 5161.93 0.962 5161.97 0.962 5162.01 0.962 5162.06 0.962 5162.10 0.962 5162.14 0.961 5162.19 0.961 5162.23 0.961 5162.27 0.961 5162.32 0.961 5162.36 0.960 5162.40 0.960 5162.45 0.960 5162.49 0.960 5162.53 0.959 5162.58 0.959 5162.62 0.959 5162.66 0.959 5162.71 0.959 5162.75 0.958 5162.80 0.958 5162.84 0.958 5162.88 0.958 5162.93 0.958 5162.97 0.957 5163.01 0.957 5163.06 0.957 5163.10 0.957 5163.14 0.957 5163.19 0.956 5163.23 0.956 5163.27 0.956 5163.32 0.956 5163.36 0.955 5163.40 0.955 5163.45 0.955 5163.49 0.954 5163.53 0.954 5163.58 0.954 5163.62 0.953 5163.66 0.953 5163.71 0.953 5163.75 0.953 5163.79 0.952 5163.84 0.952 5163.88 0.952 5163.93 0.952 5163.97 0.951 5164.01 0.951 5164.06 0.951 5164.10 0.951 5164.14 0.950 5164.19 0.950 5164.23 0.950 5164.27 0.950 5164.32 0.949 5164.36 0.949 5164.40 0.949 5164.45 0.949 5164.49 0.948 5164.53 0.948 5164.58 0.948 5164.62 0.948 5164.66 0.948 5164.71 0.948 5164.75 0.947 5164.79 0.947 5164.84 0.947 5164.88 0.947 5164.93 0.947 5164.97 0.947 5165.01 0.946 5165.06 0.946 5165.10 0.946 5165.14 0.946 5165.19 0.946 5165.23 0.945 5165.27 0.945 5165.32 0.945 5165.36 0.945 5165.40 0.945 5165.45 0.945 5165.49 0.945 5165.53 0.944 5165.58 0.944 5165.62 0.944 5165.66 0.944 5165.71 0.944 5165.75 0.944 5165.80 0.943 5165.84 0.943 5165.88 0.943 5165.93 0.943 5165.97 0.943 5166.01 0.942 5166.06 0.942 5166.10 0.942 5166.14 0.942 5166.19 0.942 5166.23 0.942 5166.27 0.942 5166.32 0.941 5166.36 0.941 5166.40 0.941 5166.45 0.941 5166.49 0.941 5166.54 0.941 5166.58 0.940 5166.62 0.940 5166.67 0.940 5166.71 0.940 5166.75 0.940 5166.80 0.939 5166.84 0.939 5166.88 0.939 5166.93 0.939 5166.97 0.939 5167.01 0.939 5167.06 0.939 5167.10 0.939 5167.14 0.939 5167.19 0.939 5167.23 0.939 5167.28 0.938 5167.32 0.938 5167.36 0.938 5167.41 0.938 5167.45 0.938 5167.49 0.938 5167.54 0.938 5167.58 0.937 5167.62 0.937 5167.67 0.937 5167.71 0.937 5167.75 0.937 5167.80 0.937 5167.84 0.937 5167.88 0.936 5167.93 0.936 5167.97 0.936 5168.02 0.936 5168.06 0.936 5168.10 0.936 5168.15 0.936 5168.19 0.936 5168.23 0.936 5168.28 0.935 5168.32 0.935 5168.36 0.935 5168.41 0.935 5168.45 0.935 5168.49 0.935 5168.54 0.935 5168.58 0.935 5168.63 0.934 5168.67 0.934 5168.71 0.934 5168.76 0.934 5168.80 0.934 5168.84 0.934 5168.89 0.934 5168.93 0.934 5168.97 0.934 5169.02 0.933 5169.06 0.933 5169.10 0.933 5169.15 0.933 5169.19 0.933 5169.24 0.932 5169.28 0.932 5169.32 0.932 5169.37 0.932 5169.41 0.932 5169.45 0.932 5169.50 0.932 5169.54 0.932 5169.58 0.931 5169.63 0.931 5169.67 0.931 5169.71 0.931 5169.76 0.931 5169.80 0.931 5169.85 0.930 5169.89 0.930 5169.93 0.930 5169.98 0.930 5170.02 0.930 5170.06 0.930 5170.11 0.930 5170.15 0.929 5170.19 0.929 5170.24 0.929 5170.28 0.929 5170.32 0.929 5170.37 0.929 5170.41 0.929 5170.46 0.929 5170.50 0.929 5170.54 0.929 5170.59 0.929 5170.63 0.928 5170.67 0.928 5170.72 0.928 5170.76 0.928 5170.80 0.928 5170.85 0.928 5170.89 0.928 5170.94 0.927 5170.98 0.927 5171.02 0.927 5171.07 0.927 5171.11 0.927 5171.15 0.927 5171.20 0.927 5171.24 0.926 5171.28 0.926 5171.33 0.926 5171.37 0.926 5171.41 0.926 5171.46 0.926 5171.50 0.925 5171.55 0.925 5171.59 0.925 5171.63 0.925 5171.68 0.925 5171.72 0.925 5171.76 0.925 5171.81 0.925 5171.85 0.925 5171.89 0.925 5171.94 0.925 5171.98 0.925 5172.03 0.924 5172.07 0.924 5172.11 0.924 5172.16 0.924 5172.20 0.924 5172.24 0.924 5172.29 0.923 5172.33 0.923 5172.37 0.923 5172.42 0.923 5172.46 0.923 5172.51 0.923 5172.55 0.922 5172.59 0.922 5172.64 0.922 5172.68 0.922 5172.72 0.922 5172.77 0.922 5172.81 0.922 5172.85 0.921 5172.90 0.921 5172.94 0.921 5172.99 0.921 5173.03 0.921 5173.07 0.921 5173.12 0.921 5173.16 0.920 5173.20 0.920 5173.25 0.920 5173.29 0.920 5173.33 0.920 5173.38 0.920 5173.42 0.920 5173.47 0.920 5173.51 0.920 5173.55 0.920 5173.60 0.919 5173.64 0.919 5173.68 0.919 5173.73 0.919 5173.77 0.919 5173.81 0.919 5173.86 0.919 5173.90 0.919 5173.95 0.919 5173.99 0.918 5174.03 0.918 5174.08 0.918 5174.12 0.918 5174.16 0.918 5174.21 0.917 5174.25 0.917 5174.30 0.917 5174.34 0.917 5174.38 0.917 5174.43 0.917 5174.47 0.917 5174.51 0.917 5174.56 0.917 5174.60 0.917 5174.64 0.916 5174.69 0.916 5174.73 0.916 5174.78 0.916 5174.82 0.916 5174.86 0.916 5174.91 0.916 5174.95 0.916 5174.99 0.916 5175.04 0.915 5175.08 0.915 5175.12 0.915 5175.17 0.915 5175.21 0.915 5175.26 0.915 5175.30 0.914 5175.34 0.914 5175.39 0.914 5175.43 0.914 5175.47 0.914 5175.52 0.914 5175.56 0.913 5175.61 0.913 5175.65 0.913 5175.69 0.913 5175.74 0.913 5175.78 0.912 5175.82 0.912 5175.87 0.912 5175.91 0.912 5175.95 0.912 5176.00 0.912 5176.04 0.912 5176.09 0.911 5176.13 0.911 5176.17 0.911 5176.22 0.911 5176.26 0.911 5176.30 0.911 5176.35 0.911 5176.39 0.911 5176.44 0.911 5176.48 0.911 5176.52 0.911 5176.57 0.911 5176.61 0.911 5176.65 0.911 5176.70 0.911 5176.74 0.910 5176.79 0.910 5176.83 0.910 5176.87 0.910 5176.92 0.910 5176.96 0.910 5177.00 0.909 5177.05 0.909 5177.09 0.909 5177.14 0.909 5177.18 0.909 5177.22 0.908 5177.27 0.908 5177.31 0.908 5177.35 0.908 5177.40 0.908 5177.44 0.907 5177.48 0.907 5177.53 0.907 5177.57 0.907 5177.62 0.906 5177.66 0.906 5177.70 0.906 5177.75 0.906 5177.79 0.906 5177.83 0.906 5177.88 0.906 5177.92 0.906 5177.97 0.905 5178.01 0.905 5178.05 0.905 5178.10 0.905 5178.14 0.905 5178.18 0.905 5178.23 0.904 5178.27 0.904 5178.32 0.904 5178.36 0.904 5178.40 0.904 5178.45 0.904 5178.49 0.904 5178.53 0.904 5178.58 0.903 5178.62 0.903 5178.67 0.903 5178.71 0.903 5178.75 0.903 5178.80 0.903 5178.84 0.903 5178.88 0.903 5178.93 0.903 5178.97 0.902 5179.02 0.902 5179.06 0.902 5179.10 0.902 5179.15 0.902 5179.19 0.902 5179.23 0.902 5179.28 0.902 5179.32 0.902 5179.37 0.902 5179.41 0.901 5179.45 0.901 5179.50 0.901 5179.54 0.901 5179.58 0.901 5179.63 0.900 5179.67 0.900 5179.72 0.900 5179.76 0.900 5179.80 0.900 5179.85 0.900 5179.89 0.900 5179.93 0.900 5179.98 0.900 5180.02 0.900 5180.07 0.899 5180.11 0.899 5180.15 0.899 5180.20 0.899 5180.24 0.899 5180.28 0.899 5180.33 0.899 5180.37 0.899 5180.42 0.899 5180.46 0.898 5180.50 0.898 5180.55 0.898 5180.59 0.898 5180.64 0.898 5180.68 0.898 5180.72 0.898 5180.77 0.898 5180.81 0.897 5180.85 0.897 5180.90 0.897 5180.94 0.897 5180.99 0.897 5181.03 0.897 5181.07 0.896 5181.12 0.896 5181.16 0.896 5181.20 0.896 5181.25 0.896 5181.29 0.896 5181.34 0.895 5181.38 0.895 5181.42 0.895 5181.47 0.895 5181.51 0.895 5181.55 0.895 5181.60 0.894 5181.64 0.894 5181.69 0.894 5181.73 0.894 5181.77 0.894 5181.82 0.894 5181.86 0.894 5181.91 0.894 5181.95 0.894 5181.99 0.894 5182.04 0.894 5182.08 0.893 5182.12 0.893 5182.17 0.893 5182.21 0.893 5182.26 0.893 5182.30 0.893 5182.34 0.893 5182.39 0.893 5182.43 0.893 5182.47 0.893 5182.52 0.892 5182.56 0.892 5182.61 0.892 5182.65 0.892 5182.69 0.892 5182.74 0.892 5182.78 0.892 5182.83 0.892 5182.87 0.892 5182.91 0.892 5182.96 0.892 5183.00 0.892 5183.04 0.891 5183.09 0.891 5183.13 0.891 5183.18 0.891 5183.22 0.891 5183.26 0.891 5183.31 0.891 5183.35 0.891 5183.39 0.891 5183.44 0.891 5183.48 0.891 5183.53 0.891 5183.57 0.891 5183.61 0.890 5183.66 0.890 5183.70 0.890 5183.75 0.890 5183.79 0.890 5183.83 0.890 5183.88 0.890 5183.92 0.890 5183.96 0.889 5184.01 0.889 5184.05 0.889 5184.10 0.889 5184.14 0.889 5184.18 0.889 5184.23 0.889 5184.27 0.888 5184.32 0.888 5184.36 0.888 5184.40 0.888 5184.45 0.888 5184.49 0.888 5184.53 0.888 5184.58 0.887 5184.62 0.887 5184.67 0.887 5184.71 0.887 5184.75 0.887 5184.80 0.886 5184.84 0.886 5184.89 0.886 5184.93 0.885 5184.97 0.885 5185.02 0.884 5185.06 0.884 5185.10 0.884 5185.15 0.883 5185.19 0.883 5185.24 0.882 5185.28 0.882 5185.32 0.882 5185.37 0.881 5185.41 0.881 5185.46 0.881 5185.50 0.881 5185.54 0.881 5185.59 0.881 5185.63 0.881 5185.68 0.881 5185.72 0.881 5185.76 0.882 5185.81 0.882 5185.85 0.882 5185.89 0.882 5185.94 0.883 5185.98 0.883 5186.03 0.883 5186.07 0.883 5186.11 0.883 5186.16 0.883 5186.20 0.883 5186.25 0.883 5186.29 0.883 5186.33 0.883 5186.38 0.883 5186.42 0.883 5186.47 0.883 5186.51 0.883 5186.55 0.883 5186.60 0.883 5186.64 0.883 5186.68 0.883 5186.73 0.883 5186.77 0.883 5186.82 0.883 5186.86 0.883 5186.90 0.882 5186.95 0.882 5186.99 0.882 5187.04 0.882 5187.08 0.882 5187.12 0.882 5187.17 0.882 5187.21 0.882 5187.26 0.882 5187.30 0.882 5187.34 0.882 5187.39 0.882 5187.43 0.882 5187.47 0.882 5187.52 0.881 5187.56 0.881 5187.61 0.881 5187.65 0.881 5187.69 0.881 5187.74 0.881 5187.78 0.881 5187.83 0.881 5187.87 0.881 5187.91 0.881 5187.96 0.880 5188.00 0.880 5188.05 0.880 5188.09 0.880 5188.13 0.880 5188.18 0.880 5188.22 0.880 5188.27 0.880 5188.31 0.880 5188.35 0.880 5188.40 0.880 5188.44 0.880 5188.48 0.879 5188.53 0.879 5188.57 0.879 5188.62 0.879 5188.66 0.879 5188.70 0.879 5188.75 0.878 5188.79 0.878 5188.84 0.878 5188.88 0.878 5188.92 0.878 5188.97 0.878 5189.01 0.878 5189.06 0.878 5189.10 0.877 5189.14 0.877 5189.19 0.877 5189.23 0.877 5189.28 0.877 5189.32 0.877 5189.36 0.877 5189.41 0.877 5189.45 0.877 5189.50 0.877 5189.54 0.876 5189.58 0.876 5189.63 0.876 5189.67 0.876 5189.72 0.876 5189.76 0.876 5189.80 0.876 5189.85 0.875 5189.89 0.875 5189.93 0.875 5189.98 0.875 5190.02 0.875 5190.07 0.875 5190.11 0.875 5190.15 0.875 5190.20 0.874 5190.24 0.874 5190.29 0.874 5190.33 0.874 5190.37 0.874 5190.42 0.874 5190.46 0.874 5190.51 0.873 5190.55 0.873 5190.59 0.873 5190.64 0.873 5190.68 0.873 5190.73 0.873 5190.77 0.873 5190.81 0.873 5190.86 0.873 5190.90 0.872 5190.95 0.872 5190.99 0.872 5191.03 0.872 5191.08 0.872 5191.12 0.872 5191.17 0.872 5191.21 0.872 5191.25 0.871 5191.30 0.871 5191.34 0.871 5191.39 0.871 5191.43 0.871 5191.47 0.870 5191.52 0.870 5191.56 0.870 5191.61 0.870 5191.65 0.870 5191.69 0.870 5191.74 0.870 5191.78 0.869 5191.83 0.869 5191.87 0.869 5191.91 0.869 5191.96 0.869 5192.00 0.869 5192.05 0.869 5192.09 0.869 5192.13 0.869 5192.18 0.868 5192.22 0.868 5192.27 0.868 5192.31 0.868 5192.35 0.868 5192.40 0.868 5192.44 0.868 5192.49 0.868 5192.53 0.868 5192.57 0.867 5192.62 0.867 5192.66 0.867 5192.71 0.867 5192.75 0.867 5192.79 0.867 5192.84 0.867 5192.88 0.866 5192.93 0.866 5192.97 0.866 5193.01 0.866 5193.06 0.866 5193.10 0.866 5193.15 0.866 5193.19 0.865 5193.23 0.865 5193.28 0.865 5193.32 0.865 5193.37 0.865 5193.41 0.865 5193.45 0.865 5193.50 0.864 5193.54 0.864 5193.59 0.864 5193.63 0.864 5193.67 0.864 5193.72 0.863 5193.76 0.863 5193.81 0.863 5193.85 0.863 5193.89 0.863 5193.94 0.862 5193.98 0.862 5194.03 0.862 5194.07 0.862 5194.11 0.862 5194.16 0.862 5194.20 0.861 5194.25 0.861 5194.29 0.861 5194.33 0.861 5194.38 0.861 5194.42 0.861 5194.47 0.861 5194.51 0.861 5194.55 0.861 5194.60 0.861 5194.64 0.861 5194.69 0.861 5194.73 0.860 5194.77 0.860 5194.82 0.860 5194.86 0.860 5194.91 0.860 5194.95 0.860 5194.99 0.859 5195.04 0.859 5195.08 0.859 5195.13 0.859 5195.17 0.859 5195.22 0.859 5195.26 0.858 5195.30 0.858 5195.35 0.858 5195.39 0.858 5195.44 0.858 5195.48 0.858 5195.52 0.858 5195.57 0.857 5195.61 0.857 5195.66 0.857 5195.70 0.857 5195.74 0.857 5195.79 0.857 5195.83 0.857 5195.88 0.856 5195.92 0.856 5195.96 0.856 5196.01 0.856 5196.05 0.856 5196.10 0.856 5196.14 0.856 5196.18 0.856 5196.23 0.856 5196.27 0.855 5196.32 0.855 5196.36 0.855 5196.40 0.855 5196.45 0.855 5196.49 0.855 5196.54 0.854 5196.58 0.854 5196.63 0.854 5196.67 0.854 5196.71 0.854 5196.76 0.854 5196.80 0.854 5196.85 0.853 5196.89 0.853 5196.93 0.853 5196.98 0.853 5197.02 0.853 5197.07 0.853 5197.11 0.853 5197.15 0.852 5197.20 0.852 5197.24 0.852 5197.29 0.852 5197.33 0.852 5197.37 0.852 5197.42 0.852 5197.46 0.852 5197.51 0.851 5197.55 0.851 5197.59 0.851 5197.64 0.851 5197.68 0.851 5197.73 0.851 5197.77 0.850 5197.82 0.850 5197.86 0.850 5197.90 0.850 5197.95 0.850 5197.99 0.850 5198.04 0.850 5198.08 0.849 5198.12 0.849 5198.17 0.849 5198.21 0.849 5198.26 0.849 5198.30 0.849 5198.34 0.849 5198.39 0.849 5198.43 0.849 5198.48 0.848 5198.52 0.848 5198.57 0.848 5198.61 0.848 5198.65 0.848 5198.70 0.848 5198.74 0.848 5198.79 0.847 5198.83 0.847 5198.87 0.847 5198.92 0.847 5198.96 0.847 5199.01 0.847 5199.05 0.847 5199.09 0.846 5199.14 0.846 5199.18 0.846 5199.23 0.846 5199.27 0.846 5199.32 0.846 5199.36 0.846 5199.40 0.845 5199.45 0.845 5199.49 0.845 5199.54 0.845 5199.58 0.845 5199.62 0.845 5199.67 0.845 5199.71 0.845 5199.76 0.845 5199.80 0.844 5199.84 0.844 5199.89 0.844 5199.93 0.844 5199.98 0.844 5200.02 0.844 5200.07 0.844 5200.11 0.843 5200.15 0.843 5200.20 0.843 5200.24 0.843 5200.29 0.843 5200.33 0.843 5200.37 0.843 5200.42 0.842 5200.46 0.842 5200.51 0.842 5200.55 0.842 5200.60 0.842 5200.64 0.842 5200.68 0.841 5200.73 0.841 5200.77 0.841 5200.82 0.841 5200.86 0.841 5200.90 0.841 5200.95 0.840 5200.99 0.840 5201.04 0.840 5201.08 0.840 5201.13 0.840 5201.17 0.840 5201.21 0.840 5201.26 0.839 5201.30 0.839 5201.35 0.839 5201.39 0.839 5201.43 0.839 5201.48 0.838 5201.52 0.838 5201.57 0.838 5201.61 0.838 5201.66 0.838 5201.70 0.838 5201.74 0.837 5201.79 0.837 5201.83 0.837 5201.88 0.837 5201.92 0.837 5201.96 0.836 5202.01 0.836 5202.05 0.836 5202.10 0.836 5202.14 0.836 5202.19 0.836 5202.23 0.836 5202.27 0.835 5202.32 0.835 5202.36 0.835 5202.41 0.835 5202.45 0.835 5202.49 0.835 5202.54 0.834 5202.58 0.834 5202.63 0.834 5202.67 0.834 5202.72 0.834 5202.76 0.833 5202.80 0.833 5202.85 0.833 5202.89 0.833 5202.94 0.833 5202.98 0.833 5203.02 0.833 5203.07 0.832 5203.11 0.832 5203.16 0.832 5203.20 0.832 5203.25 0.832 5203.29 0.832 5203.33 0.832 5203.38 0.831 5203.42 0.831 5203.47 0.831 5203.51 0.831 5203.56 0.831 5203.60 0.830 5203.64 0.830 5203.69 0.830 5203.73 0.830 5203.78 0.830 5203.82 0.829 5203.86 0.829 5203.91 0.829 5203.95 0.829 5204.00 0.829 5204.04 0.828 5204.09 0.828 5204.13 0.828 5204.17 0.828 5204.22 0.828 5204.26 0.828 5204.31 0.828 5204.35 0.827 5204.40 0.827 5204.44 0.827 5204.48 0.827 5204.53 0.827 5204.57 0.827 5204.62 0.826 5204.66 0.826 5204.70 0.826 5204.75 0.826 5204.79 0.826 5204.84 0.826 5204.88 0.826 5204.93 0.825 5204.97 0.825 5205.01 0.825 5205.06 0.825 5205.10 0.825 5205.15 0.824 5205.19 0.824 5205.24 0.824 5205.28 0.824 5205.32 0.823 5205.37 0.823 5205.41 0.823 5205.46 0.823 5205.50 0.823 5205.55 0.823 5205.59 0.822 5205.63 0.822 5205.68 0.822 5205.72 0.822 5205.77 0.822 5205.81 0.821 5205.85 0.821 5205.90 0.821 5205.94 0.821 5205.99 0.821 5206.03 0.821 5206.08 0.821 5206.12 0.821 5206.16 0.820 5206.21 0.820 5206.25 0.820 5206.30 0.820 5206.34 0.820 5206.39 0.819 5206.43 0.819 5206.47 0.819 5206.52 0.819 5206.56 0.819 5206.61 0.819 5206.65 0.818 5206.70 0.818 5206.74 0.818 5206.78 0.818 5206.83 0.818 5206.87 0.818 5206.92 0.818 5206.96 0.817 5207.01 0.817 5207.05 0.817 5207.09 0.817 5207.14 0.817 5207.18 0.816 5207.23 0.816 5207.27 0.816 5207.32 0.816 5207.36 0.816 5207.40 0.816 5207.45 0.816 5207.49 0.815 5207.54 0.815 5207.58 0.815 5207.63 0.815 5207.67 0.815 5207.71 0.815 5207.76 0.815 5207.80 0.814 5207.85 0.814 5207.89 0.814 5207.94 0.814 5207.98 0.814 5208.02 0.814 5208.07 0.813 5208.11 0.813 5208.16 0.813 5208.20 0.813 5208.25 0.813 5208.29 0.813 5208.33 0.813 5208.38 0.813 5208.42 0.812 5208.47 0.812 5208.51 0.812 5208.56 0.812 5208.60 0.812 5208.64 0.811 5208.69 0.811 5208.73 0.811 5208.78 0.811 5208.82 0.811 5208.87 0.811 5208.91 0.811 5208.95 0.810 5209.00 0.810 5209.04 0.810 5209.09 0.810 5209.13 0.810 5209.18 0.809 5209.22 0.809 5209.26 0.809 5209.31 0.809 5209.35 0.808 5209.40 0.808 5209.44 0.808 5209.49 0.808 5209.53 0.808 5209.57 0.808 5209.62 0.808 5209.66 0.808 5209.71 0.808 5209.75 0.808 5209.80 0.807 5209.84 0.807 5209.88 0.807 5209.93 0.807 5209.97 0.807 5210.02 0.807 5210.06 0.807 5210.11 0.806 5210.15 0.806 5210.19 0.806 5210.24 0.806 5210.28 0.806 5210.33 0.806 5210.37 0.805 5210.42 0.805 5210.46 0.805 5210.51 0.805 5210.55 0.805 5210.59 0.805 5210.64 0.805 5210.68 0.805 5210.73 0.805 5210.77 0.805 5210.82 0.805 5210.86 0.805 5210.90 0.804 5210.95 0.804 5210.99 0.804 5211.04 0.804 5211.08 0.804 5211.13 0.804 5211.17 0.804 5211.21 0.803 5211.26 0.803 5211.30 0.803 5211.35 0.803 5211.39 0.803 5211.44 0.803 5211.48 0.802 5211.52 0.802 5211.57 0.802 5211.61 0.802 5211.66 0.802 5211.70 0.802 5211.75 0.802 5211.79 0.802 5211.84 0.802 5211.88 0.802 5211.92 0.802 5211.97 0.801 5212.01 0.801 5212.06 0.801 5212.10 0.801 5212.15 0.801 5212.19 0.801 5212.23 0.801 5212.28 0.800 5212.32 0.800 5212.37 0.800 5212.41 0.800 5212.46 0.800 5212.50 0.800 5212.55 0.800 5212.59 0.799 5212.63 0.799 5212.68 0.799 5212.72 0.799 5212.77 0.799 5212.81 0.799 5212.86 0.799 5212.90 0.799 5212.94 0.799 5212.99 0.799 5213.03 0.798 5213.08 0.798 5213.12 0.798 5213.17 0.798 5213.21 0.798 5213.26 0.798 5213.30 0.798 5213.34 0.798 5213.39 0.798 5213.43 0.797 5213.48 0.797 5213.52 0.797 5213.57 0.797 5213.61 0.797 5213.65 0.797 5213.70 0.796 5213.74 0.796 5213.79 0.796 5213.83 0.796 5213.88 0.796 5213.92 0.796 5213.97 0.796 5214.01 0.796 5214.05 0.795 5214.10 0.795 5214.14 0.795 5214.19 0.795 5214.23 0.795 5214.28 0.795 5214.32 0.795 5214.37 0.795 5214.41 0.794 5214.45 0.794 5214.50 0.794 5214.54 0.794 5214.59 0.794 5214.63 0.794 5214.68 0.793 5214.72 0.793 5214.76 0.793 5214.81 0.793 5214.85 0.793 5214.90 0.793 5214.94 0.793 5214.99 0.793 5215.03 0.792 5215.08 0.792 5215.12 0.792 5215.16 0.792 5215.21 0.792 5215.25 0.792 5215.30 0.792 5215.34 0.792 5215.39 0.792 5215.43 0.791 5215.48 0.791 5215.52 0.791 5215.56 0.791 5215.61 0.791 5215.65 0.791 5215.70 0.791 5215.74 0.791 5215.79 0.791 5215.83 0.791 5215.88 0.790 5215.92 0.790 5215.96 0.790 5216.01 0.790 5216.05 0.790 5216.10 0.790 5216.14 0.790 5216.19 0.790 5216.23 0.789 5216.28 0.789 5216.32 0.789 5216.36 0.789 5216.41 0.789 5216.45 0.789 5216.50 0.788 5216.54 0.788 5216.59 0.788 5216.63 0.788 5216.68 0.788 5216.72 0.788 5216.76 0.787 5216.81 0.787 5216.85 0.787 5216.90 0.787 5216.94 0.787 5216.99 0.786 5217.03 0.786 5217.08 0.786 5217.12 0.786 5217.16 0.786 5217.21 0.786 5217.25 0.786 5217.30 0.785 5217.34 0.785 5217.39 0.785 5217.43 0.785 5217.48 0.785 5217.52 0.785 5217.56 0.785 5217.61 0.785 5217.65 0.785 5217.70 0.785 5217.74 0.784 5217.79 0.784 5217.83 0.784 5217.88 0.784 5217.92 0.784 5217.96 0.784 5218.01 0.784 5218.05 0.783 5218.10 0.783 5218.14 0.783 5218.19 0.783 5218.23 0.783 5218.28 0.783 5218.32 0.783 5218.36 0.783 5218.41 0.782 5218.45 0.782 5218.50 0.782 5218.54 0.782 5218.59 0.782 5218.63 0.782 5218.68 0.782 5218.72 0.781 5218.76 0.781 5218.81 0.781 5218.85 0.781 5218.90 0.781 5218.94 0.781 5218.99 0.780 5219.03 0.780 5219.08 0.780 5219.12 0.780 5219.17 0.780 5219.21 0.780 5219.25 0.780 5219.30 0.779 5219.34 0.779 5219.39 0.779 5219.43 0.779 5219.48 0.779 5219.52 0.779 5219.57 0.778 5219.61 0.778 5219.65 0.778 5219.70 0.778 5219.74 0.778 5219.79 0.778 5219.83 0.778 5219.88 0.778 5219.92 0.777 5219.97 0.777 5220.01 0.777 5220.06 0.777 5220.10 0.777 5220.14 0.776 5220.19 0.776 5220.23 0.776 5220.28 0.776 5220.32 0.776 5220.37 0.776 5220.41 0.776 5220.46 0.775 5220.50 0.775 5220.54 0.775 5220.59 0.775 5220.63 0.775 5220.68 0.775 5220.72 0.774 5220.77 0.774 5220.81 0.774 5220.86 0.774 5220.90 0.774 5220.95 0.774 5220.99 0.773 5221.03 0.773 5221.08 0.773 5221.12 0.773 5221.17 0.773 5221.21 0.773 5221.26 0.773 5221.30 0.772 5221.35 0.772 5221.39 0.772 5221.44 0.772 5221.48 0.772 5221.52 0.772 5221.57 0.772 5221.61 0.772 5221.66 0.772 5221.70 0.771 5221.75 0.771 5221.79 0.771 5221.84 0.771 5221.88 0.771 5221.93 0.771 5221.97 0.771 5222.01 0.770 5222.06 0.770 5222.10 0.770 5222.15 0.770 5222.19 0.770 5222.24 0.770 5222.28 0.770 5222.33 0.770 5222.37 0.769 5222.42 0.769 5222.46 0.769 5222.50 0.769 5222.55 0.769 5222.59 0.769 5222.64 0.769 5222.68 0.768 5222.73 0.768 5222.77 0.768 5222.82 0.768 5222.86 0.768 5222.91 0.768 5222.95 0.768 5222.99 0.767 5223.04 0.767 5223.08 0.767 5223.13 0.767 5223.17 0.767 5223.22 0.767 5223.26 0.767 5223.31 0.767 5223.35 0.767 5223.40 0.767 5223.44 0.766 5223.48 0.767 5223.53 0.767 5223.57 0.767 5223.62 0.767 5223.66 0.767 5223.71 0.767 5223.75 0.767 5223.80 0.767 5223.84 0.767 5223.89 0.766 5223.93 0.766 5223.98 0.766 5224.02 0.766 5224.06 0.766 5224.11 0.766 5224.15 0.766 5224.20 0.766 5224.24 0.766 5224.29 0.766 5224.33 0.765 5224.38 0.765 5224.42 0.765 5224.47 0.765 5224.51 0.765 5224.55 0.764 5224.60 0.764 5224.64 0.764 5224.69 0.764 5224.73 0.764 5224.78 0.763 5224.82 0.763 5224.87 0.763 5224.91 0.763 5224.96 0.763 5225.00 0.762 5225.05 0.762 5225.09 0.762 5225.13 0.762 5225.18 0.762 5225.22 0.761 5225.27 0.761 5225.31 0.761 5225.36 0.761 5225.40 0.761 5225.45 0.761 5225.49 0.760 5225.54 0.760 5225.58 0.760 5225.63 0.760 5225.67 0.760 5225.71 0.760 5225.76 0.759 5225.80 0.759 5225.85 0.759 5225.89 0.759 5225.94 0.759 5225.98 0.759 5226.03 0.759 5226.07 0.759 5226.12 0.758 5226.16 0.758 5226.21 0.758 5226.25 0.758 5226.29 0.758 5226.34 0.758 5226.38 0.757 5226.43 0.757 5226.47 0.757 5226.52 0.757 5226.56 0.757 5226.61 0.757 5226.65 0.756 5226.70 0.756 5226.74 0.756 5226.79 0.756 5226.83 0.755 5226.87 0.755 5226.92 0.755 5226.96 0.755 5227.01 0.755 5227.05 0.754 5227.10 0.754 5227.14 0.754 5227.19 0.754 5227.23 0.753 5227.28 0.753 5227.32 0.753 5227.37 0.753 5227.41 0.753 5227.45 0.752 5227.50 0.752 5227.54 0.752 5227.59 0.751 5227.63 0.751 5227.68 0.751 5227.72 0.750 5227.77 0.750 5227.81 0.750 5227.86 0.750 5227.90 0.749 5227.95 0.749 5227.99 0.749 5228.04 0.749 5228.08 0.749 5228.12 0.749 5228.17 0.748 5228.21 0.748 5228.26 0.748 5228.30 0.748 5228.35 0.748 5228.39 0.748 5228.44 0.748 5228.48 0.748 5228.53 0.748 5228.57 0.747 5228.62 0.747 5228.66 0.747 5228.71 0.747 5228.75 0.747 5228.79 0.747 5228.84 0.747 5228.88 0.747 5228.93 0.747 5228.97 0.747 5229.02 0.746 5229.06 0.746 5229.11 0.746 5229.15 0.746 5229.20 0.746 5229.24 0.746 5229.29 0.746 5229.33 0.746 5229.38 0.746 5229.42 0.746 5229.46 0.746 5229.51 0.746 5229.55 0.745 5229.60 0.745 5229.64 0.745 5229.69 0.745 5229.73 0.745 5229.78 0.745 5229.82 0.745 5229.87 0.745 5229.91 0.745 5229.96 0.745 5230.00 0.744 5230.05 0.744 5230.09 0.744 5230.14 0.744 5230.18 0.744 5230.22 0.744 5230.27 0.744 5230.31 0.744 5230.36 0.744 5230.40 0.743 5230.45 0.743 5230.49 0.743 5230.54 0.743 5230.58 0.743 5230.63 0.743 5230.67 0.743 5230.72 0.743 5230.76 0.743 5230.81 0.743 5230.85 0.742 5230.90 0.742 5230.94 0.742 5230.98 0.742 5231.03 0.742 5231.07 0.742 5231.12 0.742 5231.16 0.741 5231.21 0.741 5231.25 0.741 5231.30 0.741 5231.34 0.741 5231.39 0.741 5231.43 0.741 5231.48 0.740 5231.52 0.740 5231.57 0.740 5231.61 0.740 5231.66 0.740 5231.70 0.740 5231.74 0.740 5231.79 0.740 5231.83 0.739 5231.88 0.739 5231.92 0.739 5231.97 0.739 5232.01 0.739 5232.06 0.739 5232.10 0.739 5232.15 0.739 5232.19 0.738 5232.24 0.738 5232.28 0.738 5232.33 0.738 5232.37 0.738 5232.42 0.738 5232.46 0.737 5232.51 0.737 5232.55 0.737 5232.59 0.737 5232.64 0.737 5232.68 0.737 5232.73 0.737 5232.77 0.737 5232.82 0.736 5232.86 0.736 5232.91 0.736 5232.95 0.736 5233.00 0.736 5233.04 0.736 5233.09 0.736 5233.13 0.736 5233.18 0.736 5233.22 0.736 5233.27 0.735 5233.31 0.735 5233.36 0.735 5233.40 0.735 5233.44 0.735 5233.49 0.735 5233.53 0.735 5233.58 0.735 5233.62 0.734 5233.67 0.734 5233.71 0.734 5233.76 0.734 5233.80 0.734 5233.85 0.734 5233.89 0.734 5233.94 0.733 5233.98 0.733 5234.03 0.733 5234.07 0.733 5234.12 0.733 5234.16 0.733 5234.21 0.733 5234.25 0.733 5234.30 0.732 5234.34 0.732 5234.38 0.732 5234.43 0.732 5234.47 0.732 5234.52 0.732 5234.56 0.732 5234.61 0.732 5234.65 0.732 5234.70 0.731 5234.74 0.731 5234.79 0.731 5234.83 0.731 5234.88 0.731 5234.92 0.731 5234.97 0.731 5235.01 0.730 5235.06 0.730 5235.10 0.730 5235.15 0.730 5235.19 0.730 5235.24 0.730 5235.28 0.730 5235.33 0.730 5235.37 0.730 5235.41 0.730 5235.46 0.729 5235.50 0.729 5235.55 0.729 5235.59 0.729 5235.64 0.729 5235.68 0.729 5235.73 0.729 5235.77 0.728 5235.82 0.728 5235.86 0.728 5235.91 0.728 5235.95 0.728 5236.00 0.728 5236.04 0.728 5236.09 0.728 5236.13 0.728 5236.18 0.727 5236.22 0.727 5236.27 0.727 5236.31 0.727 5236.36 0.727 5236.40 0.727 5236.45 0.727 5236.49 0.727 5236.53 0.726 5236.58 0.726 5236.62 0.726 5236.67 0.726 5236.71 0.726 5236.76 0.726 5236.80 0.726 5236.85 0.725 5236.89 0.725 5236.94 0.725 5236.98 0.725 5237.03 0.725 5237.07 0.725 5237.12 0.725 5237.16 0.725 5237.21 0.724 5237.25 0.724 5237.30 0.724 5237.34 0.724 5237.39 0.724 5237.43 0.724 5237.48 0.724 5237.52 0.723 5237.57 0.723 5237.61 0.723 5237.66 0.723 5237.70 0.723 5237.75 0.723 5237.79 0.723 5237.83 0.723 5237.88 0.723 5237.92 0.722 5237.97 0.722 5238.01 0.722 5238.06 0.722 5238.10 0.722 5238.15 0.722 5238.19 0.722 5238.24 0.722 5238.28 0.722 5238.33 0.721 5238.37 0.721 5238.42 0.721 5238.46 0.721 5238.51 0.721 5238.55 0.721 5238.60 0.720 5238.64 0.720 5238.69 0.720 5238.73 0.720 5238.78 0.720 5238.82 0.720 5238.87 0.720 5238.91 0.720 5238.96 0.719 5239.00 0.719 5239.05 0.719 5239.09 0.719 5239.14 0.719 5239.18 0.719 5239.23 0.719 5239.27 0.719 5239.31 0.719 5239.36 0.719 5239.40 0.718 5239.45 0.718 5239.49 0.718 5239.54 0.718 5239.58 0.718 5239.63 0.718 5239.67 0.718 5239.72 0.718 5239.76 0.718 5239.81 0.717 5239.85 0.717 5239.90 0.717 5239.94 0.717 5239.99 0.717 5240.03 0.717 5240.08 0.716 5240.12 0.716 5240.17 0.716 5240.21 0.716 5240.26 0.716 5240.30 0.716 5240.35 0.716 5240.39 0.715 5240.44 0.715 5240.48 0.715 5240.53 0.715 5240.57 0.715 5240.62 0.715 5240.66 0.715 5240.71 0.715 5240.75 0.715 5240.80 0.715 5240.84 0.715 5240.89 0.714 5240.93 0.714 5240.98 0.714 5241.02 0.714 5241.07 0.714 5241.11 0.714 5241.16 0.714 5241.20 0.714 5241.24 0.713 5241.29 0.713 5241.33 0.713 5241.38 0.713 5241.42 0.713 5241.47 0.713 5241.51 0.713 5241.56 0.712 5241.60 0.712 5241.65 0.712 5241.69 0.712 5241.74 0.712 5241.78 0.712 5241.83 0.712 5241.87 0.711 5241.92 0.711 5241.96 0.711 5242.01 0.711 5242.05 0.711 5242.10 0.711 5242.14 0.711 5242.19 0.711 5242.23 0.711 5242.28 0.710 5242.32 0.710 5242.37 0.710 5242.41 0.710 5242.46 0.710 5242.50 0.710 5242.55 0.710 5242.59 0.710 5242.64 0.709 5242.68 0.709 5242.73 0.709 5242.77 0.709 5242.82 0.709 5242.86 0.709 5242.91 0.709 5242.95 0.708 5243.00 0.708 5243.04 0.708 5243.09 0.708 5243.13 0.708 5243.18 0.708 5243.22 0.708 5243.27 0.708 5243.31 0.708 5243.36 0.708 5243.40 0.707 5243.45 0.707 5243.49 0.707 5243.54 0.707 5243.58 0.707 5243.63 0.707 5243.67 0.707 5243.72 0.707 5243.76 0.706 5243.81 0.706 5243.85 0.706 5243.90 0.706 5243.94 0.706 5243.99 0.706 5244.03 0.706 5244.08 0.706 5244.12 0.706 5244.17 0.706 5244.21 0.705 5244.26 0.705 5244.30 0.705 5244.35 0.705 5244.39 0.705 5244.43 0.705 5244.48 0.705 5244.52 0.704 5244.57 0.704 5244.61 0.704 5244.66 0.704 5244.70 0.704 5244.75 0.704 5244.79 0.704 5244.84 0.704 5244.88 0.704 5244.93 0.704 5244.97 0.703 5245.02 0.703 5245.06 0.703 5245.11 0.703 5245.15 0.703 5245.20 0.703 5245.24 0.703 5245.29 0.703 5245.33 0.702 5245.38 0.702 5245.42 0.702 5245.47 0.702 5245.51 0.702 5245.56 0.702 5245.60 0.702 5245.65 0.702 5245.69 0.701 5245.74 0.701 5245.78 0.701 5245.83 0.701 5245.87 0.701 5245.92 0.701 5245.96 0.701 5246.01 0.700 5246.05 0.700 5246.10 0.700 5246.14 0.700 5246.19 0.700 5246.23 0.700 5246.28 0.700 5246.32 0.700 5246.37 0.700 5246.41 0.700 5246.46 0.699 5246.50 0.699 5246.55 0.699 5246.59 0.699 5246.64 0.698 5246.68 0.698 5246.73 0.698 5246.77 0.698 5246.82 0.698 5246.86 0.698 5246.91 0.698 5246.95 0.697 5247.00 0.697 5247.04 0.697 5247.09 0.697 5247.13 0.696 5247.18 0.696 5247.22 0.696 5247.27 0.696 5247.31 0.696 5247.36 0.696 5247.40 0.696 5247.45 0.696 5247.49 0.696 5247.54 0.696 5247.58 0.696 5247.63 0.696 5247.67 0.696 5247.72 0.696 5247.76 0.696 5247.81 0.696 5247.85 0.696 5247.90 0.696 5247.94 0.696 5247.99 0.696 5248.03 0.696 5248.08 0.696 5248.12 0.696 5248.17 0.696 5248.21 0.696 5248.26 0.696 5248.30 0.696 5248.35 0.696 5248.39 0.696 5248.44 0.695 5248.48 0.695 5248.53 0.695 5248.57 0.695 5248.62 0.695 5248.66 0.695 5248.71 0.695 5248.75 0.694 5248.80 0.694 5248.84 0.694 5248.89 0.694 5248.94 0.694 5248.98 0.694 5249.03 0.694 5249.07 0.693 5249.12 0.693 5249.16 0.693 5249.21 0.693 5249.25 0.693 5249.30 0.693 5249.34 0.693 5249.39 0.693 5249.43 0.692 5249.48 0.692 5249.52 0.692 5249.57 0.692 5249.61 0.692 5249.66 0.692 5249.70 0.692 5249.75 0.692 5249.79 0.691 5249.84 0.691 5249.88 0.691 5249.93 0.691 5249.97 0.691 5250.02 0.691 5250.06 0.691 5250.11 0.691 5250.15 0.691 5250.20 0.691 5250.24 0.691 5250.29 0.691 5250.33 0.691 5250.38 0.691 5250.42 0.691 5250.47 0.691 5250.51 0.690 5250.56 0.690 5250.60 0.690 5250.65 0.690 5250.69 0.690 5250.74 0.690 5250.78 0.690 5250.83 0.690 5250.87 0.690 5250.92 0.689 5250.96 0.689 5251.01 0.689 5251.05 0.689 5251.10 0.689 5251.14 0.689 5251.19 0.689 5251.23 0.689 5251.28 0.688 5251.32 0.688 5251.37 0.688 5251.41 0.688 5251.46 0.688 5251.50 0.688 5251.55 0.688 5251.59 0.688 5251.64 0.688 5251.68 0.688 5251.73 0.688 5251.77 0.688 5251.82 0.688 5251.86 0.687 5251.91 0.687 5251.95 0.687 5252.00 0.687 5252.05 0.687 5252.09 0.687 5252.14 0.687 5252.18 0.687 5252.23 0.687 5252.27 0.686 5252.32 0.686 5252.36 0.686 5252.41 0.686 5252.45 0.686 5252.50 0.686 5252.54 0.686 5252.59 0.686 5252.63 0.685 5252.68 0.685 5252.72 0.685 5252.77 0.685 5252.81 0.685 5252.86 0.685 5252.90 0.685 5252.95 0.685 5252.99 0.685 5253.04 0.685 5253.08 0.685 5253.13 0.685 5253.17 0.685 5253.22 0.684 5253.26 0.684 5253.31 0.684 5253.35 0.684 5253.40 0.684 5253.44 0.684 5253.49 0.684 5253.53 0.684 5253.58 0.684 5253.62 0.683 5253.67 0.683 5253.71 0.683 5253.76 0.683 5253.80 0.683 5253.85 0.683 5253.89 0.682 5253.94 0.682 5253.99 0.682 5254.03 0.682 5254.08 0.682 5254.12 0.682 5254.17 0.682 5254.21 0.682 5254.26 0.681 5254.30 0.681 5254.35 0.681 5254.39 0.681 5254.44 0.681 5254.48 0.681 5254.53 0.681 5254.57 0.681 5254.62 0.681 5254.66 0.681 5254.71 0.681 5254.75 0.681 5254.80 0.680 5254.84 0.680 5254.89 0.680 5254.93 0.680 5254.98 0.680 5255.02 0.680 5255.07 0.679 5255.11 0.679 5255.16 0.679 5255.20 0.679 5255.25 0.679 5255.29 0.679 5255.34 0.679 5255.38 0.679 5255.43 0.679 5255.48 0.678 5255.52 0.678 5255.57 0.678 5255.61 0.678 5255.66 0.678 5255.70 0.678 5255.75 0.678 5255.79 0.678 5255.84 0.678 5255.88 0.677 5255.93 0.677 5255.97 0.677 5256.02 0.677 5256.06 0.677 5256.11 0.677 5256.15 0.677 5256.20 0.676 5256.24 0.676 5256.29 0.676 5256.33 0.676 5256.38 0.676 5256.42 0.676 5256.47 0.676 5256.51 0.676 5256.56 0.675 5256.60 0.675 5256.65 0.675 5256.69 0.675 5256.74 0.675 5256.79 0.675 5256.83 0.675 5256.88 0.675 5256.92 0.675 5256.97 0.674 5257.01 0.674 5257.06 0.674 5257.10 0.674 5257.15 0.674 5257.19 0.674 5257.24 0.674 5257.28 0.674 5257.33 0.674 5257.37 0.673 5257.42 0.673 5257.46 0.673 5257.51 0.673 5257.55 0.673 5257.60 0.673 5257.64 0.673 5257.69 0.672 5257.73 0.672 5257.78 0.672 5257.82 0.672 5257.87 0.672 5257.92 0.672 5257.96 0.672 5258.01 0.672 5258.05 0.671 5258.10 0.671 5258.14 0.671 5258.19 0.671 5258.23 0.671 5258.28 0.671 5258.32 0.670 5258.37 0.670 5258.41 0.670 5258.46 0.670 5258.50 0.670 5258.55 0.670 5258.59 0.670 5258.64 0.670 5258.68 0.670 5258.73 0.669 5258.77 0.669 5258.82 0.669 5258.86 0.669 5258.91 0.669 5258.96 0.669 5259.00 0.669 5259.05 0.669 5259.09 0.668 5259.14 0.668 5259.18 0.668 5259.23 0.668 5259.27 0.668 5259.32 0.668 5259.36 0.668 5259.41 0.668 5259.45 0.667 5259.50 0.667 5259.54 0.667 5259.59 0.667 5259.63 0.667 5259.68 0.667 5259.72 0.667 5259.77 0.667 5259.81 0.667 5259.86 0.667 5259.91 0.667 5259.95 0.667 5260.00 0.666 5260.04 0.666 5260.09 0.666 5260.13 0.666 5260.18 0.666 5260.22 0.666 5260.27 0.665 5260.31 0.665 5260.36 0.665 5260.40 0.665 5260.45 0.665 5260.49 0.665 5260.54 0.665 5260.58 0.664 5260.63 0.664 5260.67 0.664 5260.72 0.664 5260.77 0.664 5260.81 0.664 5260.86 0.664 5260.90 0.664 5260.95 0.664 5260.99 0.663 5261.04 0.663 5261.08 0.663 5261.13 0.663 5261.17 0.663 5261.22 0.663 5261.26 0.663 5261.31 0.663 5261.35 0.663 5261.40 0.663 5261.44 0.663 5261.49 0.663 5261.53 0.663 5261.58 0.662 5261.63 0.662 5261.67 0.662 5261.72 0.662 5261.76 0.662 5261.81 0.662 5261.85 0.662 5261.90 0.662 5261.94 0.662 5261.99 0.661 5262.03 0.661 5262.08 0.661 5262.12 0.661 5262.17 0.661 5262.21 0.661 5262.26 0.660 5262.30 0.660 5262.35 0.660 5262.40 0.660 5262.44 0.660 5262.49 0.660 5262.53 0.659 5262.58 0.659 5262.62 0.659 5262.67 0.659 5262.71 0.659 5262.76 0.659 5262.80 0.659 5262.85 0.659 5262.89 0.659 5262.94 0.659 5262.98 0.658 5263.03 0.658 5263.07 0.658 5263.12 0.658 5263.17 0.658 5263.21 0.658 5263.26 0.657 5263.30 0.657 5263.35 0.657 5263.39 0.657 5263.44 0.657 5263.48 0.657 5263.53 0.657 5263.57 0.657 5263.62 0.657 5263.66 0.657 5263.71 0.656 5263.75 0.656 5263.80 0.656 5263.85 0.656 5263.89 0.656 5263.94 0.656 5263.98 0.656 5264.03 0.655 5264.07 0.655 5264.12 0.655 5264.16 0.655 5264.21 0.655 5264.25 0.655 5264.30 0.654 5264.34 0.654 5264.39 0.654 5264.43 0.654 5264.48 0.654 5264.52 0.654 5264.57 0.654 5264.62 0.654 5264.66 0.654 5264.71 0.653 5264.75 0.653 5264.80 0.653 5264.84 0.653 5264.89 0.653 5264.93 0.653 5264.98 0.653 5265.02 0.653 5265.07 0.652 5265.11 0.652 5265.16 0.652 5265.21 0.652 5265.25 0.652 5265.30 0.652 5265.34 0.652 5265.39 0.652 5265.43 0.652 5265.48 0.652 5265.52 0.651 5265.57 0.651 5265.61 0.651 5265.66 0.651 5265.70 0.651 5265.75 0.651 5265.79 0.651 5265.84 0.650 5265.89 0.650 5265.93 0.650 5265.98 0.650 5266.02 0.650 5266.07 0.650 5266.11 0.650 5266.16 0.650 5266.20 0.650 5266.25 0.649 5266.29 0.649 5266.34 0.649 5266.38 0.649 5266.43 0.649 5266.48 0.648 5266.52 0.648 5266.57 0.648 5266.61 0.648 5266.66 0.648 5266.70 0.647 5266.75 0.647 5266.79 0.647 5266.84 0.647 5266.88 0.647 5266.93 0.647 5266.97 0.647 5267.02 0.647 5267.06 0.647 5267.11 0.646 5267.16 0.646 5267.20 0.646 5267.25 0.646 5267.29 0.646 5267.34 0.646 5267.38 0.645 5267.43 0.645 5267.47 0.645 5267.52 0.645 5267.56 0.645 5267.61 0.645 5267.65 0.645 5267.70 0.645 5267.75 0.644 5267.79 0.644 5267.84 0.644 5267.88 0.644 5267.93 0.644 5267.97 0.644 5268.02 0.643 5268.06 0.643 5268.11 0.643 5268.15 0.643 5268.20 0.643 5268.25 0.643 5268.29 0.643 5268.34 0.643 5268.38 0.642 5268.43 0.642 5268.47 0.642 5268.52 0.642 5268.56 0.642 5268.61 0.642 5268.65 0.641 5268.70 0.641 5268.74 0.641 5268.79 0.641 5268.84 0.641 5268.88 0.641 5268.93 0.641 5268.97 0.641 5269.02 0.641 5269.06 0.640 5269.11 0.640 5269.15 0.640 5269.20 0.640 5269.24 0.640 5269.29 0.640 5269.33 0.640 5269.38 0.640 5269.43 0.639 5269.47 0.639 5269.52 0.639 5269.56 0.639 5269.61 0.639 5269.65 0.639 5269.70 0.639 5269.74 0.638 5269.79 0.638 5269.83 0.638 5269.88 0.638 5269.93 0.638 5269.97 0.638 5270.02 0.638 5270.06 0.638 5270.11 0.638 5270.15 0.637 5270.20 0.637 5270.24 0.637 5270.29 0.637 5270.33 0.637 5270.38 0.637 5270.43 0.637 5270.47 0.637 5270.52 0.637 5270.56 0.637 5270.61 0.636 5270.65 0.636 5270.70 0.636 5270.74 0.636 5270.79 0.636 5270.83 0.636 5270.88 0.636 5270.93 0.635 5270.97 0.635 5271.02 0.635 5271.06 0.635 5271.11 0.635 5271.15 0.635 5271.20 0.635 5271.24 0.635 5271.29 0.634 5271.33 0.634 5271.38 0.634 5271.43 0.634 5271.47 0.634 5271.52 0.634 5271.56 0.634 5271.61 0.633 5271.65 0.633 5271.70 0.633 5271.74 0.633 5271.79 0.633 5271.83 0.633 5271.88 0.633 5271.93 0.632 5271.97 0.632 5272.02 0.632 5272.06 0.632 5272.11 0.632 5272.15 0.632 5272.20 0.631 5272.24 0.631 5272.29 0.631 5272.33 0.631 5272.38 0.631 5272.43 0.631 5272.47 0.630 5272.52 0.630 5272.56 0.630 5272.61 0.630 5272.65 0.630 5272.70 0.630 5272.74 0.630 5272.79 0.630 5272.84 0.630 5272.88 0.629 5272.93 0.629 5272.97 0.629 5273.02 0.629 5273.06 0.629 5273.11 0.629 5273.15 0.629 5273.20 0.629 5273.24 0.628 5273.29 0.628 5273.34 0.628 5273.38 0.628 5273.43 0.628 5273.47 0.628 5273.52 0.628 5273.56 0.627 5273.61 0.627 5273.65 0.627 5273.70 0.627 5273.75 0.627 5273.79 0.627 5273.84 0.627 5273.88 0.626 5273.93 0.626 5273.97 0.626 5274.02 0.626 5274.06 0.626 5274.11 0.626 5274.15 0.626 5274.20 0.625 5274.25 0.625 5274.29 0.625 5274.34 0.625 5274.38 0.625 5274.43 0.625 5274.47 0.625 5274.52 0.624 5274.56 0.624 5274.61 0.624 5274.66 0.624 5274.70 0.624 5274.75 0.624 5274.79 0.624 5274.84 0.624 5274.88 0.624 5274.93 0.624 5274.97 0.623 5275.02 0.623 5275.07 0.623 5275.11 0.623 5275.16 0.623 5275.20 0.623 5275.25 0.623 5275.29 0.622 5275.34 0.622 5275.38 0.622 5275.43 0.622 5275.47 0.622 5275.52 0.622 5275.57 0.621 5275.61 0.621 5275.66 0.621 5275.70 0.621 5275.75 0.621 5275.79 0.621 5275.84 0.621 5275.88 0.620 5275.93 0.620 5275.98 0.620 5276.02 0.620 5276.07 0.620 5276.11 0.620 5276.16 0.619 5276.20 0.619 5276.25 0.619 5276.29 0.619 5276.34 0.619 5276.39 0.619 5276.43 0.619 5276.48 0.619 5276.52 0.619 5276.57 0.619 5276.61 0.618 5276.66 0.618 5276.70 0.618 5276.75 0.618 5276.80 0.618 5276.84 0.618 5276.89 0.618 5276.93 0.618 5276.98 0.617 5277.02 0.617 5277.07 0.617 5277.11 0.617 5277.16 0.617 5277.21 0.617 5277.25 0.616 5277.30 0.616 5277.34 0.616 5277.39 0.616 5277.43 0.616 5277.48 0.616 5277.52 0.616 5277.57 0.616 5277.62 0.615 5277.66 0.615 5277.71 0.615 5277.75 0.615 5277.80 0.615 5277.84 0.615 5277.89 0.615 5277.94 0.614 5277.98 0.614 5278.03 0.614 5278.07 0.614 5278.12 0.614 5278.16 0.614 5278.21 0.613 5278.25 0.613 5278.30 0.613 5278.35 0.613 5278.39 0.613 5278.44 0.613 5278.48 0.613 5278.53 0.612 5278.57 0.612 5278.62 0.612 5278.66 0.612 5278.71 0.612 5278.76 0.612 5278.80 0.612 5278.85 0.611 5278.89 0.611 5278.94 0.611 5278.98 0.611 5279.03 0.611 5279.07 0.611 5279.12 0.611 5279.17 0.611 5279.21 0.611 5279.26 0.611 5279.30 0.610 5279.35 0.610 5279.39 0.610 5279.44 0.610 5279.49 0.610 5279.53 0.610 5279.58 0.610 5279.62 0.610 5279.67 0.609 5279.71 0.609 5279.76 0.609 5279.80 0.609 5279.85 0.608 5279.90 0.608 5279.94 0.608 5279.99 0.608 5280.03 0.608 5280.08 0.608 5280.12 0.608 5280.17 0.608 5280.22 0.607 5280.26 0.607 5280.31 0.607 5280.35 0.607 5280.40 0.607 5280.44 0.607 5280.49 0.607 5280.53 0.606 5280.58 0.606 5280.63 0.606 5280.67 0.606 5280.72 0.606 5280.76 0.606 5280.81 0.605 5280.85 0.605 5280.90 0.605 5280.95 0.605 5280.99 0.605 5281.04 0.605 5281.08 0.605 5281.13 0.605 5281.17 0.605 5281.22 0.605 5281.26 0.604 5281.31 0.604 5281.36 0.604 5281.40 0.604 5281.45 0.604 5281.49 0.604 5281.54 0.603 5281.58 0.603 5281.63 0.603 5281.68 0.603 5281.72 0.603 5281.77 0.603 5281.81 0.603 5281.86 0.602 5281.90 0.602 5281.95 0.602 5282.00 0.602 5282.04 0.602 5282.09 0.602 5282.13 0.601 5282.18 0.601 5282.22 0.601 5282.27 0.601 5282.32 0.601 5282.36 0.601 5282.41 0.601 5282.45 0.601 5282.50 0.600 5282.54 0.600 5282.59 0.600 5282.63 0.600 5282.68 0.600 5282.73 0.600 5282.77 0.600 5282.82 0.600 5282.86 0.599 5282.91 0.599 5282.95 0.599 5283.00 0.599 5283.05 0.599 5283.09 0.599 5283.14 0.599 5283.18 0.598 5283.23 0.598 5283.27 0.598 5283.32 0.598 5283.37 0.598 5283.41 0.598 5283.46 0.598 5283.50 0.598 5283.55 0.597 5283.59 0.597 5283.64 0.597 5283.69 0.597 5283.73 0.597 5283.78 0.597 5283.82 0.597 5283.87 0.597 5283.91 0.596 5283.96 0.596 5284.01 0.596 5284.05 0.596 5284.10 0.596 5284.14 0.596 5284.19 0.596 5284.23 0.596 5284.28 0.595 5284.33 0.595 5284.37 0.595 5284.42 0.595 5284.46 0.595 5284.51 0.595 5284.55 0.595 5284.60 0.594 5284.65 0.594 5284.69 0.594 5284.74 0.594 5284.78 0.594 5284.83 0.594 5284.87 0.594 5284.92 0.594 5284.97 0.593 5285.01 0.593 5285.06 0.593 5285.10 0.593 5285.15 0.593 5285.19 0.593 5285.24 0.592 5285.29 0.592 5285.33 0.592 5285.38 0.592 5285.42 0.592 5285.47 0.592 5285.51 0.592 5285.56 0.592 5285.61 0.591 5285.65 0.591 5285.70 0.591 5285.74 0.591 5285.79 0.591 5285.83 0.590 5285.88 0.590 5285.93 0.590 5285.97 0.590 5286.02 0.590 5286.06 0.589 5286.11 0.589 5286.15 0.589 5286.20 0.589 5286.25 0.589 5286.29 0.589 5286.34 0.589 5286.38 0.588 5286.43 0.588 5286.47 0.588 5286.52 0.588 5286.57 0.588 5286.61 0.588 5286.66 0.587 5286.70 0.587 5286.75 0.587 5286.79 0.587 5286.84 0.587 5286.89 0.587 5286.93 0.587 5286.98 0.587 5287.02 0.586 5287.07 0.586 5287.11 0.586 5287.16 0.586 5287.21 0.586 5287.25 0.586 5287.30 0.586 5287.34 0.585 5287.39 0.585 5287.43 0.585 5287.48 0.585 5287.53 0.585 5287.57 0.585 5287.62 0.584 5287.66 0.584 5287.71 0.584 5287.76 0.584 5287.80 0.584 5287.85 0.584 5287.89 0.584 5287.94 0.584 5287.98 0.583 5288.03 0.583 5288.08 0.583 5288.12 0.583 5288.17 0.583 5288.21 0.583 5288.26 0.582 5288.30 0.582 5288.35 0.582 5288.40 0.582 5288.44 0.582 5288.49 0.582 5288.53 0.581 5288.58 0.581 5288.62 0.581 5288.67 0.581 5288.72 0.581 5288.76 0.581 5288.81 0.580 5288.85 0.580 5288.90 0.580 5288.95 0.580 5288.99 0.580 5289.04 0.580 5289.08 0.580 5289.13 0.580 5289.17 0.579 5289.22 0.579 5289.27 0.579 5289.31 0.579 5289.36 0.579 5289.40 0.579 5289.45 0.579 5289.50 0.578 5289.54 0.578 5289.59 0.578 5289.63 0.578 5289.68 0.578 5289.72 0.578 5289.77 0.578 5289.82 0.577 5289.86 0.577 5289.91 0.577 5289.95 0.577 5290.00 0.577 5290.04 0.577 5290.09 0.576 5290.14 0.576 5290.18 0.576 5290.23 0.576 5290.27 0.576 5290.32 0.576 5290.37 0.576 5290.41 0.576 5290.46 0.575 5290.50 0.575 5290.55 0.575 5290.59 0.575 5290.64 0.575 5290.69 0.574 5290.73 0.574 5290.78 0.574 5290.82 0.574 5290.87 0.574 5290.92 0.574 5290.96 0.574 5291.01 0.573 5291.05 0.573 5291.10 0.573 5291.14 0.573 5291.19 0.573 5291.24 0.573 5291.28 0.572 5291.33 0.572 5291.37 0.572 5291.42 0.572 5291.47 0.572 5291.51 0.572 5291.56 0.571 5291.60 0.571 5291.65 0.571 5291.69 0.571 5291.74 0.571 5291.79 0.571 5291.83 0.571 5291.88 0.571 5291.92 0.570 5291.97 0.570 5292.02 0.570 5292.06 0.570 5292.11 0.570 5292.15 0.570 5292.20 0.570 5292.24 0.569 5292.29 0.569 5292.34 0.569 5292.38 0.569 5292.43 0.569 5292.47 0.569 5292.52 0.568 5292.57 0.568 5292.61 0.568 5292.66 0.568 5292.70 0.568 5292.75 0.568 5292.79 0.567 5292.84 0.567 5292.89 0.567 5292.93 0.567 5292.98 0.567 5293.02 0.567 5293.07 0.567 5293.12 0.566 5293.16 0.566 5293.21 0.566 5293.25 0.566 5293.30 0.566 5293.35 0.566 5293.39 0.566 5293.44 0.565 5293.48 0.565 5293.53 0.565 5293.57 0.565 5293.62 0.565 5293.67 0.564 5293.71 0.564 5293.76 0.564 5293.80 0.564 5293.85 0.564 5293.90 0.564 5293.94 0.563 5293.99 0.563 5294.03 0.563 5294.08 0.563 5294.13 0.563 5294.17 0.563 5294.22 0.563 5294.26 0.562 5294.31 0.562 5294.35 0.562 5294.40 0.562 5294.45 0.562 5294.49 0.562 5294.54 0.562 5294.58 0.562 5294.63 0.561 5294.68 0.561 5294.72 0.561 5294.77 0.561 5294.81 0.561 5294.86 0.561 5294.91 0.561 5294.95 0.561 5295.00 0.560 5295.04 0.560 5295.09 0.560 5295.13 0.560 5295.18 0.560 5295.23 0.560 5295.27 0.560 5295.32 0.560 5295.36 0.559 5295.41 0.559 5295.46 0.559 5295.50 0.559 5295.55 0.559 5295.59 0.559 5295.64 0.559 5295.69 0.558 5295.73 0.558 5295.78 0.558 5295.82 0.558 5295.87 0.558 5295.92 0.558 5295.96 0.557 5296.01 0.557 5296.05 0.557 5296.10 0.557 5296.15 0.557 5296.19 0.557 5296.24 0.557 5296.28 0.556 5296.33 0.556 5296.37 0.556 5296.42 0.556 5296.47 0.556 5296.51 0.556 5296.56 0.555 5296.60 0.555 5296.65 0.555 5296.70 0.555 5296.74 0.555 5296.79 0.555 5296.83 0.555 5296.88 0.555 5296.93 0.554 5296.97 0.554 5297.02 0.554 5297.06 0.554 5297.11 0.554 5297.16 0.554 5297.20 0.553 5297.25 0.553 5297.29 0.553 5297.34 0.553 5297.39 0.553 5297.43 0.553 5297.48 0.553 5297.52 0.553 5297.57 0.552 5297.62 0.552 5297.66 0.552 5297.71 0.552 5297.75 0.552 5297.80 0.552 5297.84 0.551 5297.89 0.551 5297.94 0.551 5297.98 0.551 5298.03 0.551 5298.07 0.551 5298.12 0.551 5298.17 0.551 5298.21 0.550 5298.26 0.550 5298.30 0.550 5298.35 0.550 5298.40 0.550 5298.44 0.550 5298.49 0.549 5298.53 0.549 5298.58 0.549 5298.63 0.549 5298.67 0.549 5298.72 0.549 5298.76 0.549 5298.81 0.549 5298.86 0.549 5298.90 0.549 5298.95 0.548 5298.99 0.548 5299.04 0.548 5299.09 0.548 5299.13 0.548 5299.18 0.547 5299.22 0.547 5299.27 0.547 5299.32 0.547 5299.36 0.547 5299.41 0.547 5299.45 0.546 5299.50 0.546 5299.55 0.546 5299.59 0.546 5299.64 0.546 5299.68 0.545 5299.73 0.545 5299.78 0.545 5299.82 0.545 5299.87 0.544 5299.91 0.544 5299.96 0.544 5300.01 0.544 5300.05 0.544 5300.10 0.543 5300.14 0.543 5300.19 0.543 5300.24 0.542 5300.28 0.542 5300.33 0.542 5300.37 0.541 5300.42 0.541 5300.47 0.541 5300.51 0.541 5300.56 0.540 5300.60 0.540 5300.65 0.540 5300.70 0.540 5300.74 0.540 5300.79 0.540 5300.83 0.540 5300.88 0.539 5300.93 0.539 5300.97 0.539 5301.02 0.539 5301.06 0.539 5301.11 0.539 5301.16 0.539 5301.20 0.540 5301.25 0.540 5301.29 0.540 5301.34 0.540 5301.39 0.540 5301.43 0.540 5301.48 0.540 5301.52 0.540 5301.57 0.540 5301.62 0.539 5301.66 0.539 5301.71 0.539 5301.75 0.539 5301.80 0.539 5301.85 0.539 5301.89 0.539 5301.94 0.538 5301.98 0.538 5302.03 0.538 5302.08 0.538 5302.12 0.538 5302.17 0.538 5302.21 0.538 5302.26 0.537 5302.31 0.537 5302.35 0.537 5302.40 0.537 5302.44 0.537 5302.49 0.537 5302.54 0.537 5302.58 0.537 5302.63 0.536 5302.67 0.536 5302.72 0.536 5302.77 0.536 5302.81 0.536 5302.86 0.536 5302.91 0.536 5302.95 0.536 5303.00 0.535 5303.04 0.535 5303.09 0.535 5303.14 0.535 5303.18 0.535 5303.23 0.535 5303.27 0.535 5303.32 0.535 5303.37 0.534 5303.41 0.534 5303.46 0.534 5303.50 0.534 5303.55 0.534 5303.60 0.534 5303.64 0.534 5303.69 0.534 5303.73 0.534 5303.78 0.534 5303.83 0.533 5303.87 0.533 5303.92 0.533 5303.96 0.533 5304.01 0.533 5304.06 0.533 5304.10 0.532 5304.15 0.532 5304.19 0.532 5304.24 0.532 5304.29 0.532 5304.33 0.532 5304.38 0.532 5304.43 0.531 5304.47 0.531 5304.52 0.531 5304.56 0.531 5304.61 0.531 5304.66 0.531 5304.70 0.530 5304.75 0.530 5304.79 0.530 5304.84 0.530 5304.89 0.530 5304.93 0.530 5304.98 0.530 5305.02 0.530 5305.07 0.529 5305.12 0.529 5305.16 0.529 5305.21 0.529 5305.25 0.529 5305.30 0.529 5305.35 0.528 5305.39 0.528 5305.44 0.528 5305.49 0.528 5305.53 0.528 5305.58 0.528 5305.62 0.527 5305.67 0.527 5305.72 0.527 5305.76 0.527 5305.81 0.527 5305.85 0.527 5305.90 0.527 5305.95 0.527 5305.99 0.527 5306.04 0.527 5306.08 0.526 5306.13 0.526 5306.18 0.526 5306.22 0.526 5306.27 0.525 5306.32 0.525 5306.36 0.525 5306.41 0.525 5306.45 0.525 5306.50 0.525 5306.55 0.525 5306.59 0.525 5306.64 0.525 5306.68 0.525 5306.73 0.524 5306.78 0.524 5306.82 0.524 5306.87 0.524 5306.91 0.524 5306.96 0.524 5307.01 0.524 5307.05 0.523 5307.10 0.523 5307.15 0.523 5307.19 0.523 5307.24 0.523 5307.28 0.523 5307.33 0.522 5307.38 0.522 5307.42 0.522 5307.47 0.522 5307.51 0.522 5307.56 0.522 5307.61 0.522 5307.65 0.522 5307.70 0.521 5307.75 0.521 5307.79 0.521 5307.84 0.521 5307.88 0.521 5307.93 0.521 5307.98 0.521 5308.02 0.520 5308.07 0.520 5308.11 0.520 5308.16 0.520 5308.21 0.520 5308.25 0.520 5308.30 0.519 5308.35 0.519 5308.39 0.519 5308.44 0.519 5308.48 0.519 5308.53 0.519 5308.58 0.519 5308.62 0.518 5308.67 0.518 5308.71 0.517 5308.76 0.516 5308.81 0.514 5308.85 0.512 5308.90 0.510 5308.95 0.507 5308.99 0.505 5309.04 0.503 5309.08 0.502 5309.13 0.501 5309.18 0.501 5309.22 0.502 5309.27 0.503 5309.31 0.504 5309.36 0.505 5309.41 0.506 5309.45 0.507 5309.50 0.508 5309.55 0.509 5309.59 0.510 5309.64 0.510 5309.68 0.511 5309.73 0.511 5309.78 0.512 5309.82 0.512 5309.87 0.512 5309.91 0.512 5309.96 0.512 5310.01 0.512 5310.05 0.512 5310.10 0.512 5310.15 0.512 5310.19 0.512 5310.24 0.512 5310.28 0.512 5310.33 0.512 5310.38 0.512 5310.42 0.512 5310.47 0.512 5310.52 0.511 5310.56 0.511 5310.61 0.511 5310.65 0.511 5310.70 0.511 5310.75 0.511 5310.79 0.511 5310.84 0.511 5310.89 0.511 5310.93 0.510 5310.98 0.510 5311.02 0.510 5311.07 0.510 5311.12 0.510 5311.16 0.510 5311.21 0.510 5311.25 0.509 5311.30 0.509 5311.35 0.509 5311.39 0.509 5311.44 0.509 5311.49 0.509 5311.53 0.508 5311.58 0.508 5311.62 0.508 5311.67 0.508 5311.72 0.508 5311.76 0.508 5311.81 0.508 5311.86 0.508 5311.90 0.507 5311.95 0.507 5311.99 0.507 5312.04 0.507 5312.09 0.507 5312.13 0.507 5312.18 0.507 5312.23 0.506 5312.27 0.506 5312.32 0.506 5312.36 0.506 5312.41 0.506 5312.46 0.506 5312.50 0.506 5312.55 0.505 5312.60 0.505 5312.64 0.505 5312.69 0.505 5312.73 0.505 5312.78 0.505 5312.83 0.504 5312.87 0.504 5312.92 0.504 5312.96 0.504 5313.01 0.504 5313.06 0.504 5313.10 0.503 5313.15 0.503 5313.20 0.503 5313.24 0.503 5313.29 0.503 5313.33 0.503 5313.38 0.503 5313.43 0.503 5313.47 0.503 5313.52 0.502 5313.57 0.502 5313.61 0.502 5313.66 0.502 5313.70 0.502 5313.75 0.502 5313.80 0.501 5313.84 0.501 5313.89 0.501 5313.94 0.501 5313.98 0.501 5314.03 0.501 5314.07 0.501 5314.12 0.500 5314.17 0.500 5314.21 0.500 5314.26 0.500 5314.31 0.500 5314.35 0.500 5314.40 0.500 5314.45 0.500 5314.49 0.500 5314.54 0.499 5314.58 0.499 5314.63 0.499 5314.68 0.499 5314.72 0.499 5314.77 0.499 5314.82 0.498 5314.86 0.498 5314.91 0.498 5314.95 0.498 5315.00 0.498 5315.05 0.498 5315.09 0.498 5315.14 0.498 5315.19 0.498 5315.23 0.497 5315.28 0.497 5315.32 0.497 5315.37 0.497 5315.42 0.497 5315.46 0.496 5315.51 0.496 5315.56 0.496 5315.60 0.496 5315.65 0.496 5315.69 0.496 5315.74 0.496 5315.79 0.495 5315.83 0.495 5315.88 0.495 5315.93 0.495 5315.97 0.495 5316.02 0.495 5316.06 0.494 5316.11 0.494 5316.16 0.494 5316.20 0.494 5316.25 0.494 5316.30 0.494 5316.34 0.494 5316.39 0.494 5316.44 0.494 5316.48 0.493 5316.53 0.493 5316.57 0.493 5316.62 0.493 5316.67 0.493 5316.71 0.493 5316.76 0.493 5316.81 0.493 5316.85 0.492 5316.90 0.492 5316.94 0.492 5316.99 0.492 5317.04 0.492 5317.08 0.491 5317.13 0.491 5317.18 0.491 5317.22 0.491 5317.27 0.491 5317.32 0.491 5317.36 0.490 5317.41 0.490 5317.45 0.490 5317.50 0.490 5317.55 0.490 5317.59 0.490 5317.64 0.490 5317.69 0.489 5317.73 0.489 5317.78 0.489 5317.82 0.489 5317.87 0.489 5317.92 0.489 5317.96 0.489 5318.01 0.489 5318.06 0.489 5318.10 0.488 5318.15 0.488 5318.20 0.488 5318.24 0.488 5318.29 0.488 5318.33 0.488 5318.38 0.487 5318.43 0.487 5318.47 0.487 5318.52 0.487 5318.57 0.487 5318.61 0.487 5318.66 0.486 5318.71 0.486 5318.75 0.486 5318.80 0.486 5318.84 0.486 5318.89 0.486 5318.94 0.486 5318.98 0.486 5319.03 0.485 5319.08 0.485 5319.12 0.485 5319.17 0.485 5319.22 0.485 5319.26 0.485 5319.31 0.485 5319.35 0.485 5319.40 0.484 5319.45 0.484 5319.49 0.484 5319.54 0.484 5319.59 0.484 5319.63 0.484 5319.68 0.483 5319.73 0.483 5319.77 0.483 5319.82 0.483 5319.86 0.483 5319.91 0.483 5319.96 0.483 5320.00 0.482 5320.05 0.482 5320.10 0.482 5320.14 0.482 5320.19 0.482 5320.24 0.482 5320.28 0.482 5320.33 0.482 5320.37 0.482 5320.42 0.482 5320.47 0.482 5320.51 0.481 5320.56 0.481 5320.61 0.481 5320.65 0.481 5320.70 0.481 5320.75 0.481 5320.79 0.480 5320.84 0.480 5320.88 0.480 5320.93 0.480 5320.98 0.480 5321.02 0.480 5321.07 0.480 5321.12 0.479 5321.16 0.479 5321.21 0.479 5321.26 0.479 5321.30 0.479 5321.35 0.479 5321.40 0.478 5321.44 0.478 5321.49 0.478 5321.53 0.478 5321.58 0.478 5321.63 0.478 5321.67 0.478 5321.72 0.477 5321.77 0.477 5321.81 0.477 5321.86 0.477 5321.91 0.477 5321.95 0.477 5322.00 0.477 5322.04 0.476 5322.09 0.476 5322.14 0.476 5322.18 0.476 5322.23 0.476 5322.28 0.476 5322.32 0.476 5322.37 0.476 5322.42 0.475 5322.46 0.475 5322.51 0.475 5322.56 0.475 5322.60 0.475 5322.65 0.475 5322.69 0.475 5322.74 0.475 5322.79 0.474 5322.83 0.474 5322.88 0.474 5322.93 0.474 5322.97 0.474 5323.02 0.474 5323.07 0.473 5323.11 0.473 5323.16 0.473 5323.21 0.473 5323.25 0.473 5323.30 0.473 5323.34 0.472 5323.39 0.472 5323.44 0.472 5323.48 0.472 5323.53 0.472 5323.58 0.472 5323.62 0.472 5323.67 0.472 5323.72 0.471 5323.76 0.471 5323.81 0.471 5323.86 0.471 5323.90 0.471 5323.95 0.471 5323.99 0.470 5324.04 0.470 5324.09 0.470 5324.13 0.470 5324.18 0.470 5324.23 0.470 5324.27 0.470 5324.32 0.470 5324.37 0.470 5324.41 0.469 5324.46 0.469 5324.51 0.469 5324.55 0.469 5324.60 0.469 5324.65 0.468 5324.69 0.468 5324.74 0.468 5324.78 0.468 5324.83 0.468 5324.88 0.468 5324.92 0.467 5324.97 0.467 5325.02 0.467 5325.06 0.467 5325.11 0.467 5325.16 0.467 5325.20 0.467 5325.25 0.466 5325.30 0.466 5325.34 0.466 5325.39 0.466 5325.44 0.466 5325.48 0.466 5325.53 0.466 5325.57 0.466 5325.62 0.466 5325.67 0.465 5325.71 0.465 5325.76 0.465 5325.81 0.465 5325.85 0.465 5325.90 0.465 5325.95 0.465 5325.99 0.464 5326.04 0.464 5326.09 0.464 5326.13 0.464 5326.18 0.464 5326.23 0.464 5326.27 0.463 5326.32 0.463 5326.36 0.463 5326.41 0.463 5326.46 0.463 5326.50 0.463 5326.55 0.463 5326.60 0.462 5326.64 0.462 5326.69 0.462 5326.74 0.462 5326.78 0.462 5326.83 0.462 5326.88 0.462 5326.92 0.462 5326.97 0.462 5327.02 0.461 5327.06 0.461 5327.11 0.461 5327.16 0.461 5327.20 0.461 5327.25 0.461 5327.29 0.461 5327.34 0.460 5327.39 0.460 5327.43 0.460 5327.48 0.460 5327.53 0.460 5327.57 0.460 5327.62 0.460 5327.67 0.459 5327.71 0.459 5327.76 0.459 5327.81 0.459 5327.85 0.459 5327.90 0.459 5327.95 0.459 5327.99 0.458 5328.04 0.458 5328.09 0.458 5328.13 0.458 5328.18 0.458 5328.23 0.458 5328.27 0.457 5328.32 0.457 5328.36 0.457 5328.41 0.457 5328.46 0.457 5328.50 0.457 5328.55 0.457 5328.60 0.456 5328.64 0.456 5328.69 0.456 5328.74 0.456 5328.78 0.456 5328.83 0.456 5328.88 0.456 5328.92 0.455 5328.97 0.455 5329.02 0.455 5329.06 0.455 5329.11 0.455 5329.16 0.455 5329.20 0.455 5329.25 0.455 5329.30 0.454 5329.34 0.454 5329.39 0.454 5329.44 0.454 5329.48 0.454 5329.53 0.454 5329.57 0.454 5329.62 0.454 5329.67 0.454 5329.71 0.454 5329.76 0.453 5329.81 0.453 5329.85 0.453 5329.90 0.453 5329.95 0.453 5329.99 0.453 5330.04 0.452 5330.09 0.452 5330.13 0.452 5330.18 0.452 5330.23 0.452 5330.27 0.452 5330.32 0.452 5330.37 0.452 5330.41 0.452 5330.46 0.452 5330.51 0.451 5330.55 0.451 5330.60 0.451 5330.65 0.451 5330.69 0.451 5330.74 0.451 5330.79 0.451 5330.83 0.451 5330.88 0.450 5330.93 0.450 5330.97 0.450 5331.02 0.450 5331.06 0.450 5331.11 0.450 5331.16 0.450 5331.20 0.449 5331.25 0.449 5331.30 0.449 5331.34 0.449 5331.39 0.449 5331.44 0.448 5331.48 0.448 5331.53 0.448 5331.58 0.448 5331.62 0.448 5331.67 0.448 5331.72 0.447 5331.76 0.447 5331.81 0.447 5331.86 0.447 5331.90 0.447 5331.95 0.447 5332.00 0.447 5332.04 0.446 5332.09 0.446 5332.14 0.446 5332.18 0.446 5332.23 0.446 5332.28 0.446 5332.32 0.446 5332.37 0.446 5332.42 0.445 5332.46 0.445 5332.51 0.445 5332.56 0.445 5332.60 0.445 5332.65 0.445 5332.70 0.444 5332.74 0.444 5332.79 0.444 5332.84 0.444 5332.88 0.444 5332.93 0.444 5332.98 0.443 5333.02 0.443 5333.07 0.443 5333.12 0.443 5333.16 0.443 5333.21 0.443 5333.26 0.443 5333.30 0.442 5333.35 0.442 5333.40 0.442 5333.44 0.442 5333.49 0.442 5333.53 0.442 5333.58 0.442 5333.63 0.442 5333.67 0.442 5333.72 0.441 5333.77 0.441 5333.81 0.441 5333.86 0.441 5333.91 0.441 5333.95 0.441 5334.00 0.441 5334.05 0.441 5334.09 0.441 5334.14 0.440 5334.19 0.440 5334.23 0.440 5334.28 0.440 5334.33 0.440 5334.37 0.440 5334.42 0.440 5334.47 0.439 5334.51 0.439 5334.56 0.439 5334.61 0.439 5334.65 0.439 5334.70 0.439 5334.75 0.438 5334.79 0.438 5334.84 0.438 5334.89 0.438 5334.93 0.438 5334.98 0.438 5335.03 0.438 5335.07 0.438 5335.12 0.438 5335.17 0.437 5335.21 0.437 5335.26 0.437 5335.31 0.437 5335.35 0.437 5335.40 0.437 5335.45 0.437 5335.49 0.436 5335.54 0.436 5335.59 0.436 5335.63 0.436 5335.68 0.436 5335.73 0.436 5335.77 0.436 5335.82 0.436 5335.87 0.435 5335.91 0.435 5335.96 0.435 5336.01 0.435 5336.05 0.435 5336.10 0.435 5336.15 0.435 5336.19 0.435 5336.24 0.434 5336.29 0.434 5336.33 0.434 5336.38 0.434 5336.43 0.434 5336.47 0.434 5336.52 0.434 5336.57 0.433 5336.61 0.433 5336.66 0.433 5336.71 0.433 5336.75 0.433 5336.80 0.433 5336.85 0.433 5336.89 0.432 5336.94 0.432 5336.99 0.432 5337.03 0.432 5337.08 0.432 5337.13 0.432 5337.17 0.432 5337.22 0.431 5337.27 0.431 5337.31 0.431 5337.36 0.431 5337.41 0.431 5337.45 0.430 5337.50 0.430 5337.55 0.430 5337.59 0.430 5337.64 0.430 5337.69 0.430 5337.74 0.430 5337.78 0.430 5337.83 0.430 5337.88 0.429 5337.92 0.429 5337.97 0.429 5338.02 0.429 5338.06 0.429 5338.11 0.429 5338.16 0.429 5338.20 0.429 5338.25 0.428 5338.30 0.428 5338.34 0.428 5338.39 0.428 5338.44 0.428 5338.48 0.428 5338.53 0.428 5338.58 0.427 5338.62 0.427 5338.67 0.427 5338.72 0.427 5338.76 0.427 5338.81 0.427 5338.86 0.427 5338.90 0.427 5338.95 0.426 5339.00 0.426 5339.04 0.426 5339.09 0.426 5339.14 0.426 5339.18 0.425 5339.23 0.425 5339.28 0.425 5339.32 0.425 5339.37 0.425 5339.42 0.425 5339.46 0.425 5339.51 0.425 5339.56 0.424 5339.60 0.424 5339.65 0.424 5339.70 0.424 5339.74 0.424 5339.79 0.424 5339.84 0.424 5339.88 0.424 5339.93 0.424 5339.98 0.424 5340.02 0.424 5340.07 0.424 5340.12 0.424 5340.16 0.423 5340.21 0.423 5340.26 0.423 5340.31 0.423 5340.35 0.423 5340.40 0.423 5340.45 0.423 5340.49 0.422 5340.54 0.422 5340.59 0.422 5340.63 0.422 5340.68 0.422 5340.73 0.422 5340.77 0.422 5340.82 0.421 5340.87 0.421 5340.91 0.421 5340.96 0.421 5341.01 0.421 5341.05 0.421 5341.10 0.421 5341.15 0.420 5341.19 0.420 5341.24 0.420 5341.29 0.420 5341.33 0.420 5341.38 0.420 5341.43 0.420 5341.47 0.420 5341.52 0.419 5341.57 0.419 5341.61 0.419 5341.66 0.419 5341.71 0.419 5341.76 0.419 5341.80 0.418 5341.85 0.418 5341.90 0.418 5341.94 0.418 5341.99 0.418 5342.04 0.418 5342.08 0.418 5342.13 0.418 5342.18 0.417 5342.22 0.417 5342.27 0.417 5342.32 0.417 5342.36 0.417 5342.41 0.417 5342.46 0.416 5342.50 0.416 5342.55 0.416 5342.60 0.416 5342.64 0.416 5342.69 0.416 5342.74 0.416 5342.78 0.416 5342.83 0.416 5342.88 0.415 5342.92 0.415 5342.97 0.415 5343.02 0.415 5343.07 0.415 5343.11 0.415 5343.16 0.415 5343.21 0.415 5343.25 0.415 5343.30 0.414 5343.35 0.414 5343.39 0.414 5343.44 0.414 5343.49 0.414 5343.53 0.414 5343.58 0.414 5343.63 0.414 5343.67 0.414 5343.72 0.413 5343.77 0.413 5343.81 0.413 5343.86 0.413 5343.91 0.413 5343.95 0.413 5344.00 0.413 5344.05 0.412 5344.10 0.412 5344.14 0.412 5344.19 0.412 5344.24 0.412 5344.28 0.412 5344.33 0.411 5344.38 0.411 5344.42 0.411 5344.47 0.411 5344.52 0.411 5344.56 0.411 5344.61 0.411 5344.66 0.411 5344.70 0.411 5344.75 0.411 5344.80 0.410 5344.84 0.410 5344.89 0.410 5344.94 0.410 5344.99 0.410 5345.03 0.410 5345.08 0.410 5345.13 0.410 5345.17 0.409 5345.22 0.409 5345.27 0.409 5345.31 0.409 5345.36 0.409 5345.41 0.409 5345.45 0.409 5345.50 0.409 5345.55 0.408 5345.59 0.408 5345.64 0.408 5345.69 0.408 5345.73 0.408 5345.78 0.408 5345.83 0.408 5345.88 0.407 5345.92 0.407 5345.97 0.407 5346.02 0.407 5346.06 0.407 5346.11 0.407 5346.16 0.407 5346.20 0.407 5346.25 0.407 5346.30 0.406 5346.34 0.406 5346.39 0.406 5346.44 0.406 5346.48 0.406 5346.53 0.406 5346.58 0.406 5346.63 0.405 5346.67 0.405 5346.72 0.405 5346.77 0.405 5346.81 0.405 5346.86 0.405 5346.91 0.405 5346.95 0.404 5347.00 0.404 5347.05 0.404 5347.09 0.404 5347.14 0.404 5347.19 0.404 5347.23 0.403 5347.28 0.403 5347.33 0.403 5347.38 0.403 5347.42 0.403 5347.47 0.403 5347.52 0.403 5347.56 0.402 5347.61 0.402 5347.66 0.402 5347.70 0.402 5347.75 0.402 5347.80 0.402 5347.84 0.402 5347.89 0.401 5347.94 0.401 5347.99 0.401 5348.03 0.401 5348.08 0.401 5348.13 0.401 5348.17 0.401 5348.22 0.400 5348.27 0.400 5348.31 0.400 5348.36 0.400 5348.41 0.400 5348.45 0.400 5348.50 0.400 5348.55 0.400 5348.59 0.400 5348.64 0.400 5348.69 0.399 5348.74 0.399 5348.78 0.399 5348.83 0.399 5348.88 0.399 5348.92 0.399 5348.97 0.399 5349.02 0.399 5349.06 0.398 5349.11 0.398 5349.16 0.398 5349.20 0.398 5349.25 0.398 5349.30 0.398 5349.35 0.398 5349.39 0.397 5349.44 0.397 5349.49 0.397 5349.53 0.397 5349.58 0.397 5349.63 0.397 5349.67 0.396 5349.72 0.396 5349.77 0.396 5349.81 0.396 5349.86 0.396 5349.91 0.396 5349.96 0.396 5350.00 0.396 5350.05 0.396 5350.10 0.396 5350.14 0.396 5350.19 0.396 5350.24 0.397 5350.28 0.397 5350.33 0.397 5350.38 0.397 5350.43 0.396 5350.47 0.396 5350.52 0.396 5350.57 0.395 5350.61 0.395 5350.66 0.395 5350.71 0.394 5350.75 0.394 5350.80 0.394 5350.85 0.394 5350.89 0.393 5350.94 0.393 5350.99 0.393 5351.04 0.393 5351.08 0.393 5351.13 0.392 5351.18 0.392 5351.22 0.392 5351.27 0.392 5351.32 0.392 5351.36 0.392 5351.41 0.391 5351.46 0.391 5351.51 0.391 5351.55 0.391 5351.60 0.391 5351.65 0.391 5351.69 0.391 5351.74 0.391 5351.79 0.390 5351.83 0.390 5351.88 0.390 5351.93 0.390 5351.97 0.390 5352.02 0.390 5352.07 0.390 5352.12 0.389 5352.16 0.389 5352.21 0.389 5352.26 0.389 5352.30 0.389 5352.35 0.389 5352.40 0.388 5352.44 0.388 5352.49 0.388 5352.54 0.388 5352.59 0.388 5352.63 0.388 5352.68 0.388 5352.73 0.388 5352.77 0.388 5352.82 0.388 5352.87 0.388 5352.91 0.388 5352.96 0.388 5353.01 0.387 5353.06 0.387 5353.10 0.387 5353.15 0.387 5353.20 0.387 5353.24 0.387 5353.29 0.387 5353.34 0.387 5353.38 0.387 5353.43 0.386 5353.48 0.386 5353.53 0.386 5353.57 0.386 5353.62 0.386 5353.67 0.386 5353.71 0.386 5353.76 0.386 5353.81 0.385 5353.85 0.385 5353.90 0.385 5353.95 0.385 5354.00 0.385 5354.04 0.385 5354.09 0.385 5354.14 0.384 5354.18 0.384 5354.23 0.384 5354.28 0.384 5354.32 0.384 5354.37 0.384 5354.42 0.384 5354.47 0.383 5354.51 0.383 5354.56 0.383 5354.61 0.383 5354.65 0.383 5354.70 0.383 5354.75 0.383 5354.80 0.383 5354.84 0.383 5354.89 0.383 5354.94 0.382 5354.98 0.382 5355.03 0.382 5355.08 0.382 5355.12 0.382 5355.17 0.382 5355.22 0.382 5355.27 0.381 5355.31 0.381 5355.36 0.381 5355.41 0.381 5355.45 0.381 5355.50 0.381 5355.55 0.381 5355.59 0.381 5355.64 0.380 5355.69 0.380 5355.74 0.380 5355.78 0.380 5355.83 0.380 5355.88 0.380 5355.92 0.380 5355.97 0.380 5356.02 0.380 5356.07 0.380 5356.11 0.380 5356.16 0.379 5356.21 0.379 5356.25 0.379 5356.30 0.379 5356.35 0.379 5356.39 0.379 5356.44 0.378 5356.49 0.378 5356.54 0.378 5356.58 0.378 5356.63 0.378 5356.68 0.378 5356.72 0.378 5356.77 0.378 5356.82 0.377 5356.87 0.377 5356.91 0.377 5356.96 0.377 5357.01 0.377 5357.05 0.377 5357.10 0.377 5357.15 0.377 5357.19 0.376 5357.24 0.376 5357.29 0.376 5357.34 0.376 5357.38 0.376 5357.43 0.376 5357.48 0.376 5357.52 0.376 5357.57 0.376 5357.62 0.376 5357.67 0.376 5357.71 0.375 5357.76 0.375 5357.81 0.375 5357.85 0.375 5357.90 0.375 5357.95 0.375 5358.00 0.375 5358.04 0.375 5358.09 0.375 5358.14 0.374 5358.18 0.374 5358.23 0.374 5358.28 0.374 5358.32 0.374 5358.37 0.374 5358.42 0.374 5358.47 0.374 5358.51 0.373 5358.56 0.373 5358.61 0.373 5358.65 0.373 5358.70 0.373 5358.75 0.373 5358.80 0.373 5358.84 0.373 5358.89 0.373 5358.94 0.372 5358.98 0.372 5359.03 0.372 5359.08 0.372 5359.13 0.372 5359.17 0.372 5359.22 0.371 5359.27 0.371 5359.31 0.371 5359.36 0.371 5359.41 0.371 5359.46 0.371 5359.50 0.371 5359.55 0.370 5359.60 0.370 5359.64 0.370 5359.69 0.370 5359.74 0.370 5359.79 0.370 5359.83 0.370 5359.88 0.370 5359.93 0.369 5359.97 0.369 5360.02 0.369 5360.07 0.369 5360.12 0.369 5360.16 0.369 5360.21 0.368 5360.26 0.368 5360.30 0.368 5360.35 0.368 5360.40 0.368 5360.45 0.368 5360.49 0.368 5360.54 0.368 5360.59 0.367 5360.63 0.367 5360.68 0.367 5360.73 0.367 5360.78 0.367 5360.82 0.367 5360.87 0.367 5360.92 0.367 5360.96 0.366 5361.01 0.366 5361.06 0.366 5361.11 0.366 5361.15 0.366 5361.20 0.366 5361.25 0.366 5361.29 0.366 5361.34 0.365 5361.39 0.365 5361.44 0.365 5361.48 0.365 5361.53 0.365 5361.58 0.365 5361.62 0.365 5361.67 0.365 5361.72 0.365 5361.77 0.365 5361.81 0.365 5361.86 0.364 5361.91 0.364 5361.95 0.364 5362.00 0.364 5362.05 0.364 5362.10 0.364 5362.14 0.364 5362.19 0.363 5362.24 0.363 5362.28 0.363 5362.33 0.363 5362.38 0.363 5362.43 0.363 5362.47 0.362 5362.52 0.362 5362.57 0.362 5362.61 0.362 5362.66 0.362 5362.71 0.362 5362.76 0.362 5362.80 0.362 5362.85 0.361 5362.90 0.361 5362.94 0.361 5362.99 0.361 5363.04 0.361 5363.09 0.361 5363.13 0.361 5363.18 0.360 5363.23 0.360 5363.27 0.360 5363.32 0.360 5363.37 0.360 5363.42 0.360 5363.46 0.360 5363.51 0.360 5363.56 0.360 5363.61 0.359 5363.65 0.359 5363.70 0.359 5363.75 0.359 5363.79 0.359 5363.84 0.359 5363.89 0.359 5363.94 0.359 5363.98 0.358 5364.03 0.358 5364.08 0.358 5364.12 0.358 5364.17 0.358 5364.22 0.358 5364.27 0.357 5364.31 0.357 5364.36 0.357 5364.41 0.357 5364.45 0.357 5364.50 0.357 5364.55 0.357 5364.60 0.357 5364.64 0.357 5364.69 0.356 5364.74 0.356 5364.79 0.356 5364.83 0.356 5364.88 0.356 5364.93 0.356 5364.97 0.356 5365.02 0.356 5365.07 0.355 5365.12 0.355 5365.16 0.355 5365.21 0.355 5365.26 0.355 5365.30 0.355 5365.35 0.355 5365.40 0.355 5365.45 0.355 5365.49 0.355 5365.54 0.355 5365.59 0.354 5365.64 0.354 5365.68 0.354 5365.73 0.354 5365.78 0.354 5365.82 0.354 5365.87 0.354 5365.92 0.354 5365.97 0.354 5366.01 0.354 5366.06 0.353 5366.11 0.353 5366.16 0.353 5366.20 0.353 5366.25 0.353 5366.30 0.353 5366.34 0.353 5366.39 0.352 5366.44 0.352 5366.49 0.352 5366.53 0.352 5366.58 0.352 5366.63 0.352 5366.67 0.351 5366.72 0.351 5366.77 0.351 5366.82 0.351 5366.86 0.351 5366.91 0.351 5366.96 0.351 5367.01 0.351 5367.05 0.351 5367.10 0.351 5367.15 0.350 5367.19 0.350 5367.24 0.350 5367.29 0.350 5367.34 0.350 5367.38 0.350 5367.43 0.350 5367.48 0.350 5367.53 0.350 5367.57 0.349 5367.62 0.349 5367.67 0.349 5367.71 0.349 5367.76 0.349 5367.81 0.349 5367.86 0.349 5367.90 0.349 5367.95 0.348 5368.00 0.348 5368.05 0.348 5368.09 0.348 5368.14 0.348 5368.19 0.348 5368.23 0.348 5368.28 0.348 5368.33 0.347 5368.38 0.347 5368.42 0.347 5368.47 0.347 5368.52 0.347 5368.57 0.347 5368.61 0.347 5368.66 0.347 5368.71 0.346 5368.75 0.346 5368.80 0.346 5368.85 0.346 5368.90 0.346 5368.94 0.346 5368.99 0.346 5369.04 0.345 5369.09 0.345 5369.13 0.345 5369.18 0.345 5369.23 0.345 5369.28 0.345 5369.32 0.345 5369.37 0.345 5369.42 0.344 5369.46 0.344 5369.51 0.344 5369.56 0.344 5369.61 0.344 5369.65 0.344 5369.70 0.344 5369.75 0.344 5369.80 0.343 5369.84 0.343 5369.89 0.343 5369.94 0.343 5369.98 0.343 5370.03 0.343 5370.08 0.343 5370.13 0.343 5370.17 0.343 5370.22 0.342 5370.27 0.342 5370.32 0.342 5370.36 0.342 5370.41 0.342 5370.46 0.342 5370.51 0.342 5370.55 0.342 5370.60 0.341 5370.65 0.341 5370.69 0.341 5370.74 0.341 5370.79 0.341 5370.84 0.341 5370.88 0.341 5370.93 0.341 5370.98 0.341 5371.03 0.340 5371.07 0.340 5371.12 0.340 5371.17 0.340 5371.22 0.340 5371.26 0.340 5371.31 0.340 5371.36 0.340 5371.40 0.340 5371.45 0.340 5371.50 0.339 5371.55 0.339 5371.59 0.339 5371.64 0.339 5371.69 0.339 5371.74 0.339 5371.78 0.339 5371.83 0.339 5371.88 0.338 5371.93 0.338 5371.97 0.338 5372.02 0.338 5372.07 0.338 5372.12 0.338 5372.16 0.338 5372.21 0.337 5372.26 0.337 5372.30 0.337 5372.35 0.337 5372.40 0.337 5372.45 0.337 5372.49 0.337 5372.54 0.337 5372.59 0.337 5372.64 0.336 5372.68 0.336 5372.73 0.336 5372.78 0.336 5372.83 0.336 5372.87 0.336 5372.92 0.336 5372.97 0.336 5373.02 0.336 5373.06 0.335 5373.11 0.335 5373.16 0.335 5373.20 0.335 5373.25 0.335 5373.30 0.335 5373.35 0.335 5373.39 0.334 5373.44 0.334 5373.49 0.334 5373.54 0.334 5373.58 0.334 5373.63 0.334 5373.68 0.334 5373.73 0.334 5373.77 0.333 5373.82 0.333 5373.87 0.333 5373.92 0.333 5373.96 0.333 5374.01 0.333 5374.06 0.333 5374.11 0.333 5374.15 0.332 5374.20 0.332 5374.25 0.332 5374.29 0.332 5374.34 0.332 5374.39 0.332 5374.44 0.331 5374.48 0.331 5374.53 0.331 5374.58 0.331 5374.63 0.331 5374.67 0.331 5374.72 0.331 5374.77 0.331 5374.82 0.330 5374.86 0.330 5374.91 0.330 5374.96 0.330 5375.01 0.330 5375.05 0.330 5375.10 0.329 5375.15 0.329 5375.20 0.329 5375.24 0.329 5375.29 0.329 5375.34 0.328 5375.39 0.328 5375.43 0.328 5375.48 0.328 5375.53 0.328 5375.57 0.328 5375.62 0.328 5375.67 0.328 5375.72 0.328 5375.76 0.328 5375.81 0.327 5375.86 0.327 5375.91 0.327 5375.95 0.327 5376.00 0.327 5376.05 0.327 5376.10 0.327 5376.14 0.326 5376.19 0.326 5376.24 0.326 5376.29 0.326 5376.33 0.326 5376.38 0.326 5376.43 0.326 5376.48 0.326 5376.52 0.326 5376.57 0.326 5376.62 0.325 5376.67 0.325 5376.71 0.325 5376.76 0.325 5376.81 0.325 5376.86 0.325 5376.90 0.324 5376.95 0.324 5377.00 0.324 5377.05 0.324 5377.09 0.324 5377.14 0.324 5377.19 0.324 5377.24 0.324 5377.28 0.324 5377.33 0.323 5377.38 0.323 5377.43 0.323 5377.47 0.323 5377.52 0.323 5377.57 0.323 5377.61 0.323 5377.66 0.323 5377.71 0.322 5377.76 0.322 5377.80 0.322 5377.85 0.322 5377.90 0.322 5377.95 0.321 5377.99 0.321 5378.04 0.321 5378.09 0.321 5378.14 0.321 5378.18 0.321 5378.23 0.321 5378.28 0.321 5378.33 0.320 5378.37 0.320 5378.42 0.320 5378.47 0.320 5378.52 0.320 5378.56 0.320 5378.61 0.320 5378.66 0.320 5378.71 0.320 5378.75 0.320 5378.80 0.319 5378.85 0.319 5378.90 0.319 5378.94 0.319 5378.99 0.319 5379.04 0.319 5379.09 0.318 5379.13 0.318 5379.18 0.318 5379.23 0.318 5379.28 0.318 5379.32 0.318 5379.37 0.318 5379.42 0.318 5379.47 0.317 5379.51 0.317 5379.56 0.317 5379.61 0.317 5379.66 0.317 5379.70 0.317 5379.75 0.317 5379.80 0.317 5379.85 0.317 5379.89 0.316 5379.94 0.316 5379.99 0.316 5380.04 0.316 5380.08 0.316 5380.13 0.316 5380.18 0.316 5380.23 0.315 5380.27 0.315 5380.32 0.315 5380.37 0.315 5380.42 0.315 5380.46 0.315 5380.51 0.315 5380.56 0.314 5380.61 0.314 5380.65 0.314 5380.70 0.314 5380.75 0.314 5380.80 0.313 5380.84 0.313 5380.89 0.313 5380.94 0.313 5380.99 0.313 5381.03 0.313 5381.08 0.313 5381.13 0.313 5381.18 0.312 5381.22 0.312 5381.27 0.312 5381.32 0.312 5381.37 0.312 5381.41 0.312 5381.46 0.312 5381.51 0.312 5381.56 0.312 5381.60 0.312 5381.65 0.311 5381.70 0.311 5381.75 0.311 5381.80 0.311 5381.84 0.311 5381.89 0.311 5381.94 0.311 5381.99 0.310 5382.03 0.310 5382.08 0.310 5382.13 0.310 5382.18 0.310 5382.22 0.310 5382.27 0.310 5382.32 0.309 5382.37 0.309 5382.41 0.309 5382.46 0.309 5382.51 0.309 5382.56 0.309 5382.60 0.309 5382.65 0.308 5382.70 0.308 5382.75 0.308 5382.79 0.308 5382.84 0.308 5382.89 0.308 5382.94 0.307 5382.98 0.307 5383.03 0.307 5383.08 0.307 5383.13 0.307 5383.17 0.307 5383.22 0.307 5383.27 0.307 5383.32 0.306 5383.36 0.306 5383.41 0.306 5383.46 0.306 5383.51 0.306 5383.55 0.306 5383.60 0.306 5383.65 0.306 5383.70 0.305 5383.75 0.305 5383.79 0.305 5383.84 0.305 5383.89 0.305 5383.94 0.305 5383.98 0.304 5384.03 0.304 5384.08 0.304 5384.13 0.304 5384.17 0.304 5384.22 0.304 5384.27 0.304 5384.32 0.304 5384.36 0.303 5384.41 0.303 5384.46 0.303 5384.51 0.303 5384.55 0.303 5384.60 0.302 5384.65 0.302 5384.70 0.302 5384.74 0.302 5384.79 0.302 5384.84 0.302 5384.89 0.302 5384.93 0.302 5384.98 0.302 5385.03 0.302 5385.08 0.301 5385.13 0.301 5385.17 0.301 5385.22 0.301 5385.27 0.301 5385.32 0.300 5385.36 0.300 5385.41 0.300 5385.46 0.300 5385.51 0.300 5385.55 0.300 5385.60 0.300 5385.65 0.299 5385.70 0.299 5385.74 0.299 5385.79 0.299 5385.84 0.299 5385.89 0.299 5385.93 0.299 5385.98 0.299 5386.03 0.298 5386.08 0.298 5386.13 0.298 5386.17 0.298 5386.22 0.298 5386.27 0.298 5386.32 0.297 5386.36 0.297 5386.41 0.297 5386.46 0.297 5386.51 0.297 5386.55 0.297 5386.60 0.296 5386.65 0.296 5386.70 0.296 5386.74 0.296 5386.79 0.296 5386.84 0.296 5386.89 0.296 5386.94 0.295 5386.98 0.295 5387.03 0.295 5387.08 0.295 5387.13 0.295 5387.17 0.295 5387.22 0.294 5387.27 0.294 5387.32 0.294 5387.36 0.294 5387.41 0.294 5387.46 0.294 5387.51 0.294 5387.55 0.293 5387.60 0.293 5387.65 0.293 5387.70 0.293 5387.75 0.293 5387.79 0.293 5387.84 0.293 5387.89 0.293 5387.94 0.292 5387.98 0.292 5388.03 0.292 5388.08 0.292 5388.13 0.292 5388.17 0.292 5388.22 0.292 5388.27 0.291 5388.32 0.291 5388.36 0.291 5388.41 0.291 5388.46 0.291 5388.51 0.291 5388.56 0.291 5388.60 0.291 5388.65 0.290 5388.70 0.290 5388.75 0.290 5388.79 0.290 5388.84 0.290 5388.89 0.290 5388.94 0.290 5388.98 0.289 5389.03 0.289 5389.08 0.289 5389.13 0.289 5389.18 0.289 5389.22 0.288 5389.27 0.288 5389.32 0.288 5389.37 0.288 5389.41 0.288 5389.46 0.288 5389.51 0.288 5389.56 0.287 5389.60 0.287 5389.65 0.287 5389.70 0.287 5389.75 0.287 5389.80 0.287 5389.84 0.286 5389.89 0.286 5389.94 0.286 5389.99 0.286 5390.03 0.286 5390.08 0.286 5390.13 0.286 5390.18 0.285 5390.22 0.285 5390.27 0.285 5390.32 0.285 5390.37 0.285 5390.42 0.285 5390.46 0.285 5390.51 0.285 5390.56 0.284 5390.61 0.284 5390.65 0.284 5390.70 0.284 5390.75 0.284 5390.80 0.284 5390.84 0.284 5390.89 0.283 5390.94 0.283 5390.99 0.283 5391.04 0.283 5391.08 0.283 5391.13 0.283 5391.18 0.283 5391.23 0.282 5391.27 0.282 5391.32 0.282 5391.37 0.282 5391.42 0.282 5391.46 0.282 5391.51 0.281 5391.56 0.281 5391.61 0.281 5391.66 0.281 5391.70 0.281 5391.75 0.281 5391.80 0.281 5391.85 0.280 5391.89 0.280 5391.94 0.280 5391.99 0.280 5392.04 0.280 5392.09 0.280 5392.13 0.279 5392.18 0.279 5392.23 0.279 5392.28 0.279 5392.32 0.279 5392.37 0.279 5392.42 0.279 5392.47 0.278 5392.52 0.278 5392.56 0.278 5392.61 0.278 5392.66 0.278 5392.71 0.278 5392.75 0.278 5392.80 0.277 5392.85 0.277 5392.90 0.277 5392.94 0.277 5392.99 0.277 5393.04 0.277 5393.09 0.277 5393.14 0.277 5393.18 0.276 5393.23 0.276 5393.28 0.276 5393.33 0.276 5393.37 0.276 5393.42 0.276 5393.47 0.276 5393.52 0.275 5393.57 0.275 5393.61 0.275 5393.66 0.275 5393.71 0.275 5393.76 0.275 5393.80 0.275 5393.85 0.274 5393.90 0.274 5393.95 0.274 5394.00 0.274 5394.04 0.274 5394.09 0.274 5394.14 0.274 5394.19 0.274 5394.23 0.273 5394.28 0.273 5394.33 0.273 5394.38 0.273 5394.43 0.273 5394.47 0.273 5394.52 0.273 5394.57 0.272 5394.62 0.272 5394.66 0.272 5394.71 0.272 5394.76 0.272 5394.81 0.272 5394.86 0.272 5394.90 0.271 5394.95 0.271 5395.00 0.271 5395.05 0.271 5395.09 0.271 5395.14 0.271 5395.19 0.271 5395.24 0.271 5395.29 0.271 5395.33 0.270 5395.38 0.270 5395.43 0.270 5395.48 0.270 5395.53 0.270 5395.57 0.270 5395.62 0.270 5395.67 0.270 5395.72 0.269 5395.76 0.269 5395.81 0.269 5395.86 0.269 5395.91 0.269 5395.96 0.268 5396.00 0.268 5396.05 0.268 5396.10 0.268 5396.15 0.268 5396.19 0.268 5396.24 0.268 5396.29 0.268 5396.34 0.268 5396.39 0.267 5396.43 0.267 5396.48 0.267 5396.53 0.267 5396.58 0.267 5396.62 0.267 5396.67 0.267 5396.72 0.267 5396.77 0.266 5396.82 0.266 5396.86 0.266 5396.91 0.266 5396.96 0.266 5397.01 0.266 5397.06 0.265 5397.10 0.265 5397.15 0.265 5397.20 0.265 5397.25 0.265 5397.29 0.265 5397.34 0.265 5397.39 0.264 5397.44 0.264 5397.49 0.264 5397.53 0.264 5397.58 0.264 5397.63 0.264 5397.68 0.264 5397.73 0.263 5397.77 0.263 5397.82 0.263 5397.87 0.263 5397.92 0.263 5397.96 0.263 5398.01 0.263 5398.06 0.263 5398.11 0.262 5398.16 0.262 5398.20 0.262 5398.25 0.262 5398.30 0.262 5398.35 0.262 5398.40 0.261 5398.44 0.261 5398.49 0.261 5398.54 0.261 5398.59 0.261 5398.63 0.261 5398.68 0.260 5398.73 0.260 5398.78 0.260 5398.83 0.260 5398.87 0.260 5398.92 0.260 5398.97 0.260 5399.02 0.260 5399.07 0.260 5399.11 0.259 5399.16 0.259 5399.21 0.259 5399.26 0.259 5399.30 0.259 5399.35 0.259 5399.40 0.258 5399.45 0.258 5399.50 0.258 5399.54 0.258 5399.59 0.257 5399.64 0.257 5399.69 0.257 5399.74 0.257 5399.78 0.257 5399.83 0.257 5399.88 0.257 5399.93 0.257 5399.97 0.257 5400.02 0.257 5400.07 0.257 5400.12 0.256 5400.17 0.256 5400.21 0.256 5400.26 0.256 5400.31 0.256 5400.36 0.256 5400.41 0.256 5400.45 0.256 5400.50 0.255 5400.55 0.255 5400.60 0.255 5400.65 0.255 5400.69 0.255 5400.74 0.254 5400.79 0.254 5400.84 0.254 5400.88 0.254 5400.93 0.254 5400.98 0.254 5401.03 0.254 5401.08 0.254 5401.12 0.254 5401.17 0.253 5401.22 0.253 5401.27 0.253 5401.32 0.253 5401.36 0.253 5401.41 0.253 5401.46 0.252 5401.51 0.252 5401.56 0.252 5401.60 0.252 5401.65 0.252 5401.70 0.252 5401.75 0.252 5401.80 0.252 5401.84 0.252 5401.89 0.252 5401.94 0.251 5401.99 0.251 5402.03 0.251 5402.08 0.251 5402.13 0.251 5402.18 0.250 5402.23 0.250 5402.27 0.250 5402.32 0.250 5402.37 0.250 5402.42 0.250 5402.47 0.250 5402.51 0.249 5402.56 0.249 5402.61 0.249 5402.66 0.249 5402.71 0.249 5402.75 0.248 5402.80 0.248 5402.85 0.248 5402.90 0.248 5402.95 0.248 5402.99 0.248 5403.04 0.248 5403.09 0.248 5403.14 0.248 5403.19 0.247 5403.23 0.247 5403.28 0.247 5403.33 0.247 5403.38 0.247 5403.43 0.247 5403.47 0.247 5403.52 0.247 5403.57 0.246 5403.62 0.246 5403.67 0.246 5403.71 0.246 5403.76 0.246 5403.81 0.246 5403.86 0.246 5403.90 0.246 5403.95 0.245 5404.00 0.245 5404.05 0.245 5404.10 0.245 5404.14 0.245 5404.19 0.245 5404.24 0.244 5404.29 0.244 5404.34 0.244 5404.38 0.244 5404.43 0.244 5404.48 0.244 5404.53 0.244 5404.58 0.243 5404.62 0.243 5404.67 0.243 5404.72 0.243 5404.77 0.243 5404.82 0.243 5404.86 0.243 5404.91 0.243 5404.96 0.242 5405.01 0.242 5405.06 0.242 5405.10 0.242 5405.15 0.242 5405.20 0.242 5405.25 0.242 5405.30 0.242 5405.34 0.242 5405.39 0.241 5405.44 0.241 5405.49 0.241 5405.54 0.241 5405.58 0.241 5405.63 0.241 5405.68 0.241 5405.73 0.240 5405.78 0.240 5405.82 0.240 5405.87 0.240 5405.92 0.240 5405.97 0.240 5406.02 0.240 5406.06 0.239 5406.11 0.239 5406.16 0.239 5406.21 0.239 5406.26 0.239 5406.30 0.239 5406.35 0.239 5406.40 0.239 5406.45 0.238 5406.50 0.238 5406.54 0.238 5406.59 0.238 5406.64 0.238 5406.69 0.238 5406.74 0.237 5406.78 0.237 5406.83 0.237 5406.88 0.237 5406.93 0.237 5406.98 0.237 5407.02 0.237 5407.07 0.237 5407.12 0.236 5407.17 0.236 5407.22 0.236 5407.26 0.236 5407.31 0.236 5407.36 0.236 5407.41 0.236 5407.46 0.235 5407.50 0.235 5407.55 0.235 5407.60 0.235 5407.65 0.235 5407.70 0.235 5407.75 0.235 5407.79 0.235 5407.84 0.234 5407.89 0.234 5407.94 0.234 5407.99 0.234 5408.03 0.234 5408.08 0.234 5408.13 0.234 5408.18 0.234 5408.23 0.233 5408.27 0.233 5408.32 0.233 5408.37 0.233 5408.42 0.233 5408.47 0.233 5408.51 0.233 5408.56 0.233 5408.61 0.232 5408.66 0.232 5408.71 0.232 5408.75 0.232 5408.80 0.232 5408.85 0.232 5408.90 0.232 5408.95 0.232 5408.99 0.231 5409.04 0.231 5409.09 0.231 5409.14 0.231 5409.19 0.231 5409.23 0.231 5409.28 0.231 5409.33 0.230 5409.38 0.230 5409.43 0.230 5409.47 0.230 5409.52 0.230 5409.57 0.230 5409.62 0.230 5409.67 0.229 5409.72 0.229 5409.76 0.229 5409.81 0.229 5409.86 0.229 5409.91 0.229 5409.96 0.229 5410.00 0.228 5410.05 0.228 5410.10 0.228 5410.15 0.228 5410.20 0.228 5410.24 0.228 5410.29 0.227 5410.34 0.227 5410.39 0.227 5410.44 0.227 5410.48 0.227 5410.53 0.227 5410.58 0.227 5410.63 0.227 5410.68 0.227 5410.73 0.227 5410.77 0.226 5410.82 0.226 5410.87 0.226 5410.92 0.226 5410.97 0.226 5411.01 0.226 5411.06 0.226 5411.11 0.225 5411.16 0.225 5411.21 0.225 5411.25 0.225 5411.30 0.225 5411.35 0.225 5411.40 0.225 5411.45 0.224 5411.49 0.224 5411.54 0.224 5411.59 0.224 5411.64 0.224 5411.69 0.224 5411.74 0.223 5411.78 0.223 5411.83 0.223 5411.88 0.223 5411.93 0.223 5411.98 0.223 5412.02 0.223 5412.07 0.223 5412.12 0.222 5412.17 0.222 5412.22 0.222 5412.26 0.222 5412.31 0.222 5412.36 0.222 5412.41 0.222 5412.46 0.222 5412.51 0.222 5412.55 0.221 5412.60 0.221 5412.65 0.221 5412.70 0.221 5412.75 0.221 5412.79 0.221 5412.84 0.221 5412.89 0.221 5412.94 0.220 5412.99 0.220 5413.03 0.220 5413.08 0.220 5413.13 0.220 5413.18 0.220 5413.23 0.219 5413.28 0.219 5413.32 0.219 5413.37 0.219 5413.42 0.219 5413.47 0.219 5413.52 0.219 5413.56 0.219 5413.61 0.218 5413.66 0.218 5413.71 0.218 5413.76 0.218 5413.81 0.218 5413.85 0.218 5413.90 0.218 5413.95 0.217 5414.00 0.217 5414.05 0.217 5414.09 0.217 5414.14 0.217 5414.19 0.217 5414.24 0.217 5414.29 0.217 5414.33 0.217 5414.38 0.216 5414.43 0.216 5414.48 0.216 5414.53 0.216 5414.58 0.216 5414.62 0.216 5414.67 0.216 5414.72 0.216 5414.77 0.216 5414.82 0.216 5414.86 0.215 5414.91 0.215 5414.96 0.215 5415.01 0.215 5415.06 0.214 5415.11 0.214 5415.15 0.214 5415.20 0.214 5415.25 0.214 5415.30 0.214 5415.35 0.214 5415.39 0.213 5415.44 0.213 5415.49 0.213 5415.54 0.213 5415.59 0.213 5415.64 0.213 5415.68 0.213 5415.73 0.213 5415.78 0.213 5415.83 0.212 5415.88 0.212 5415.92 0.212 5415.97 0.212 5416.02 0.212 5416.07 0.212 5416.12 0.212 5416.17 0.212 5416.21 0.212 5416.26 0.211 5416.31 0.211 5416.36 0.211 5416.41 0.211 5416.45 0.211 5416.50 0.211 5416.55 0.211 5416.60 0.210 5416.65 0.210 5416.70 0.210 5416.74 0.210 5416.79 0.210 5416.84 0.209 5416.89 0.209 5416.94 0.209 5416.99 0.209 5417.03 0.209 5417.08 0.209 5417.13 0.209 5417.18 0.209 5417.23 0.209 5417.27 0.208 5417.32 0.208 5417.37 0.208 5417.42 0.208 5417.47 0.208 5417.52 0.208 5417.56 0.208 5417.61 0.208 5417.66 0.207 5417.71 0.207 5417.76 0.207 5417.81 0.207 5417.85 0.207 5417.90 0.207 5417.95 0.207 5418.00 0.206 5418.05 0.206 5418.09 0.206 5418.14 0.206 5418.19 0.206 5418.24 0.206 5418.29 0.205 5418.34 0.205 5418.38 0.205 5418.43 0.205 5418.48 0.205 5418.53 0.205 5418.58 0.205 5418.63 0.205 5418.67 0.205 5418.72 0.205 5418.77 0.204 5418.82 0.204 5418.87 0.204 5418.91 0.204 5418.96 0.204 5419.01 0.204 5419.06 0.204 5419.11 0.204 5419.16 0.203 5419.20 0.203 5419.25 0.203 5419.30 0.203 5419.35 0.203 5419.40 0.202 5419.45 0.202 5419.49 0.202 5419.54 0.202 5419.59 0.202 5419.64 0.202 5419.69 0.202 5419.74 0.202 5419.78 0.202 5419.83 0.201 5419.88 0.201 5419.93 0.201 5419.98 0.201 5420.02 0.201 5420.07 0.201 5420.12 0.201 5420.17 0.200 5420.22 0.200 5420.27 0.200 5420.31 0.200 5420.36 0.200 5420.41 0.200 5420.46 0.199 5420.51 0.199 5420.56 0.199 5420.60 0.199 5420.65 0.199 5420.70 0.199 5420.75 0.199 5420.80 0.198 5420.85 0.198 5420.89 0.198 5420.94 0.197 5420.99 0.197 5421.04 0.197 5421.09 0.197 5421.14 0.197 5421.18 0.196 5421.23 0.196 5421.28 0.196 5421.33 0.196 5421.38 0.195 5421.43 0.195 5421.47 0.195 5421.52 0.194 5421.57 0.194 5421.62 0.194 5421.67 0.194 5421.71 0.193 5421.76 0.193 5421.81 0.193 5421.86 0.192 5421.91 0.192 5421.96 0.192 5422.00 0.191 5422.05 0.191 5422.10 0.191 5422.15 0.190 5422.20 0.190 5422.25 0.190 5422.29 0.189 5422.34 0.189 5422.39 0.189 5422.44 0.189 5422.49 0.188 5422.54 0.188 5422.58 0.188 5422.63 0.187 5422.68 0.187 5422.73 0.187 5422.78 0.187 5422.83 0.187 5422.87 0.187 5422.92 0.187 5422.97 0.187 5423.02 0.187 5423.07 0.187 5423.12 0.187 5423.16 0.187 5423.21 0.188 5423.26 0.188 5423.31 0.188 5423.36 0.188 5423.41 0.188 5423.45 0.188 5423.50 0.188 5423.55 0.188 5423.60 0.189 5423.65 0.189 5423.70 0.189 5423.74 0.189 5423.79 0.189 5423.84 0.189 5423.89 0.189 5423.94 0.189 5423.99 0.189 5424.03 0.189 5424.08 0.189 5424.13 0.189 5424.18 0.189 5424.23 0.189 5424.28 0.189 5424.32 0.189 5424.37 0.189 5424.42 0.189 5424.47 0.189 5424.52 0.188 5424.57 0.188 5424.61 0.188 5424.66 0.188 5424.71 0.188 5424.76 0.188 5424.81 0.188 5424.86 0.188 5424.91 0.188 5424.95 0.188 5425.00 0.188 5425.05 0.188 5425.10 0.188 5425.15 0.188 5425.20 0.187 5425.24 0.187 5425.29 0.187 5425.34 0.187 5425.39 0.187 5425.44 0.187 5425.49 0.187 5425.53 0.186 5425.58 0.186 5425.63 0.186 5425.68 0.186 5425.73 0.186 5425.78 0.186 5425.82 0.186 5425.87 0.186 5425.92 0.186 5425.97 0.186 5426.02 0.186 5426.07 0.185 5426.11 0.185 5426.16 0.185 5426.21 0.185 5426.26 0.185 5426.31 0.185 5426.36 0.185 5426.40 0.184 5426.45 0.184 5426.50 0.184 5426.55 0.184 5426.60 0.184 5426.65 0.184 5426.70 0.184 5426.74 0.184 5426.79 0.184 5426.84 0.184 5426.89 0.183 5426.94 0.183 5426.99 0.183 5427.03 0.183 5427.08 0.183 5427.13 0.183 5427.18 0.183 5427.23 0.182 5427.28 0.182 5427.32 0.182 5427.37 0.182 5427.42 0.182 5427.47 0.181 5427.52 0.180 5427.57 0.180 5427.62 0.179 5427.66 0.178 5427.71 0.177 5427.76 0.177 5427.81 0.176 5427.86 0.176 5427.91 0.176 5427.95 0.175 5428.00 0.175 5428.05 0.175 5428.10 0.175 5428.15 0.174 5428.20 0.174 5428.24 0.175 5428.29 0.175 5428.34 0.176 5428.39 0.176 5428.44 0.177 5428.49 0.177 5428.54 0.177 5428.58 0.178 5428.63 0.178 5428.68 0.177 5428.73 0.178 5428.78 0.178 5428.83 0.177 5428.87 0.177 5428.92 0.177 5428.97 0.177 5429.02 0.177 5429.07 0.177 5429.12 0.177 5429.16 0.177 5429.21 0.177 5429.26 0.177 5429.31 0.177 5429.36 0.176 5429.41 0.176 5429.46 0.176 5429.50 0.176 5429.55 0.176 5429.60 0.176 5429.65 0.175 5429.70 0.175 5429.75 0.175 5429.79 0.175 5429.84 0.175 5429.89 0.175 5429.94 0.175 5429.99 0.175 5430.04 0.175 5430.09 0.175 5430.13 0.174 5430.18 0.174 5430.23 0.174 5430.28 0.174 5430.33 0.174 5430.38 0.174 5430.42 0.174 5430.47 0.174 5430.52 0.173 5430.57 0.173 5430.62 0.173 5430.67 0.173 5430.72 0.173 5430.76 0.173 5430.81 0.173 5430.86 0.172 5430.91 0.172 5430.96 0.172 5431.01 0.172 5431.06 0.172 5431.10 0.172 5431.15 0.172 5431.20 0.172 5431.25 0.172 5431.30 0.172 5431.35 0.171 5431.39 0.171 5431.44 0.171 5431.49 0.171 5431.54 0.171 5431.59 0.171 5431.64 0.171 5431.69 0.170 5431.73 0.170 5431.78 0.170 5431.83 0.170 5431.88 0.170 5431.93 0.170 5431.98 0.170 5432.03 0.169 5432.07 0.169 5432.12 0.169 5432.17 0.169 5432.22 0.169 5432.27 0.169 5432.32 0.169 5432.36 0.169 5432.41 0.169 5432.46 0.169 5432.51 0.169 5432.56 0.168 5432.61 0.168 5432.66 0.168 5432.70 0.168 5432.75 0.168 5432.80 0.167 5432.85 0.167 5432.90 0.167 5432.95 0.167 5433.00 0.167 5433.04 0.167 5433.09 0.167 5433.14 0.167 5433.19 0.167 5433.24 0.166 5433.29 0.166 5433.34 0.166 5433.38 0.166 5433.43 0.166 5433.48 0.166 5433.53 0.166 5433.58 0.165 5433.63 0.165 5433.67 0.165 5433.72 0.165 5433.77 0.165 5433.82 0.165 5433.87 0.165 5433.92 0.165 5433.97 0.165 5434.01 0.165 5434.06 0.164 5434.11 0.164 5434.16 0.164 5434.21 0.164 5434.26 0.164 5434.31 0.164 5434.35 0.163 5434.40 0.163 5434.45 0.163 5434.50 0.163 5434.55 0.163 5434.60 0.163 5434.65 0.163 5434.69 0.163 5434.74 0.162 5434.79 0.162 5434.84 0.162 5434.89 0.162 5434.94 0.162 5434.99 0.162 5435.03 0.162 5435.08 0.162 5435.13 0.161 5435.18 0.161 5435.23 0.161 5435.28 0.161 5435.33 0.161 5435.37 0.161 5435.42 0.161 5435.47 0.161 5435.52 0.160 5435.57 0.160 5435.62 0.160 5435.67 0.160 5435.71 0.160 5435.76 0.160 5435.81 0.160 5435.86 0.160 5435.91 0.159 5435.96 0.159 5436.01 0.159 5436.05 0.159 5436.10 0.159 5436.15 0.159 5436.20 0.159 5436.25 0.158 5436.30 0.158 5436.35 0.158 5436.39 0.158 5436.44 0.158 5436.49 0.158 5436.54 0.158 5436.59 0.158 5436.64 0.157 5436.69 0.157 5436.73 0.157 5436.78 0.157 5436.83 0.156 5436.88 0.156