I don't think there is much published on that, so it is worth trying and see what you get.
Anatoly
 
-----Original Message-----
From: ifeffit-bounces@millenia.cars.aps.anl.gov [mailto:ifeffit-bounces@millenia.cars.aps.anl.gov]On Behalf Of Debora Meira
Sent: Friday, April 17, 2009 10:23 AM
To: ifeffit@millenia.cars.aps.anl.gov
Subject: [Ifeffit] Multiple data set fit

Dear all,
I'd like to know a reference that has multiple set data fit as a function of temperature in nanoparticles. Is the relation of Debye Waller factor (s2 = ss2 + sd2) valid for the higher shells? In particular, can I use the Einstein model for sd2
 
Thanks in advance, Débora