Hi Paul,
normally I use BN and I leave it in the dry box.
I prepare these bags outside the glovebox.  I seal them on the sides to place the pellet more easily and seal the open side inside the glovebox.
I do not enjoy the glovebox time, so I prefer to prepare all I can outside and minimize the time working there. 
Best regards.


81f89be0-980e-4247-92dc-2bdc07d970ba.jpg





On Thu, Feb 27, 2025 at 10:57 AM Paul Aronstein via Ifeffit <ifeffit@millenia.cars.aps.anl.gov> wrote:
Hello, I'm looking for some advice on binder alternatives for preparing either pellets or packed powder samples in a dry glovebox. Please also note if the binder requires preparation (i. e. desiccated prior to use, etc) or if there are other
ZjQcmQRYFpfptBannerStart
This Message Is From an External Sender
This message came from outside your organization.
 
ZjQcmQRYFpfptBannerEnd
Hello,
I'm looking for some advice on binder alternatives for preparing either pellets or packed powder samples in a dry glovebox. Please also note if the binder requires preparation (i.e. desiccated prior to use, etc) or if there are other considerations.

Thank you,