# data : Fe, using Feff standard # chi: from skey ASCII of newfe.b # using simple minimization # e0 = 7110.98; pre-edge range =[ -200.0 -50.0]; edge step = 2.108 # k range=[ 1.00 17.60]; k weight= 1.00; sills dk1, dk2 = 0.00 0.00 # bkg r =[ 0.00 0.98]; 11 knots in spline # inpdat: no document line found # ---------------------------------------------------------------------- # k chi(k) 0.5000000E-01 0.0000000E+00 0.1000000E+00 0.0000000E+00 0.1500000E+00 0.0000000E+00 0.2000000E+00 0.0000000E+00 0.2500000E+00 0.0000000E+00 0.3000000E+00 0.0000000E+00 0.3500000E+00 0.0000000E+00 0.4000000E+00 0.0000000E+00 0.4500000E+00 0.0000000E+00 0.5000000E+00 0.0000000E+00 0.5500000E+00 0.0000000E+00 0.6000000E+00 0.0000000E+00 0.6500000E+00 0.0000000E+00 0.7000000E+00 0.0000000E+00 0.7500000E+00 0.0000000E+00 0.8000000E+00 0.0000000E+00 0.8500000E+00 0.0000000E+00 0.9000000E+00 0.0000000E+00 0.9500000E+00 0.5655127E-01 0.1000000E+01 0.2060084E+00 0.1050000E+01 0.2808007E+00 0.1100000E+01 0.2122846E+00 0.1150000E+01 0.1469233E+00 0.1200000E+01 0.8558236E-01 0.1250000E+01 0.3885868E-01 0.1300000E+01 -.3205625E-02 0.1350000E+01 -.2988494E-01 0.1400000E+01 -.5032800E-01 0.1450000E+01 -.6352721E-01 0.1500000E+01 -.6917974E-01 0.1550000E+01 -.6984850E-01 0.1600000E+01 -.6646661E-01 0.1650000E+01 -.6563130E-01 0.1700000E+01 -.6711814E-01 0.1750000E+01 -.6834159E-01 0.1800000E+01 -.6921581E-01 0.1850000E+01 -.6814639E-01 0.1900000E+01 -.6501906E-01 0.1950000E+01 -.5765744E-01 0.2000000E+01 -.4453135E-01 0.2050000E+01 -.2401327E-01 0.2100000E+01 0.7335357E-02 0.2150000E+01 0.4488946E-01 0.2200000E+01 0.7977872E-01 0.2250000E+01 0.9853840E-01 0.2300000E+01 0.9232492E-01 0.2350000E+01 0.6178783E-01 0.2400000E+01 0.2341145E-01 0.2450000E+01 -.1390825E-01 0.2500000E+01 -.3846206E-01 0.2550000E+01 -.5195529E-01 0.2600000E+01 -.5546389E-01 0.2650000E+01 -.4779275E-01 0.2700000E+01 -.3509258E-01 0.2750000E+01 -.2234229E-01 0.2800000E+01 -.1596326E-01 0.2850000E+01 -.1899550E-01 0.2900000E+01 -.2327369E-01 0.2950000E+01 -.2792808E-01 0.3000000E+01 -.2152839E-01 0.3050000E+01 -.8976581E-02 0.3100000E+01 0.9856174E-02 0.3150000E+01 0.2660002E-01 0.3200000E+01 0.3893804E-01 0.3250000E+01 0.4660523E-01 0.3300000E+01 0.5051752E-01 0.3350000E+01 0.5078438E-01 0.3400000E+01 0.4720417E-01 0.3450000E+01 0.4192519E-01 0.3500000E+01 0.3830658E-01 0.3550000E+01 0.3661301E-01 0.3600000E+01 0.3510318E-01 0.3650000E+01 0.3195203E-01 0.3700000E+01 0.2673356E-01 0.3750000E+01 0.2157586E-01 0.3800000E+01 0.1734317E-01 0.3850000E+01 0.1420028E-01 0.3900000E+01 0.1007945E-01 0.3950000E+01 0.3650033E-02 0.4000000E+01 -.5376017E-02 0.4050000E+01 -.1947654E-01 0.4100000E+01 -.3440827E-01 0.4150000E+01 -.5013820E-01 0.4200000E+01 -.6089725E-01 0.4250000E+01 -.6645940E-01 0.4300000E+01 -.6661560E-01 0.4350000E+01 -.6047763E-01 0.4400000E+01 -.5072961E-01 0.4450000E+01 -.3719363E-01 0.4500000E+01 -.1978667E-01 0.4550000E+01 -.1746187E-02 0.4600000E+01 0.1679161E-01 0.4650000E+01 0.2691962E-01 0.4700000E+01 0.2806893E-01 0.4750000E+01 0.2038168E-01 0.4800000E+01 0.3018849E-02 0.4850000E+01 -.1650919E-01 0.4900000E+01 -.3837207E-01 0.4950000E+01 -.5877454E-01 0.5000000E+01 -.7065932E-01 0.5050000E+01 -.7365970E-01 0.5100000E+01 -.4566274E-01 0.5150000E+01 -.5775657E-02 0.5200000E+01 0.4637155E-01 0.5250000E+01 0.1188507E+00 0.5300000E+01 0.1364345E+00 0.5350000E+01 0.1535101E+00 0.5400000E+01 0.1421802E+00 0.5450000E+01 0.1174440E+00 0.5500000E+01 0.8106687E-01 0.5550000E+01 0.3828398E-01 0.5600000E+01 -.2915186E-02 0.5650000E+01 -.4199471E-01 0.5700000E+01 -.6625038E-01 0.5750000E+01 -.8051391E-01 0.5800000E+01 -.8474813E-01 0.5850000E+01 -.7489974E-01 0.5900000E+01 -.6144758E-01 0.5950000E+01 -.4510938E-01 0.6000000E+01 -.3562258E-01 0.6050000E+01 -.3317802E-01 0.6100000E+01 -.3701793E-01 0.6150000E+01 -.4274058E-01 0.6200000E+01 -.4226617E-01 0.6250000E+01 -.3624063E-01 0.6300000E+01 -.2621241E-01 0.6350000E+01 -.1714197E-01 0.6400000E+01 -.8579194E-02 0.6450000E+01 0.5889795E-02 0.6500000E+01 0.2112563E-01 0.6550000E+01 0.3640528E-01 0.6600000E+01 0.4407941E-01 0.6650000E+01 0.5381595E-01 0.6700000E+01 0.6523077E-01 0.6750000E+01 0.7810715E-01 0.6800000E+01 0.8461104E-01 0.6850000E+01 0.8472789E-01 0.6900000E+01 0.6481350E-01 0.6950000E+01 0.4050279E-01 0.7000000E+01 0.1361891E-01 0.7050000E+01 -.7456295E-02 0.7100000E+01 -.2335217E-01 0.7150000E+01 -.3496600E-01 0.7200000E+01 -.3856641E-01 0.7250000E+01 -.3877619E-01 0.7300000E+01 -.3681451E-01 0.7350000E+01 -.3596700E-01 0.7400000E+01 -.3518155E-01 0.7450000E+01 -.3437710E-01 0.7500000E+01 -.3310297E-01 0.7550000E+01 -.3291784E-01 0.7600000E+01 -.3388389E-01 0.7650000E+01 -.3860017E-01 0.7700000E+01 -.4055087E-01 0.7750000E+01 -.3946792E-01 0.7800000E+01 -.2831430E-01 0.7850000E+01 -.1267608E-01 0.7900000E+01 0.5823306E-02 0.7950000E+01 0.2277069E-01 0.8000000E+01 0.3800438E-01 0.8050000E+01 0.5176166E-01 0.8100000E+01 0.6261042E-01 0.8150000E+01 0.6892227E-01 0.8200000E+01 0.7097669E-01 0.8250000E+01 0.6260683E-01 0.8300000E+01 0.4178878E-01 0.8350000E+01 0.1626553E-01 0.8400000E+01 -.6038480E-02 0.8450000E+01 -.2388303E-01 0.8500000E+01 -.3694926E-01 0.8550000E+01 -.3524959E-01 0.8600000E+01 -.3015273E-01 0.8650000E+01 -.2355439E-01 0.8700000E+01 -.2037353E-01 0.8750000E+01 -.1821713E-01 0.8800000E+01 -.1653979E-01 0.8850000E+01 -.1375826E-01 0.8900000E+01 -.1138593E-01 0.8950000E+01 -.9640670E-02 0.9000000E+01 -.1064719E-01 0.9050000E+01 -.1333986E-01 0.9100000E+01 -.1657897E-01 0.9150000E+01 -.1563255E-01 0.9200000E+01 -.1256403E-01 0.9250000E+01 -.7546475E-02 0.9300000E+01 0.2051769E-02 0.9350000E+01 0.1206484E-01 0.9400000E+01 0.2186381E-01 0.9450000E+01 0.2696188E-01 0.9500000E+01 0.2956321E-01 0.9550000E+01 0.3024703E-01 0.9600000E+01 0.2829097E-01 0.9650000E+01 0.2347386E-01 0.9700000E+01 0.1677168E-01 0.9750000E+01 0.9652683E-02 0.9800000E+01 0.4160130E-02 0.9850000E+01 -.3509654E-03 0.9900000E+01 -.5822503E-02 0.9950000E+01 -.1127272E-01 0.1000000E+02 -.1622435E-01 0.1005000E+02 -.1683732E-01 0.1010000E+02 -.1495159E-01 0.1015000E+02 -.1141029E-01 0.1020000E+02 -.8467363E-02 0.1025000E+02 -.7214359E-02 0.1030000E+02 -.7081313E-02 0.1035000E+02 -.6969263E-02 0.1040000E+02 -.6049700E-02 0.1045000E+02 -.4485105E-02 0.1050000E+02 -.1890426E-02 0.1055000E+02 -.4006150E-03 0.1060000E+02 0.2384959E-03 0.1065000E+02 0.4834935E-04 0.1070000E+02 0.5550277E-03 0.1075000E+02 0.1837278E-02 0.1080000E+02 0.5715432E-02 0.1085000E+02 0.9587295E-02 0.1090000E+02 0.1308050E-01 0.1095000E+02 0.1318570E-01 0.1100000E+02 0.1114541E-01 0.1105000E+02 0.7585354E-02 0.1110000E+02 0.2712361E-02 0.1115000E+02 -.6231128E-03 0.1120000E+02 -.2699086E-02 0.1125000E+02 -.2748458E-02 0.1130000E+02 -.2100015E-02 0.1135000E+02 -.1248769E-02 0.1140000E+02 -.1850160E-02 0.1145000E+02 -.3015104E-02 0.1150000E+02 -.4079884E-02 0.1155000E+02 -.3113230E-02 0.1160000E+02 -.1657446E-02 0.1165000E+02 -.2912073E-03 0.1170000E+02 -.4868633E-03 0.1175000E+02 -.1869108E-02 0.1180000E+02 -.3666880E-02 0.1185000E+02 -.5012533E-02 0.1190000E+02 -.5430240E-02 0.1195000E+02 -.5244704E-02 0.1200000E+02 -.4244526E-02 0.1205000E+02 -.2583137E-02 0.1210000E+02 -.5613900E-03 0.1215000E+02 0.1682533E-02 0.1220000E+02 0.3550175E-02 0.1225000E+02 0.4962454E-02 0.1230000E+02 0.5145181E-02 0.1235000E+02 0.4521211E-02 0.1240000E+02 0.3616649E-02 0.1245000E+02 0.3025508E-02 0.1250000E+02 0.2215167E-02 0.1255000E+02 0.1239767E-02 0.1260000E+02 -.2847800E-04 0.1265000E+02 -.8736346E-03 0.1270000E+02 -.1316044E-02 0.1275000E+02 -.8352873E-03 0.1280000E+02 -.6000087E-03 0.1285000E+02 -.4739623E-03 0.1290000E+02 -.3565089E-03 0.1295000E+02 -.4024917E-03 0.1300000E+02 -.4363919E-03 0.1305000E+02 -.3624008E-03 0.1310000E+02 -.7849469E-03 0.1315000E+02 -.1377900E-02 0.1320000E+02 -.1829544E-02 0.1325000E+02 -.1978357E-02 0.1330000E+02 -.1991908E-02 0.1335000E+02 -.1994725E-02 0.1340000E+02 -.1674267E-02 0.1345000E+02 -.1130186E-02 0.1350000E+02 -.2546223E-03 0.1355000E+02 0.3457512E-03 0.1360000E+02 0.7712489E-03 0.1365000E+02 0.9736323E-03 0.1370000E+02 0.1358593E-02 0.1375000E+02 0.1724298E-02 0.1380000E+02 0.1785105E-02 0.1385000E+02 0.1780056E-02 0.1390000E+02 0.1757546E-02 0.1395000E+02 0.1751808E-02 0.1400000E+02 0.1557674E-02 0.1405000E+02 0.1208145E-02 0.1410000E+02 0.5929779E-03 0.1415000E+02 0.1590665E-04 0.1420000E+02 -.4447771E-03 0.1425000E+02 -.6156127E-03 0.1430000E+02 -.8032330E-03 0.1435000E+02 -.1024020E-02 0.1440000E+02 -.1324153E-02 0.1445000E+02 -.1426800E-02 0.1450000E+02 -.1421690E-02 0.1455000E+02 -.1298981E-02 0.1460000E+02 -.1064565E-02 0.1465000E+02 -.8379684E-03 0.1470000E+02 -.7302711E-03 0.1475000E+02 -.4886224E-03 0.1480000E+02 -.1990857E-03 0.1485000E+02 0.1052605E-03 0.1490000E+02 0.1942373E-03 0.1495000E+02 0.2691299E-03 0.1500000E+02 0.5241699E-03 0.1505000E+02 0.8470850E-03 0.1510000E+02 0.1166101E-02 0.1515000E+02 0.1410443E-02 0.1520000E+02 0.1331813E-02 0.1525000E+02 0.1170310E-02 0.1530000E+02 0.1064512E-02 0.1535000E+02 0.1075089E-02 0.1540000E+02 0.1058487E-02 0.1545000E+02 0.8618844E-03 0.1550000E+02 0.6286561E-03 0.1555000E+02 0.3808540E-03 0.1560000E+02 0.1252981E-03 0.1565000E+02 -.6006536E-05 0.1570000E+02 -.1575533E-03 0.1575000E+02 -.4507753E-03 0.1580000E+02 -.7327566E-03 0.1585000E+02 -.9702140E-03 0.1590000E+02 -.1102900E-02 0.1595000E+02 -.1169751E-02 0.1600000E+02 -.1133195E-02 0.1605000E+02 -.8941141E-03 0.1610000E+02 -.5937479E-03 0.1615000E+02 -.3343632E-03 0.1620000E+02 -.1908709E-03 0.1625000E+02 -.2359518E-03 0.1630000E+02 -.2929784E-03 0.1635000E+02 -.2980764E-03 0.1640000E+02 -.1112639E-03 0.1645000E+02 0.7653150E-04 0.1650000E+02 0.2066564E-03 0.1655000E+02 0.1606287E-03 0.1660000E+02 0.1655405E-03 0.1665000E+02 0.2988958E-03 0.1670000E+02 0.1807189E-03 0.1675000E+02 0.7222002E-04 0.1680000E+02 0.3070354E-04 0.1685000E+02 -.4413221E-06 0.1690000E+02 -.2450598E-04 0.1695000E+02 -.3979294E-04 0.1700000E+02 -.6977463E-04 0.1705000E+02 -.1955277E-03 0.1710000E+02 -.4606000E-03 0.1715000E+02 -.3961522E-03 0.1720000E+02 -.3095174E-03 0.1725000E+02 -.2382947E-03 0.1730000E+02 -.1022920E-03 0.1735000E+02 0.3222296E-04 0.1740000E+02 0.1552839E-03 0.1745000E+02 0.3968782E-03 0.1750000E+02 0.5713292E-03 0.1755000E+02 0.6374749E-03