MRCAT_XAFS V0.3 Datafile "fefoil.004" created at APS 10ID on Sun Mar 28 16:40:40 2010 Ring energy= 7.00 GeV E0= 25514.00 NUM_REGIONS= 1 SRB= 6900 SRSS= 0.5 SPP= 0.05 Settling time= 0 Offsets= 12587.00 11343.00 10668.00 13225.00 0.00 0.00 0.00 0.00 0.00 0.00 0.00 0.00 0.00 0.00 0.00 0.00 Gains= 8.00 6.00 6.00 7.00 1.00 1.00 1.00 1.00 1.00 1.00 1.00 1.00 1.00 1.00 1.00 1.00 und 7.8 2 beam 100x1000 ------------------------------------------------------------------------------------------------ energy mcs3 mcs4 mcs5 mcs6 6899.8267 74900 70340 53020 8780 6899.8267 74900 70320 53020 8800 6899.8267 74840 70240 52960 8780 6899.8267 74860 70280 53000 8780 6899.8267 74880 70300 53000 8780 6899.8267 74760 70160 52940 8800 6899.8267 74720 70140 52880 8780 6899.8267 74840 70240 52980 8760 6899.8267 74840 70260 52960 8740 6899.8267 74720 70120 52900 8760 6899.8267 74680 70100 52860 8780 6899.8267 74660 70060 52820 8760 6899.8267 74700 70100 52880 8760 6899.8267 74780 70180 52920 8760 6899.8267 74660 70060 52840 8780 6899.8267 74700 70100 52880 8780 6899.8267 74980 70360 53060 8820 6899.8267 74880 70280 53020 8800 6899.8267 74780 70200 52920 8760 6899.8267 75000 70380 53100 8820 6899.8267 75140 70520 53180 8800 6899.9474 75020 70400 53100 8800 6900.3802 74660 70060 52840 8800 6900.9036 74500 69920 52760 8760 6901.3264 74880 70340 53060 8780 6901.7593 75180 70620 53320 8840 6902.2124 75200 70660 53340 8860 6902.6354 75260 70760 53440 8860 6903.0383 75260 70760 53460 8840 6903.4613 75340 70880 53560 8880 6903.8744 75560 71120 53760 8880 6904.2875 75760 71300 53920 8880 6904.7107 75780 71360 53960 8900 6905.134 75760 71380 54000 8920 6905.5473 75800 71400 54040 8940 6905.9606 75860 71520 54140 8920 6906.3739 75880 71540 54160 8940 6906.7974 75880 71560 54200 8940 6907.221 76000 71700 54320 8960 6907.6345 76120 71840 54420 8980 6908.0582 76160 71880 54500 8980 6908.4819 76260 72020 54600 8980 6908.8956 76360 72100 54680 8980 6909.3093 76300 72100 54680 9020 6909.7332 76320 72120 54720 9040 6910.147 76360 72180 54800 9040 6910.5609 76400 72260 54840 9020 6910.9849 76460 72320 54920 9020 6911.409 76580 72480 55060 9020 6911.8332 76640 72540 55100 9020 6912.2473 76640 72560 55160 9020 6912.6614 76640 72580 55180 9040 6913.0857 76580 72560 55160 9020 6913.5101 76620 72600 55220 9040 6913.9345 76700 72700 55320 9020 6914.3489 76620 72660 55280 9040 6914.7633 76660 72700 55340 9040 6915.1879 76420 72500 55200 9000 6915.6024 76040 72160 54960 9000 6916.017 76240 72380 55140 9000 6916.4417 76680 72820 55500 9080 6916.8665 76800 72960 55600 9100 6917.2913 76960 73120 55740 9080 6917.7061 77100 73280 55880 9120 6918.1209 77120 73340 55940 9120 6918.5459 77200 73420 56020 9140 6918.9609 77240 73480 56100 9140 6919.3759 77240 73520 56100 9140 6919.801 77340 73620 56220 9160 6920.2263 77520 73820 56400 9180 6920.6515 77680 74000 56540 9180 6921.0769 77700 74020 56580 9180 6921.4921 77760 74120 56640 9220 6921.9074 77840 74220 56760 9240 6922.3228 77900 74300 56800 9240 6922.7483 77840 74260 56820 9180 6923.1739 77840 74260 56820 9180 6923.5895 77940 74400 56940 9200 6924.0152 77980 74460 57000 9220 6924.4308 77900 74400 56980 9220 6924.8566 77940 74460 57060 9200 6925.2825 77920 74480 57060 9200 6925.6881 77840 74380 57040 9220 6926.104 78000 74600 57180 9240 6926.53 78180 74800 57360 9300 6926.9561 78300 74920 57480 9300 6927.3822 78300 74940 57520 9320 6927.8084 78340 75000 57580 9340 6928.2245 78480 75160 57700 9340 6928.6407 78640 75340 57860 9360 6929.067 78640 75360 57900 9320 6929.4934 78720 75480 58000 9320 6929.9098 78760 75500 58040 9340 6930.3261 78680 75460 58020 9360 6930.7527 78680 75500 58060 9320 6931.1793 78720 75560 58100 9320 6931.5958 78760 75620 58200 9300 6932.0124 78900 75760 58320 9340 6932.4392 78960 75860 58420 9380 6932.8661 79040 75980 58520 9380 6933.2828 79200 76140 58640 9440 6933.6996 79380 76340 58840 9480 6934.1266 79500 76480 58960 9480 6934.5435 79580 76580 59040 9460 6934.9706 79680 76700 59160 9440 6935.3978 79700 76780 59200 9440 6935.8148 79740 76820 59280 9480 6936.2421 79780 76880 59360 9480 6936.6694 79740 76880 59340 9480 6937.0968 79720 76880 59380 9480 6937.5141 79780 76960 59440 9460 6937.9314 79800 76980 59480 9460 6938.3488 79700 76920 59440 9440 6938.7662 79840 77060 59560 9500 6939.1939 80020 77280 59760 9500 6939.6114 80200 77460 59920 9520 6940.0392 80040 77340 59840 9500 6940.467 80060 77380 59880 9480 6940.8847 80260 77620 60060 9540 6941.3126 80220 77580 60080 9560 6941.7304 80260 77660 60140 9560 6942.1483 80440 77840 60300 9560 6942.5764 80320 77760 60260 9560 6943.0045 80380 77840 60320 9580 6943.4327 80560 78040 60500 9600 6943.861 80560 78040 60540 9640 6944.2791 80580 78100 60580 9620 6944.6973 80720 78260 60720 9620 6945.1257 80780 78320 60800 9640 6945.544 80860 78460 60900 9640 6945.9623 80940 78540 61000 9620 6946.3909 81020 78620 61080 9640 6946.8093 81000 78640 61120 9680 6947.2278 81080 78760 61220 9680 6947.6565 81200 78880 61340 9700 6948.0853 81360 79080 61500 9720 6948.5142 81460 79180 61600 9720 6948.9431 81400 79160 61580 9700 6949.3619 81400 79180 61620 9700 6949.7807 81500 79300 61760 9720 6950.2098 81640 79460 61880 9720 6950.6287 81720 79560 61960 9760 6951.0477 81740 79600 62020 9740 6951.4769 81620 79500 61960 9720 6951.9062 81700 79600 62060 9720 6952.3355 81780 79720 62160 9720 6952.7547 81820 79800 62220 9760 6953.174 81940 79900 62360 9780 6953.6035 82120 80140 62540 9820 6954.0331 82260 80260 62660 9820 6954.4524 82340 80400 62800 9840 6954.8719 82400 80460 62840 9840 6955.3016 82380 80500 62880 9820 6955.7314 82480 80580 62980 9820 6956.151 82540 80700 63080 9880 6956.5707 82500 80680 63080 9880 6957.0007 82400 80600 63060 9840 6957.4307 82480 80700 63140 9840 6957.8607 82460 80700 63160 9820 6958.2806 82400 80680 63160 9840 6958.7005 82560 80840 63300 9900 6959.1205 82620 80940 63400 9940 6959.5508 82540 80900 63380 9880 6959.9811 82660 81020 63480 9920 6960.4013 82780 81180 63620 9940 6960.8317 82880 81280 63740 9920 6961.2622 82900 81320 63780 9920 6961.6928 82800 81280 63740 9920 6962.1132 82900 81380 63860 9940 6962.5336 83080 81580 64040 9960 6962.9643 83020 81560 64040 9940 6963.3848 83140 81680 64160 9940 6963.8054 83280 81880 64300 10000 6964.2363 83300 81880 64360 9980 6964.657 83160 81800 64280 9980 6965.0777 83260 81920 64400 9980 6965.5088 83280 81940 64440 10000 6965.9399 83340 82060 64540 9980 6966.371 83440 82160 64640 10000 6966.8023 83440 82180 64680 9980 6967.2233 83600 82380 64840 10020 6967.6443 83620 82420 64900 9980 6968.0757 83600 82440 64920 10000 6968.4969 83720 82580 65040 10040 6968.9181 83800 82680 65140 10060 6969.3496 83820 82720 65200 10080 6969.7813 83900 82800 65280 10080 6970.2129 83920 82860 65360 10080 6970.6446 83900 82860 65360 10100 6971.0661 83860 82840 65360 10080 6971.4877 83920 82920 65460 10080 6971.9093 84080 83120 65620 10120 6972.3309 84140 83200 65700 10100 6972.7629 84100 83200 65700 10140 6973.195 84120 83220 65760 10140 6973.6271 84140 83280 65820 10120 6974.0489 84180 83320 65880 10140 6974.4708 84200 83380 65940 10140 6974.9031 84280 83480 66020 10140 6975.3251 84340 83580 66120 10140 6975.7472 84340 83580 66140 10160 6976.1797 84320 83580 66160 10140 6976.6121 84300 83580 66180 10100 6977.0344 84220 83540 66160 10100 6977.4567 84340 83660 66280 10120 6977.8893 84440 83800 66420 10120 6978.3221 84580 83940 66540 10160 6978.7548 84620 84040 66620 10200 6979.1773 84660 84080 66680 10240 6979.5999 84620 84100 66700 10220 6980.0328 84680 84160 66800 10180 6980.4555 84720 84260 66860 10220 6980.8782 84740 84280 66920 10200 6981.3113 84700 84260 66920 10200 6981.7445 84660 84260 66920 10200 6982.1777 84660 84300 66980 10200 6982.611 84620 84260 66960 10200 6983.034 84600 84280 67000 10220 6983.457 84580 84260 66980 10180 6983.8801 84480 84220 66980 10200 6984.3136 84660 84380 67140 10200 6984.7472 84800 84580 67300 10200 6985.1704 84920 84720 67420 10220 6985.6041 85060 84880 67580 10240 6986.0378 85060 84900 67620 10240 6986.4716 85060 84940 67660 10240 6986.8951 85140 85020 67760 10300 6987.3186 85200 85100 67820 10340 6987.7525 85180 85140 67880 10340 6988.1762 85100 85060 67840 10320 6988.5999 85060 85040 67820 10280 6989.034 85120 85120 67920 10280 6989.4578 85140 85160 67960 10300 6989.8817 85080 85140 67960 10280 6990.3159 85140 85220 68040 10280 6990.7503 85180 85300 68140 10280 6991.1743 85260 85380 68220 10280 6991.5984 85260 85420 68240 10260 6992.0329 85260 85440 68300 10300 6992.4674 85260 85440 68320 10300 6992.8917 85140 85380 68280 10260 6993.3263 84980 85220 68160 10260 6993.761 84980 85260 68220 10300 6994.1854 85200 85500 68420 10320 6994.6203 85180 85520 68440 10340 6995.0448 85060 85420 68400 10320 6995.4694 85280 85660 68620 10340 6995.9043 85280 85700 68660 10340 6996.3394 85180 85620 68620 10340 6996.7745 85200 85640 68660 10320 6997.1993 85160 85640 68660 10320 6997.6241 85180 85700 68720 10340 6998.049 85220 85780 68820 10340 6998.4844 85260 85820 68880 10360 6998.9197 85420 86020 69040 10340 6999.3448 85580 86220 69240 10360 6999.7803 85540 86220 69220 10380 7000.2158 85540 86220 69260 10340 7000.6411 85660 86380 69420 10380 7001.0664 85520 86260 69340 10360 7001.5021 85420 86200 69280 10360 7001.9379 85440 86240 69360 10360 7002.3737 85420 86240 69340 10320 7002.7992 85420 86260 69400 10340 7003.2247 85520 86400 69540 10400 7003.6607 85640 86500 69640 10420 7004.0864 85660 86580 69700 10400 7004.5121 85680 86620 69780 10420 7004.9483 85480 86440 69620 10400 7005.3845 85240 86240 69500 10360 7005.8104 85300 86320 69560 10340 7006.2363 85160 86200 69480 10320 7006.6727 84940 86000 69340 10300 7007.1092 85000 86060 69420 10300 7007.5457 85220 86340 69660 10340 7007.9718 85500 86640 69940 10400 7008.3981 85800 86980 70220 10480 7008.8347 85980 87160 70380 10440 7009.2714 85900 87120 70360 10440 7009.6978 85940 87160 70440 10440 7010.1243 85980 87240 70500 10440 7010.5612 85980 87260 70540 10420 7010.9981 85820 87140 70440 10380 7011.4247 85860 87200 70540 10420 7011.8514 85880 87260 70600 10440 7012.2885 85880 87280 70620 10460 7012.7152 85920 87340 70680 10480 7013.1421 85960 87420 70780 10480 7013.5793 85920 87400 70780 10480 7014.0167 85800 87300 70720 10440 7014.4541 85900 87440 70840 10460 7014.8811 86060 87620 71000 10480 7015.3186 86060 87660 71060 10480 7015.7562 86060 87640 71080 10460 7016.1834 86000 87640 71060 10460 7016.6107 85980 87640 71100 10440 7017.038 85840 87520 71020 10440 7017.4758 85800 87480 71000 10480 7017.9032 85700 87420 70980 10460 7018.3411 85540 87260 70860 10460 7018.7791 85540 87300 70920 10460 7019.2066 85560 87340 70940 10460 7019.6447 85660 87440 71080 10480 7020.0828 85560 87380 71040 10440 7020.521 85500 87360 71000 10460 7020.9488 85660 87520 71180 10440 7021.3767 85720 87640 71300 10440 7021.8046 85800 87700 71360 10440 7022.2326 85840 87800 71460 10460 7022.6711 85900 87900 71560 10480 7023.1096 86020 88040 71680 10480 7023.5482 86060 88080 71740 10480 7023.9764 85780 87840 71580 10460 7024.4046 85620 87700 71460 10460 7024.8434 85860 87980 71720 10520 7025.2717 86000 88160 71860 10500 7025.7001 86060 88240 71960 10500 7026.1391 86040 88260 71980 10500 7026.578 85980 88200 71980 10520 7027.0066 85980 88260 72020 10520 7027.4353 86040 88320 72100 10540 7027.8744 86000 88320 72100 10520 7028.3136 85920 88280 72100 10520 7028.7529 85880 88240 72080 10500 7029.1817 85820 88180 72060 10500 7029.6106 85740 88160 72040 10480 7030.0501 85720 88140 72080 10480 7030.4791 85760 88240 72140 10480 7030.9082 85840 88340 72260 10500 7031.3478 85780 88280 72220 10480 7031.7874 85680 88240 72200 10500 7032.2271 85620 88180 72180 10480 7032.6564 85440 88020 72060 10460 7033.0858 85380 88000 72060 10440 7033.5257 85500 88120 72180 10440 7033.9656 85560 88240 72280 10460 7034.3951 85640 88340 72400 10500 7034.8247 85720 88460 72500 10500 7035.2648 85600 88360 72440 10480 7035.705 85360 88120 72280 10480 7036.1452 85380 88180 72320 10480 7036.575 85340 88180 72360 10480 7037.0049 85260 88100 72300 10440 7037.4452 85240 88100 72320 10440 7037.8752 85300 88180 72400 10460 7038.3052 85340 88280 72500 10460 7038.7458 85340 88300 72540 10440 7039.1864 85340 88320 72560 10440 7039.6271 85340 88340 72620 10460 7040.0573 85380 88440 72700 10480 7040.4876 85460 88520 72800 10460 7040.9285 85400 88480 72760 10480 7041.3694 85160 88260 72620 10480 7041.7999 85300 88460 72760 10500 7042.2304 85500 88660 72960 10500 7042.6714 85440 88640 72980 10480 7043.1021 85380 88620 72960 10460 7043.5433 85400 88640 73020 10480 7043.9845 85360 88640 73020 10500 7044.4153 85340 88660 73040 10480 7044.8567 85360 88720 73120 10520 7045.2981 85440 88820 73220 10500 7045.7291 85480 88880 73300 10480 7046.1601 85500 88920 73340 10500 7046.6017 85480 88960 73380 10520 7047.0328 85440 88920 73380 10500 7047.464 85440 88960 73440 10540 7047.9058 85440 89000 73460 10520 7048.3476 85340 88900 73420 10520 7048.7894 85140 88720 73280 10500 7049.2209 85080 88680 73260 10440 7049.6523 85180 88820 73380 10460 7050.0944 85360 89020 73580 10480 7050.5259 85460 89140 73680 10500 7050.9576 85300 89020 73620 10480 7051.3998 85260 89000 73600 10520 7051.8421 85340 89120 73720 10520 7052.2739 85420 89220 73860 10520 7052.7057 85460 89280 73900 10520 7053.1482 85500 89360 73960 10500 7053.5907 85400 89260 73920 10460 7054.0332 85220 89120 73800 10480 7054.4653 85180 89100 73800 10480 7054.8975 85260 89200 73900 10520 7055.3402 85320 89300 74000 10540 7055.783 85340 89360 74060 10540 7056.2153 85300 89340 74080 10500 7056.6476 85300 89340 74100 10520 7057.0906 85300 89380 74160 10520 7057.5336 85280 89400 74160 10520 7057.9662 85300 89420 74200 10520 7058.3987 85160 89300 74140 10500 7058.8419 85000 89140 74020 10480 7059.2852 85000 89180 74060 10480 7059.7285 84940 89140 74020 10480 7060.1613 84860 89080 73980 10440 7060.5942 84860 89120 74040 10480 7061.0376 84800 89060 74040 10500 7061.4812 84620 88920 73920 10440 7061.9142 84180 88480 73580 10440 7062.3473 83500 87780 73000 10400 7062.791 83520 87860 73100 10380 7063.2242 84320 88720 73800 10440 7063.6575 84920 89380 74360 10460 7064.1013 85020 89520 74500 10480 7064.5453 85000 89520 74520 10500 7064.9893 85000 89540 74560 10460 7065.4227 85040 89620 74620 10460 7065.8563 85060 89680 74700 10480 7066.3005 84960 89580 74620 10520 7066.7447 84880 89520 74620 10500 7067.1784 84680 89340 74460 10500 7067.6121 84300 88980 74180 10420 7068.0565 84080 88760 74000 10420 7068.4904 84240 88960 74180 10420 7068.9243 84460 89220 74400 10460 7069.3689 84560 89360 74540 10460 7069.8135 84620 89420 74620 10460 7070.2582 84520 89380 74600 10440 7070.6924 84420 89260 74520 10440 7071.1266 84220 89080 74400 10400 7071.5609 84200 89100 74400 10380 7071.9952 84280 89200 74500 10380 7072.4402 84300 89240 74560 10440 7072.8852 84220 89200 74520 10420 7073.3303 84260 89260 74600 10440 7073.7754 84320 89360 74700 10440 7074.21 84280 89360 74680 10440 7074.6553 84320 89420 74760 10440 7075.1006 84320 89440 74800 10460 7075.5354 84280 89420 74780 10460 7075.9702 83960 89140 74560 10440 7076.4051 83620 88780 74280 10380 7076.8507 83360 88520 74060 10340 7077.2963 82680 87860 73520 10240 7077.7313 82460 87620 73340 10260 7078.1771 82800 88000 73680 10300 7078.6228 83020 88280 73900 10320 7079.0581 83200 88500 74100 10300 7079.4934 83300 88640 74220 10320 7079.9287 83440 88800 74360 10340 7080.3747 83320 88700 74300 10360 7080.8208 83340 88740 74340 10360 7081.2563 83440 88860 74440 10400 7081.6919 83420 88880 74460 10400 7082.1381 83340 88820 74440 10380 7082.5844 83360 88860 74480 10380 7083.0308 83360 88880 74500 10400 7083.4666 83160 88700 74340 10340 7083.9024 83160 88740 74400 10340 7084.3489 83140 88740 74380 10340 7084.7955 83100 88680 74380 10320 7085.2316 83120 88760 74440 10360 7085.6676 83060 88740 74420 10360 7086.1144 82920 88620 74300 10340 7086.5612 82880 88560 74300 10320 7087.0081 83020 88780 74440 10320 7087.4444 83220 89000 74640 10340 7087.8808 83300 89120 74760 10360 7088.3172 83260 89080 74720 10360 7088.7537 83160 89020 74660 10380 7089.2008 83180 89080 74700 10380 7089.6481 83120 89000 74660 10380 7090.0954 82920 88820 74500 10340 7090.5321 82780 88720 74380 10320 7090.9795 82660 88600 74300 10300 7091.4269 82840 88820 74480 10300 7091.8638 82860 88880 74500 10320 7092.3114 82700 88720 74380 10280 7092.7484 82840 88880 74520 10320 7093.1854 82920 89020 74600 10320 7093.6332 82860 88960 74560 10320 7094.081 82800 88940 74500 10300 7094.5182 82620 88760 74340 10320 7094.9555 82440 88600 74220 10280 7095.4034 82360 88560 74140 10280 7095.8515 82380 88600 74160 10300 7096.2889 82480 88720 74240 10320 7096.7264 82440 88720 74240 10320 7097.1746 82500 88800 74260 10300 7097.6123 82500 88820 74240 10280 7098.0499 82280 88620 74080 10240 7098.4983 82260 88620 74020 10260 7098.9468 82240 88620 74000 10260 7099.3953 82060 88480 73800 10220 7099.8332 82160 88560 73840 10240 7100.2818 82240 88720 73920 10300 7100.7305 82220 88680 73860 10320 7101.1579 82220 88740 73800 10320 7101.596 82320 88860 73880 10300 7102.0449 82340 88920 73820 10320 7102.4938 82200 88800 73660 10300 7102.9321 82120 88720 73480 10300 7103.3704 82100 88740 73380 10300 7103.8302 82040 88680 73260 10260 7104.2794 81940 88620 73040 10240 7104.7179 82020 88720 72980 10280 7105.1672 82080 88820 72900 10260 7105.6058 81840 88600 72520 10240 7106.0445 81660 88400 72140 10240 7106.494 81860 88660 72100 10240 7106.9328 81960 88820 71880 10260 7107.3716 81880 88740 71440 10260 7107.8212 81880 88780 70980 10240 7108.2709 81860 88780 70360 10240 7108.7207 81880 88840 69560 10220 7109.1598 81820 88800 68400 10220 7109.5989 81640 88600 66540 10220 7110.0488 81580 88600 63680 10200 7110.4988 81460 88460 58900 10200 7110.9381 81260 88280 52300 10180 7111.3775 81120 88180 45520 10180 7111.8277 81020 88060 39980 10140 7112.2779 80820 87900 35960 10120 7112.7174 80700 87800 33140 10120 7113.157 80440 87540 30880 10100 7113.6074 80280 87380 29100 10100 7114.0472 80320 87460 27640 10100 7114.4869 80300 87440 26520 10060 7114.9375 80320 87520 25780 10080 7115.3881 80380 87600 25300 10100 7115.8388 80300 87540 24940 10100 7116.2788 80260 87520 24500 10080 7116.7189 80140 87400 23780 10100 7117.1697 80060 87360 22640 10080 7117.6207 80080 87380 21140 10060 7118.0716 80020 87360 19460 10080 7118.5119 79800 87140 17700 10060 7118.9523 79600 86940 15980 10020 7119.4034 79340 86680 14380 9980 7119.8547 79200 86560 12880 10000 7120.2952 79140 86520 11560 10000 7120.7358 79080 86460 10440 9960 7121.1872 79020 86400 9500 9920 7121.6386 78980 86440 8760 9920 7122.0794 78940 86380 8200 9940 7122.5202 78980 86460 7720 9940 7122.961 78900 86400 7320 9940 7123.4127 78820 86340 6960 9940 7123.8645 78740 86300 6660 9900 7124.3055 78700 86240 6400 9900 7124.7574 78540 86100 6140 9920 7125.2093 78460 86040 5940 9920 7125.6505 78320 85920 5720 9880 7126.0918 78100 85700 5500 9840 7126.5439 77940 85560 5280 9840 7126.9853 77820 85460 5080 9820 7127.4375 77700 85340 4840 9800 7127.8898 77560 85220 4580 9800 7128.3313 77500 85180 4340 9820 7128.7729 77440 85160 4120 9780 7129.2254 77300 85000 3900 9760 7129.6887 76920 84620 3700 9700 7130.1413 76700 84360 3580 9680 7130.5831 76620 84360 3520 9640 7131.0142 76480 84180 3520 9640 7131.4562 76420 84120 3560 9660 7131.909 76460 84220 3700 9700 7132.3511 76460 84240 3840 9660 7132.804 76440 84220 4040 9640 7133.257 76340 84160 4200 9640 7133.6993 76200 84020 4400 9600 7134.1524 76020 83860 4540 9600 7134.6055 75880 83700 4680 9560 7135.048 75780 83640 4800 9600 7135.4904 75680 83560 4860 9540 7135.9438 75680 83580 4920 9600 7136.3864 75780 83700 4960 9620 7136.8291 75760 83740 4980 9600 7137.2826 75840 83820 4940 9620 7137.7361 75940 83980 4900 9620 7138.1898 75740 83780 4840 9600 7138.6435 75540 83560 4740 9580 7139.0864 75520 83580 4660 9580 7139.5294 75520 83580 4600 9560 7139.9725 75440 83520 4520 9560 7140.4156 75460 83580 4500 9580 7140.8696 75520 83660 4460 9620 7141.3237 75520 83700 4460 9600 7141.7778 75500 83660 4440 9580 7142.232 75540 83760 4480 9600 7142.6862 75520 83760 4500 9620 7143.1297 75460 83720 4520 9600 7143.5732 75500 83780 4540 9580 7144.0168 75420 83760 4560 9560 7144.4604 75360 83700 4560 9560 7144.915 75360 83720 4540 9580 7145.3696 75320 83700 4520 9540 7145.8242 75340 83740 4480 9560 7146.2681 75380 83820 4420 9580 7146.712 75380 83840 4340 9560 7147.1669 75320 83780 4260 9540 7147.6217 75220 83720 4180 9520 7148.0659 75120 83680 4100 9560 7148.51 75040 83560 4020 9540 7148.9651 74980 83540 3960 9520 7149.4202 75040 83620 3900 9540 7149.8646 75060 83660 3880 9540 7150.309 74960 83540 3840 9540 7150.7643 74820 83460 3800 9560 7151.2196 74720 83360 3780 9520 7151.6751 74580 83220 3740 9500 7152.1197 74520 83180 3740 9480 7152.5644 74520 83220 3720 9480 7153.0091 74480 83160 3700 9480 7153.454 74440 83180 3700 9460 7153.9097 74460 83200 3700 9460 7154.3655 74360 83120 3720 9460 7154.8213 74320 83100 3720 9420 7155.2772 74220 83020 3740 9380 7155.7332 74120 82900 3760 9400 7156.1783 74060 82880 3760 9380 7156.6235 73920 82740 3780 9400 7157.0688 73800 82640 3780 9380 7157.5142 73820 82680 3800 9420 7157.9704 73680 82540 3800 9420 7158.4267 73700 82560 3800 9380 7158.8723 73860 82820 3820 9420 7159.3178 73980 82940 3820 9400 7159.7743 73980 82980 3820 9400 7160.2309 73980 83020 3840 9420 7160.6766 74020 83060 3840 9420 7161.1224 73920 82980 3840 9400 7161.5792 73900 82980 3860 9440 7162.036 74020 83160 3880 9420 7162.4928 74020 83180 3900 9460 7162.9389 73880 83040 3900 9440 7163.385 73840 83020 3940 9440 7163.842 74020 83260 3940 9460 7164.2991 74100 83360 3980 9440 7164.7454 74080 83380 4000 9440 7165.1917 74000 83300 4020 9420 7165.649 73920 83240 4000 9440 7166.0955 73840 83180 4040 9440 7166.542 73700 83060 4020 9420 7166.9994 73640 83020 4040 9420 7167.4569 73600 82980 4060 9400 7167.9145 73480 82900 4040 9420 7168.3722 73440 82880 4080 9380 7168.819 73340 82760 4060 9340 7169.2658 73180 82620 4080 9340 7169.7236 73080 82540 4100 9320 7170.1706 73060 82520 4120 9300 7170.6177 73060 82600 4140 9320 7171.0757 73060 82620 4160 9300 7171.5337 73080 82680 4220 9340 7171.9809 73020 82640 4240 9320 7172.4282 73000 82600 4280 9340 7172.8865 73020 82680 4320 9360 7173.3448 72960 82640 4380 9360 7173.8031 72900 82560 4400 9320 7174.2506 72940 82660 4480 9320 7174.6982 73140 82900 4540 9340 7175.1567 73300 83080 4600 9360 7175.6153 73320 83160 4660 9380 7176.0631 73400 83220 4720 9380 7176.5109 73340 83200 4780 9400 7176.9697 73260 83120 4840 9380 7177.4285 73140 83040 4880 9340 7177.8765 73100 82980 4920 9360 7178.3245 72960 82880 4960 9360 7178.7836 72960 82880 4980 9360 7179.2317 73000 82940 5020 9400 7179.6909 72880 82820 5020 9380 7180.1501 72740 82680 5020 9360 7180.5984 72800 82800 5040 9320 7181.0468 72840 82840 5040 9340 7181.4952 72880 82920 5040 9320 7181.9547 72940 83000 5040 9340 7182.4142 72960 83080 5020 9360 7182.8738 72920 83020 5000 9360 7183.3334 72860 83000 5000 9340 7183.7822 72820 83000 4960 9340 7184.231 72640 82800 4920 9320 7184.6798 72600 82780 4880 9320 7185.1288 72660 82900 4860 9320 7185.5887 72680 82920 4800 9320 7186.0487 72700 82980 4780 9320 7186.5087 72760 83080 4720 9320 7186.9579 72800 83120 4680 9340 7187.4181 72880 83240 4640 9360 7187.8783 72980 83400 4620 9360 7188.3276 73020 83440 4540 9380 7188.788 72940 83400 4520 9340 7189.2375 72820 83260 4440 9320 7189.687 72760 83240 4400 9340 7190.1475 72740 83240 4340 9360 7190.6081 72620 83120 4300 9340 7191.0578 72480 82980 4220 9300 7191.5076 72480 83000 4200 9280 7191.9683 72500 83040 4140 9300 7192.4292 72540 83120 4120 9300 7192.8901 72520 83120 4080 9300 7193.3401 72500 83140 4060 9320 7193.7901 72520 83160 4040 9320 7194.2512 72560 83220 4060 9320 7194.7014 72600 83300 4040 9340 7195.1516 72600 83300 4060 9360 7195.6129 72620 83380 4080 9340 7196.0742 72740 83520 4120 9360 7196.5246 72820 83600 4140 9380 7196.9751 72780 83620 4180 9380 7197.4366 72640 83480 4220 9380 7197.8872 72520 83340 4240 9340 7198.3488 72500 83360 4300 9320 7198.8105 72460 83340 4340 9340 7199.2723 72580 83500 4420 9360 7199.7341 72740 83700 4460 9360 7200.185 72800 83800 4540 9360 7200.6359 72820 83840 4600 9380 7201.0869 72800 83860 4660 9380 7201.549 72680 83720 4720 9380 7202.0001 72580 83600 4800 9360 7202.4513 72400 83460 4840 9320 7202.9135 72360 83420 4920 9360 7203.3758 72440 83540 4980 9340 7203.8382 72440 83540 5080 9360 7204.3006 72400 83540 5140 9340 7204.7521 72420 83580 5200 9360 7205.2036 72480 83680 5280 9360 7205.6663 72420 83640 5320 9360 7206.1289 72400 83600 5360 9320 7206.5807 72320 83560 5400 9320 7207.0324 72340 83620 5400 9320 7207.4953 72260 83540 5420 9340 7207.9582 72040 83300 5400 9300 7208.4102 71980 83260 5360 9260 7208.8622 71980 83320 5320 9300 7209.3142 71880 83180 5260 9320 7209.7664 71900 83260 5180 9320 7210.2296 71960 83340 5120 9340 7210.6929 72140 83560 5000 9360 7211.1562 72200 83680 4920 9360 7211.6086 72060 83520 4780 9340 7212.061 72000 83500 4640 9360 7212.5246 71960 83460 4500 9380 7212.9771 71860 83380 4360 9320 7213.4297 71840 83380 4240 9340 7213.8934 71920 83480 4140 9300 7214.3572 71760 83340 3980 9260 7214.821 71620 83180 3880 9260 7215.2849 71620 83220 3760 9260 7215.7379 71580 83200 3680 9260 7216.1908 71580 83200 3560 9280 7216.6549 71620 83280 3500 9280 7217.1191 71600 83300 3440 9300 7217.5722 71560 83260 3360 9300 7218.0254 71500 83220 3300 9260 7218.4897 71660 83400 3280 9280 7218.9431 71780 83600 3240 9300 7219.3965 71800 83640 3220 9300 7219.861 71720 83560 3200 9300 7220.3256 71760 83640 3200 9300 7220.7902 71700 83560 3180 9280 7221.2549 71580 83480 3200 9280 7221.7086 71540 83460 3200 9280 7222.1623 71680 83620 3240 9300 7222.6161 71840 83840 3280 9320 7223.07 72060 84140 3340 9380 7223.535 72260 84380 3400 9360 7224.0001 72220 84360 3460 9380 7224.4652 72120 84260 3520 9360 7224.9304 72040 84180 3580 9340 7225.3846 71940 84100 3660 9320 7225.8388 72000 84200 3740 9360 7226.3042 71980 84200 3820 9340 7226.7585 71840 84040 3900 9340 7227.224 71780 84020 3980 9320 7227.6896 71620 83840 4060 9300 7228.1441 71540 83740 4160 9260 7228.5987 71660 83960 4280 9320 7229.0534 71840 84160 4380 9300 7229.5192 71920 84300 4500 9340 7229.985 71620 83960 4580 9280 7230.451 71120 83400 4660 9240 7230.917 70840 83080 4740 9240 7231.3719 71180 83520 4880 9280 7231.8269 71680 84120 5020 9320 7232.2931 72100 84640 5140 9380 7232.7482 72320 84920 5260 9400 7233.2034 72220 84820 5360 9400 7233.6698 72020 84640 5440 9400 7234.1362 72060 84680 5520 9360 7234.6027 72060 84700 5600 9340 7235.0582 71980 84660 5660 9380 7235.5137 71960 84620 5720 9380 7235.9803 71880 84580 5780 9380 7236.4359 71840 84560 5820 9400 7236.8916 71860 84600 5860 9360 7237.3585 71780 84520 5880 9360 7237.8143 71740 84520 5900 9340 7238.2701 71840 84660 5920 9360 7238.7372 71900 84760 5940 9360 7239.2043 71860 84720 5920 9360 7239.6715 71760 84640 5900 9340 7240.1387 71620 84500 5900 9340 7240.5948 71500 84380 5860 9320 7241.0511 71440 84320 5820 9320 7241.5185 71280 84160 5800 9300 7241.9748 71060 83920 5720 9240 7242.4312 70920 83760 5680 9240 7242.8988 70860 83740 5640 9240 7243.3665 70880 83780 5600 9240 7243.8342 70920 83880 5560 9240 7244.302 70980 83940 5520 9260 7244.7587 70960 83960 5480 9240 7245.2155 70920 83900 5440 9240 7245.6835 70740 83740 5380 9200 7246.1404 70500 83460 5320 9200 7246.5973 70080 83000 5260 9180 7247.0655 69500 82320 5200 9160 7247.5226 69200 82020 5140 9120 7247.9908 69520 82400 5140 9100 7248.4592 69920 82920 5160 9140 7248.9164 70300 83380 5180 9160 7249.3849 70480 83640 5200 9200 7249.8423 70560 83740 5200 9220 7250.2997 70420 83600 5200 9240 7250.7684 70340 83500 5200 9200 7251.2259 70220 83420 5220 9200 7251.6836 70080 83260 5200 9160 7252.1636 69940 83120 5240 9160 7252.6325 70080 83320 5260 9160 7253.0903 70340 83660 5300 9220 7253.5593 70520 83900 5360 9240 7254.0172 70640 84060 5380 9260 7254.4752 70680 84120 5420 9260 7254.9444 70660 84140 5440 9240 7255.4026 70740 84240 5460 9260 7255.8607 70780 84320 5460 9260 7256.3301 70860 84420 5500 9300 7256.7996 70800 84380 5500 9320 7257.2691 70500 84040 5460 9240 7257.7387 70280 83820 5440 9240 7258.1972 70220 83740 5420 9220 7258.6557 70200 83780 5420 9200 7259.1255 70200 83780 5400 9220 7259.5842 70220 83820 5380 9220 7260.0429 70100 83720 5340 9220 7260.5129 69960 83560 5320 9160 7260.9829 69880 83500 5280 9160 7261.453 69880 83540 5280 9160 7261.912 69820 83460 5240 9160 7262.371 69560 83180 5200 9140 7262.8413 69380 82960 5160 9100 7263.3004 68780 82300 5100 9020 7263.7596 66780 79900 4940 8760 7264.2301 63880 76420 4720 8400 7264.7006 62980 75400 4640 8280 7265.1712 65120 78020 4780 8560 7265.6307 67700 81180 4960 8860 7266.0902 69140 82880 5040 9100 7266.561 69600 83460 5080 9120 7267.0206 69600 83480 5040 9120 7267.4803 69460 83360 5020 9140 7267.9513 69460 83340 5000 9120 7268.4223 69500 83440 4980 9140 7268.8934 69480 83420 4940 9120 7269.3646 69340 83300 4900 9120 7269.8246 69160 83100 4860 9100 7270.2846 69020 82960 4820 9100 7270.756 69200 83200 4780 9100 7271.2162 69400 83460 4780 9120 7271.6764 69540 83640 4740 9140 7272.1479 69600 83780 4720 9140 7272.6195 69740 83920 4700 9200 7273.08 69820 84040 4660 9200 7273.5405 69960 84240 4660 9200 7274.0123 70060 84380 4620 9200 7274.4841 69980 84300 4620 9200 7274.956 69760 84060 4580 9200 7275.4168 69560 83860 4560 9180 7275.8776 69540 83840 4540 9180 7276.3497 69500 83820 4520 9160 7276.8106 69340 83640 4520 9160 7277.2716 69140 83420 4480 9120 7277.7439 69060 83360 4480 9100 7278.2162 68900 83200 4440 9060 7278.6774 68720 83000 4420 9040 7279.1499 68700 83020 4420 9060 7279.6224 68840 83200 4400 9080 7280.0838 69020 83440 4400 9120 7280.5452 69060 83500 4380 9120 7281.0067 68780 83200 4360 9120 7281.4795 68540 82940 4320 9140 7281.9523 68740 83200 4300 9160 7282.4253 69140 83700 4320 9180 7282.887 69380 84020 4300 9180 7283.3488 69480 84120 4300 9180 7283.8219 69500 84180 4260 9180 7284.295 69500 84220 4260 9180 7284.7683 69500 84240 4220 9160 7285.2303 69520 84280 4220 9180 7285.6924 69620 84420 4200 9160 7286.1658 69740 84600 4200 9180 7286.6281 69840 84740 4200 9220 7287.0903 69900 84820 4200 9240 7287.564 69940 84940 4180 9240 7288.0376 69880 84880 4180 9220 7288.5114 69800 84780 4180 9260 7288.9739 69460 84420 4180 9220 7289.4365 68320 83020 4120 9060 7289.9104 67640 82240 4100 8940 7290.3732 68300 83060 4160 9040 7290.8359 68980 83940 4220 9160 7291.31 69340 84400 4300 9180 7291.7842 69500 84600 4340 9180 7292.2585 69580 84740 4400 9200 7292.7215 69660 84820 4440 9200 7293.1846 69640 84860 4520 9220 7293.659 69700 84920 4560 9220 7294.1335 69740 85040 4620 9240 7294.5968 69820 85100 4700 9260 7295.0601 69840 85200 4760 9280 7295.5348 69880 85220 4820 9260 7296.0096 69900 85320 4900 9260 7296.4731 69980 85400 4940 9300 7296.9367 69920 85380 5020 9260 7297.4116 69780 85220 5080 9280 7297.8867 69520 84920 5120 9240 7298.3504 68980 84280 5120 9200 7298.8143 68420 83620 5160 9100 7299.2895 68340 83560 5180 9080 7299.7534 68680 83980 5280 9100 7300.2174 69020 84440 5360 9160 7300.6928 69340 84840 5440 9160 7301.1683 69580 85160 5500 9200 7301.6438 69700 85340 5560 9240 7302.1081 69760 85440 5620 9240 7302.5724 69800 85520 5680 9260 7303.0481 69920 85680 5700 9240 7303.5125 70040 85860 5780 9260 7303.977 70160 86020 5800 9300 7304.4643 70280 86180 5860 9280 7304.9403 70380 86340 5900 9320 7305.405 70440 86460 5940 9380 7305.881 70420 86440 5960 9340 7306.3459 70360 86340 5980 9320 7306.8108 70340 86400 6020 9340 7307.287 70380 86440 6020 9340 7307.7634 70280 86360 6060 9340 7308.2285 70320 86420 6040 9340 7308.6936 70320 86460 6080 9360 7309.1701 70380 86560 6080 9340 7309.6354 70480 86700 6100 9380 7310.1007 70480 86700 6100 9360 7310.5774 70440 86740 6100 9380 7311.0542 70440 86720 6100 9340 7311.5311 70380 86660 6100 9360 7312.008 70480 86860 6120 9380 7312.4737 70560 86940 6100 9380 7312.928 70580 87020 6120 9380 7313.4051 70620 87060 6120 9380 7313.8823 70620 87100 6100 9380 7314.3482 70740 87260 6140 9420 7314.8255 70880 87480 6140 9440 7315.3029 71140 87820 6180 9480 7315.7689 71300 88040 6180 9500 7316.2351 71360 88140 6200 9520 7316.7126 71400 88200 6220 9520 7317.1903 71340 88180 6200 9520 7317.668 71200 88000 6200 9500 7318.1343 71180 88020 6220 9480 7318.6008 71340 88240 6220 9520 7319.0787 71540 88500 6240 9560 7319.5452 71740 88800 6280 9580 7320.0119 71880 88980 6300 9580 7320.4899 71780 88900 6280 9580 7320.9681 71800 88940 6300 9560 7321.4463 71880 89040 6300 9560 7321.9132 71980 89220 6320 9600 7322.3801 72100 89360 6340 9620 7322.8471 72060 89320 6340 9600 7323.3256 72040 89360 6340 9620 7323.8155 72020 89340 6340 9640 7324.2827 72020 89340 6340 9620 7324.75 72120 89540 6340 9640 7325.2287 72280 89720 6380 9660 7325.6961 72360 89900 6380 9680 7326.1635 72400 89920 6400 9660 7326.6424 72340 89920 6380 9620 7327.1214 72440 90040 6400 9680 7327.6005 72640 90340 6420 9700 7328.0682 72800 90520 6440 9700 7328.5359 72900 90700 6460 9700 7329.0152 73000 90820 6460 9740 7329.483 73080 90960 6500 9760 7329.9624 73120 91040 6520 9780 7330.4418 73000 90920 6500 9740 7330.8985 72900 90800 6520 9740 7331.3666 72840 90780 6540 9760 7331.8463 72760 90700 6540 9740 7332.3259 72760 90740 6560 9740 7332.8057 72840 90860 6580 9760 7333.2741 72800 90820 6620 9740 7333.754 72860 90920 6640 9740 7334.2339 72980 91100 6660 9760 7334.7025 73160 91360 6700 9800 7335.1826 73300 91560 6760 9800 7335.6513 73440 91740 6760 9800 7336.12 73560 91920 6800 9820 7336.6003 73700 92120 6840 9820 7337.0806 73880 92360 6840 9880 7337.5496 74040 92600 6880 9900 7338.0186 74140 92740 6900 9920 7338.4991 74220 92880 6920 9940 7338.9797 74340 93020 6920 9940 7339.4489 74380 93140 6920 9940 7339.9182 74500 93280 6920 9960 7340.399 74600 93420 6940 9980 7340.8799 74600 93480 6900 10000 7341.3493 74480 93360 6900 9980 7341.8188 74240 93080 6840 9940 7342.2999 74300 93180 6820 9940 7342.781 74380 93320 6800 9960 7343.2622 74400 93360 6780 9960 7343.7319 74520 93540 6740 10020 7344.2018 74720 93840 6740 10020 7344.6717 74960 94120 6700 10040 7345.1417 75080 94320 6700 10060 7345.6232 75160 94460 6640 10080 7346.1047 75320 94680 6620 10120 7346.5863 75260 94620 6580 10120 7347.0566 75220 94580 6520 10100 7347.5383 75120 94480 6480 10100 7348.0201 74960 94320 6400 10060 7348.4906 74740 94080 6360 10040 7348.9725 74700 94020 6320 10040 7349.443 74800 94180 6280 10080 7349.9136 75120 94620 6280 10100 7350.3958 75480 95080 6280 10160 7350.878 75720 95440 6240 10180 7351.3488 75940 95720 6240 10220 7351.8197 76080 95920 6220 10240 7352.3021 76140 96020 6180 10240 7352.7845 76180 96100 6160 10220 7353.2556 76280 96260 6140 10240 7353.7267 76380 96400 6120 10260 7354.2094 76500 96580 6080 10280 7354.6921 76460 96580 6080 10260 7355.1634 76360 96460 6020 10280 7355.6347 76360 96500 6000 10280 7356.1177 76400 96600 5980 10300 7356.6007 76420 96620 5960 10300 7357.0722 76440 96680 5940 10320 7357.5553 76420 96720 5900 10300 7358.0385 76440 96720 5880 10300 7358.5103 76440 96780 5860 10320 7358.9821 76540 96900 5860 10340 7359.454 76700 97160 5840 10340 7359.9374 76880 97420 5840 10320 7360.4209 77020 97620 5820 10340 7360.893 77080 97720 5800 10400 7361.3766 77180 97880 5820 10420 7361.8603 77240 97960 5780 10400 7362.3326 77260 98040 5800 10420 7362.8049 77380 98200 5780 10440 7363.2773 77540 98420 5780 10440 7363.7613 77680 98640 5800 10480 7364.2453 77880 98920 5800 10480 7364.7179 77940 99040 5800 10500 7365.1905 77900 98980 5820 10480 7365.6747 77780 98860 5780 10460 7366.159 77580 98640 5780 10440 7366.6434 77400 98440 5780 10460 7367.1163 77380 98440 5780 10460 7367.5892 77520 98640 5800 10460 7368.0738 77720 98940 5840 10460 7368.5469 78000 99320 5880 10500 7369.02 78140 99500 5900 10540 7369.5048 78160 99540 5940 10560 7369.9896 78200 99640 5960 10560 7370.4745 78360 99900 6020 10600 7370.9594 78640 100260 6060 10580 7371.4329 78800 100500 6100 10620 7371.9064 78700 100380 6140 10620 7372.38 78760 100500 6200 10620 7372.8537 78840 100640 6240 10640 7373.339 78800 100580 6300 10620 7373.8243 78760 100560 6340 10620 7374.3097 78920 100820 6420 10700 7374.7952 79120 101100 6520 10740 7375.2692 79120 101120 6560 10720 7375.7432 79000 100980 6640 10700 7376.2289 79080 101120 6700 10720 7376.7146 79200 101300 6800 10720 7377.1889 79220 101340 6880 10720 7377.6632 79340 101520 6960 10780 7378.1491 79460 101700 7080 10780 7378.6351 79600 101920 7180 10800 7379.1096 79560 101900 7260 10760 7379.5842 79560 101920 7340 10760 7380.0704 79520 101900 7440 10780 7380.5566 79440 101840 7520 10780 7381.043 79340 101700 7580 10760 7381.5178 79320 101720 7660 10780 7381.9927 79560 102060 7780 10780 7382.4792 79700 102280 7860 10780 7382.9542 79720 102340 7920 10800 7383.4293 79860 102520 8000 10840 7383.916 80040 102800 8100 10860 7384.4028 80040 102840 8120 10840 7384.8896 80040 102840 8180 10840 7385.365 80020 102860 8220 10840 7385.8404 80040 102920 8260 10860 7386.3158 80180 103120 8280 10860 7386.803 80360 103400 8340 10900 7387.2901 80520 103600 8380 10920 7387.7658 80480 103600 8360 10900 7388.2531 80240 103320 8360 10860 7388.7405 80260 103360 8360 10900 7389.2163 80580 103800 8380 10920 7389.6922 80860 104200 8420 10960 7390.1798 81060 104460 8440 11000 7390.6559 81120 104580 8420 11000 7391.132 81120 104620 8420 11020 7391.6197 81220 104760 8420 11040 7392.096 81400 105040 8420 11060 7392.5723 81400 105040 8400 11100 7393.0603 81400 105060 8380 11080 7393.5483 81240 104900 8360 11060 7394.0364 81020 104640 8320 11020 7394.513 80860 104460 8280 10980 7394.9896 80740 104360 8260 10940 7395.4779 80640 104220 8240 10920 7395.9663 80640 104260 8220 10960 7396.4547 80600 104260 8220 10980 7396.9432 80460 104060 8180 10960 7397.4202 80400 104040 8180 10920 7397.8972 80280 103920 8160 10900 7398.3859 80240 103900 8160 10920 7398.863 80340 104040 8180 10940 7399.3402 80420 104200 8180 10960 7399.8291 80600 104460 8200 10980 7400.3181 80700 104580 8220 10980 7400.7955 80740 104680 8220 10980 7401.2729 80800 104820 8240 11000 7401.7621 80820 104860 8260 11000 7402.2397 80800 104840 8240 11000 7402.729 80900 105000 8280 11000 7403.2184 80940 105120 8280 10980 7403.6962 80820 104960 8260 11020 7404.1857 80620 104720 8260 10980 7404.6636 80460 104560 8240 10960 7405.1416 80580 104720 8260 11000 7405.6313 80780 105040 8280 11040 7406.121 80920 105240 8300 11060 7406.6109 80980 105300 8300 11060 7407.0891 80920 105300 8300 11060 7407.5674 81020 105460 8320 11060 7408.0574 81160 105660 8320 11100 7408.5476 81320 105900 8340 11120 7409.0261 81280 105860 8360 11120 7409.5046 81140 105740 8320 11080 7409.9949 81100 105680 8320 11060 7410.4853 81080 105700 8320 11040 7410.964 80980 105600 8320 11020 7411.4429 80920 105540 8300 11020 7411.9334 80840 105480 8300 11040 7412.4241 80940 105600 8300 11060 7412.9148 80960 105680 8320 11080 7413.3939 80940 105680 8320 11060 7413.873 80920 105700 8300 11060 7414.3639 80980 105800 8320 11040 7414.8549 81000 105860 8340 11060 7415.3342 81100 106020 8340 11080 7415.8136 81180 106140 8360 11080 7416.2931 81160 106160 8360 11080 7416.7726 81220 106240 8360 11100 7417.2756 81260 106340 8400 11100 7417.767 81240 106340 8380 11100 7418.2468 81240 106380 8420 11120 7418.7266 81240 106400 8400 11100 7419.2064 81220 106360 8440 11080 7419.6981 81160 106360 8420 11080 7420.1898 81000 106140 8440 11080 7420.6815 80840 106000 8420 11040 7421.1617 80780 105900 8440 11040 7421.6418 80680 105820 8460 11020 7422.1338 80540 105700 8460 11020 7422.6141 80500 105620 8460 11020 7423.1062 80400 105560 8480 11000 7423.5984 80460 105640 8520 11000 7424.0789 80580 105840 8540 11040 7424.5712 80660 105960 8580 11040 7425.0519 80740 106100 8620 11040 7425.5326 80820 106240 8640 11060 7426.0251 80800 106240 8660 11040 7426.5177 80760 106200 8660 11080 7426.9986 80800 106300 8700 11120 7427.4796 80860 106420 8700 11100 7427.9724 80880 106440 8720 11120 7428.4535 80860 106440 8740 11100 7428.9346 80740 106340 8720 11060 7429.4276 80600 106160 8720 11040 7429.9207 80440 106020 8700 11040 7430.4138 80360 105900 8680 11040 7430.9069 80260 105820 8680 11020 7431.3884 80140 105680 8680 11020 7431.87 79980 105500 8640 10980 7432.3634 79860 105380 8640 10960 7432.8451 79840 105380 8620 10960 7433.3269 79840 105380 8640 10980 7433.8204 79720 105280 8620 10960 7434.3141 79520 105040 8580 10940 7434.8078 79520 105040 8580 10900 7435.2898 79540 105120 8580 10920 7435.7719 79480 105060 8560 10920 7436.2658 79460 105080 8560 10920 7436.7598 79580 105240 8560 10920 7437.2421 79640 105340 8540 10900 7437.7245 79660 105400 8540 10940 7438.2187 79660 105460 8520 10940 7438.7011 79640 105420 8500 10940 7439.1837 79700 105540 8500 10940 7439.6781 79980 105980 8500 10980 7440.1725 80220 106280 8500 11020 7440.6671 80300 106420 8500 11020 7441.1617 80220 106380 8460 11000 7441.6445 80000 106100 8400 10980 7442.1275 79860 105920 8380 10980 7442.6105 79880 106000 8360 11000 7443.1054 79920 106080 8320 11000 7443.6003 79940 106140 8300 10980 7444.0835 79860 106040 8280 11000 7444.5786 79560 105700 8220 10940 7445.0737 79300 105360 8180 10940 7445.5571 79180 105260 8140 10920 7446.0406 79200 105300 8120 10940 7446.5241 79260 105400 8100 10960 7447.0077 79160 105320 8080 10940 7447.5032 79060 105200 8060 10920 7447.9987 79000 105120 8020 10900 7448.4943 78800 104920 8000 10860 7448.9782 78840 104960 7980 10860 7449.4622 79040 105300 8000 10920 7449.958 79160 105460 8020 10900 7450.4538 79180 105520 8000 10880 7450.938 78780 105000 7960 10800 7451.4222 77600 103440 7820 10660 7451.9183 76820 102460 7760 10580 7452.4144 77480 103360 7820 10640 7452.8988 78440 104660 7920 10780 7453.3833 78980 105420 7980 10880 7453.8796 79100 105600 8000 10880 7454.376 79100 105660 8000 10920 7454.8725 79020 105580 8000 10920 7455.3573 78780 105240 7960 10860 7455.8421 78540 104980 7960 10820 7456.3387 78440 104880 7940 10860 7456.8355 78500 104960 7980 10900 7457.3323 78760 105360 7980 10880 7457.8174 79100 105840 8040 10960 7458.3025 79340 106200 8080 10940 7458.7877 79420 106300 8080 10960 7459.273 79500 106460 8120 10980 7459.7701 79500 106500 8120 11020 7460.2674 79320 106300 8120 11000 7460.7647 78840 105640 8060 10940 7461.2502 77920 104440 8000 10780 7461.7358 77100 103380 7920 10700 7462.2333 77580 104060 7980 10760 7462.7309 78460 105280 8100 10900 7463.2285 78920 105920 8160 10940 7463.7144 78940 106000 8180 10920 7464.2003 78880 105900 8200 10880 7464.6981 78960 106060 8220 10900 7465.1961 79080 106280 8260 10940 7465.6822 79140 106340 8300 10960 7466.1684 79140 106400 8320 10980 7466.6665 79080 106340 8340 10960 7467.1528 79080 106380 8360 10960 7467.6392 79180 106540 8420 10960 7468.1375 79260 106660 8440 10980 7468.6359 79240 106660 8480 10960 7469.1344 79280 106760 8520 10980 7469.621 79220 106680 8540 10980 7470.1078 79020 106460 8560 10920 7470.6064 78860 106260 8560 10920 7471.1052 78920 106360 8600 10960 7471.5921 78980 106480 8640 10980 7472.0791 78920 106420 8660 10960 7472.578 78780 106240 8680 10920 7473.0651 78520 105940 8700 10840 7473.5642 78360 105760 8700 10860 7474.0634 78300 105700 8720 10860 7474.5507 78280 105700 8740 10860 7475.05 78160 105560 8740 10840 7475.5374 78080 105480 8780 10840 7476.025 78100 105540 8800 10820 7476.5244 78120 105560 8820 10840 7477.024 78180 105720 8860 10860 7477.5117 78220 105800 8900 10860 7477.9995 78280 105900 8900 10840 7478.5112 78360 106040 8960 10860 7479.011 78380 106100 8960 10880 7479.499 78360 106100 9000 10880 7479.987 78340 106100 9000 10860 7480.4752 78360 106160 9040 10880 7480.9753 78400 106240 9060 10880 7481.4635 78440 106340 9100 10880 7481.9519 78540 106480 9120 10920 7482.4522 78540 106540 9160 10900 7482.9525 78480 106460 9180 10920 7483.4411 78320 106260 9180 10880 7483.9416 78240 106220 9200 10900 7484.4422 78160 106120 9220 10900 7484.9309 78000 105920 9220 10880 7485.4316 77940 105860 9260 10840 7485.9205 77980 105960 9280 10880 7486.4094 78020 106060 9320 10880 7486.9103 77960 105980 9340 10860 7487.4113 78000 106060 9380 10880 7487.9124 77940 105980 9400 10840 7488.4016 77800 105860 9400 10820 7488.8909 77640 105640 9420 10780 7489.3921 77580 105600 9440 10820 7489.8815 77640 105720 9460 10860 7490.371 77780 105920 9520 10840 7490.8725 77840 106040 9540 10880 7491.374 77980 106260 9580 10860 7491.8637 78060 106400 9620 10880 7492.3534 78040 106400 9660 10880 7492.8552 77920 106260 9640 10860 7493.357 77700 105980 9640 10820 7493.847 77660 105980 9640 10780 7494.337 77700 106060 9660 10800 7494.839 77580 105880 9660 10800 7495.3411 77460 105800 9660 10780 7495.8313 77540 105900 9680 10780 7496.3216 77740 106220 9700 10840 7496.8239 77860 106420 9740 10860 7497.3262 77940 106520 9740 10880 7497.8287 77980 106640 9740 10880 7498.3192 78020 106720 9760 10900 7498.8098 77940 106640 9760 10900 7499.3125 77860 106560 9740 10880 7499.8032 77860 106580 9720 10880 7500.294 77860 106620 9740 10880 7500.7969 77860 106620 9720 10900 7501.2998 77840 106640 9740 10900 7501.8028 77740 106560 9700 10900 7502.3059 77740 106540 9720 10900 7502.797 77760 106620 9700 10880 7503.2883 77700 106580 9700 10900 7503.7796 77800 106740 9700 10880 7504.2709 78060 107100 9720 10880 7504.7743 78080 107180 9740 10940 7505.2778 78000 107080 9740 10940 7505.7813 77920 107000 9700 10920 7506.273 77840 106940 9720 10880 7506.7647 77820 106920 9700 10900 7507.2684 77980 107180 9720 10920 7507.7722 78140 107440 9740 10960 7508.2761 78240 107600 9760 10980 7508.7681 78260 107660 9780 10960 7509.2601 78320 107760 9780 10980 7509.7642 78320 107800 9780 10980 7510.2564 78380 107900 9800 10980 7510.7606 78360 107920 9820 10960 7511.2529 78320 107860 9800 10940 7511.7453 78240 107820 9820 10980 7512.2618 78220 107780 9820 10980 7512.7663 78340 107980 9840 11000 7513.2589 78460 108180 9860 11020 7513.7515 78480 108260 9880 11020 7514.2562 78520 108300 9900 11040 7514.749 78480 108280 9900 11000 7515.2419 78380 108160 9900 11000 7515.7468 78360 108200 9900 10980 7516.2518 78520 108420 9940 11000 7516.7569 78600 108580 9960 11020 7517.25 78540 108520 9960 11040 7517.7432 78460 108440 9960 11020 7518.2485 78320 108260 9940 10980 7518.7538 78280 108240 9960 11000 7519.2472 78360 108360 9980 10980 7519.7407 78360 108440 9980 11000 7520.2462 78460 108580 10000 11020 7520.7398 78440 108560 10020 11020 7521.2335 78280 108400 10000 11000 7521.7393 78200 108300 9980 11020 7522.2451 78160 108260 10000 11040 7522.751 78180 108340 10000 11000 7523.245 78360 108600 10020 11000 7523.739 78460 108780 10040 11000 7524.2451 78440 108800 10060 11000 7524.7392 78380 108700 10040 10960 7525.2334 78280 108620 10040 11000 7525.7398 78180 108520 10020 11000 7526.2462 78300 108700 10040 11020 7526.7526 78420 108900 10060 11020 7527.2471 78520 109080 10080 11040 7527.7417 78620 109220 10080 11040 7528.2363 78580 109200 10100 11000 7528.743 78580 109240 10080 11020 7529.2498 78720 109460 10120 11040 7529.7447 78740 109540 10100 11100 7530.2516 78840 109680 10140 11120 7530.7587 78940 109880 10140 11100 7531.2658 78920 109840 10140 11120 7531.7609 78880 109840 10140 11120 7532.256 78840 109840 10120 11140 7532.7633 78860 109880 10160 11140 7533.2586 78720 109700 10120 11100 7533.754 78640 109620 10120 11100 7534.2615 78660 109700 10120 11060 7534.757 78620 109680 10140 11080 7535.2526 78660 109740 10140 11100 7535.7603 78780 109920 10160 11080 7536.2681 78720 109920 10180 11080 7536.776 78720 109880 10180 11040 7537.2839 78640 109820 10160 11080 7537.7798 78620 109800 10200 11100 7538.2758 78420 109560 10160 11040 7538.784 78200 109240 10140 11000 7539.2801 78300 109460 10160 11020 7539.7763 78500 109740 10200 11060 7540.2847 78600 109900 10240 11080 7540.7931 78600 109960 10240 11100 7541.3016 78620 110020 10260 11080 7541.7981 78700 110140 10260 11080 7542.2946 78880 110400 10320 11120 7542.7912 79000 110600 10320 11140 7543.3 79080 110780 10360 11140 7543.8088 79120 110840 10380 11160 7544.3056 79120 110880 10400 11160 7544.8025 79140 110920 10400 11180 7545.3116 79100 110900 10400 11160 7545.8207 78980 110760 10380 11140 7546.3178 78980 110780 10400 11140 7546.8271 79000 110840 10420 11180 7547.3364 79040 110920 10440 11160 7547.8337 79120 111080 10440 11180 7548.3311 79240 111260 10460 11200 7548.8406 79240 111300 10480 11220 7549.3502 79200 111280 10480 11200 7549.8599 79180 111280 10480 11240 7550.3576 79200 111300 10480 11220 7550.8553 79080 111200 10480 11200 7551.3652 79000 111100 10460 11180 7551.863 78860 110940 10440 11120 7552.3609 78900 111020 10440 11120 7552.8711 79080 111320 10480 11180 7553.3691 79320 111680 10500 11200 7553.8794 79400 111840 10520 11240 7554.3897 79460 111940 10520 11260 7554.888 79520 112020 10500 11240 7555.3984 79480 112040 10520 11240 7555.8968 79480 112060 10500 11240 7556.3953 79500 112100 10480 11260 7556.906 79460 112080 10500 11260 7557.4167 79400 112020 10460 11220 7557.9276 79520 112200 10480 11240 7558.4263 79680 112480 10500 11280 7558.9251 79940 112860 10520 11320 7559.4362 80160 113220 10540 11360 7559.9473 80260 113360 10560 11380 7560.4463 80320 113500 10560 11400 7560.9454 80340 113560 10560 11400 7561.4567 80380 113660 10560 11400 7561.9559 80460 113780 10580 11380 7562.4552 80520 113880 10580 11440 7562.9667 80540 113960 10580 11440 7563.4783 80600 114060 10580 11420 7563.99 80600 114120 10600 11440 7564.4896 80640 114180 10600 11460 7564.9892 80620 114200 10600 11440 7565.5011 80560 114140 10600 11380 7566.0131 80540 114140 10600 11400 7566.5129 80600 114260 10620 11440 7567.0128 80600 114260 10640 11440 7567.525 80540 114220 10620 11440 7568.0373 80400 114060 10640 11380 7568.5496 80480 114200 10660 11440 7569.0498 80680 114520 10680 11480 7569.55 80940 114900 10740 11540 7570.0626 81060 115120 10780 11540 7570.563 81120 115220 10800 11520 7571.0634 81000 115100 10800 11560 7571.5762 81000 115120 10820 11540 7572.089 81180 115380 10860 11520 7572.5897 81200 115460 10880 11540 7573.0904 81280 115620 10920 11560 7573.6035 81360 115760 10960 11560 7574.1166 81360 115800 10980 11560 7574.6297 81380 115840 11020 11580 7575.1308 81340 115820 11040 11560 7575.6441 81280 115760 11040 11560 7576.1575 81260 115760 11080 11560 7576.6587 81180 115700 11100 11520 7577.16 81160 115680 11100 11520 7577.6614 81120 115640 11140 11520 7578.175 81000 115520 11160 11520 7578.6888 80940 115460 11180 11520 7579.1904 81020 115620 11200 11520 7579.7043 81080 115740 11260 11560 7580.2182 81160 115880 11280 11580 7580.72 81220 115980 11340 11580 7581.2219 81300 116140 11360 11600 7581.7238 81380 116320 11400 11600 7582.238 81540 116540 11460 11580 7582.7524 81480 116520 11480 11620 7583.2545 81460 116480 11480 11600 7583.7567 81340 116360 11500 11620 7584.2712 81400 116460 11540 11620 7584.7858 81500 116660 11580 11620 7585.3005 81580 116800 11600 11600 7585.8153 81780 117100 11660 11640 7586.3178 81840 117220 11680 11640 7586.8204 81800 117200 11680 11620 7587.3354 81720 117100 11700 11660 7587.8382 81720 117120 11720 11660 7588.341 81640 117060 11720 11680 7588.8562 81560 117000 11720 11660 7589.3714 81620 117080 11760 11680 7589.8867 81600 117100 11760 11700 7590.3899 81520 117000 11760 11620 7590.8931 81460 116980 11760 11620 7591.3963 81400 116880 11760 11600 7591.8996 81340 116820 11780 11620 7592.4153 81320 116860 11760 11600 7592.9311 81200 116700 11780 11600 7593.4469 81120 116620 11760 11580 7593.9505 81060 116560 11780 11560 7594.4542 81060 116600 11760 11580 7594.9702 81120 116680 11800 11580 7595.4863 81200 116860 11800 11580 7596.0025 81280 117000 11840 11620 7596.5065 81460 117300 11860 11620 7597.0105 81300 117100 11840 11620 7597.5269 80860 116480 11800 11580 7598.031 80880 116540 11800 11580 7598.5353 81340 117240 11880 11660 7599.0519 81640 117700 11920 11680 7599.5686 81700 117820 11940 11700 7600.0853 81580 117640 11920 11680 7600.5899 81420 117460 11900 11620 7601.0944 81100 117040 11880 11600 7601.5991 80780 116620 11840 11520 7602.1161 81020 116980 11880 11580 7602.6333 81420 117600 11940 11640 7603.1381 81540 117800 11980 11640 7603.6554 81560 117860 12000 11640 7604.1727 81520 117820 12000 11640 7604.6778 81500 117840 12000 11620 7605.183 81560 117920 12040 11680 7605.7005 81580 118040 12040 11700 7606.2181 81560 118000 12060 11720 7606.7235 81580 118080 12080 11720 7607.2289 81720 118320 12120 11720 7607.7468 81740 118380 12140 11760 7608.2647 81560 118140 12120 11720 7608.7703 81480 118060 12140 11700 7609.276 81580 118220 12160 11720 7609.7942 81580 118280 12180 11760 7610.3124 81520 118200 12200 11720 7610.8306 81560 118260 12200 11700 7611.3366 81480 118240 12220 11680 7611.8427 81420 118120 12220 11680 7612.3612 81220 117900 12220 11640 7612.8798 81160 117800 12220 11640 7613.386 81040 117720 12240 11600 7613.8924 81040 117700 12240 11620 7614.4112 81060 117800 12240 11640 7614.93 81080 117840 12280 11620 7615.4366 81100 117900 12280 11600 7615.9432 81000 117780 12280 11640 7616.4623 80880 117620 12280 11600 7616.9814 80820 117580 12260 11580 7617.4883 80920 117760 12300 11600 7617.9952 80860 117700 12300 11580 7618.5145 80800 117640 12280 11580 7619.034 80740 117600 12300 11600 7619.5411 80900 117840 12320 11620 7620.0483 80980 118040 12340 11620 7620.568 80920 117940 12320 11660 7621.0877 81000 118080 12360 11660 7621.6075 81060 118220 12360 11700 7622.115 81020 118180 12360 11700 7622.6225 80720 117800 12320 11660 7623.1425 80400 117320 12260 11580 7623.6626 80320 117280 12260 11560 7624.1828 80360 117380 12280 11580 7624.6906 80360 117420 12280 11580 7625.1861 80440 117540 12300 11600 7625.6941 80620 117840 12320 11620 7626.2146 80640 117900 12340 11620 7626.7351 80580 117840 12340 11620 7627.2557 80660 117960 12340 11600 7627.7763 80740 118160 12380 11660 7628.2847 80780 118220 12400 11640 7628.7931 80700 118140 12380 11640 7629.314 80560 117980 12380 11620 7629.8349 80360 117740 12360 11600 7630.3435 80240 117600 12360 11580 7630.8522 80320 117740 12380 11580 7631.361 80380 117840 12380 11600 7631.8822 80300 117760 12400 11560 7632.4036 80140 117580 12380 11540 7632.9125 79980 117340 12380 11540 7633.434 79800 117100 12380 11500 7633.9555 79820 117180 12380 11520 7634.4772 79920 117320 12420 11520 7634.9864 79980 117480 12440 11560 7635.4958 80060 117580 12480 11540 7636.0052 80000 117560 12480 11520 7636.5146 80020 117600 12520 11540 7637.0366 79960 117520 12520 11560 7637.5587 80020 117660 12540 11580 7638.0808 80080 117760 12560 11580 7638.603 80040 117740 12600 11600 7639.1252 79960 117640 12580 11580 7639.6352 79880 117540 12600 11560 7640.1451 79980 117760 12640 11560 7640.6552 79940 117680 12640 11560 7641.1653 79840 117560 12660 11520 7641.6879 79820 117560 12660 11520 7642.1982 79600 117280 12640 11500 7642.721 79500 117140 12640 11480 7643.2438 79500 117200 12680 11480 7643.7543 79540 117260 12680 11520 7644.2773 79580 117360 12720 11500 7644.7879 79640 117480 12740 11520 7645.2986 79640 117500 12760 11520 7645.8218 79640 117540 12780 11540 7646.3451 79620 117520 12800 11540 7646.8685 79640 117600 12800 11560 7647.3795 79580 117520 12820 11540 7647.8905 79720 117760 12840 11560 7648.4141 79780 117880 12880 11560 7648.9378 79680 117760 12860 11540 7649.449 79700 117800 12900 11520 7649.9604 79600 117720 12900 11540 7650.4843 79420 117460 12860 11520 7650.9957 79320 117340 12860 11460 7651.5073 79260 117320 12880 11460 7652.0314 79180 117220 12860 11460 7652.5556 78920 116860 12840 11420 7653.0798 78620 116420 12780 11380 7653.6041 78580 116420 12800 11380 7654.1161 78660 116580 12820 11440 7654.628 78580 116500 12820 11440 7655.1526 78440 116280 12820 11400 7655.6647 78200 115980 12760 11360 7656.1894 77980 115700 12740 11320 7656.7142 77940 115640 12760 11320 7657.2265 77800 115460 12740 11280 7657.7514 77600 115220 12700 11240 7658.2639 77080 114440 12640 11160 7658.7765 75260 111760 12340 10920 7659.3016 74080 110060 12160 10740 7659.8268 75300 111900 12360 10900 7660.3396 76900 114340 12640 11180 7660.8524 77680 115540 12780 11300 7661.3778 77980 115960 12820 11360 7661.8908 77980 116020 12840 11340 7662.4039 77880 115860 12820 11320 7662.9295 77780 115760 12800 11280 7663.4553 77680 115640 12800 11260 7663.9811 77660 115620 12800 11240 7664.5069 77620 115620 12800 11280 7665.0204 77440 115380 12760 11260 7665.5339 77080 114840 12720 11200 7666.0474 76640 114240 12640 11120 7666.5736 76660 114320 12660 11100 7667.0998 76880 114660 12700 11160 7667.6136 77060 114980 12720 11220 7668.1275 77140 115100 12740 11240 7668.6539 77240 115320 12760 11220 7669.1805 77240 115320 12760 11200 7669.6945 77100 115140 12760 11200 7670.2212 76920 114920 12720 11160 7670.7354 76920 114900 12720 11160 7671.2497 76880 114900 12720 11160 7671.7766 76900 114940 12720 11200 7672.3036 76800 114820 12720 11200 7672.8181 76700 114740 12700 11160 7673.3327 76660 114680 12680 11160 7673.8599 76600 114620 12700 11140 7674.3872 76540 114560 12680 11140 7674.9145 76600 114660 12700 11140 7675.4294 76540 114600 12680 11160 7675.9443 76380 114420 12680 11140 7676.4719 76200 114160 12640 11080 7676.987 76120 114080 12640 11080 7677.5021 76180 114200 12640 11100 7678.0299 76120 114120 12640 11100 7678.5578 75940 113920 12620 11060 7679.0858 75840 113780 12600 11040 7679.6012 75720 113620 12580 11020 7680.1167 75640 113500 12580 11040 7680.6449 75640 113580 12580 11040 7681.1606 75640 113580 12600 11020 7681.6763 75480 113360 12580 11000 7682.2047 75260 113080 12540 10960 7682.7331 74840 112460 12480 10920 7683.2617 73620 110660 12280 10780 7683.7777 70620 106140 11800 10360 7684.2938 68740 103360 11480 10080 7684.8226 70460 106000 11800 10300 7685.3514 73120 110060 12240 10680 7685.8803 74620 112340 12500 10900 7686.3967 75040 112980 12580 10960 7686.9132 75220 113280 12600 11000 7687.4297 75380 113540 12640 11000 7687.9463 75400 113580 12660 11000 7688.4756 75340 113540 12680 10980 7689.0176 75380 113640 12700 10980 7689.547 75380 113660 12720 11020 7690.0639 75460 113800 12760 11000 7690.5809 75600 114040 12780 11020 7691.0853 75600 114120 12820 11060 7691.6151 75600 114100 12820 11060 7692.1449 75460 113940 12800 11040 7692.6621 75360 113780 12820 11040 7693.1921 75200 113620 12800 11000 7693.7221 75120 113480 12800 10980 7694.2522 75060 113460 12800 10940 7694.7824 75120 113540 12840 10960 7695.3 75080 113500 12840 11000 7695.8178 75080 113540 12840 11000 7696.3482 75020 113500 12880 10960 7696.8786 74980 113440 12860 10940 7697.3966 74860 113320 12860 10940 7697.9146 74780 113220 12880 10960 7698.4453 74820 113280 12880 10980 7698.976 74780 113280 12900 10980 7699.5069 74660 113080 12880 10980 7700.0252 74500 112900 12880 10960 7700.5436 74460 112840 12880 10960 7701.062 74160 112440 12860 10920 7701.5805 73420 111320 12720 10760 7702.1117 73000 110700 12680 10680 7702.643 73520 111540 12780 10760 7703.1618 74220 112640 12900 10900 7703.6806 74620 113280 13000 10940 7704.2121 74780 113560 13040 10980 7704.7437 74800 113580 13060 10980 7705.2627 74780 113580 13080 10960 7705.7818 74600 113360 13060 10960 7706.3136 74640 113440 13080 10940 7706.8456 74700 113560 13100 10960 7707.3649 74640 113500 13100 10920 7707.8843 74620 113500 13120 10960 7708.4164 74620 113520 13140 10980 7708.9486 74540 113440 13140 10940 7709.4809 74500 113400 13160 10940 7710.0006 74360 113240 13140 10960 7710.5203 74340 113200 13140 10920 7711.0401 74400 113360 13200 10920 7711.5727 74440 113460 13200 10960 7712.1054 74400 113400 13220 10940 7712.6254 74320 113360 13220 10940 7713.1582 74300 113320 13240 10940 7713.6911 74300 113380 13260 10940 7714.2241 74260 113340 13260 10940 7714.7444 74240 113300 13260 10920 7715.2648 74200 113300 13300 10940 7715.798 73980 112980 13260 10920 7716.3186 73580 112380 13200 10860 7716.8392 73500 112320 13220 10840 7717.3726 73860 112900 13280 10860 7717.9061 74120 113320 13360 10880 7718.4397 74300 113600 13420 10920 7718.9733 74340 113740 13420 10940 7719.4943 74320 113680 13460 10940 7720.0154 74160 113480 13420 10920 7720.5366 74080 113400 13440 10920 7721.0705 74060 113380 13420 10900 7721.6045 74160 113540 13480 10900 7722.1259 74280 113780 13500 10920 7722.6473 74280 113800 13520 10920 7723.1689 74300 113860 13540 10960 7723.7032 74220 113780 13540 10920 7724.2376 74120 113620 13520 10920 7724.772 73860 113260 13500 10860 7725.3066 73020 112000 13360 10760 7725.8285 72280 110880 13220 10640 7726.3504 72560 111360 13280 10720 7726.8852 73260 112460 13440 10820 7727.4073 73680 113140 13520 10900 7727.9295 73860 113440 13560 10920 7728.4645 73960 113600 13580 10940 7728.9996 74020 113740 13620 10920 7729.5347 74060 113800 13620 10940 7730.0572 74080 113860 13660 10920 7730.5798 74040 113840 13640 10940 7731.1152 74120 113960 13680 10940 7731.6379 74160 114060 13680 10940 7732.1607 74200 114140 13720 10940 7732.6963 74260 114260 13720 10960 7733.2319 74300 114360 13740 10960 7733.7549 74320 114400 13760 10940 7734.278 74220 114300 13760 10920 7734.8139 74220 114300 13740 10920 7735.3499 74320 114500 13800 10920 7735.886 74420 114680 13820 11000 7736.4221 74460 114760 13860 11000 7736.9456 74480 114840 13860 11020 7737.4691 74560 114980 13880 11020 7737.9927 74580 115040 13900 10980 7738.5164 74620 115120 13920 11000 7739.0529 74640 115180 13940 11020 7739.5895 74620 115200 13960 11020 7740.1261 74680 115300 13960 11020 7740.6629 74600 115220 13960 11020 7741.1869 74580 115220 13980 11020 7741.711 74560 115200 13980 11020 7742.248 74600 115300 14000 11040 7742.7723 74700 115480 14040 11040 7743.2966 74680 115480 14040 11060 7743.8338 74740 115600 14060 11060 7744.3711 74760 115640 14080 11100 7744.9085 74740 115660 14100 11060 7745.4459 74740 115680 14100 11040 7745.9706 74720 115720 14100 11060 7746.4954 74800 115840 14140 11040 7747.0203 74860 115960 14160 11040 7747.5452 74900 116060 14180 11080 7748.083 74920 116120 14180 11100 7748.6209 74880 116080 14200 11080 7749.1461 74960 116260 14220 11080 7749.6713 74980 116320 14240 11080 7750.2094 75000 116380 14260 11080 7750.7476 75100 116520 14280 11100 7751.2859 75000 116440 14260 11120 7751.8114 75020 116480 14300 11120 7752.337 75200 116800 14320 11200 7752.8755 75340 117060 14380 11220 7753.4013 75500 117340 14400 11260 7753.9271 75600 117520 14460 11240 7754.4658 75660 117620 14460 11240 7755.0046 75660 117660 14480 11220 7755.5435 75740 117860 14520 11220 7756.0697 75800 117920 14540 11260 7756.5959 75660 117760 14520 11280 7757.135 75720 117880 14540 11260 7757.6742 75720 117900 14560 11240 7758.2006 75680 117900 14560 11200 7758.7271 75680 117880 14580 11200 7759.2665 75640 117880 14580 11240 7759.806 75620 117860 14600 11240 7760.3456 75700 118040 14620 11260 7760.8724 75880 118320 14680 11260 7761.3993 75960 118480 14700 11260 7761.9391 75840 118300 14700 11220 7762.4661 75780 118240 14700 11200 7762.9932 76000 118620 14760 11280 7763.5333 76160 118880 14820 11300 7764.0734 76240 119060 14840 11340 7764.6007 76300 119180 14880 11340 7765.141 76280 119180 14880 11360 7765.6813 76240 119160 14900 11340 7766.2089 76200 119120 14880 11360 7766.7365 76240 119180 14920 11400 7767.2642 76180 119140 14940 11360 7767.8049 76140 119100 14920 11360 7768.3456 76200 119220 14980 11340 7768.8735 76260 119340 14980 11360 7769.4144 76300 119460 15020 11380 7769.9554 76400 119620 15060 11400 7770.4835 76460 119760 15080 11380 7771.0246 76540 119940 15120 11380 7771.5658 76440 119760 15120 11400 7772.0942 76400 119760 15120 11380 7772.6227 76400 119780 15140 11340 7773.1512 76300 119620 15120 11360 7773.6798 76220 119600 15140 11320 7774.2214 76340 119760 15160 11360 7774.763 76480 120040 15220 11440 7775.3047 76800 120580 15300 11480 7775.8466 76840 120660 15320 11480 7776.3755 76620 120340 15280 11440 7776.9046 76780 120640 15340 11460 7777.4466 77040 121100 15400 11520 7777.9758 77060 121140 15420 11500 7778.5051 77000 121080 15420 11480 7779.0474 76980 121100 15440 11480 7779.5898 76960 121080 15460 11480 7780.1322 77000 121160 15460 11480 7780.6618 76980 121200 15480 11520 7781.1914 77100 121380 15520 11520 7781.7341 77200 121580 15560 11500 7782.2639 77220 121660 15560 11520 7782.7938 77240 121700 15580 11540 7783.3367 77280 121760 15600 11520 7783.8796 77200 121700 15600 11500 7784.4227 77240 121760 15600 11520 7784.9529 77260 121840 15640 11500 7785.4832 77100 121620 15620 11540 7786.0264 76960 121400 15600 11540 7786.5698 76940 121440 15620 11520 7787.1132 76980 121520 15620 11500 7787.6438 77000 121600 15640 11500 7788.1744 77020 121640 15660 11500 7788.7181 77160 121880 15700 11520 7789.2619 77300 122160 15760 11580 7789.7927 77480 122460 15800 11620 7790.3237 77560 122600 15820 11600 7790.8677 77620 122740 15840 11620 7791.4117 77660 122860 15880 11600 7791.9429 77640 122820 15900 11600 7792.4741 77740 123040 15920 11620 7793.0184 77840 123220 15940 11620 7793.5498 77820 123200 15960 11640 7794.0813 77820 123240 15960 11640 7794.6258 77860 123340 16000 11620 7795.1704 77800 123280 15980 11640 7795.7021 77740 123220 16000 11640 7796.2339 77860 123420 16020 11680 7796.7788 77920 123600 16060 11700 7797.3237 77960 123660 16080 11680 7797.8687 78000 123760 16080 11700 7798.4007 78040 123860 16120 11700 7798.9329 78100 123960 16120 11680 7799.4781 78140 124120 16160 11700 7800.0104 78200 124220 16160 11720 7800.5428 78320 124420 16220 11720 7801.0883 78400 124600 16240 11720 7801.6338 78400 124640 16240 11740 7802.1794 78320 124540 16260 11720 7802.7121 78340 124600 16260 11720 7803.2449 78520 124900 16300 11740 7803.7907 78560 125040 16320 11740 7804.3237 78640 125160 16360 11760 7804.8567 78600 125140 16360 11760 7805.4028 78740 125400 16400 11820 7805.9489 79000 125800 16460 11860 7806.4951 79000 125900 16480 11880 7807.0285 78880 125680 16460 11880 7807.5748 78820 125640 16460 11840 7808.1213 78880 125760 16480 11860 7808.6549 78980 125940 16500 11860 7809.1885 78920 125900 16520 11900 7809.7222 78840 125780 16500 11860 7810.2689 78740 125660 16480 11840 7810.8158 78900 125940 16540 11860 7811.3627 78940 126060 16560 11880 7811.8967 79040 126200 16580 11880 7812.4308 79040 126280 16600 11900 7812.978 79120 126440 16640 11880 7813.5122 79320 126760 16680 11940 7814.0465 79360 126840 16700 11940 7814.5939 79380 126940 16720 11980 7815.1414 79400 126980 16740 11980 7815.6759 79280 126820 16720 11940 7816.2105 79300 126900 16740 11940 7816.7583 79440 127160 16780 11920 7817.3061 79380 127120 16780 11940 7817.8539 79440 127200 16820 11920 7818.4019 79560 127440 16840 11960 7818.9369 79580 127520 16880 11940 7819.472 79620 127580 16880 11960 7820.0071 79640 127640 16900 11980 7820.5423 79600 127620 16920 11980 7821.0907 79620 127680 16920 12000 7821.6391 79600 127660 16940 11960 7822.1876 79620 127760 16940 12000 7822.7362 79680 127860 16980 12020 7823.2718 79600 127780 16980 11980 7823.8075 79720 128000 17020 12020 7824.3433 79820 128200 17060 12040 7824.8791 79940 128400 17080 12040 7825.4281 79960 128480 17100 12080 7825.9771 79920 128460 17120 12040 7826.5263 79780 128260 17080 12020 7827.0624 79700 128160 17100 12000 7827.5986 79640 128100 17080 11960 7828.148 79620 128080 17100 11960 7828.6975 79620 128160 17120 12000 7829.247 79600 128120 17120 11960 7829.7835 79460 127960 17100 11960 7830.3201 79600 128200 17160 11960 7830.8568 79660 128320 17160 11980 7831.3936 79680 128400 17200 12000 7831.9435 79580 128240 17160 11980 7832.4935 79440 128080 17180 11960 7833.0436 79360 127920 17140 11980 7833.5937 79220 127780 17140 11960 7834.1309 79200 127740 17140 11960 7834.6681 79240 127860 17180 11960 7835.2185 79420 128200 17220 11980 7835.7559 79540 128400 17260 11980 7836.2933 79460 128260 17260 11980 7836.844 79080 127700 17180 11960 7837.3947 78640 127040 17100 11900 7837.9455 78580 126980 17100 11880 7838.4832 78960 127600 17200 11960 7839.0211 79160 127980 17280 11960 7839.5721 79280 128200 17300 11980 7840.1101 79320 128280 17320 11980 7840.6482 79340 128340 17340 11980 7841.1994 79140 128060 17320 11980 7841.7508 79140 128080 17320 11980 7842.3022 79280 128360 17380 12000 7842.8406 79320 128420 17400 11980 7843.3922 79380 128560 17420 12020 7843.9439 79380 128600 17440 11980 7844.4825 79360 128580 17460 12000 7845.0212 79320 128580 17460 12000 7845.5599 79300 128540 17480 11980 7846.1119 79340 128640 17500 11980 7846.664 79340 128680 17500 12020 7847.2161 79080 128320 17480 12000 7847.7552 78600 127540 17380 11900 7848.2944 78360 127200 17340 11860 7848.8467 78540 127500 17400 11880 7849.3992 78700 127820 17440 11940 7849.9386 78760 127940 17480 11940 7850.4781 78780 128000 17500 11940 7851.0308 78720 127920 17500 11940 7851.5835 78740 127980 17520 11940 7852.1232 78660 127900 17500 11900 7852.663 78540 127740 17500 11880 7853.216 78480 127660 17500 11860 7853.7691 78520 127760 17520 11900 7854.3091 78640 127980 17560 11940 7854.8492 78640 128040 17600 11940 7855.4026 78520 127840 17560 11920 7855.956 78420 127720 17560 11920 7856.4963 78400 127700 17580 11940 7857.0367 78400 127760 17600 11920 7857.5904 78380 127760 17600 11920 7858.1441 78280 127580 17580 11880 7858.6847 78200 127520 17600 11880 7859.2254 78220 127600 17620 11900 7859.7794 78280 127700 17660 11880 7860.3335 78140 127500 17640 11880 7860.8876 77980 127280 17620 11840 7861.4286 77980 127300 17620 11800 7861.9697 78060 127480 17680 11820 7862.5241 78140 127620 17700 11820 7863.0653 78060 127580 17720 11840 7863.6067 78100 127640 17720 11860 7864.1613 78080 127660 17760 11860 7864.716 77920 127420 17720 11840 7865.2708 77800 127260 17720 11820 7865.8124 77720 127180 17740 11820 7866.3541 77560 126920 17700 11760 7866.9091 77500 126860 17700 11740 7867.4642 77660 127160 17760 11780 7868.0062 77800 127400 17820 11840 7868.5482 77780 127420 17820 11840 7869.1036 77800 127460 17840 11840 7869.659 77680 127300 17840 11820 7870.2145 77620 127240 17840 11820 7870.7568 77620 127260 17840 11820 7871.2992 77600 127260 17880 11840 7871.855 77500 127120 17860 11820 7872.3976 77380 126940 17860 11800 7872.9402 77300 126840 17840 11820 7873.4962 77220 126740 17840 11780 7874.0523 77000 126440 17820 11740 7874.6084 76760 126060 17780 11700 7875.1646 76640 125920 17760 11680 7875.7077 76700 126000 17780 11660 7876.2508 76660 125980 17800 11660 7876.8073 76500 125760 17780 11660 7877.3505 76300 125460 17760 11640 7877.8939 76200 125320 17740 11640 7878.4506 76180 125320 17760 11640 7879.0074 76140 125260 17760 11620 7879.551 75960 125000 17740 11540 7880.0947 75860 124880 17740 11540 7880.6517 75780 124780 17720 11520 7881.2088 75700 124660 17720 11520 7881.766 75580 124500 17720 11520 7882.31 75460 124360 17700 11520 7882.8541 75440 124320 17720 11540 7883.3982 75440 124400 17720 11520 7883.9424 75540 124580 17780 11520 7884.5 75520 124520 17780 11520 7885.0577 75440 124500 17780 11500 7885.6154 75340 124340 17760 11460 7886.1733 75320 124300 17780 11480 7886.7179 75360 124440 17820 11460 7887.2626 75340 124420 17820 11500 7887.8074 75340 124440 17840 11520 7888.3522 75380 124560 17880 11540 7888.9104 75280 124420 17860 11540 7889.4688 75200 124300 17860 11500 7890.0272 75060 124100 17820 11480 7890.5856 74880 123840 17820 11460 7891.1309 74820 123760 17800 11440 7891.6762 74920 123960 17860 11500 7892.2216 74880 123920 17860 11460 7892.7804 74720 123700 17820 11420 7893.3393 74540 123420 17800 11360 7893.8849 74420 123240 17800 11380 7894.444 74400 123240 17800 11360 7895.0031 74360 123220 17800 11380 7895.5623 74300 123100 17800 11360 7896.1083 74240 123100 17820 11360 7896.6543 74280 123140 17820 11340 7897.2138 74180 123040 17840 11340 7897.76 74180 123080 17840 11340 7898.3062 74120 122960 17840 11340 7898.8526 73960 122780 17820 11340 7899.4124 73880 122620 17820 11320 7899.9722 73760 122480 17800 11300 7900.5188 73580 122220 17780 11260 7901.0788 73420 121960 17740 11260 7901.6389 73300 121820 17740 11260 7902.1857 73280 121860 17760 11260 7902.7327 73420 122080 17800 11280 7903.293 73380 122040 17820 11280 7903.8401 73260 121880 17800 11240 7904.4006 73200 121800 17800 11240 7904.9611 73060 121580 17760 11200 7905.5084 72960 121480 17780 11220 7906.0692 72860 121300 17760 11180 7906.6167 72660 121040 17720 11160 7907.1776 72580 120880 17720 11120 7907.7385 72600 120960 17740 11120 7908.2862 72620 121020 17760 11140 7908.834 72540 120920 17760 11140 7909.3819 72440 120760 17720 11160 7909.9432 72400 120740 17760 11120 7910.4912 72300 120620 17740 11100 7911.0527 72340 120700 17760 11080 7911.6143 72340 120760 17800 11100 7912.1625 72300 120700 17780 11060 7912.7242 72220 120580 17780 11080 7913.2727 72180 120580 17780 11080 7913.8212 72120 120460 17780 11060 7914.3831 72120 120500 17800 11040 7914.9452 72060 120460 17800 11020 7915.4939 72000 120400 17800 11060 7916.0427 71900 120240 17800 11060 7916.605 71760 120040 17760 11060 7917.1674 71740 120020 17780 11040 7917.7298 71680 119980 17780 11060 7918.279 71600 119840 17780 11000 7918.8282 71540 119800 17780 10960 7919.3909 71500 119740 17760 10980 7919.9402 71400 119600 17780 11000 7920.4897 71260 119420 17760 11000 7921.0526 71080 119100 17720 11000 7921.6157 70920 118900 17700 10960 7922.1788 71080 119200 17740 10940 7922.7285 71140 119320 17780 10980 7923.2784 71080 119240 17780 10940 7923.8418 71060 119220 17780 10940 7924.4052 71060 119220 17800 10940 7924.9553 70960 119160 17800 10940 7925.5055 70960 119140 17800 10940 7926.0691 70900 119120 17820 10940 7926.6329 70820 118980 17800 10920 7927.1967 70740 118900 17800 10880 7927.7472 70640 118760 17780 10880 7928.2978 70540 118620 17780 10880 7928.8619 70460 118520 17780 10900 7929.4261 70400 118420 17760 10860 7929.9769 70300 118300 17760 10840 7930.5278 70300 118340 17780 10840 7931.0922 70300 118360 17800 10820 7931.6567 70300 118360 17800 10840 7932.2078 70300 118400 17820 10840 7932.759 70380 118580 17860 10860 7933.3238 70420 118660 17860 10860 7933.8886 70420 118700 17900 10860 7934.4401 70380 118640 17880 10860 7934.9916 70360 118660 17900 10860 7935.5567 70400 118740 17940 10880 7936.1218 70340 118660 17920 10840 7936.6871 70280 118600 17920 10820 7937.2389 70240 118560 17920 10800 7937.7909 70100 118380 17900 10780 7938.3429 69940 118100 17880 10800 7938.895 69160 116840 17680 10700 7939.4741 68680 116040 17580 10600 7940.0398 69240 117040 17740 10680 7940.5922 69840 118060 17880 10720 7941.1446 70120 118540 17980 10760 7941.6971 70260 118860 18020 10840 7942.2631 70240 118800 18040 10860 7942.8158 70200 118800 18040 10840 7943.3685 70220 118820 18060 10860 7943.9348 70160 118760 18060 10840 7944.5012 70080 118680 18040 10820 7945.0677 70160 118820 18080 10820 7945.6208 70140 118820 18080 10840 7946.1739 70060 118680 18080 10820 7946.7406 69980 118600 18080 10800 7947.3074 69960 118580 18080 10820 7947.8608 70000 118680 18100 10800 7948.4143 70040 118800 18140 10820 7948.9813 70020 118780 18140 10840 7949.5485 70100 118920 18160 10840 7950.1157 70160 119060 18200 10880 7950.6695 70160 119120 18220 10880 7951.2233 70120 119040 18200 10840 7951.7908 70060 118980 18220 10840 7952.3583 70000 118920 18220 10820 7952.9125 70040 119000 18220 10820 7953.4666 70000 118980 18260 10820 7954.0344 69980 118960 18240 10800 7954.6023 69960 118920 18260 10820 7955.1703 69900 118900 18260 10820 7955.7248 69860 118820 18260 10800 7956.2794 69940 119000 18300 10840 7956.8476 69960 119080 18320 10820 7957.4024 69860 118900 18300 10820 7957.9572 69720 118680 18280 10820 7958.5256 69600 118560 18280 10800 7959.0807 69640 118620 18280 10800 7959.6493 69840 119000 18360 10820 7960.218 69940 119160 18400 10840 7960.7732 69940 119240 18400 10840 7961.3421 69980 119320 18440 10860 7961.911 70040 119440 18460 10860 7962.4665 70000 119400 18460 10860 7963.0221 70040 119480 18480 10880 7963.5913 69980 119440 18500 10840 7964.147 69880 119260 18460 10860 7964.7029 69880 119320 18500 10860 7965.2723 69960 119500 18520 10840 7965.8418 69960 119520 18540 10860 7966.4115 69860 119360 18520 10840 7966.9812 69760 119200 18520 10840 7967.5374 69740 119200 18500 10820 7968.0937 69780 119300 18540 10820 7968.6501 69820 119380 18560 10820 7969.2201 69820 119420 18580 10820 7969.7902 69760 119360 18580 10820 7970.3468 69700 119260 18580 10760 7970.9171 69600 119120 18560 10780 7971.4875 69580 119140 18560 10780 7972.0444 69560 119120 18580 10780 7972.6013 69540 119100 18580 10800 7973.1583 69480 119000 18580 10820 7973.7155 69480 119040 18580 10800 7974.2862 69640 119380 18660 10840 7974.8571 69820 119720 18720 10840 7975.4281 69900 119880 18740 10840 7975.9855 70060 120140 18800 10900 7976.543 69960 120040 18800 10880 7977.1142 69840 119840 18760 10860 7977.6855 69800 119800 18780 10860 7978.2433 69880 119960 18800 10860 7978.8011 69840 119920 18820 10880 7979.3726 69820 119940 18820 10860 7979.9443 69820 119960 18840 10860 7980.5024 69940 120200 18880 10900 7981.0605 70100 120500 18920 10920 7981.6324 70200 120680 18980 10920 7982.2044 70220 120740 19000 10920 7982.7764 70220 120780 19020 10920 7983.3349 70140 120680 19000 10940 7983.8935 70060 120560 19020 10900 7984.4658 69960 120420 18980 10900 7985.0381 69960 120420 19000 10900 7985.597 69940 120440 19020 10880 7986.1559 69920 120440 19020 10860 7986.7285 69860 120380 19020 10880 7987.2876 69820 120280 19020 10860 7987.8604 69720 120200 19040 10860 7988.4332 69640 120060 19000 10860 7988.9926 69620 120020 19040 10840 7989.5656 69700 120260 19060 10860 7990.1387 69820 120420 19100 10900 7990.6983 69860 120560 19140 10880 7991.2579 69780 120460 19140 10880 7991.8313 69760 120420 19140 10860 7992.3911 69800 120540 19180 10880 7992.951 69840 120640 19180 10900 7993.5246 69860 120700 19220 10900 7994.0984 69880 120740 19240 10940 7994.6722 69840 120700 19240 10940 7995.2324 69760 120600 19240 10900 7995.7927 69840 120760 19280 10880 7996.3667 69900 120900 19300 10940 7996.9272 69880 120880 19320 10960 7997.4877 69840 120880 19340 10940 7998.0621 69860 120880 19340 10960 7998.6364 69900 121020 19380 10940 7999.2109 70040 121300 19420 10940 7999.7718 70080 121340 19460 10940 8000.3327 70020 121320 19460 10940 8000.9075 70100 121420 19500 10960 8001.4823 70100 121520 19500 10960 8002.0435 70160 121620 19540 10980 8002.6048 70160 121660 19560 10980 8003.1798 70220 121760 19580 11000 8003.755 70260 121880 19620 11020 8004.3165 70180 121780 19600 11000 8004.8781 69980 121440 19580 10960 8005.4535 69900 121320 19560 10940 8006.029 69880 121340 19580 10920 8006.6046 69920 121440 19600 10920 8007.1665 70060 121700 19660 10960 8007.7286 70180 121920 19700 11020 8008.3044 70140 121900 19700 11000 8008.8666 70140 121900 19720 10960 8009.4289 70260 122180 19780 10960 8010.0049 70380 122420 19840 11040 8010.5811 70500 122620 19880 11060 8011.1574 70600 122860 19920 11060 8011.72 70720 123060 19980 11100 8012.2827 70760 123200 20000 11120 8012.8592 70920 123460 20060 11120 8013.422 70940 123540 20100 11120 8013.9849 71020 123740 20120 11140 8014.5617 71260 124140 20220 11160 8015.1385 71480 124580 20300 11220 8015.7017 71680 124940 20360 11220 8016.2787 71560 124800 20360 11240 8016.8696 71460 124600 20340 11200 8017.433 71560 124820 20380 11220 8017.9965 71600 124960 20420 11240 8018.5601 71600 124940 20440 11220 8019.1238 71520 124820 20420 11200 8019.7013 71380 124620 20400 11160 8020.2652 71380 124660 20420 11180 8020.8429 71380 124700 20440 11200 8021.4206 71340 124660 20440 11240 8021.9847 71400 124780 20480 11200 8022.5627 71520 125040 20540 11240 8023.1269 71640 125240 20560 11240 8023.6913 71740 125500 20640 11240 8024.2695 71760 125520 20660 11260 8024.834 71660 125380 20640 11240 8025.3986 71540 125180 20600 11240 8025.9908 71440 125060 20620 11240 8026.5693 71420 125040 20620 11220 8027.1342 71320 124900 20600 11240 8027.6991 71260 124780 20600 11200 8028.2641 71240 124840 20640 11180 8028.843 71380 125080 20660 11240 8029.422 71500 125340 20740 11240 8029.9872 71660 125640 20800 11280 8030.5526 71720 125780 20840 11300 8031.1318 71620 125620 20820 11260 8031.7111 71520 125480 20820 11220 8032.2905 71540 125540 20820 11260 8032.8562 71580 125660 20860 11280 8033.4219 71600 125700 20900 11260 8034.0016 71480 125540 20860 11260 8034.5813 71280 125220 20820 11200 8035.1473 71240 125180 20840 11220 8035.7134 71300 125320 20880 11240 8036.2934 71320 125400 20880 11200 8036.8734 71460 125660 20960 11240 8037.4536 71640 126000 21020 11260 8038.02 71620 126020 21040 11240 8038.5865 71480 125780 21020 11240 8039.1531 71340 125540 21000 11240 8039.7198 71180 125320 20960 11180 8040.3004 71140 125280 20960 11200 8040.8811 70940 124960 20920 11160 8041.4618 70200 123640 20720 11100 8042.0427 69580 122600 20560 10980 8042.6098 69440 122380 20540 10960 8043.1769 69900 123220 20680 10980 8043.758 70520 124400 20880 11080 8044.3254 71020 125260 21060 11180 8044.8928 71360 125880 21160 11240 8045.4742 71460 126100 21220 11240 8046.0556 71420 126080 21240 11240 8046.6233 71440 126100 21240 11240 8047.1911 71480 126220 21280 11300 8047.7728 71460 126240 21280 11280 8048.3545 71420 126180 21320 11240 8048.9364 71400 126160 21300 11260 8049.5184 71420 126220 21340 11260 8050.0865 71300 126060 21320 11240 8050.6548 71160 125820 21300 11220 8051.2232 70940 125460 21240 11200 8051.7916 70500 124700 21140 11120 8052.374 69640 123240 20900 10980 8052.9565 67720 119820 20320 10680 8053.539 63960 113140 19220 10100 8054.1217 59220 104740 17800 9380 8054.6905 55840 98840 16800 8880 8055.2595 55600 98500 16760 8800 8055.8424 58500 103680 17640 9240 8056.4115 62420 110720 18860 9860 8056.9807 65600 116380 19820 10340 8057.5638 67760 120180 20500 10700 8058.1471 69080 122560 20920 10920 8058.7165 69980 124160 21200 11020 8059.286 70660 125400 21420 11140 8059.8695 71260 126520 21640 11260 8060.4531 71740 127320 21780 11340 8061.0229 72000 127860 21900 11380 8061.5928 72060 128000 21920 11400 8062.1766 72220 128320 22000 11480 8062.7605 72340 128560 22060 11500 8063.3307 72240 128420 22040 11500 8063.9009 72100 128220 22020 11460 8064.4851 72020 128060 22020 11400 8065.0693 71820 127760 21980 11360 8065.6537 71760 127700 21980 11320 8066.2242 71400 127060 21880 11260 8066.7949 70120 124800 21500 11140 8067.3795 68960 122740 21160 10960 8067.9642 69620 124020 21400 11060 8068.5351 71000 126500 21820 11240 8069.106 71720 127820 22080 11340 8069.691 72020 128400 22200 11400 8070.2761 72140 128600 22240 11440 8070.8612 72080 128520 22240 11440 8071.4325 72040 128500 22260 11440 8072.0039 71960 128360 22240 11400 8072.5893 71920 128360 22260 11420 8073.1609 71900 128340 22260 11420 8073.7325 71900 128340 22280 11380 8074.3182 72000 128560 22320 11400 8074.89 72080 128760 22380 11400 8075.4619 72180 128920 22420 11400 8076.0478 72400 129380 22520 11440 8076.6338 72600 129780 22600 11520 8077.2199 72640 129840 22620 11500 8077.8061 72580 129780 22620 11520 8078.3784 72520 129700 22620 11520 8078.9508 72360 129480 22600 11460 8079.5233 72280 129320 22580 11420 8080.0958 72160 129180 22560 11460 8080.6824 72020 128940 22540 11460 8081.2692 71320 127680 22320 11380 8081.8559 69620 124660 21840 11120 8082.4428 68920 123460 21620 10980 8083.0158 70180 125780 22020 11120 8083.5889 71580 128280 22480 11360 8084.1621 72320 129680 22760 11480 8084.7353 72680 130300 22860 11560 8085.3226 72740 130440 22900 11580 8085.91 72680 130360 22900 11580 8086.4975 72560 130200 22900 11560 8087.0851 72480 130080 22860 11560 8087.6588 72480 130100 22900 11540 8088.2325 72640 130400 22960 11560 8088.8203 72700 130580 23000 11560 8089.4083 72740 130620 23020 11620 8089.9823 72700 130600 23020 11580 8090.5564 72520 130320 23000 11500 8091.1446 72400 130120 22960 11480 8091.7328 72380 130100 22980 11520 8092.3072 72460 130280 23020 11540 8092.8816 72600 130600 23080 11580 8093.4702 72740 130840 23140 11600 8094.0588 72740 130900 23160 11660 8094.6335 72820 131080 23180 11680 8095.2083 72760 131000 23200 11620 8095.7971 72680 130880 23180 11600 8096.3861 72680 130940 23220 11580 8096.9611 72620 130840 23200 11600 8097.5363 72480 130620 23160 11540 8098.1255 72360 130440 23160 11520 8098.7148 72360 130500 23160 11540 8099.3042 72440 130640 23200 11580 8099.8797 72480 130720 23240 11580 8100.4552 72340 130560 23200 11520 8101.0449 72360 130580 23240 11540 8101.6347 72500 130880 23280 11560 8102.2105 72640 131140 23360 11640 8102.7864 72680 131240 23360 11600 8103.3764 72620 131160 23380 11580 8103.9665 72500 131000 23380 11560 8104.5426 72460 130920 23340 11540 8105.1189 72520 131080 23400 11580 8105.7092 72600 131280 23440 11580 8106.2997 72640 131340 23460 11620 8106.8762 72620 131340 23480 11600 8107.4528 72640 131420 23500 11560 8108.0294 72660 131500 23540 11580 8108.6202 72660 131500 23540 11540 8109.2111 72620 131480 23560 11580 8109.788 72620 131540 23560 11580 8110.3791 72740 131740 23640 11580 8110.9703 72860 132020 23680 11620 8111.5615 72960 132200 23740 11660 8112.1388 72940 132220 23740 11640 8112.7161 72880 132160 23760 11640 8113.2936 72980 132340 23780 11620 8113.8852 73080 132560 23860 11640 8114.4769 73080 132620 23860 11660 8115.0546 73180 132760 23920 11680 8115.6464 73260 133000 23960 11740 8116.2384 73300 133080 24000 11720 8116.8163 73320 133160 24020 11700 8117.3944 73220 132960 24000 11680 8117.9725 73200 133000 24020 11660 8118.5507 73340 133260 24080 11700 8119.1431 73580 133720 24160 11720 8119.7355 73680 133920 24240 11760 8120.3281 73560 133720 24200 11760 8120.9208 73380 133460 24160 11740 8121.4994 73260 133260 24140 11720 8122.0923 73280 133340 24180 11700 8122.6852 73420 133600 24240 11740 8123.25 73500 133780 24280 11780 8123.8289 73620 134040 24340 11800 8124.4221 73700 134200 24380 11820 8125.0154 73640 134160 24380 11840 8125.6088 73660 134200 24420 11780 8126.1881 73600 134140 24400 11800 8126.7816 73600 134160 24440 11780 8127.3753 73660 134320 24460 11800 8127.9548 73700 134400 24500 11820 8128.5345 73700 134400 24520 11800 8129.1143 73680 134440 24540 11840 8129.7083 73740 134560 24560 11820 8130.3023 73800 134700 24600 11820 8130.8823 73860 134860 24640 11820 8131.4624 73880 134900 24680 11840 8132.0568 73920 135020 24700 11840 8132.6512 73980 135160 24740 11860 8133.2457 74060 135280 24780 11860 8133.8403 74200 135640 24840 11900 8134.4209 74360 135920 24940 11960 8134.9873 74420 136060 24960 11960 8135.568 74460 136160 24980 12000 8136.163 74540 136360 25060 11980 8136.758 74560 136460 25080 11960 8137.339 74600 136540 25100 11960 8137.9342 74580 136560 25120 11960 8138.5295 74460 136400 25100 11960 8139.1108 74400 136320 25100 11960 8139.7063 74380 136300 25120 11960 8140.2877 74260 136100 25080 11920 8140.8691 74040 135740 25020 11960 8141.4649 73880 135460 25000 11880 8142.0608 73840 135460 25000 11880 8142.6567 73920 135620 25040 11920 8143.2385 73960 135720 25080 11900 8143.8204 73900 135640 25080 11920 8144.4167 73940 135760 25100 11880 8145.0129 73980 135860 25140 11860 8145.6093 73980 135900 25160 11900 8146.1916 73920 135800 25160 11900 8146.774 73860 135780 25160 11900 8147.3564 73840 135720 25160 11880 8147.9389 73840 135760 25200 11860 8148.5357 73720 135580 25180 11820 8149.1327 73560 135320 25140 11800 8149.7297 73520 135260 25140 11820 8150.3268 73480 135220 25160 11820 8150.9097 73460 135220 25160 11820 8151.4928 73400 135100 25140 11800 8152.0759 73320 134980 25140 11780 8152.6591 73260 134900 25140 11780 8153.2567 73320 135040 25200 11780 8153.8543 73380 135180 25220 11840 8154.452 73380 135200 25240 11840 8155.0498 73380 135260 25260 11840 8155.6335 73340 135160 25260 11800 8156.2173 73340 135240 25280 11800 8156.8153 73420 135380 25320 11820 8157.3993 73380 135360 25340 11800 8157.9833 73480 135580 25400 11800 8158.5816 73700 136000 25480 11860 8159.18 73880 136340 25560 11940 8159.7643 73860 136380 25600 11960 8160.3487 73880 136400 25600 11920 8160.9474 73840 136380 25620 11920 8161.5462 73860 136460 25660 11960 8162.145 73880 136500 25680 11920 8162.7298 73860 136520 25680 11960 8163.3146 73820 136440 25700 11940 8163.9137 73900 136640 25720 11920 8164.4987 73940 136780 25780 11920 8165.0837 74020 136960 25820 11960 8165.6832 73940 136820 25820 11960 8166.2827 73940 136860 25820 11980 8166.8823 73980 136980 25880 11980 8167.482 74080 137180 25920 11960 8168.0675 74080 137200 25960 11980 8168.653 74040 137140 25940 11980 8169.253 73900 136960 25920 11960 8169.8388 73760 136700 25880 11920 8170.4246 73640 136500 25860 11920 8171.0248 73540 136400 25860 11920 8171.6252 73560 136440 25880 11900 8172.2256 73560 136440 25900 11860 8172.8118 73500 136400 25900 11860 8173.3981 73480 136340 25900 11840 8173.9987 73480 136420 25940 11900 8174.5852 73420 136340 25940 11860 8175.1717 73400 136320 25960 11860 8175.7727 73420 136380 25980 11840 8176.3737 73460 136480 26000 11880 8176.9605 73440 136500 26040 11900 8177.5474 73380 136440 26020 11900 8178.1488 73100 135880 25940 11860 8178.7501 71960 133840 25560 11680 8179.3373 70660 131440 25120 11480 8179.9246 71220 132540 25360 11560 8180.5262 72560 135040 25820 11760 8181.128 73180 136280 26100 11880 8181.7298 73440 136740 26200 11900 8182.3175 73600 137060 26280 11920 8182.9051 73640 137180 26300 11940 8183.5073 73600 137140 26320 11900 8184.1095 73660 137300 26380 11920 8184.7118 73760 137500 26420 11960 8185.2998 73780 137560 26440 11980 8185.888 73720 137460 26460 11940 8186.4762 73620 137340 26440 11960 8187.0789 73560 137200 26420 11960 8187.6816 73560 137280 26440 11960 8188.2701 73560 137320 26480 11960 8188.873 73560 137320 26500 11900 8189.4761 73660 137540 26540 11920 8190.0648 73680 137640 26580 11900 8190.6537 73720 137720 26620 11940