#S 6328 quickScanPosCapture oh_dcm_energy 8800 10000 1000 300 -1 #U sicilia #D 1360110339 #C Acquisition started at Wed Feb 6 1:25:39 2013 #N 14 #L Pt_No energyc eh_ic1_l eh_ic1_r eh_ic1_3 eh_ic1_4 eh_ic2_l eh_ic2_r eh_ic3_l eh_ic3_r adlink2005_ai_ch0 adlink2005_ai_ch1 adlink2005_ai_ch2 adlink2005_ai_ch3 1 8799.690839 -3.50E-12 2.49E-06 -2.51E-06 1.03E-10 2.03E-06 2.19E-06 1.47E-10 1.24E-10 -2.389584351 2.386724854 2.038369751 2.187765503 2 8799.684178 -8.05E-11 2.50E-06 -2.51E-06 8.65E-11 2.03E-06 2.19E-06 1.47E-10 1.24E-10 -2.387011719 2.383355713 2.035446167 2.184805298 3 8799.874013 -9.70E-11 2.49E-06 -2.51E-06 5.90E-11 2.03E-06 2.19E-06 1.47E-10 1.24E-10 -2.382150269 2.37611084 2.031619263 2.180517578 4 8800.170439 -2.00E-11 2.50E-06 -2.51E-06 4.80E-11 2.03E-06 2.19E-06 1.47E-10 1.23E-10 -2.389096069 2.386462402 2.038613892 2.188284302 5 8800.470216 2.95E-11 2.49E-06 -2.51E-06 5.35E-11 2.03E-06 2.19E-06 1.47E-10 1.23E-10 -2.386807251 2.382171631 2.036459351 2.185583496 6 8800.78667 3.50E-11 2.50E-06 -2.51E-06 6.45E-11 2.03E-06 2.19E-06 1.47E-10 1.23E-10 -2.388363647 2.384265137 2.039102173 2.188247681 7 8801.123137 3.50E-11 2.50E-06 -2.51E-06 3.70E-11 2.03E-06 2.20E-06 1.47E-10 1.23E-10 -2.390118408 2.385974121 2.041116333 2.190515137 8 8801.482952 -4.20E-11 2.50E-06 -2.51E-06 3.70E-11 2.03E-06 2.20E-06 1.48E-10 1.24E-10 -2.388937378 2.384899902 2.040750122 2.189862061 9 8801.892778 -1.41E-10 2.49E-06 -2.51E-06 1.20E-10 2.03E-06 2.20E-06 1.48E-10 1.24E-10 -2.38687439 2.381811523 2.040338135 2.188897705 10 8802.68922 4.05E-11 2.50E-06 -2.51E-06 1.14E-10 2.03E-06 2.20E-06 1.48E-10 1.24E-10 -2.387689209 2.383169556 2.042047119 2.190689087 11 8803.695813 2.00E-12 2.50E-06 -2.51E-06 7.00E-11 2.03E-06 2.20E-06 1.48E-10 1.24E-10 -2.389224243 2.385641479 2.045709229 2.194784546 12 8804.705977 -2.00E-11 2.49E-06 -2.51E-06 6.45E-11 2.03E-06 2.20E-06 1.48E-10 1.24E-10 -2.384381104 2.378942871 2.042901611 2.191287231 13 8805.719714 -5.85E-11 2.50E-06 -2.51E-06 5.35E-11 2.03E-06 2.20E-06 1.48E-10 1.25E-10 -2.387582397 2.3840271 2.047915649 2.196640015 14 8806.737027 -1.80E-10 2.49E-06 -2.51E-06 3.70E-11 2.04E-06 2.20E-06 1.48E-10 1.25E-10 -2.388308716 2.385491943 2.049234009 2.198474121 15 8807.764591 -9.70E-11 2.49E-06 -2.51E-06 3.15E-11 2.04E-06 2.20E-06 1.48E-10 1.25E-10 -2.386062622 2.380795288 2.04831543 2.197784424 16 8808.792401 -1.45E-11 2.49E-06 -2.51E-06 1.25E-10 2.04E-06 2.21E-06 1.49E-10 1.25E-10 -2.388287354 2.385357666 2.052593994 2.202163696 17 8809.823795 -2.24E-10 2.49E-06 -2.51E-06 5.90E-11 2.04E-06 2.21E-06 1.48E-10 1.25E-10 -2.386697388 2.382925415 2.052438354 2.201644897 18 8810.862116 2.40E-11 2.49E-06 -2.51E-06 9.20E-11 2.04E-06 2.21E-06 1.49E-10 1.25E-10 -2.38364563 2.378561401 2.050750732 2.200158691 19 8811.880648 -3.10E-11 2.49E-06 -2.50E-06 4.80E-11 2.04E-06 2.21E-06 1.49E-10 1.25E-10 -2.379559326 2.375747681 2.048730469 2.197817993 20 8812.912785 -1.03E-10 2.44E-06 -2.46E-06 1.14E-10 2.04E-06 2.20E-06 1.48E-10 1.25E-10 -2.33196106 2.327627563 2.008956909 2.155007935 21 8813.951854 2.40E-11 2.48E-06 -2.49E-06 3.70E-11 2.03E-06 2.20E-06 1.48E-10 1.25E-10 -2.381216431 2.376190186 2.052514648 2.201931763 22 8814.977804 4.60E-11 2.49E-06 -2.51E-06 2.60E-11 2.03E-06 2.20E-06 1.48E-10 1.25E-10 -2.386776733 2.381713867 2.0597229 2.209231567 23 8816.010686 7.50E-12 2.50E-06 -2.51E-06 1.03E-10 2.03E-06 2.20E-06 1.48E-10 1.25E-10 -2.390002441 2.387744141 2.064746094 2.21477356 24 8817.060536 5.70E-11 2.49E-06 -2.51E-06 1.50E-11 2.05E-06 2.21E-06 1.49E-10 1.26E-10 -2.388400269 2.38487854 2.064306641 2.214407349 25 8818.090575 -9.00E-12 2.49E-06 -2.51E-06 1.14E-10 2.05E-06 2.22E-06 1.50E-10 1.26E-10 -2.387625122 2.383847046 2.065200806 2.215261841 26 8819.124206 -2.00E-11 2.50E-06 -2.51E-06 3.70E-11 2.05E-06 2.22E-06 1.50E-10 1.26E-10 -2.387930298 2.384481812 2.067315674 2.217547607 27 8820.174817 -7.50E-11 2.49E-06 -2.51E-06 -3.45E-11 2.05E-06 2.22E-06 1.50E-10 1.26E-10 -2.385739136 2.380584717 2.066424561 2.216894531 28 8821.215644 -1.52E-10 2.50E-06 -2.51E-06 5.35E-11 2.06E-06 2.23E-06 1.50E-10 1.27E-10 -2.386856079 2.382519531 2.069451904 2.219781494 29 8822.246679 1.30E-11 2.49E-06 -2.51E-06 5.90E-11 2.06E-06 2.23E-06 1.50E-10 1.27E-10 -2.387057495 2.383337402 2.071325684 2.22175293 30 8823.291357 2.00E-12 2.49E-06 -2.51E-06 1.03E-10 2.06E-06 2.23E-06 1.51E-10 1.27E-10 -2.383825684 2.379928589 2.070135498 2.220440674 31 8824.336288 -4.75E-11 2.49E-06 -2.51E-06 1.14E-10 2.06E-06 2.23E-06 1.51E-10 1.27E-10 -2.386541748 2.382666016 2.073519897 2.224234009 32 8825.378123 -2.07E-10 2.48E-06 -2.50E-06 2.05E-11 2.06E-06 2.23E-06 1.51E-10 1.27E-10 -2.376248169 2.372421265 2.06585083 2.215786743 33 8826.426914 4.60E-11 2.45E-06 -2.46E-06 3.70E-11 2.06E-06 2.22E-06 1.50E-10 1.27E-10 -2.343395996 2.339715576 2.03868103 2.186380005 34 8827.472608 -6.95E-11 2.47E-06 -2.49E-06 1.25E-10 2.05E-06 2.22E-06 1.50E-10 1.26E-10 -2.379821777 2.37522583 2.073043823 2.222943115 35 8828.521909 6.25E-11 2.50E-06 -2.51E-06 1.14E-10 2.05E-06 2.22E-06 1.50E-10 1.26E-10 -2.389736938 2.385421753 2.082922363 2.234164429 36 8829.558052 2.40E-11 2.50E-06 -2.51E-06 6.45E-11 2.06E-06 2.22E-06 1.50E-10 1.27E-10 -2.39102478 2.388085938 2.08656311 2.237649536 37 8830.607862 4.60E-11 2.50E-06 -2.51E-06 9.50E-12 2.07E-06 2.24E-06 1.51E-10 1.27E-10 -2.390447998 2.386663818 2.086871338 2.238104248 38 8831.654573 -7.50E-11 2.50E-06 -2.51E-06 7.00E-11 2.07E-06 2.24E-06 1.51E-10 1.27E-10 -2.388064575 2.382131958 2.085491943 2.236404419 39 8832.708251 -8.05E-11 2.50E-06 -2.51E-06 7.00E-11 2.08E-06 2.25E-06 1.52E-10 1.28E-10 -2.390078735 2.386123657 2.089068604 2.240402222 40 8833.755473 -9.00E-12 2.49E-06 -2.51E-06 4.80E-11 2.08E-06 2.25E-06 1.52E-10 1.28E-10 -2.38894043 2.385501099 2.089666748 2.241122437 41 8834.816382 4.60E-11 2.50E-06 -2.51E-06 5.35E-11 2.08E-06 2.25E-06 1.52E-10 1.28E-10 -2.390029907 2.386291504 2.092288208 2.243756104 42 8835.864117 -1.14E-10 2.49E-06 -2.51E-06 9.50E-12 2.08E-06 2.25E-06 1.52E-10 1.28E-10 -2.387722778 2.38276062 2.091500854 2.242907715 43 8836.915467 -4.75E-11 2.50E-06 -2.51E-06 4.00E-12 2.08E-06 2.25E-06 1.52E-10 1.28E-10 -2.390734863 2.388156128 2.096417236 2.248147583 44 8837.967074 -8.05E-11 2.49E-06 -2.51E-06 -1.50E-12 2.08E-06 2.25E-06 1.52E-10 1.28E-10 -2.386257935 2.382568359 2.094436646 2.245217896 45 8839.018937 -1.19E-10 2.50E-06 -2.51E-06 1.42E-10 2.09E-06 2.25E-06 1.52E-10 1.28E-10 -2.387335205 2.383145142 2.097134399 2.248019409 46 8840.07442 -1.47E-10 2.50E-06 -2.51E-06 4.25E-11 2.09E-06 2.26E-06 1.52E-10 1.28E-10 -2.389163208 2.385281372 2.099987793 2.251568604 47 8841.130161 6.25E-11 2.50E-06 -2.51E-06 7.55E-11 2.09E-06 2.26E-06 1.52E-10 1.28E-10 -2.38840332 2.384613037 2.101358032 2.252825928 48 8842.182798 -7.50E-11 2.50E-06 -2.51E-06 6.45E-11 2.09E-06 2.26E-06 1.52E-10 1.29E-10 -2.389685059 2.386126709 2.103439331 2.255297852 49 8843.245785 -5.30E-11 2.50E-06 -2.51E-06 5.90E-11 2.09E-06 2.26E-06 1.52E-10 1.29E-10 -2.388586426 2.385757446 2.104354858 2.256634521 50 8844.298938 -4.75E-11 2.50E-06 -2.51E-06 5.90E-11 2.09E-06 2.26E-06 1.52E-10 1.29E-10 -2.391574097 2.388735962 2.107730103 2.260464478 51 8845.35235 5.70E-11 2.49E-06 -2.51E-06 3.15E-11 2.09E-06 2.26E-06 1.53E-10 1.29E-10 -2.38805542 2.38409729 2.106298828 2.258306885 52 8846.412752 -6.95E-11 2.50E-06 -2.51E-06 7.00E-11 2.10E-06 2.27E-06 1.53E-10 1.29E-10 -2.389346313 2.386413574 2.109384155 2.261587524 53 8847.473415 -8.05E-11 2.49E-06 -2.51E-06 4.25E-11 2.10E-06 2.27E-06 1.53E-10 1.29E-10 -2.387979126 2.384310913 2.109457397 2.261779785 54 8848.530971 -9.70E-11 2.50E-06 -2.51E-06 4.00E-12 2.10E-06 2.27E-06 1.53E-10 1.29E-10 -2.387792969 2.38354187 2.110772705 2.263262939 55 8849.585417 1.56E-10 2.50E-06 -2.51E-06 6.45E-11 2.10E-06 2.27E-06 1.53E-10 1.29E-10 -2.388287354 2.383770752 2.113296509 2.265350342 56 8850.646862 -1.45E-11 2.50E-06 -2.51E-06 1.14E-10 2.10E-06 2.27E-06 1.53E-10 1.29E-10 -2.388027954 2.384100342 2.114743042 2.267050171 57 8851.708567 -1.45E-11 2.50E-06 -2.51E-06 7.55E-11 2.10E-06 2.27E-06 1.53E-10 1.29E-10 -2.390020752 2.38711853 2.118417358 2.270843506 58 8852.767162 3.50E-11 2.49E-06 -2.51E-06 3.70E-11 2.10E-06 2.28E-06 1.53E-10 1.29E-10 -2.387194824 2.383071899 2.116763306 2.268911743 59 8853.82939 -7.50E-11 2.50E-06 -2.51E-06 7.00E-11 2.11E-06 2.28E-06 1.54E-10 1.30E-10 -2.388049316 2.384725952 2.1199646 2.27220459 60 8854.898626 -3.50E-12 2.50E-06 -2.51E-06 5.90E-11 2.11E-06 2.28E-06 1.54E-10 1.30E-10 -2.390847778 2.387597656 2.123995972 2.276425171 61 8855.958005 -1.25E-10 2.49E-06 -2.51E-06 4.80E-11 2.11E-06 2.28E-06 1.54E-10 1.30E-10 -2.385577393 2.380834961 2.120907593 2.273239136 62 8857.014269 -1.25E-10 2.50E-06 -2.51E-06 1.47E-10 2.11E-06 2.28E-06 1.54E-10 1.30E-10 -2.387783813 2.38394165 2.123974609 2.276821899 63 8858.080919 -4.75E-11 2.49E-06 -2.50E-06 2.60E-11 2.11E-06 2.28E-06 1.54E-10 1.30E-10 -2.384112549 2.379702759 2.121984863 2.274343872 64 8859.134325 -1.08E-10 2.48E-06 -2.49E-06 9.75E-11 2.11E-06 2.28E-06 1.54E-10 1.30E-10 -2.361557007 2.357791138 2.103335571 2.253790283 65 8860.194744 -4.75E-11 2.45E-06 -2.46E-06 1.42E-10 2.10E-06 2.27E-06 1.54E-10 1.30E-10 -2.35022583 2.345492554 2.094561768 2.245629883 66 8861.258802 -6.95E-11 2.49E-06 -2.50E-06 1.20E-10 2.10E-06 2.27E-06 1.53E-10 1.30E-10 -2.386230469 2.382498169 2.129406738 2.282293701 67 8862.323122 -7.50E-11 2.50E-06 -2.51E-06 6.45E-11 2.10E-06 2.27E-06 1.53E-10 1.30E-10 -2.390179443 2.386904907 2.134683228 2.288146973 68 8863.394465 -1.30E-10 2.49E-06 -2.51E-06 8.10E-11 2.11E-06 2.28E-06 1.54E-10 1.30E-10 -2.38722229 2.383618164 2.13380127 2.287036133 69 8864.459312 -6.95E-11 2.50E-06 -2.51E-06 7.55E-11 2.12E-06 2.29E-06 1.55E-10 1.31E-10 -2.388412476 2.384280396 2.136227417 2.289663696 70 8865.517657 6.25E-11 2.50E-06 -2.51E-06 1.03E-10 2.12E-06 2.30E-06 1.55E-10 1.31E-10 -2.388473511 2.38510437 2.138208008 2.291555786 71 8866.576263 -1.45E-11 2.50E-06 -2.51E-06 -2.90E-11 2.13E-06 2.30E-06 1.55E-10 1.31E-10 -2.387478638 2.382675171 2.138803101 2.292129517 72 8867.638511 2.40E-11 2.50E-06 -2.51E-06 1.36E-10 2.13E-06 2.30E-06 1.55E-10 1.32E-10 -2.388796997 2.384725952 2.142184448 2.294934082 73 8868.707788 -5.30E-11 2.49E-06 -2.51E-06 8.10E-11 2.13E-06 2.30E-06 1.55E-10 1.31E-10 -2.389190674 2.3855896 2.144262695 2.29708252 74 8869.767176 3.50E-11 2.49E-06 -2.51E-06 7.00E-11 2.13E-06 2.30E-06 1.55E-10 1.31E-10 -2.389013672 2.385372925 2.145751953 2.298623657 75 8870.840366 1.85E-11 2.50E-06 -2.51E-06 6.45E-11 2.13E-06 2.31E-06 1.55E-10 1.31E-10 -2.3890625 2.3855896 2.147293091 2.300695801 76 8871.903663 -7.50E-11 2.50E-06 -2.51E-06 1.14E-10 2.13E-06 2.31E-06 1.55E-10 1.31E-10 -2.388690186 2.385369873 2.147918701 2.30145874 77 8872.970609 5.70E-11 2.50E-06 -2.51E-06 3.70E-11 2.13E-06 2.31E-06 1.56E-10 1.32E-10 -2.390310669 2.387332153 2.151425171 2.305264282 78 8874.037818 -1.63E-10 2.49E-06 -2.51E-06 7.00E-11 2.14E-06 2.31E-06 1.56E-10 1.32E-10 -2.38598938 2.381738281 2.148840332 2.302746582 79 8875.10868 -9.70E-11 2.50E-06 -2.51E-06 1.36E-10 2.14E-06 2.31E-06 1.57E-10 1.33E-10 -2.387921143 2.384347534 2.152468872 2.306289673 80 8876.169637 -7.50E-11 2.49E-06 -2.51E-06 4.25E-11 2.14E-06 2.31E-06 1.57E-10 1.33E-10 -2.386361694 2.381582642 2.152209473 2.305563354 81 8877.237637 -1.14E-10 2.50E-06 -2.51E-06 4.80E-11 2.14E-06 2.31E-06 1.57E-10 1.33E-10 -2.386422729 2.382226563 2.153753662 2.307870483 82 8878.309291 -2.55E-11 2.49E-06 -2.50E-06 -1.50E-12 2.14E-06 2.32E-06 1.57E-10 1.33E-10 -2.380477905 2.376000977 2.150228882 2.303887939 83 8879.371034 5.70E-11 2.46E-06 -2.47E-06 1.36E-10 2.14E-06 2.31E-06 1.57E-10 1.33E-10 -2.349182129 2.345330811 2.123452759 2.275622559 84 8880.43643 7.50E-12 2.46E-06 -2.48E-06 9.75E-11 2.13E-06 2.30E-06 1.56E-10 1.32E-10 -2.36277771 2.358813477 2.138253784 2.289886475 85 8881.51906 2.00E-12 2.49E-06 -2.51E-06 1.36E-10 2.13E-06 2.30E-06 1.56E-10 1.32E-10 -2.389456177 2.385693359 2.163540649 2.317874146 86 8882.581591 -5.30E-11 2.49E-06 -2.51E-06 8.65E-11 2.13E-06 2.31E-06 1.57E-10 1.33E-10 -2.388040161 2.383572388 2.163934326 2.318252563 87 8883.647778 7.90E-11 2.50E-06 -2.51E-06 6.45E-11 2.14E-06 2.31E-06 1.57E-10 1.33E-10 -2.39230957 2.389370728 2.169528198 2.324676514 88 8884.727815 -1.03E-10 2.49E-06 -2.51E-06 8.10E-11 2.15E-06 2.32E-06 1.57E-10 1.33E-10 -2.386679077 2.38117981 2.165853882 2.320159912 89 8885.784338 -1.03E-10 2.50E-06 -2.51E-06 2.60E-11 2.15E-06 2.33E-06 1.58E-10 1.34E-10 -2.390768433 2.386904907 2.171136475 2.326107788 90 8886.854713 -3.10E-11 2.50E-06 -2.51E-06 4.80E-11 2.16E-06 2.33E-06 1.58E-10 1.34E-10 -2.388641357 2.384579468 2.171002197 2.325518799 91 8887.921953 5.70E-11 2.50E-06 -2.51E-06 5.35E-11 2.16E-06 2.33E-06 1.58E-10 1.34E-10 -2.391201782 2.387973022 2.175701904 2.330453491 92 8888.992856 7.50E-12 2.50E-06 -2.51E-06 3.70E-11 2.16E-06 2.34E-06 1.59E-10 1.35E-10 -2.39017334 2.385864258 2.175888062 2.330279541 93 8890.064024 7.35E-11 2.50E-06 -2.51E-06 1.47E-10 2.16E-06 2.34E-06 1.59E-10 1.35E-10 -2.39130249 2.388208008 2.178717041 2.333609009 94 8891.14226 -1.03E-10 2.50E-06 -2.51E-06 1.42E-10 2.16E-06 2.34E-06 1.59E-10 1.35E-10 -2.387310791 2.382601929 2.176025391 2.330184937 95 8892.203752 -7.50E-11 2.50E-06 -2.51E-06 9.20E-11 2.16E-06 2.34E-06 1.59E-10 1.35E-10 -2.390478516 2.387496948 2.181195068 2.335910034 96 8893.279118 -2.55E-11 2.50E-06 -2.51E-06 3.70E-11 2.17E-06 2.34E-06 1.59E-10 1.35E-10 -2.389572144 2.384591675 2.181314087 2.335684204 97 8894.344537 -8.05E-11 2.50E-06 -2.51E-06 8.10E-11 2.17E-06 2.34E-06 1.59E-10 1.35E-10 -2.3890625 2.385571289 2.183499146 2.338305664 98 8895.42384 -2.55E-11 2.49E-06 -2.51E-06 1.53E-10 2.17E-06 2.34E-06 1.59E-10 1.35E-10 -2.386871338 2.382180786 2.182583618 2.337509155 99 8896.493193 6.25E-11 2.50E-06 -2.51E-06 1.20E-10 2.17E-06 2.35E-06 1.59E-10 1.35E-10 -2.391375732 2.387927246 2.188821411 2.3440979 100 8897.566216 1.01E-10 2.50E-06 -2.51E-06 3.15E-11 2.17E-06 2.35E-06 1.60E-10 1.36E-10 -2.388613892 2.384887695 2.188287354 2.343099976 101 8898.646321 2.40E-11 2.50E-06 -2.51E-06 7.00E-11 2.17E-06 2.35E-06 1.60E-10 1.36E-10 -2.391168213 2.388034058 2.191763306 2.347137451 102 8899.706243 7.50E-12 2.50E-06 -2.51E-06 8.65E-11 2.18E-06 2.35E-06 1.60E-10 1.36E-10 -2.39178772 2.388980103 2.194165039 2.349359131 103 8900.786881 -2.00E-11 2.50E-06 -2.51E-06 8.10E-11 2.18E-06 2.35E-06 1.60E-10 1.36E-10 -2.388601685 2.384307861 2.192016602 2.347091675 104 8901.864378 -1.41E-10 2.50E-06 -2.51E-06 8.65E-11 2.18E-06 2.36E-06 1.60E-10 1.36E-10 -2.392672729 2.389712524 2.198025513 2.353521729 105 8902.931909 -3.65E-11 2.50E-06 -2.51E-06 7.00E-11 2.18E-06 2.36E-06 1.60E-10 1.36E-10 -2.388247681 2.383816528 2.195089722 2.350143433 106 8904.009939 4.05E-11 2.49E-06 -2.51E-06 5.35E-11 2.18E-06 2.36E-06 1.60E-10 1.36E-10 -2.385559082 2.37963562 2.193951416 2.348608398 107 8905.077998 6.25E-11 2.50E-06 -2.51E-06 4.25E-11 2.18E-06 2.36E-06 1.61E-10 1.36E-10 -2.38961792 2.385827637 2.199533081 2.354614258 108 8906.149734 -1.03E-10 2.49E-06 -2.51E-06 7.55E-11 2.19E-06 2.36E-06 1.61E-10 1.36E-10 -2.386502075 2.38163147 2.198486328 2.35362854 109 8907.228563 -5.85E-11 2.50E-06 -2.51E-06 -7.00E-12 2.19E-06 2.36E-06 1.61E-10 1.37E-10 -2.387609863 2.383050537 2.201184082 2.356274414 110 8908.30083 -1.69E-10 2.49E-06 -2.51E-06 1.14E-10 2.19E-06 2.36E-06 1.61E-10 1.37E-10 -2.391268921 2.388378906 2.206588745 2.362216187 111 8909.383611 6.25E-11 2.50E-06 -2.51E-06 1.03E-10 2.19E-06 2.37E-06 1.61E-10 1.37E-10 -2.388342285 2.384249878 2.205444336 2.361068726 112 8910.459827 -2.55E-11 2.50E-06 -2.51E-06 1.03E-10 2.19E-06 2.37E-06 1.61E-10 1.37E-10 -2.390390015 2.386523438 2.208908081 2.364953613 113 8911.543146 2.95E-11 2.50E-06 -2.51E-06 2.60E-11 2.19E-06 2.37E-06 1.61E-10 1.37E-10 -2.38734436 2.383010864 2.207467651 2.363012695 114 8912.616479 1.34E-10 2.50E-06 -2.51E-06 1.03E-10 2.20E-06 2.37E-06 1.62E-10 1.37E-10 -2.390124512 2.386715698 2.212283325 2.368304443 115 8913.686658 -1.36E-10 2.49E-06 -2.51E-06 6.45E-11 2.20E-06 2.37E-06 1.62E-10 1.37E-10 -2.385760498 2.380563354 2.209414673 2.364892578 116 8914.760521 1.85E-11 2.50E-06 -2.51E-06 4.25E-11 2.20E-06 2.38E-06 1.62E-10 1.38E-10 -2.39057312 2.387121582 2.215716553 2.371826172 117 8915.848334 -1.91E-10 2.49E-06 -2.51E-06 9.20E-11 2.20E-06 2.38E-06 1.62E-10 1.38E-10 -2.387838745 2.383532715 2.214730835 2.370532227 118 8916.929575 -2.55E-11 2.49E-06 -2.51E-06 7.55E-11 2.20E-06 2.38E-06 1.62E-10 1.38E-10 -2.386560059 2.382443237 2.215301514 2.370935059 119 8918.011086 1.30E-11 2.50E-06 -2.51E-06 1.20E-10 2.20E-06 2.38E-06 1.62E-10 1.38E-10 -2.389022827 2.385192871 2.219329834 2.375408936 120 8919.103137 -1.14E-10 2.49E-06 -2.51E-06 9.20E-11 2.21E-06 2.38E-06 1.63E-10 1.38E-10 -2.389212036 2.385372925 2.22043457 2.376644897 121 8920.168065 -5.85E-11 2.50E-06 -2.51E-06 6.45E-11 2.21E-06 2.38E-06 1.63E-10 1.38E-10 -2.388778687 2.384820557 2.22154541 2.378335571 122 8921.240105 -1.47E-10 2.49E-06 -2.51E-06 8.10E-11 2.21E-06 2.38E-06 1.62E-10 1.38E-10 -2.386621094 2.382363892 2.221273804 2.378158569 123 8922.329541 2.00E-12 2.49E-06 -2.51E-06 2.60E-11 2.21E-06 2.39E-06 1.63E-10 1.38E-10 -2.38354187 2.379263306 2.220822144 2.376577759 124 8923.402114 1.30E-11 2.49E-06 -2.51E-06 1.25E-10 2.21E-06 2.39E-06 1.62E-10 1.38E-10 -2.387875366 2.38366394 2.226086426 2.382519531 125 8924.481808 -1.45E-11 2.49E-06 -2.51E-06 5.90E-11 2.21E-06 2.39E-06 1.62E-10 1.38E-10 -2.387814331 2.383404541 2.227700806 2.38404541 126 8925.565199 -6.40E-11 2.50E-06 -2.51E-06 1.14E-10 2.21E-06 2.39E-06 1.63E-10 1.38E-10 -2.389093018 2.38454895 2.229974365 2.386709595 127 8926.63857 -8.05E-11 2.50E-06 -2.51E-06 7.00E-11 2.22E-06 2.39E-06 1.63E-10 1.38E-10 -2.389251709 2.386209106 2.232022095 2.389361572 128 8927.725929 -6.40E-11 2.50E-06 -2.51E-06 8.10E-11 2.22E-06 2.40E-06 1.63E-10 1.39E-10 -2.389450073 2.385494995 2.232800293 2.390512085 129 8928.803265 -3.65E-11 2.50E-06 -2.51E-06 7.00E-11 2.22E-06 2.40E-06 1.64E-10 1.39E-10 -2.388928223 2.385131836 2.235028076 2.392459106 130 8929.891164 -1.58E-10 2.50E-06 -2.51E-06 6.45E-11 2.22E-06 2.40E-06 1.64E-10 1.39E-10 -2.389227295 2.385299683 2.236358643 2.393862915 131 8930.965603 -9.00E-12 2.50E-06 -2.51E-06 6.45E-11 2.22E-06 2.40E-06 1.64E-10 1.39E-10 -2.388061523 2.384402466 2.237405396 2.395010376 132 8932.05061 -6.95E-11 2.50E-06 -2.51E-06 8.65E-11 2.22E-06 2.40E-06 1.64E-10 1.39E-10 -2.386074829 2.381298828 2.236868286 2.394458008 133 8933.129017 -1.80E-10 2.49E-06 -2.51E-06 4.25E-11 2.23E-06 2.40E-06 1.64E-10 1.40E-10 -2.387094116 2.382785034 2.239660645 2.397158813 134 8934.214562 -1.58E-10 2.49E-06 -2.51E-06 7.55E-11 2.23E-06 2.41E-06 1.65E-10 1.40E-10 -2.390881348 2.387460327 2.24446106 2.402749634 135 8935.290069 6.25E-11 2.49E-06 -2.51E-06 5.90E-11 2.23E-06 2.41E-06 1.64E-10 1.40E-10 -2.388330078 2.383486938 2.244122314 2.401818848 136 8936.376153 7.50E-12 2.50E-06 -2.51E-06 8.10E-11 2.23E-06 2.41E-06 1.65E-10 1.40E-10 -2.388821411 2.385348511 2.24593811 2.404083252 137 8937.462508 5.70E-11 2.49E-06 -2.51E-06 4.25E-11 2.23E-06 2.41E-06 1.65E-10 1.40E-10 -2.38760376 2.384002686 2.246884155 2.404916382 138 8938.552574 -4.20E-11 2.50E-06 -2.51E-06 6.45E-11 2.23E-06 2.41E-06 1.65E-10 1.40E-10 -2.388745117 2.385803223 2.249554443 2.407446289 139 8939.636032 2.00E-12 2.49E-06 -2.50E-06 8.65E-11 2.23E-06 2.41E-06 1.65E-10 1.41E-10 -2.385394287 2.380718994 2.247528076 2.405322266 140 8940.716318 1.30E-11 2.49E-06 -2.51E-06 1.14E-10 2.24E-06 2.41E-06 1.66E-10 1.41E-10 -2.383825684 2.379541016 2.247344971 2.404821777 141 8941.796873 7.90E-11 2.48E-06 -2.50E-06 6.45E-11 2.24E-06 2.41E-06 1.66E-10 1.41E-10 -2.368463135 2.363494873 2.234024048 2.39024353 142 8942.877696 -8.05E-11 2.44E-06 -2.45E-06 2.05E-11 2.23E-06 2.40E-06 1.65E-10 1.41E-10 -2.324700928 2.322155762 2.195571899 2.348406982 143 8943.969116 -1.25E-10 2.45E-06 -2.47E-06 4.80E-11 2.21E-06 2.39E-06 1.64E-10 1.40E-10 -2.359533691 2.354089355 2.22722168 2.384420776 144 8945.057366 1.30E-11 2.50E-06 -2.51E-06 8.65E-11 2.21E-06 2.39E-06 1.64E-10 1.40E-10 -2.391101074 2.388656616 2.260159302 2.418765259 145 8946.142442 -8.60E-11 2.49E-06 -2.51E-06 5.35E-11 2.22E-06 2.40E-06 1.64E-10 1.40E-10 -2.387350464 2.382537842 2.257867432 2.41625061 146 8947.231235 -2.00E-11 2.50E-06 -2.51E-06 2.60E-11 2.24E-06 2.41E-06 1.65E-10 1.41E-10 -2.390490723 2.388250732 2.263442993 2.421377563 147 8948.313405 -2.51E-10 2.49E-06 -2.51E-06 5.35E-11 2.25E-06 2.42E-06 1.66E-10 1.41E-10 -2.388903809 2.384387207 2.263110352 2.421139526 148 8949.402739 -8.60E-11 2.50E-06 -2.51E-06 3.15E-11 2.25E-06 2.43E-06 1.67E-10 1.42E-10 -2.390090942 2.386032104 2.265890503 2.424185181 149 8950.488897 -9.00E-12 2.50E-06 -2.51E-06 7.00E-11 2.25E-06 2.43E-06 1.67E-10 1.42E-10 -2.388925171 2.384664917 2.266033936 2.424850464 150 8951.568427 6.80E-11 2.50E-06 -2.51E-06 8.65E-11 2.25E-06 2.43E-06 1.67E-10 1.42E-10 -2.389706421 2.385449219 2.268795776 2.427441406 151 8952.662025 -9.00E-12 2.50E-06 -2.51E-06 9.75E-11 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.389047241 2.383926392 2.268676758 2.427529907 152 8953.745543 -5.85E-11 2.50E-06 -2.51E-06 9.75E-11 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.389157104 2.385592651 2.271206665 2.429812622 153 8954.839687 -1.19E-10 2.50E-06 -2.51E-06 3.15E-11 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.391534424 2.387994385 2.274932861 2.434005737 154 8955.920293 -3.50E-12 2.49E-06 -2.51E-06 8.65E-11 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.387155151 2.382827759 2.271069336 2.429779053 155 8957.014981 -6.40E-11 2.50E-06 -2.51E-06 3.15E-11 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.389050293 2.386114502 2.275585938 2.434283447 156 8958.103035 -5.85E-11 2.49E-06 -2.51E-06 -1.50E-12 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.387680054 2.383480835 2.274951172 2.433502197 157 8959.194816 -1.47E-10 2.49E-06 -2.51E-06 6.45E-11 2.26E-06 2.44E-06 1.68E-10 1.43E-10 -2.382086182 2.377178955 2.269979858 2.428363037 158 8960.283413 7.90E-11 2.48E-06 -2.50E-06 5.90E-11 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.377236938 2.373144531 2.266400146 2.42482605 159 8961.365368 2.00E-12 2.48E-06 -2.50E-06 6.45E-11 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.376852417 2.372738647 2.267172241 2.42555542 160 8962.454506 7.35E-11 2.49E-06 -2.50E-06 8.10E-11 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.377224731 2.372949219 2.268780518 2.427249146 161 8963.550833 2.40E-11 2.48E-06 -2.49E-06 9.20E-11 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.373846436 2.369784546 2.267080688 2.424996948 162 8964.637057 -5.30E-11 2.48E-06 -2.49E-06 3.15E-11 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.375335693 2.3715271 2.269793701 2.427215576 163 8965.730472 -5.30E-11 2.48E-06 -2.49E-06 4.80E-11 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.375067139 2.371304321 2.270947266 2.42807312 164 8966.831083 -1.41E-10 2.48E-06 -2.50E-06 6.45E-11 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.374331665 2.370812988 2.271148682 2.428128052 165 8967.911197 -1.36E-10 2.48E-06 -2.49E-06 3.70E-11 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.374533081 2.370617676 2.270690918 2.427172852 166 8968.998505 -9.15E-11 2.49E-06 -2.50E-06 9.20E-11 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.376818848 2.372259521 2.272875977 2.430007935 167 8970.089547 -1.30E-10 2.49E-06 -2.50E-06 2.05E-11 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.38449707 2.380374146 2.280206299 2.437969971 168 8971.191256 5.15E-11 2.49E-06 -2.50E-06 3.15E-11 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.380053711 2.37505188 2.27628479 2.433792114 169 8972.272448 -1.52E-10 2.49E-06 -2.50E-06 1.25E-10 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.381338501 2.37833252 2.276742554 2.434207153 170 8973.374707 -6.95E-11 2.47E-06 -2.49E-06 4.00E-12 2.26E-06 2.44E-06 1.67E-10 1.42E-10 -2.361651611 2.357632446 2.254345703 2.410998535 171 8974.470309 -9.70E-11 2.44E-06 -2.45E-06 1.50E-11 2.26E-06 2.44E-06 1.66E-10 1.41E-10 -2.329159546 2.326223755 2.218774414 2.372729492 172 8975.559249 7.35E-11 2.44E-06 -2.45E-06 8.65E-11 2.24E-06 2.42E-06 1.64E-10 1.40E-10 -2.339056396 2.333911133 2.219091797 2.371255493 173 8976.655398 -1.14E-10 2.48E-06 -2.50E-06 -1.50E-12 2.23E-06 2.40E-06 1.62E-10 1.37E-10 -2.381848145 2.378744507 2.256771851 2.412722778 174 8977.748351 -2.13E-10 2.49E-06 -2.50E-06 3.70E-11 2.23E-06 2.40E-06 1.58E-10 1.33E-10 -2.380706787 2.376239014 2.247836304 2.403771973 175 8978.841578 -1.08E-10 2.49E-06 -2.50E-06 2.05E-11 2.23E-06 2.40E-06 1.51E-10 1.26E-10 -2.380169678 2.376489258 2.227142334 2.381167603 176 8979.931605 -8.60E-11 2.49E-06 -2.50E-06 1.36E-10 2.23E-06 2.40E-06 1.45E-10 1.20E-10 -2.380166626 2.375515747 2.190960693 2.34173584 177 8981.032323 -2.00E-11 2.48E-06 -2.50E-06 8.10E-11 2.20E-06 2.37E-06 1.40E-10 1.14E-10 -2.379199219 2.37543335 2.121878052 2.267727661 178 8982.122896 2.00E-12 2.49E-06 -2.50E-06 2.05E-11 2.15E-06 2.32E-06 1.35E-10 1.10E-10 -2.378512573 2.374200439 1.99982605 2.136825562 179 8983.217215 -5.85E-11 2.49E-06 -2.50E-06 1.03E-10 2.07E-06 2.24E-06 1.31E-10 1.06E-10 -2.378988647 2.376065063 1.885205078 2.014273071 180 8984.318759 -4.20E-11 2.48E-06 -2.50E-06 5.90E-11 1.98E-06 2.14E-06 1.25E-10 1.01E-10 -2.376657104 2.373184204 1.827957153 1.953250122 181 8985.41015 5.15E-11 2.48E-06 -2.50E-06 8.65E-11 1.89E-06 2.04E-06 1.19E-10 9.52E-11 -2.377368164 2.374142456 1.79050293 1.912866211 182 8986.505291 -2.55E-11 2.48E-06 -2.49E-06 8.10E-11 1.82E-06 1.96E-06 1.13E-10 8.98E-11 -2.375219727 2.371530151 1.721173096 1.838150024 183 8987.604184 -6.95E-11 2.48E-06 -2.50E-06 8.65E-11 1.77E-06 1.91E-06 1.09E-10 8.56E-11 -2.374926758 2.371438599 1.63001709 1.74045105 184 8988.699873 -9.00E-12 2.48E-06 -2.49E-06 1.25E-10 1.71E-06 1.84E-06 1.03E-10 8.05E-11 -2.37350769 2.368765259 1.521514893 1.623965454 185 8989.795837 1.34E-10 2.48E-06 -2.49E-06 9.75E-11 1.61E-06 1.74E-06 9.62E-11 7.39E-11 -2.37270813 2.367279053 1.397555542 1.491021729 186 8990.892074 6.80E-11 2.48E-06 -2.49E-06 4.25E-11 1.50E-06 1.62E-06 8.81E-11 6.66E-11 -2.375018311 2.372158813 1.319830322 1.407748413 187 8991.99903 -1.36E-10 2.48E-06 -2.49E-06 4.80E-11 1.40E-06 1.51E-06 8.10E-11 6.01E-11 -2.37321167 2.368737793 1.270407104 1.354495239 188 8993.085372 -1.58E-10 2.48E-06 -2.50E-06 8.10E-11 1.32E-06 1.42E-06 7.61E-11 5.58E-11 -2.375479126 2.3724823 1.230657959 1.312161255 189 8994.189399 -1.14E-10 2.48E-06 -2.49E-06 7.00E-11 1.26E-06 1.36E-06 7.32E-11 5.32E-11 -2.371514893 2.366342163 1.189929199 1.26829834 190 8995.286735 1.30E-11 2.48E-06 -2.50E-06 1.47E-10 1.22E-06 1.31E-06 7.15E-11 5.17E-11 -2.378189087 2.374938965 1.172332764 1.248867798 191 8996.394801 -8.05E-11 2.48E-06 -2.49E-06 9.20E-11 1.19E-06 1.28E-06 7.08E-11 5.12E-11 -2.370437622 2.36451416 1.177679443 1.254431152 192 8997.482232 3.50E-11 2.48E-06 -2.50E-06 4.25E-11 1.18E-06 1.27E-06 7.08E-11 5.13E-11 -2.375280762 2.37121582 1.206552124 1.285873413 193 8998.58388 -7.50E-11 2.48E-06 -2.49E-06 7.55E-11 1.19E-06 1.27E-06 7.12E-11 5.17E-11 -2.373153687 2.368267822 1.237979126 1.319842529 194 8999.682316 2.00E-12 2.48E-06 -2.49E-06 8.10E-11 1.21E-06 1.30E-06 7.22E-11 5.25E-11 -2.372357178 2.367071533 1.279592896 1.364334106 195 9000.781028 -4.75E-11 2.48E-06 -2.49E-06 7.55E-11 1.23E-06 1.33E-06 7.28E-11 5.29E-11 -2.373516846 2.37015686 1.321173096 1.409030151 196 9001.886993 -8.05E-11 2.48E-06 -2.49E-06 6.45E-11 1.27E-06 1.36E-06 7.39E-11 5.38E-11 -2.373760986 2.369741821 1.353775024 1.443682861 197 9002.989746 -1.25E-10 2.48E-06 -2.49E-06 1.14E-10 1.31E-06 1.41E-06 7.56E-11 5.51E-11 -2.374377441 2.370672607 1.384231567 1.476574707 198 9004.085795 1.30E-11 2.48E-06 -2.49E-06 6.45E-11 1.34E-06 1.45E-06 7.75E-11 5.67E-11 -2.374368286 2.371557617 1.41211853 1.50640564 199 9005.189101 -1.19E-10 2.48E-06 -2.49E-06 8.65E-11 1.38E-06 1.48E-06 8.01E-11 5.91E-11 -2.370980835 2.366320801 1.427987671 1.523214722 200 9006.292685 4.60E-11 2.48E-06 -2.49E-06 2.60E-11 1.40E-06 1.51E-06 8.21E-11 6.08E-11 -2.37142334 2.36763916 1.435028076 1.530889893 201 9007.396545 2.40E-11 2.48E-06 -2.49E-06 1.31E-10 1.42E-06 1.52E-06 8.38E-11 6.24E-11 -2.373355103 2.368948364 1.436401367 1.532141113 202 9008.493694 -7.50E-11 2.48E-06 -2.50E-06 1.36E-10 1.42E-06 1.53E-06 8.50E-11 6.35E-11 -2.372717285 2.368496704 1.434359741 1.530252075 203 9009.598109 4.60E-11 2.48E-06 -2.49E-06 9.75E-11 1.43E-06 1.54E-06 8.57E-11 6.41E-11 -2.372967529 2.368765259 1.434811401 1.530453491 204 9010.7028 -1.41E-10 2.48E-06 -2.49E-06 8.65E-11 1.43E-06 1.54E-06 8.61E-11 6.46E-11 -2.372970581 2.368945313 1.43694458 1.533065796 205 9011.800776 -3.50E-12 2.48E-06 -2.49E-06 5.90E-11 1.43E-06 1.54E-06 8.64E-11 6.48E-11 -2.374484253 2.371875 1.442138672 1.538360596 206 9012.906021 -7.50E-11 2.48E-06 -2.49E-06 9.75E-11 1.43E-06 1.54E-06 8.60E-11 6.44E-11 -2.368740845 2.363644409 1.442825317 1.539041138 207 9014.011545 6.25E-11 2.47E-06 -2.49E-06 4.80E-11 1.43E-06 1.54E-06 8.59E-11 6.42E-11 -2.366452026 2.363598633 1.4472229 1.54354248 208 9015.113847 -1.08E-10 2.46E-06 -2.47E-06 1.69E-10 1.43E-06 1.54E-06 8.59E-11 6.41E-11 -2.352572632 2.347558594 1.444949341 1.541641235 209 9016.216425 -6.40E-11 2.46E-06 -2.48E-06 2.05E-11 1.44E-06 1.55E-06 8.57E-11 6.39E-11 -2.363348389 2.358551025 1.46060791 1.557907104 210 9017.315779 1.23E-10 2.48E-06 -2.49E-06 7.55E-11 1.45E-06 1.56E-06 8.61E-11 6.42E-11 -2.372225952 2.368511963 1.477755737 1.576412964 211 9018.415407 -2.55E-11 2.47E-06 -2.49E-06 4.25E-11 1.46E-06 1.57E-06 8.62E-11 6.43E-11 -2.370596313 2.366326904 1.4902771 1.590036011 212 9019.51531 -9.15E-11 2.48E-06 -2.49E-06 1.09E-10 1.47E-06 1.58E-06 8.64E-11 6.43E-11 -2.372149658 2.36791687 1.503701782 1.603909302 213 9020.636514 2.00E-12 2.48E-06 -2.49E-06 1.14E-10 1.48E-06 1.60E-06 8.67E-11 6.45E-11 -2.372900391 2.369812012 1.515689087 1.616882324 214 9021.740478 -1.69E-10 2.48E-06 -2.49E-06 3.15E-11 1.49E-06 1.61E-06 8.68E-11 6.45E-11 -2.373410034 2.369470215 1.523571777 1.625494385 215 9022.85173 4.05E-11 2.48E-06 -2.49E-06 4.25E-11 1.51E-06 1.62E-06 8.69E-11 6.46E-11 -2.374298096 2.369671631 1.529467773 1.631622314 216 9023.95625 -4.20E-11 2.48E-06 -2.49E-06 1.42E-10 1.51E-06 1.63E-06 8.70E-11 6.45E-11 -2.370251465 2.365197754 1.530969238 1.633126831 217 9025.05754 3.50E-11 2.48E-06 -2.49E-06 2.60E-11 1.52E-06 1.64E-06 8.71E-11 6.47E-11 -2.373562622 2.370251465 1.535092163 1.637310791 218 9026.166122 -2.55E-11 2.47E-06 -2.49E-06 1.25E-10 1.52E-06 1.64E-06 8.73E-11 6.48E-11 -2.370074463 2.365655518 1.531091309 1.632983398 219 9027.267965 1.30E-11 2.48E-06 -2.49E-06 8.65E-11 1.52E-06 1.64E-06 8.77E-11 6.51E-11 -2.368719482 2.364221191 1.524960327 1.626501465 220 9028.380614 -7.50E-11 2.48E-06 -2.49E-06 9.20E-11 1.52E-06 1.64E-06 8.79E-11 6.54E-11 -2.370605469 2.36769104 1.51953125 1.620904541 221 9029.483011 -1.45E-11 2.48E-06 -2.49E-06 3.15E-11 1.52E-06 1.63E-06 8.82E-11 6.58E-11 -2.369451904 2.364703369 1.510632324 1.611114502 222 9030.585684 -2.07E-10 2.48E-06 -2.49E-06 5.35E-11 1.51E-06 1.63E-06 8.86E-11 6.62E-11 -2.372036743 2.368362427 1.503579712 1.603323364 223 9031.695659 8.45E-11 2.47E-06 -2.49E-06 5.90E-11 1.50E-06 1.62E-06 8.88E-11 6.65E-11 -2.372259521 2.368792725 1.493710327 1.59296875 224 9032.805914 -1.19E-10 2.47E-06 -2.49E-06 8.10E-11 1.49E-06 1.61E-06 8.88E-11 6.65E-11 -2.368978882 2.365866089 1.481970215 1.580426025 225 9033.916449 2.40E-11 2.47E-06 -2.49E-06 9.75E-11 1.48E-06 1.60E-06 8.86E-11 6.64E-11 -2.369921875 2.365878296 1.472134399 1.569827271 226 9035.016716 -2.55E-11 2.47E-06 -2.49E-06 4.25E-11 1.47E-06 1.59E-06 8.84E-11 6.62E-11 -2.3684021 2.364343262 1.460617065 1.557519531 227 9036.27199 4.60E-11 2.48E-06 -2.49E-06 9.50E-12 1.46E-06 1.57E-06 8.82E-11 6.60E-11 -2.368157959 2.363690186 1.451806641 1.548126221 228 9037.376363 -8.05E-11 2.47E-06 -2.49E-06 3.70E-11 1.45E-06 1.56E-06 8.80E-11 6.59E-11 -2.366149902 2.361608887 1.441357422 1.536993408 229 9038.470458 -2.51E-10 2.48E-06 -2.49E-06 3.70E-11 1.44E-06 1.55E-06 8.76E-11 6.56E-11 -2.369525146 2.366415405 1.435128784 1.530252075 230 9039.578902 5.70E-11 2.48E-06 -2.49E-06 1.03E-10 1.43E-06 1.54E-06 8.67E-11 6.47E-11 -2.369412231 2.366268921 1.427853394 1.522253418 231 9040.701706 -8.60E-11 2.47E-06 -2.49E-06 7.55E-11 1.43E-06 1.53E-06 8.62E-11 6.43E-11 -2.367944336 2.363299561 1.421386719 1.515115356 232 9041.803668 -1.45E-11 2.47E-06 -2.49E-06 4.80E-11 1.42E-06 1.53E-06 8.59E-11 6.41E-11 -2.369265747 2.365341187 1.417520142 1.511138916 233 9042.916472 -1.14E-10 2.47E-06 -2.49E-06 7.00E-11 1.41E-06 1.52E-06 8.57E-11 6.38E-11 -2.367654419 2.364395142 1.413574219 1.506747437 234 9044.036603 -1.14E-10 2.47E-06 -2.49E-06 5.35E-11 1.41E-06 1.52E-06 8.59E-11 6.41E-11 -2.365115356 2.360018921 1.408551025 1.501217651 235 9045.1394 -2.55E-11 2.47E-06 -2.49E-06 9.75E-11 1.41E-06 1.51E-06 8.57E-11 6.38E-11 -2.366323853 2.362487793 1.405966187 1.498590088 236 9046.242472 -2.00E-11 2.47E-06 -2.48E-06 8.10E-11 1.40E-06 1.51E-06 8.55E-11 6.37E-11 -2.364346313 2.358969116 1.402114868 1.494400024 237 9047.359922 -9.00E-12 2.47E-06 -2.49E-06 1.09E-10 1.40E-06 1.50E-06 8.53E-11 6.35E-11 -2.369390869 2.365856934 1.404037476 1.496343994 238 9048.470602 -3.65E-11 2.47E-06 -2.48E-06 1.47E-10 1.40E-06 1.50E-06 8.51E-11 6.32E-11 -2.364367676 2.360424805 1.401187134 1.493234253 239 9049.585089 -4.20E-11 2.48E-06 -2.49E-06 7.55E-11 1.40E-06 1.50E-06 8.50E-11 6.32E-11 -2.36937561 2.366519165 1.40539856 1.49777832 240 9050.699858 1.95E-10 2.47E-06 -2.49E-06 2.05E-11 1.40E-06 1.50E-06 8.48E-11 6.30E-11 -2.367095947 2.362850952 1.406268311 1.498803711 241 9051.818437 -1.08E-10 2.47E-06 -2.49E-06 4.80E-11 1.40E-06 1.50E-06 8.50E-11 6.31E-11 -2.365795898 2.361047363 1.408303833 1.500982666 242 9052.930239 4.05E-11 2.47E-06 -2.48E-06 5.90E-11 1.40E-06 1.50E-06 8.50E-11 6.31E-11 -2.365618896 2.362237549 1.41242981 1.505349731 243 9054.045853 -3.10E-11 2.47E-06 -2.48E-06 9.20E-11 1.40E-06 1.51E-06 8.50E-11 6.32E-11 -2.362652588 2.35980835 1.415414429 1.508227539 244 9055.16528 -5.30E-11 2.47E-06 -2.48E-06 9.20E-11 1.40E-06 1.51E-06 8.51E-11 6.33E-11 -2.355545044 2.349545288 1.414022827 1.506713867 245 9056.274393 -6.95E-11 2.44E-06 -2.45E-06 5.90E-11 1.40E-06 1.51E-06 8.50E-11 6.31E-11 -2.32644043 2.32359314 1.400982666 1.492800903 246 9057.401453 -6.40E-11 2.43E-06 -2.44E-06 8.65E-11 1.40E-06 1.51E-06 8.49E-11 6.30E-11 -2.3315979 2.326580811 1.407611084 1.500570679 247 9058.511127 8.45E-11 2.47E-06 -2.48E-06 6.45E-11 1.40E-06 1.51E-06 8.50E-11 6.31E-11 -2.365637207 2.363186646 1.433233643 1.527410889 248 9059.635222 1.85E-11 2.47E-06 -2.49E-06 8.10E-11 1.41E-06 1.52E-06 8.52E-11 6.33E-11 -2.366714478 2.361508179 1.437973022 1.532577515 249 9060.741921 2.40E-11 2.47E-06 -2.49E-06 1.09E-10 1.42E-06 1.53E-06 8.58E-11 6.37E-11 -2.370672607 2.367446899 1.445303345 1.540344238 250 9061.870121 -5.85E-11 2.47E-06 -2.48E-06 1.31E-10 1.43E-06 1.54E-06 8.61E-11 6.39E-11 -2.367068481 2.362863159 1.447424316 1.542462158 251 9062.984456 -8.60E-11 2.47E-06 -2.49E-06 5.90E-11 1.44E-06 1.54E-06 8.64E-11 6.41E-11 -2.36569519 2.361566162 1.450326538 1.545651245 252 9064.10615 -1.14E-10 2.47E-06 -2.49E-06 7.00E-11 1.44E-06 1.55E-06 8.65E-11 6.42E-11 -2.366690063 2.363095093 1.455108643 1.550857544 253 9065.228129 -3.50E-12 2.47E-06 -2.49E-06 5.35E-11 1.44E-06 1.55E-06 8.67E-11 6.43E-11 -2.364910889 2.359622192 1.457357788 1.553207397 254 9066.343311 -6.95E-11 2.48E-06 -2.49E-06 1.50E-11 1.45E-06 1.56E-06 8.69E-11 6.44E-11 -2.368145752 2.364083862 1.462820435 1.559030151 255 9067.458774 6.80E-11 2.48E-06 -2.49E-06 7.00E-11 1.45E-06 1.56E-06 8.69E-11 6.44E-11 -2.370968628 2.367681885 1.468435669 1.565075684 256 9068.585146 -9.00E-12 2.47E-06 -2.49E-06 9.20E-11 1.45E-06 1.56E-06 8.69E-11 6.44E-11 -2.36913147 2.3652771 1.471368408 1.567880249 257 9069.697632 -5.30E-11 2.48E-06 -2.49E-06 1.50E-11 1.46E-06 1.57E-06 8.70E-11 6.44E-11 -2.370080566 2.365716553 1.475134277 1.571838379 258 9070.817486 -4.20E-11 2.47E-06 -2.49E-06 8.65E-11 1.46E-06 1.57E-06 8.72E-11 6.46E-11 -2.367852783 2.364086914 1.477374268 1.574487305 259 9071.944713 -2.55E-11 2.47E-06 -2.49E-06 2.05E-11 1.47E-06 1.58E-06 8.73E-11 6.48E-11 -2.36781311 2.362963867 1.480136108 1.576916504 260 9073.065136 2.00E-12 2.47E-06 -2.49E-06 1.20E-10 1.47E-06 1.58E-06 8.77E-11 6.51E-11 -2.368286133 2.364065552 1.483404541 1.58062439 261 9074.185842 -1.41E-10 2.47E-06 -2.49E-06 3.70E-11 1.47E-06 1.58E-06 8.80E-11 6.53E-11 -2.366448975 2.36114502 1.48505249 1.58236084 262 9075.303285 2.00E-12 2.47E-06 -2.49E-06 1.31E-10 1.48E-06 1.59E-06 8.84E-11 6.58E-11 -2.370565796 2.367266846 1.491113281 1.5887146 263 9076.431655 8.45E-11 2.47E-06 -2.49E-06 7.00E-11 1.48E-06 1.59E-06 8.89E-11 6.63E-11 -2.365542603 2.360113525 1.49017334 1.587756348 264 9077.546115 -4.75E-11 2.48E-06 -2.49E-06 -7.00E-12 1.48E-06 1.59E-06 8.93E-11 6.66E-11 -2.37098999 2.367227173 1.496310425 1.594265747 265 9078.671507 -2.00E-11 2.47E-06 -2.49E-06 5.90E-11 1.48E-06 1.60E-06 8.98E-11 6.70E-11 -2.366363525 2.361758423 1.495977783 1.593835449 266 9079.800736 -6.95E-11 2.47E-06 -2.49E-06 3.70E-11 1.49E-06 1.60E-06 9.02E-11 6.74E-11 -2.370184326 2.366772461 1.500924683 1.599215698 267 9080.919596 -1.03E-10 2.48E-06 -2.49E-06 8.65E-11 1.49E-06 1.60E-06 9.07E-11 6.79E-11 -2.367654419 2.363528442 1.501159668 1.599307251 268 9082.035186 -1.96E-10 2.47E-06 -2.49E-06 5.35E-11 1.49E-06 1.60E-06 9.12E-11 6.82E-11 -2.367318726 2.364321899 1.503829956 1.602252197 269 9083.158165 -2.00E-11 2.48E-06 -2.49E-06 7.55E-11 1.49E-06 1.61E-06 9.17E-11 6.88E-11 -2.369039917 2.365151978 1.506967163 1.605422974 270 9084.281428 -8.60E-11 2.47E-06 -2.49E-06 1.36E-10 1.50E-06 1.61E-06 9.22E-11 6.91E-11 -2.366452026 2.361849976 1.507376099 1.60579834 271 9085.397864 -1.19E-10 2.47E-06 -2.49E-06 1.09E-10 1.50E-06 1.61E-06 9.26E-11 6.95E-11 -2.366210938 2.361611938 1.508816528 1.60723877 272 9086.532366 -1.58E-10 2.47E-06 -2.49E-06 2.60E-11 1.50E-06 1.61E-06 9.30E-11 6.99E-11 -2.369165039 2.365606689 1.511853027 1.610940552 273 9087.64937 -8.05E-11 2.47E-06 -2.48E-06 1.03E-10 1.50E-06 1.61E-06 9.31E-11 7.01E-11 -2.362863159 2.357675171 1.509558105 1.608120728 274 9088.766654 -9.00E-12 2.47E-06 -2.48E-06 3.15E-11 1.50E-06 1.61E-06 9.36E-11 7.05E-11 -2.362371826 2.359851074 1.510092163 1.609140015 275 9089.902019 -4.75E-11 2.45E-06 -2.46E-06 1.31E-10 1.50E-06 1.61E-06 9.30E-11 6.99E-11 -2.34074707 2.337158203 1.49743042 1.595272827 276 9091.019871 -4.75E-11 2.45E-06 -2.46E-06 1.36E-10 1.50E-06 1.61E-06 9.21E-11 6.90E-11 -2.349285889 2.344604492 1.504916382 1.602410889 277 9092.14869 2.95E-11 2.47E-06 -2.49E-06 4.25E-11 1.50E-06 1.61E-06 9.21E-11 6.91E-11 -2.368951416 2.365911865 1.518533325 1.617486572 278 9093.277796 1.30E-11 2.47E-06 -2.49E-06 7.00E-11 1.50E-06 1.61E-06 9.27E-11 6.96E-11 -2.36479187 2.360574341 1.51711731 1.616183472 279 9094.400063 7.90E-11 2.47E-06 -2.49E-06 8.65E-11 1.51E-06 1.62E-06 9.39E-11 7.07E-11 -2.367306519 2.3631073 1.520269775 1.619454956 280 9095.522614 -5.85E-11 2.47E-06 -2.49E-06 4.80E-11 1.51E-06 1.62E-06 9.50E-11 7.18E-11 -2.367602539 2.36307373 1.521304321 1.620736694 281 9096.645449 -1.03E-10 2.47E-06 -2.49E-06 1.42E-10 1.51E-06 1.63E-06 9.55E-11 7.23E-11 -2.368655396 2.364871216 1.523266602 1.622503662 282 9097.793529 -2.62E-10 2.47E-06 -2.49E-06 1.25E-10 1.51E-06 1.63E-06 9.58E-11 7.25E-11 -2.369476318 2.365396118 1.525222778 1.624206543 283 9098.909805 4.60E-11 2.47E-06 -2.49E-06 4.25E-11 1.51E-06 1.63E-06 9.61E-11 7.28E-11 -2.368002319 2.363900757 1.525418091 1.624139404 284 9100.051336 -2.55E-11 2.47E-06 -2.49E-06 1.14E-10 1.52E-06 1.63E-06 9.62E-11 7.29E-11 -2.368881226 2.365310669 1.526992798 1.625952148 285 9101.182454 -7.50E-11 2.47E-06 -2.48E-06 6.45E-11 1.52E-06 1.63E-06 9.61E-11 7.28E-11 -2.365725708 2.361950684 1.526791382 1.625390625 286 9102.303152 -2.00E-11 2.48E-06 -2.49E-06 6.45E-11 1.52E-06 1.63E-06 9.61E-11 7.27E-11 -2.368252563 2.363790894 1.528994751 1.628106689 287 9103.424133 -6.40E-11 2.47E-06 -2.49E-06 1.31E-10 1.52E-06 1.63E-06 9.60E-11 7.25E-11 -2.367913818 2.363848877 1.529827881 1.628451538 288 9104.556111 5.15E-11 2.47E-06 -2.49E-06 4.80E-11 1.52E-06 1.63E-06 9.58E-11 7.24E-11 -2.367703247 2.363916016 1.53012085 1.629089355 289 9105.674088 -5.30E-11 2.47E-06 -2.49E-06 1.03E-10 1.52E-06 1.63E-06 9.56E-11 7.21E-11 -2.36725769 2.363037109 1.530853271 1.6296875 290 9106.817359 1.30E-11 2.47E-06 -2.49E-06 3.15E-11 1.52E-06 1.63E-06 9.54E-11 7.20E-11 -2.36932373 2.366333008 1.533007813 1.63197937 291 9107.946628 -9.15E-11 2.47E-06 -2.49E-06 5.35E-11 1.52E-06 1.64E-06 9.53E-11 7.19E-11 -2.363519287 2.358276367 1.530007935 1.628991699 292 9109.079759 -9.70E-11 2.47E-06 -2.49E-06 7.00E-11 1.52E-06 1.64E-06 9.52E-11 7.18E-11 -2.369223022 2.36708374 1.534811401 1.633789063 293 9110.202451 1.30E-11 2.47E-06 -2.48E-06 7.55E-11 1.52E-06 1.64E-06 9.52E-11 7.18E-11 -2.365979004 2.362271118 1.534002686 1.633004761 294 9111.343311 5.15E-11 2.47E-06 -2.49E-06 1.31E-10 1.52E-06 1.64E-06 9.50E-11 7.16E-11 -2.367111206 2.363861084 1.536132813 1.635394287 295 9112.47373 9.55E-11 2.47E-06 -2.48E-06 -1.50E-12 1.53E-06 1.64E-06 9.49E-11 7.15E-11 -2.363131714 2.35847168 1.534500122 1.633459473 296 9113.604437 4.60E-11 2.47E-06 -2.49E-06 8.65E-11 1.53E-06 1.64E-06 9.51E-11 7.16E-11 -2.366134644 2.362802124 1.537481689 1.6362854 297 9114.735431 4.05E-11 2.47E-06 -2.48E-06 1.36E-10 1.53E-06 1.64E-06 9.52E-11 7.17E-11 -2.364001465 2.358972168 1.535812378 1.634927368 298 9115.863133 -1.14E-10 2.47E-06 -2.49E-06 1.09E-10 1.53E-06 1.64E-06 9.52E-11 7.16E-11 -2.365194702 2.359951782 1.536819458 1.635601807 299 9116.998283 -9.00E-12 2.47E-06 -2.48E-06 2.05E-11 1.53E-06 1.64E-06 9.55E-11 7.19E-11 -2.368252563 2.36456604 1.539447021 1.638677979 300 9118.126558 2.40E-11 2.47E-06 -2.49E-06 2.05E-11 1.53E-06 1.64E-06 9.52E-11 7.17E-11 -2.36630249 2.363464355 1.538174438 1.637564087 301 9119.269453 -2.00E-11 2.47E-06 -2.48E-06 1.14E-10 1.53E-06 1.64E-06 9.52E-11 7.17E-11 -2.361972046 2.357141113 1.535314941 1.634182739 302 9120.39472 -1.36E-10 2.47E-06 -2.49E-06 4.80E-11 1.53E-06 1.64E-06 9.53E-11 7.18E-11 -2.367214966 2.3640625 1.538418579 1.637615967 303 9121.534612 -8.60E-11 2.47E-06 -2.48E-06 1.03E-10 1.53E-06 1.64E-06 9.51E-11 7.16E-11 -2.362316895 2.356982422 1.534051514 1.63336792 304 9122.667625 -9.15E-11 2.47E-06 -2.49E-06 1.09E-10 1.53E-06 1.64E-06 9.51E-11 7.16E-11 -2.366204834 2.362374878 1.535861206 1.635122681 305 9123.800925 -1.03E-10 2.47E-06 -2.48E-06 7.55E-11 1.53E-06 1.64E-06 9.49E-11 7.14E-11 -2.36494751 2.360482788 1.534005737 1.63321228 306 9124.927339 -1.03E-10 2.47E-06 -2.48E-06 7.55E-11 1.53E-06 1.64E-06 9.45E-11 7.10E-11 -2.363589478 2.358929443 1.53263855 1.63142395 307 9126.068392 1.30E-11 2.47E-06 -2.48E-06 2.60E-11 1.53E-06 1.64E-06 9.42E-11 7.06E-11 -2.36569519 2.361700439 1.533508301 1.63170166 308 9127.202559 -9.00E-12 2.47E-06 -2.48E-06 7.00E-11 1.53E-06 1.64E-06 9.37E-11 7.01E-11 -2.36305542 2.358068848 1.531399536 1.629348755 309 9128.337015 -1.45E-11 2.47E-06 -2.48E-06 7.55E-11 1.52E-06 1.64E-06 9.33E-11 6.98E-11 -2.365158081 2.362130737 1.531768799 1.630502319 310 9129.482533 -3.50E-12 2.47E-06 -2.48E-06 5.90E-11 1.52E-06 1.64E-06 9.32E-11 6.97E-11 -2.363900757 2.359509277 1.530960083 1.629568481 311 9130.613978 -3.10E-11 2.47E-06 -2.48E-06 1.80E-10 1.52E-06 1.64E-06 9.31E-11 6.95E-11 -2.364993286 2.361639404 1.531832886 1.630444336 312 9131.749302 -2.00E-11 2.47E-06 -2.48E-06 7.00E-11 1.52E-06 1.64E-06 9.32E-11 6.96E-11 -2.363223267 2.358410645 1.530609131 1.629092407 313 9132.884916 -1.25E-10 2.47E-06 -2.48E-06 1.50E-11 1.52E-06 1.64E-06 9.33E-11 6.97E-11 -2.365945435 2.362646484 1.533425903 1.63203125 314 9134.02082 9.00E-11 2.47E-06 -2.48E-06 7.55E-11 1.52E-06 1.64E-06 9.33E-11 6.98E-11 -2.362304688 2.357699585 1.531808472 1.630471802 315 9135.160609 -3.10E-11 2.47E-06 -2.48E-06 6.45E-11 1.52E-06 1.64E-06 9.35E-11 6.99E-11 -2.362850952 2.358532715 1.533236694 1.631921387 316 9136.297092 1.85E-11 2.47E-06 -2.48E-06 7.55E-11 1.52E-06 1.64E-06 9.36E-11 7.00E-11 -2.363623047 2.359609985 1.534585571 1.633135986 317 9137.437463 6.80E-11 2.47E-06 -2.48E-06 4.80E-11 1.52E-06 1.64E-06 9.37E-11 7.01E-11 -2.366427612 2.362814331 1.537350464 1.636447144 318 9138.574527 -1.45E-11 2.47E-06 -2.48E-06 4.80E-11 1.53E-06 1.64E-06 9.41E-11 7.04E-11 -2.364318848 2.360906982 1.537249756 1.636184692 319 9139.704682 -5.30E-11 2.47E-06 -2.48E-06 8.65E-11 1.53E-06 1.64E-06 9.41E-11 7.04E-11 -2.362924194 2.358288574 1.537261963 1.636254883 320 9140.856727 7.90E-11 2.47E-06 -2.48E-06 8.65E-11 1.53E-06 1.64E-06 9.45E-11 7.08E-11 -2.364804077 2.360803223 1.540383911 1.639654541 321 9141.983858 -1.41E-10 2.47E-06 -2.48E-06 3.15E-11 1.53E-06 1.64E-06 9.49E-11 7.11E-11 -2.363180542 2.35920105 1.540826416 1.639944458 322 9143.125685 -4.75E-11 2.47E-06 -2.48E-06 7.00E-11 1.53E-06 1.65E-06 9.52E-11 7.15E-11 -2.362542725 2.35796814 1.541546631 1.64067688 323 9144.25339 -1.30E-10 2.47E-06 -2.48E-06 9.50E-12 1.53E-06 1.65E-06 9.61E-11 7.23E-11 -2.364910889 2.360617065 1.544146729 1.643026733 324 9145.392192 -9.00E-12 2.47E-06 -2.48E-06 7.00E-11 1.53E-06 1.65E-06 9.65E-11 7.28E-11 -2.362051392 2.357415771 1.54413147 1.64319458 325 9146.534891 -5.30E-11 2.47E-06 -2.48E-06 7.55E-11 1.54E-06 1.65E-06 9.70E-11 7.32E-11 -2.361782837 2.357522583 1.546173096 1.644992065 326 9147.67067 6.80E-11 2.47E-06 -2.48E-06 1.03E-10 1.54E-06 1.65E-06 9.75E-11 7.37E-11 -2.363189697 2.358966064 1.548779297 1.648138428 327 9148.806738 1.23E-10 2.47E-06 -2.49E-06 6.45E-11 1.54E-06 1.65E-06 9.81E-11 7.43E-11 -2.367544556 2.365307617 1.553115845 1.652572632 328 9149.957527 -2.55E-11 2.46E-06 -2.48E-06 1.36E-10 1.54E-06 1.65E-06 9.85E-11 7.46E-11 -2.361282349 2.35652771 1.550357056 1.649487305 329 9151.097786 -1.03E-10 2.47E-06 -2.48E-06 5.90E-11 1.54E-06 1.66E-06 9.88E-11 7.50E-11 -2.361633301 2.357244873 1.552890015 1.652093506 330 9152.234727 -4.75E-11 2.46E-06 -2.48E-06 7.55E-11 1.54E-06 1.66E-06 9.93E-11 7.55E-11 -2.361343384 2.356063843 1.553619385 1.653274536 331 9153.371956 -8.05E-11 2.47E-06 -2.48E-06 5.90E-11 1.54E-06 1.66E-06 9.99E-11 7.60E-11 -2.361312866 2.356893921 1.55617981 1.655834961 332 9154.509476 -4.75E-11 2.47E-06 -2.48E-06 4.25E-11 1.55E-06 1.66E-06 1.00E-10 7.65E-11 -2.3621521 2.357427979 1.559255981 1.659088135 333 9155.65451 -1.47E-10 2.47E-06 -2.48E-06 8.10E-11 1.55E-06 1.66E-06 1.01E-10 7.71E-11 -2.361367798 2.357418823 1.561474609 1.661444092 334 9156.792611 -8.60E-11 2.47E-06 -2.48E-06 1.53E-10 1.55E-06 1.67E-06 1.01E-10 7.73E-11 -2.364294434 2.360800171 1.565536499 1.665881348 335 9157.952688 -4.20E-11 2.47E-06 -2.48E-06 8.10E-11 1.55E-06 1.67E-06 1.02E-10 7.76E-11 -2.360653687 2.357150269 1.565304565 1.665585327 336 9159.076913 -2.02E-10 2.47E-06 -2.48E-06 7.00E-11 1.56E-06 1.67E-06 1.02E-10 7.78E-11 -2.361611938 2.357794189 1.568936157 1.669174194 337 9160.241199 -1.03E-10 2.47E-06 -2.48E-06 -1.50E-12 1.56E-06 1.67E-06 1.02E-10 7.79E-11 -2.362319946 2.359225464 1.572155762 1.67270813 338 9161.373234 -2.55E-11 2.47E-06 -2.48E-06 8.65E-11 1.56E-06 1.68E-06 1.02E-10 7.81E-11 -2.359988403 2.355502319 1.574176025 1.67460022 339 9162.5345 2.00E-12 2.47E-06 -2.48E-06 1.03E-10 1.56E-06 1.68E-06 1.02E-10 7.82E-11 -2.361752319 2.358206177 1.578088379 1.679147339 340 9163.670735 -4.20E-11 2.47E-06 -2.48E-06 1.36E-10 1.57E-06 1.68E-06 1.02E-10 7.78E-11 -2.360961914 2.356430054 1.580621338 1.681567383 341 9164.814499 1.85E-11 2.47E-06 -2.48E-06 1.25E-10 1.57E-06 1.69E-06 1.02E-10 7.77E-11 -2.359512329 2.35458374 1.5831604 1.683868408 342 9165.962175 1.30E-11 2.47E-06 -2.48E-06 1.09E-10 1.57E-06 1.69E-06 1.01E-10 7.71E-11 -2.36222229 2.358557129 1.587921143 1.689434814 343 9167.095659 -2.55E-11 2.47E-06 -2.48E-06 7.55E-11 1.58E-06 1.69E-06 1.01E-10 7.70E-11 -2.361196899 2.357449341 1.590771484 1.692025757 344 9168.247544 -9.00E-12 2.47E-06 -2.48E-06 8.10E-11 1.58E-06 1.70E-06 1.01E-10 7.71E-11 -2.363858032 2.360342407 1.595944214 1.697906494 345 9169.392478 -2.00E-11 2.46E-06 -2.48E-06 3.15E-11 1.58E-06 1.70E-06 1.01E-10 7.69E-11 -2.362008667 2.357824707 1.597454834 1.699462891 346 9170.537706 -1.74E-10 2.47E-06 -2.48E-06 3.15E-11 1.59E-06 1.70E-06 1.02E-10 7.73E-11 -2.362783813 2.358602905 1.600476074 1.702719116 347 9171.686851 -7.50E-11 2.47E-06 -2.48E-06 5.90E-11 1.59E-06 1.71E-06 1.01E-10 7.72E-11 -2.363006592 2.358856201 1.603012085 1.705145264 348 9172.829039 -1.03E-10 2.46E-06 -2.48E-06 9.75E-11 1.59E-06 1.71E-06 1.02E-10 7.72E-11 -2.359313965 2.353662109 1.602316284 1.704309082 349 9173.971518 -3.65E-11 2.47E-06 -2.48E-06 1.09E-10 1.59E-06 1.71E-06 1.02E-10 7.73E-11 -2.363070679 2.359487915 1.607623291 1.709936523 350 9175.114289 7.50E-12 2.46E-06 -2.48E-06 5.35E-11 1.60E-06 1.71E-06 1.02E-10 7.73E-11 -2.356799316 2.351766968 1.605169678 1.706933594 351 9176.26824 -4.20E-11 2.47E-06 -2.48E-06 8.10E-11 1.60E-06 1.71E-06 1.02E-10 7.72E-11 -2.359927368 2.356912231 1.609246826 1.711251831 352 9177.426117 1.30E-11 2.46E-06 -2.47E-06 9.20E-11 1.60E-06 1.72E-06 1.02E-10 7.73E-11 -2.352490234 2.348452759 1.604537964 1.705886841 353 9178.573401 -3.65E-11 2.44E-06 -2.45E-06 8.65E-11 1.60E-06 1.71E-06 1.02E-10 7.72E-11 -2.332409668 2.328274536 1.591030884 1.691970825 354 9179.724611 -2.55E-11 2.44E-06 -2.45E-06 1.14E-10 1.59E-06 1.71E-06 1.01E-10 7.70E-11 -2.339276123 2.33421936 1.595132446 1.697262573 355 9180.872484 -1.30E-10 2.46E-06 -2.47E-06 6.45E-11 1.59E-06 1.71E-06 1.02E-10 7.72E-11 -2.360092163 2.356039429 1.610632324 1.713363647 356 9182.017016 6.25E-11 2.47E-06 -2.48E-06 8.10E-11 1.59E-06 1.71E-06 1.02E-10 7.74E-11 -2.362759399 2.358850098 1.612838745 1.71546936 357 9183.165476 -4.75E-11 2.47E-06 -2.48E-06 9.50E-12 1.60E-06 1.71E-06 1.02E-10 7.77E-11 -2.363018799 2.359603882 1.613800049 1.716506958 358 9184.314231 -3.50E-12 2.47E-06 -2.48E-06 5.90E-11 1.60E-06 1.72E-06 1.02E-10 7.80E-11 -2.359115601 2.353875732 1.611413574 1.714047241 359 9185.459643 -3.65E-11 2.47E-06 -2.48E-06 8.10E-11 1.60E-06 1.72E-06 1.03E-10 7.81E-11 -2.364212036 2.360934448 1.616098022 1.718792725 360 9186.61626 -4.75E-11 2.47E-06 -2.48E-06 8.10E-11 1.60E-06 1.72E-06 1.03E-10 7.82E-11 -2.362493896 2.359109497 1.615670776 1.718380737 361 9187.776815 -5.30E-11 2.47E-06 -2.48E-06 7.55E-11 1.61E-06 1.72E-06 1.03E-10 7.84E-11 -2.363461304 2.359896851 1.61673584 1.719396973 362 9188.926751 5.70E-11 2.47E-06 -2.48E-06 -1.50E-12 1.61E-06 1.72E-06 1.03E-10 7.85E-11 -2.363265991 2.359680176 1.617752075 1.720422363 363 9190.073342 -6.40E-11 2.47E-06 -2.48E-06 1.14E-10 1.61E-06 1.73E-06 1.03E-10 7.87E-11 -2.361068726 2.357254028 1.617715454 1.720394897 364 9191.227508 2.00E-12 2.47E-06 -2.48E-06 8.10E-11 1.61E-06 1.73E-06 1.03E-10 7.88E-11 -2.362268066 2.357888794 1.619714355 1.72244873 365 9192.381972 -2.55E-11 2.47E-06 -2.48E-06 -1.50E-12 1.61E-06 1.73E-06 1.04E-10 7.90E-11 -2.359341431 2.353863525 1.619061279 1.721902466 366 9193.529446 -7.50E-11 2.47E-06 -2.48E-06 3.15E-11 1.61E-06 1.73E-06 1.04E-10 7.91E-11 -2.362387085 2.359866333 1.623672485 1.726498413 367 9194.677214 -8.05E-11 2.46E-06 -2.48E-06 2.05E-11 1.61E-06 1.73E-06 1.04E-10 7.93E-11 -2.357785034 2.353051758 1.621905518 1.724386597 368 9195.82892 2.00E-12 2.47E-06 -2.48E-06 7.00E-11 1.61E-06 1.73E-06 1.04E-10 7.96E-11 -2.363092041 2.35980835 1.627816772 1.730715942 369 9196.977276 4.05E-11 2.47E-06 -2.48E-06 5.90E-11 1.62E-06 1.73E-06 1.04E-10 7.97E-11 -2.362149048 2.358670044 1.629238892 1.732156372 370 9198.136867 4.05E-11 2.47E-06 -2.48E-06 5.35E-11 1.62E-06 1.74E-06 1.04E-10 7.98E-11 -2.363113403 2.359875488 1.631393433 1.734268188 371 9199.293109 2.95E-11 2.47E-06 -2.48E-06 1.09E-10 1.62E-06 1.74E-06 1.04E-10 7.97E-11 -2.357415771 2.351931763 1.62890625 1.731692505 372 9200.435054 7.50E-12 2.46E-06 -2.48E-06 1.09E-10 1.62E-06 1.74E-06 1.04E-10 7.96E-11 -2.360809326 2.357235718 1.63343811 1.73631897 373 9201.602837 -3.65E-11 2.46E-06 -2.48E-06 7.55E-11 1.62E-06 1.74E-06 1.04E-10 7.94E-11 -2.358569336 2.353411865 1.633184814 1.736407471 374 9202.74902 1.73E-10 2.47E-06 -2.48E-06 6.45E-11 1.62E-06 1.74E-06 1.04E-10 7.93E-11 -2.358004761 2.354229736 1.635070801 1.737921143 375 9203.90645 2.95E-11 2.46E-06 -2.48E-06 5.35E-11 1.62E-06 1.74E-06 1.04E-10 7.95E-11 -2.355429077 2.349932861 1.634893799 1.738238525 376 9205.049568 -3.65E-11 2.47E-06 -2.48E-06 1.31E-10 1.63E-06 1.75E-06 1.04E-10 7.96E-11 -2.362374878 2.358773804 1.641479492 1.744943237 377 9206.211245 8.45E-11 2.46E-06 -2.48E-06 -4.00E-11 1.63E-06 1.75E-06 1.04E-10 7.97E-11 -2.358700562 2.353924561 1.640515137 1.74395752 378 9207.354949 5.70E-11 2.46E-06 -2.48E-06 1.47E-10 1.63E-06 1.75E-06 1.04E-10 7.96E-11 -2.358197021 2.354574585 1.642138672 1.745513916 379 9208.524533 1.23E-10 2.46E-06 -2.48E-06 2.60E-11 1.63E-06 1.75E-06 1.04E-10 7.93E-11 -2.358227539 2.354040527 1.643017578 1.746612549 380 9209.683451 -9.00E-12 2.46E-06 -2.48E-06 1.14E-10 1.63E-06 1.75E-06 1.04E-10 7.89E-11 -2.361077881 2.358050537 1.646572876 1.750393677 381 9210.831697 7.35E-11 2.47E-06 -2.48E-06 7.55E-11 1.63E-06 1.75E-06 1.04E-10 7.87E-11 -2.357885742 2.354101563 1.646206665 1.749752808 382 9211.980236 1.45E-10 2.46E-06 -2.48E-06 9.75E-11 1.64E-06 1.76E-06 1.04E-10 7.90E-11 -2.356744385 2.351925659 1.645806885 1.749465942 383 9213.140046 -3.65E-11 2.46E-06 -2.48E-06 9.75E-11 1.64E-06 1.76E-06 1.04E-10 7.94E-11 -2.358865356 2.355499268 1.648556519 1.751876831 384 9214.292834 -2.55E-11 2.46E-06 -2.48E-06 7.55E-11 1.64E-06 1.76E-06 1.05E-10 7.99E-11 -2.355102539 2.349981689 1.646081543 1.749511719 385 9215.456902 -1.14E-10 2.46E-06 -2.48E-06 9.20E-11 1.64E-06 1.76E-06 1.05E-10 8.01E-11 -2.358203125 2.354153442 1.64927063 1.752941895 386 9216.60296 -8.05E-11 2.46E-06 -2.47E-06 9.20E-11 1.64E-06 1.76E-06 1.05E-10 8.01E-11 -2.35741272 2.353430176 1.649041748 1.752496338 387 9217.771288 -8.60E-11 2.46E-06 -2.48E-06 5.35E-11 1.64E-06 1.76E-06 1.05E-10 8.01E-11 -2.357562256 2.353939819 1.649682617 1.753186035 388 9218.917937 -9.00E-12 2.45E-06 -2.47E-06 8.10E-11 1.64E-06 1.76E-06 1.05E-10 8.03E-11 -2.341235352 2.336212158 1.638485718 1.741766357 389 9220.075871 -3.50E-12 2.44E-06 -2.45E-06 7.55E-11 1.64E-06 1.75E-06 1.06E-10 8.05E-11 -2.333129883 2.329849243 1.633837891 1.736364746 390 9221.241436 2.00E-12 2.44E-06 -2.46E-06 4.25E-11 1.63E-06 1.75E-06 1.06E-10 8.05E-11 -2.342218018 2.33788147 1.641369629 1.743740845 391 9222.399968 6.25E-11 2.46E-06 -2.47E-06 6.45E-11 1.63E-06 1.75E-06 1.06E-10 8.08E-11 -2.355477905 2.35067749 1.650701904 1.75385437 392 9223.562467 7.50E-12 2.46E-06 -2.48E-06 1.50E-11 1.63E-06 1.75E-06 1.06E-10 8.10E-11 -2.357559204 2.352862549 1.652615356 1.756332397 393 9224.71426 -3.65E-11 2.47E-06 -2.48E-06 5.90E-11 1.64E-06 1.76E-06 1.06E-10 8.13E-11 -2.361477661 2.357907104 1.656484985 1.760562134 394 9225.877356 -4.75E-11 2.46E-06 -2.47E-06 5.35E-11 1.64E-06 1.76E-06 1.07E-10 8.17E-11 -2.353140259 2.347177124 1.651156616 1.754864502 395 9227.037082 2.00E-12 2.46E-06 -2.48E-06 5.35E-11 1.65E-06 1.77E-06 1.07E-10 8.21E-11 -2.358843994 2.355349731 1.657107544 1.760925293 396 9228.208121 -1.19E-10 2.46E-06 -2.47E-06 5.90E-11 1.65E-06 1.77E-06 1.08E-10 8.26E-11 -2.356204224 2.351681519 1.656640625 1.760525513 397 9229.37212 -1.45E-11 2.47E-06 -2.48E-06 4.25E-11 1.65E-06 1.77E-06 1.08E-10 8.28E-11 -2.35769043 2.354159546 1.660595703 1.764089966 398 9230.536419 7.50E-12 2.46E-06 -2.48E-06 5.35E-11 1.65E-06 1.77E-06 1.08E-10 8.31E-11 -2.358660889 2.354208374 1.662661743 1.766751099 399 9231.689996 -1.96E-10 2.46E-06 -2.48E-06 2.05E-11 1.65E-06 1.77E-06 1.09E-10 8.35E-11 -2.356695557 2.351968384 1.662811279 1.767007446 400 9232.847544 -5.30E-11 2.46E-06 -2.48E-06 5.35E-11 1.65E-06 1.77E-06 1.09E-10 8.40E-11 -2.356420898 2.35218811 1.664950562 1.769317627 401 9234.012742 -7.50E-11 2.46E-06 -2.47E-06 1.14E-10 1.65E-06 1.78E-06 1.10E-10 8.44E-11 -2.354003906 2.348681641 1.665328979 1.76975708 402 9235.178241 1.23E-10 2.46E-06 -2.48E-06 8.10E-11 1.66E-06 1.78E-06 1.10E-10 8.46E-11 -2.360089111 2.357009888 1.671893311 1.776635742 403 9236.344041 -3.10E-11 2.46E-06 -2.48E-06 4.80E-11 1.66E-06 1.78E-06 1.10E-10 8.49E-11 -2.35809021 2.354000854 1.672402954 1.777108765 404 9237.499105 -5.30E-11 2.46E-06 -2.47E-06 1.69E-10 1.66E-06 1.78E-06 1.10E-10 8.51E-11 -2.3550354 2.350045776 1.671725464 1.776409912 405 9238.669185 2.40E-11 2.46E-06 -2.48E-06 1.50E-11 1.66E-06 1.78E-06 1.11E-10 8.53E-11 -2.359362793 2.355474854 1.676470947 1.781442261 406 9239.828526 -9.00E-12 2.46E-06 -2.47E-06 7.55E-11 1.66E-06 1.79E-06 1.11E-10 8.52E-11 -2.35657959 2.353823853 1.676733398 1.7818573 407 9240.984483 -5.30E-11 2.46E-06 -2.48E-06 3.15E-11 1.67E-06 1.79E-06 1.11E-10 8.53E-11 -2.354797363 2.349609375 1.676580811 1.781414795 408 9242.166517 1.30E-11 2.46E-06 -2.47E-06 6.45E-11 1.67E-06 1.79E-06 1.11E-10 8.53E-11 -2.357171631 2.353317261 1.679989624 1.784805298 409 9243.315705 2.00E-12 2.46E-06 -2.47E-06 5.90E-11 1.67E-06 1.79E-06 1.11E-10 8.55E-11 -2.352828979 2.347756958 1.677468872 1.782299805 410 9244.487295 -1.19E-10 2.46E-06 -2.47E-06 1.25E-10 1.67E-06 1.79E-06 1.11E-10 8.58E-11 -2.355889893 2.351953125 1.680987549 1.785870361 411 9245.651817 -9.70E-11 2.46E-06 -2.47E-06 6.45E-11 1.67E-06 1.79E-06 1.11E-10 8.58E-11 -2.350622559 2.345385742 1.678335571 1.782962036 412 9246.81664 2.40E-11 2.46E-06 -2.47E-06 1.47E-10 1.67E-06 1.79E-06 1.11E-10 8.59E-11 -2.35696106 2.354470825 1.683850098 1.789178467 413 9247.989139 -6.95E-11 2.46E-06 -2.47E-06 1.64E-10 1.67E-06 1.79E-06 1.11E-10 8.60E-11 -2.352319336 2.348071289 1.681768799 1.786914063 414 9249.147188 -1.36E-10 2.46E-06 -2.48E-06 7.00E-11 1.67E-06 1.79E-06 1.11E-10 8.60E-11 -2.358248901 2.355490112 1.687374878 1.792687988 415 9250.320292 -4.20E-11 2.46E-06 -2.47E-06 4.80E-11 1.67E-06 1.79E-06 1.12E-10 8.61E-11 -2.354199219 2.350680542 1.68576355 1.791131592 416 9251.478939 -2.55E-11 2.46E-06 -2.47E-06 5.35E-11 1.68E-06 1.80E-06 1.12E-10 8.61E-11 -2.354086304 2.350033569 1.687030029 1.792056274 417 9252.652649 -3.50E-12 2.46E-06 -2.47E-06 8.65E-11 1.68E-06 1.80E-06 1.12E-10 8.62E-11 -2.353790283 2.348370361 1.687612915 1.792816162 418 9253.822971 1.85E-11 2.46E-06 -2.47E-06 8.10E-11 1.68E-06 1.80E-06 1.12E-10 8.63E-11 -2.355978394 2.352749634 1.690670776 1.796170044 419 9254.98621 -1.03E-10 2.46E-06 -2.47E-06 5.90E-11 1.68E-06 1.80E-06 1.12E-10 8.67E-11 -2.355102539 2.35050354 1.690942383 1.79624939 420 9256.149748 -5.30E-11 2.46E-06 -2.47E-06 3.15E-11 1.68E-06 1.80E-06 1.12E-10 8.66E-11 -2.357568359 2.35440979 1.694778442 1.800091553 421 9257.320977 -8.60E-11 2.46E-06 -2.47E-06 4.80E-11 1.68E-06 1.80E-06 1.12E-10 8.67E-11 -2.353604126 2.34932251 1.693533325 1.798855591 422 9258.492509 -3.10E-11 2.46E-06 -2.47E-06 6.45E-11 1.68E-06 1.81E-06 1.12E-10 8.67E-11 -2.354815674 2.351779175 1.695843506 1.801055908 423 9259.660647 7.90E-11 2.46E-06 -2.47E-06 9.20E-11 1.69E-06 1.81E-06 1.13E-10 8.69E-11 -2.352182007 2.348190308 1.695492554 1.800616455 424 9260.836483 2.95E-11 2.46E-06 -2.47E-06 1.09E-10 1.69E-06 1.81E-06 1.13E-10 8.69E-11 -2.354397583 2.350393677 1.697979736 1.803427124 425 9262.005228 -9.00E-12 2.46E-06 -2.47E-06 1.14E-10 1.69E-06 1.81E-06 1.13E-10 8.70E-11 -2.352572632 2.347967529 1.697763062 1.803121948 426 9263.159474 4.05E-11 2.46E-06 -2.47E-06 4.80E-11 1.69E-06 1.81E-06 1.13E-10 8.70E-11 -2.352645874 2.347851563 1.699679565 1.805282593 427 9264.339921 2.00E-12 2.46E-06 -2.47E-06 4.80E-11 1.69E-06 1.81E-06 1.13E-10 8.71E-11 -2.353518677 2.348620605 1.701864624 1.807641602 428 9265.520677 5.15E-11 2.46E-06 -2.47E-06 8.65E-11 1.69E-06 1.81E-06 1.13E-10 8.71E-11 -2.351104736 2.346536255 1.702612305 1.808404541 429 9266.679523 -6.40E-11 2.46E-06 -2.47E-06 5.90E-11 1.69E-06 1.81E-06 1.13E-10 8.70E-11 -2.351760864 2.348257446 1.705593872 1.811383057 430 9267.86089 -9.00E-12 2.46E-06 -2.47E-06 7.00E-11 1.69E-06 1.82E-06 1.13E-10 8.71E-11 -2.355612183 2.351852417 1.709750366 1.815893555 431 9269.027745 -9.70E-11 2.46E-06 -2.47E-06 -2.35E-11 1.70E-06 1.82E-06 1.13E-10 8.72E-11 -2.352600098 2.348452759 1.70960083 1.815933228 432 9270.202313 -1.19E-10 2.46E-06 -2.47E-06 5.90E-11 1.70E-06 1.82E-06 1.13E-10 8.73E-11 -2.352880859 2.349035645 1.711947632 1.818325806 433 9271.362359 -9.00E-12 2.45E-06 -2.47E-06 8.65E-11 1.70E-06 1.82E-06 1.13E-10 8.75E-11 -2.352386475 2.34861145 1.714242554 1.820581055 434 9272.552363 -7.50E-11 2.46E-06 -2.47E-06 1.09E-10 1.70E-06 1.83E-06 1.13E-10 8.76E-11 -2.351141357 2.346463013 1.715536499 1.821932983 435 9273.720429 -7.50E-11 2.46E-06 -2.47E-06 3.70E-11 1.71E-06 1.83E-06 1.13E-10 8.74E-11 -2.3525177 2.348297119 1.718539429 1.825134277 436 9274.892505 2.40E-11 2.46E-06 -2.47E-06 8.65E-11 1.71E-06 1.83E-06 1.13E-10 8.75E-11 -2.350613403 2.346170044 1.719033813 1.825952148 437 9276.061174 5.70E-11 2.46E-06 -2.47E-06 4.80E-11 1.71E-06 1.83E-06 1.14E-10 8.77E-11 -2.351031494 2.347195435 1.72199707 1.828652954 438 9277.233856 -4.20E-11 2.46E-06 -2.47E-06 1.20E-10 1.71E-06 1.83E-06 1.14E-10 8.78E-11 -2.351708984 2.347857666 1.724014282 1.831002808 439 9278.406842 2.95E-11 2.46E-06 -2.47E-06 3.70E-11 1.71E-06 1.84E-06 1.14E-10 8.82E-11 -2.352398682 2.34770813 1.725921631 1.833087158 440 9279.580132 8.45E-11 2.46E-06 -2.47E-06 8.65E-11 1.71E-06 1.84E-06 1.14E-10 8.84E-11 -2.354888916 2.351730347 1.730145264 1.837219238 441 9280.75744 3.50E-11 2.45E-06 -2.47E-06 3.15E-11 1.72E-06 1.84E-06 1.14E-10 8.84E-11 -2.350189209 2.345153809 1.72762146 1.834527588 442 9281.935053 -3.10E-11 2.46E-06 -2.47E-06 1.20E-10 1.72E-06 1.84E-06 1.14E-10 8.85E-11 -2.353652954 2.350006104 1.731881714 1.838900757 443 9283.101824 -1.36E-10 2.45E-06 -2.47E-06 1.20E-10 1.72E-06 1.84E-06 1.15E-10 8.86E-11 -2.348358154 2.343496704 1.729656982 1.836569214 444 9284.276329 1.23E-10 2.46E-06 -2.47E-06 7.55E-11 1.72E-06 1.85E-06 1.15E-10 8.86E-11 -2.351611328 2.347399902 1.73359375 1.840997314 445 9285.443703 -1.19E-10 2.46E-06 -2.47E-06 1.09E-10 1.72E-06 1.85E-06 1.15E-10 8.89E-11 -2.350177002 2.345574951 1.733532715 1.840515137 446 9286.618815 -1.36E-10 2.45E-06 -2.47E-06 -1.50E-12 1.72E-06 1.85E-06 1.15E-10 8.89E-11 -2.35027771 2.345419312 1.735125732 1.842599487 447 9287.805392 -2.00E-11 2.46E-06 -2.47E-06 5.35E-11 1.73E-06 1.85E-06 1.15E-10 8.88E-11 -2.353094482 2.350082397 1.739294434 1.846676636 448 9288.969953 -4.20E-11 2.45E-06 -2.47E-06 1.03E-10 1.73E-06 1.85E-06 1.15E-10 8.89E-11 -2.351309204 2.347311401 1.739086914 1.846643066 449 9290.16459 -9.70E-11 2.46E-06 -2.47E-06 5.90E-11 1.73E-06 1.85E-06 1.15E-10 8.89E-11 -2.348428345 2.343612671 1.738604736 1.845825195 450 9291.337203 -4.20E-11 2.46E-06 -2.47E-06 9.50E-12 1.73E-06 1.85E-06 1.15E-10 8.89E-11 -2.352633667 2.348834229 1.743386841 1.850973511 451 9292.513843 -9.15E-11 2.45E-06 -2.47E-06 7.55E-11 1.73E-06 1.85E-06 1.15E-10 8.90E-11 -2.349499512 2.344946289 1.742172241 1.849682617 452 9293.690788 4.05E-11 2.46E-06 -2.47E-06 1.50E-11 1.73E-06 1.86E-06 1.15E-10 8.91E-11 -2.350164795 2.346047974 1.743817139 1.851525879 453 9294.871765 1.51E-10 2.45E-06 -2.47E-06 6.45E-11 1.73E-06 1.86E-06 1.15E-10 8.93E-11 -2.348956299 2.343814087 1.744592285 1.852105713 454 9296.045594 -1.03E-10 2.46E-06 -2.47E-06 1.20E-10 1.74E-06 1.86E-06 1.16E-10 8.95E-11 -2.351483154 2.347714233 1.748498535 1.856472778 455 9297.230911 7.50E-12 2.46E-06 -2.47E-06 3.70E-11 1.74E-06 1.86E-06 1.16E-10 8.96E-11 -2.35317688 2.34982605 1.75151062 1.859301758 456 9298.40908 -6.95E-11 2.46E-06 -2.47E-06 7.00E-11 1.74E-06 1.86E-06 1.16E-10 8.98E-11 -2.350924683 2.346420288 1.751123047 1.858883667 457 9299.591284 -1.45E-11 2.46E-06 -2.47E-06 9.75E-11 1.74E-06 1.87E-06 1.16E-10 9.00E-11 -2.352502441 2.349523926 1.754592896 1.862722778 458 9300.770066 -9.15E-11 2.45E-06 -2.47E-06 9.20E-11 1.74E-06 1.87E-06 1.16E-10 9.00E-11 -2.348602295 2.344927979 1.753201294 1.860894775 459 9301.949153 2.00E-12 2.46E-06 -2.47E-06 1.58E-10 1.74E-06 1.87E-06 1.17E-10 9.03E-11 -2.353286743 2.350485229 1.758505249 1.866705322 460 9303.124813 7.50E-12 2.45E-06 -2.47E-06 2.05E-11 1.75E-06 1.87E-06 1.17E-10 9.03E-11 -2.345983887 2.340359497 1.75473938 1.862612915 461 9304.300778 -9.15E-11 2.46E-06 -2.47E-06 1.47E-10 1.75E-06 1.87E-06 1.17E-10 9.05E-11 -2.34967041 2.345574951 1.759051514 1.866998291 462 9305.477047 3.50E-11 2.46E-06 -2.47E-06 5.90E-11 1.75E-06 1.87E-06 1.17E-10 9.08E-11 -2.35055542 2.345812988 1.760604858 1.868765259 463 9306.661092 2.00E-12 2.45E-06 -2.47E-06 4.80E-11 1.75E-06 1.87E-06 1.17E-10 9.10E-11 -2.34984436 2.34548645 1.762625122 1.870837402 464 9307.834236 1.56E-10 2.46E-06 -2.47E-06 5.35E-11 1.75E-06 1.88E-06 1.18E-10 9.15E-11 -2.349395752 2.344998169 1.763891602 1.872415161 465 9309.018895 -4.20E-11 2.45E-06 -2.47E-06 4.25E-11 1.75E-06 1.88E-06 1.18E-10 9.17E-11 -2.353009033 2.351156616 1.769049072 1.877545166 466 9310.207601 7.90E-11 2.45E-06 -2.47E-06 1.31E-10 1.76E-06 1.88E-06 1.18E-10 9.20E-11 -2.345343018 2.3400177 1.764169312 1.872665405 467 9311.377921 -3.65E-11 2.46E-06 -2.47E-06 9.75E-11 1.76E-06 1.88E-06 1.19E-10 9.22E-11 -2.350482178 2.347265625 1.770123291 1.879067993 468 9312.570984 -9.00E-12 2.45E-06 -2.46E-06 3.70E-11 1.76E-06 1.88E-06 1.19E-10 9.23E-11 -2.345043945 2.340753174 1.767416382 1.876062012 469 9313.76062 -1.25E-10 2.45E-06 -2.46E-06 1.50E-11 1.76E-06 1.88E-06 1.19E-10 9.25E-11 -2.345901489 2.342218018 1.770535278 1.879116821 470 9314.931854 4.60E-11 2.45E-06 -2.46E-06 5.35E-11 1.76E-06 1.89E-06 1.19E-10 9.25E-11 -2.342312622 2.337094116 1.769818115 1.878070068 471 9316.107133 1.18E-10 2.45E-06 -2.46E-06 1.03E-10 1.76E-06 1.89E-06 1.19E-10 9.27E-11 -2.347573853 2.343927002 1.775308228 1.88430481 472 9317.297693 -9.00E-12 2.45E-06 -2.46E-06 3.15E-11 1.76E-06 1.89E-06 1.19E-10 9.29E-11 -2.346005249 2.341574097 1.776141357 1.885037231 473 9318.481074 -1.36E-10 2.45E-06 -2.46E-06 4.25E-11 1.77E-06 1.89E-06 1.20E-10 9.31E-11 -2.342944336 2.339224243 1.775396729 1.884280396 474 9319.664763 -1.03E-10 2.43E-06 -2.44E-06 1.36E-10 1.76E-06 1.89E-06 1.20E-10 9.33E-11 -2.30843811 2.304745483 1.750912476 1.858099365 475 9320.845012 4.60E-11 2.43E-06 -2.45E-06 8.65E-11 1.76E-06 1.89E-06 1.20E-10 9.32E-11 -2.338409424 2.334725952 1.775787354 1.884637451 476 9322.033064 -4.75E-11 2.45E-06 -2.47E-06 9.75E-11 1.76E-06 1.89E-06 1.20E-10 9.33E-11 -2.346060181 2.34168396 1.783441162 1.892730713 477 9323.213927 -8.05E-11 2.46E-06 -2.47E-06 -1.50E-12 1.77E-06 1.89E-06 1.20E-10 9.34E-11 -2.34828186 2.345040894 1.786669922 1.895904541 478 9324.398847 -1.14E-10 2.45E-06 -2.46E-06 9.20E-11 1.77E-06 1.90E-06 1.20E-10 9.37E-11 -2.342654419 2.337478638 1.784112549 1.893292236 479 9325.576572 -1.45E-11 2.45E-06 -2.47E-06 8.65E-11 1.78E-06 1.90E-06 1.21E-10 9.41E-11 -2.347619629 2.343508911 1.78890686 1.898266602 480 9326.769611 1.23E-10 2.45E-06 -2.46E-06 1.03E-10 1.78E-06 1.90E-06 1.21E-10 9.42E-11 -2.346826172 2.343200684 1.789959717 1.898825073 481 9327.95921 -1.80E-10 2.45E-06 -2.46E-06 7.55E-11 1.78E-06 1.91E-06 1.21E-10 9.43E-11 -2.345181274 2.340765381 1.789242554 1.898458862 482 9329.137856 -6.40E-11 2.43E-06 -2.45E-06 1.09E-10 1.78E-06 1.90E-06 1.21E-10 9.44E-11 -2.320516968 2.317651367 1.771600342 1.880194092 483 9330.316808 -7.50E-11 2.43E-06 -2.44E-06 3.70E-11 1.77E-06 1.90E-06 1.21E-10 9.41E-11 -2.330053711 2.325445557 1.780703735 1.88927002 484 9331.514845 -5.85E-11 2.45E-06 -2.47E-06 2.60E-11 1.77E-06 1.90E-06 1.21E-10 9.43E-11 -2.349456787 2.346563721 1.797323608 1.90663147 485 9332.713196 1.85E-11 2.45E-06 -2.47E-06 7.55E-11 1.78E-06 1.90E-06 1.21E-10 9.45E-11 -2.345187378 2.340222168 1.795193481 1.904858398 486 9333.881799 3.50E-11 2.45E-06 -2.46E-06 7.55E-11 1.78E-06 1.91E-06 1.21E-10 9.46E-11 -2.348114014 2.344604492 1.799716187 1.909335327 487 9335.077014 -5.85E-11 2.45E-06 -2.46E-06 1.50E-11 1.79E-06 1.91E-06 1.22E-10 9.50E-11 -2.344873047 2.339422607 1.797091675 1.906832886 488 9336.249982 -9.70E-11 2.45E-06 -2.47E-06 1.25E-10 1.79E-06 1.92E-06 1.22E-10 9.52E-11 -2.348876953 2.344558716 1.802328491 1.912115479 489 9337.442057 -2.55E-11 2.45E-06 -2.46E-06 9.75E-11 1.79E-06 1.92E-06 1.22E-10 9.54E-11 -2.345843506 2.340991211 1.80218811 1.911645508 490 9338.623158 4.60E-11 2.46E-06 -2.47E-06 3.70E-11 1.79E-06 1.92E-06 1.23E-10 9.59E-11 -2.349182129 2.34616394 1.806549072 1.916760254 491 9339.808328 -3.65E-11 2.45E-06 -2.47E-06 4.25E-11 1.79E-06 1.92E-06 1.23E-10 9.62E-11 -2.34664917 2.342062378 1.8052948 1.915512085 492 9341.001333 5.15E-11 2.45E-06 -2.47E-06 1.20E-10 1.80E-06 1.92E-06 1.23E-10 9.64E-11 -2.345880127 2.341470337 1.807174683 1.917181396 493 9342.18712 -9.00E-12 2.45E-06 -2.47E-06 8.65E-11 1.80E-06 1.92E-06 1.23E-10 9.64E-11 -2.348587036 2.345648193 1.811380005 1.921200562 494 9343.384513 9.00E-11 2.45E-06 -2.46E-06 4.00E-12 1.80E-06 1.93E-06 1.23E-10 9.65E-11 -2.344448853 2.339367676 1.809463501 1.919067383 495 9344.563386 1.30E-11 2.45E-06 -2.46E-06 9.75E-11 1.80E-06 1.93E-06 1.23E-10 9.65E-11 -2.339001465 2.334210205 1.807189941 1.916491699 496 9345.753867 -4.75E-11 2.44E-06 -2.46E-06 9.75E-11 1.80E-06 1.93E-06 1.24E-10 9.67E-11 -2.341351318 2.336981201 1.81104126 1.920562744 497 9346.955965 -9.70E-11 2.45E-06 -2.46E-06 7.00E-11 1.80E-06 1.93E-06 1.24E-10 9.69E-11 -2.342996216 2.338891602 1.813885498 1.923574829 498 9348.135761 -1.36E-10 2.45E-06 -2.47E-06 9.50E-12 1.80E-06 1.93E-06 1.24E-10 9.69E-11 -2.346740723 2.342666626 1.818487549 1.92850647 499 9349.330945 4.60E-11 2.45E-06 -2.46E-06 8.65E-11 1.80E-06 1.93E-06 1.24E-10 9.71E-11 -2.34604187 2.34258728 1.820425415 1.930526733 500 9350.526441 3.50E-11 2.45E-06 -2.47E-06 3.70E-11 1.81E-06 1.93E-06 1.24E-10 9.73E-11 -2.345101929 2.341070557 1.821350098 1.93163147 501 9351.726023 -2.51E-10 2.45E-06 -2.46E-06 3.15E-11 1.81E-06 1.94E-06 1.24E-10 9.73E-11 -2.347171021 2.343673706 1.824554443 1.934707642 502 9352.907052 2.95E-11 2.45E-06 -2.46E-06 1.14E-10 1.81E-06 1.94E-06 1.24E-10 9.75E-11 -2.343032837 2.338217163 1.822714233 1.932815552 503 9354.09971 5.15E-11 2.45E-06 -2.46E-06 4.00E-12 1.81E-06 1.94E-06 1.24E-10 9.75E-11 -2.346435547 2.343026733 1.827322388 1.937054443 504 9355.288903 -4.20E-11 2.45E-06 -2.46E-06 9.20E-11 1.81E-06 1.94E-06 1.25E-10 9.76E-11 -2.341122437 2.336315918 1.823831177 1.934405518 505 9356.478406 -4.75E-11 2.45E-06 -2.46E-06 4.25E-11 1.81E-06 1.94E-06 1.25E-10 9.80E-11 -2.340383911 2.335900879 1.824554443 1.934771729 506 9357.68333 -4.20E-11 2.43E-06 -2.45E-06 1.20E-10 1.81E-06 1.94E-06 1.25E-10 9.79E-11 -2.324105835 2.318518066 1.813598633 1.922589111 507 9358.877234 -5.30E-11 2.42E-06 -2.44E-06 3.70E-11 1.81E-06 1.94E-06 1.25E-10 9.76E-11 -2.319052124 2.316448975 1.811853027 1.920901489 508 9360.079011 -9.00E-12 2.42E-06 -2.43E-06 2.60E-11 1.81E-06 1.93E-06 1.24E-10 9.74E-11 -2.314111328 2.310263062 1.808441162 1.918218994 509 9361.269761 -9.15E-11 2.42E-06 -2.43E-06 1.31E-10 1.80E-06 1.93E-06 1.24E-10 9.72E-11 -2.321188354 2.31675415 1.81368103 1.92427063 510 9362.464602 1.23E-10 2.44E-06 -2.45E-06 4.00E-12 1.80E-06 1.93E-06 1.24E-10 9.75E-11 -2.339541626 2.336605835 1.831039429 1.94201355 511 9363.724061 2.40E-11 2.45E-06 -2.46E-06 3.70E-11 1.81E-06 1.94E-06 1.25E-10 9.77E-11 -2.343386841 2.339120483 1.835836792 1.945983887 512 9364.953597 -8.60E-11 2.45E-06 -2.46E-06 7.55E-11 1.81E-06 1.94E-06 1.25E-10 9.79E-11 -2.340078735 2.334750366 1.833139038 1.943960571 513 9366.122909 -5.30E-11 2.45E-06 -2.46E-06 1.14E-10 1.82E-06 1.95E-06 1.25E-10 9.83E-11 -2.344525146 2.340222168 1.838201904 1.949221802 514 9367.296305 5.70E-11 2.45E-06 -2.46E-06 7.00E-11 1.83E-06 1.95E-06 1.25E-10 9.83E-11 -2.340597534 2.335067749 1.836373901 1.947067261 515 9368.473788 6.25E-11 2.45E-06 -2.46E-06 1.36E-10 1.83E-06 1.96E-06 1.26E-10 9.85E-11 -2.345092773 2.342462158 1.841772461 1.952902222 516 9369.685663 -3.50E-12 2.45E-06 -2.46E-06 4.25E-11 1.83E-06 1.96E-06 1.26E-10 9.85E-11 -2.342840576 2.339257813 1.841104126 1.952020264 517 9370.875127 -8.05E-11 2.45E-06 -2.46E-06 7.00E-11 1.83E-06 1.96E-06 1.26E-10 9.88E-11 -2.343191528 2.33890686 1.842199707 1.953161621 518 9372.057322 -2.46E-10 2.45E-06 -2.46E-06 6.45E-11 1.83E-06 1.96E-06 1.26E-10 9.89E-11 -2.342959595 2.338922119 1.843499756 1.954653931 519 9373.247402 5.15E-11 2.45E-06 -2.46E-06 9.75E-11 1.83E-06 1.96E-06 1.26E-10 9.90E-11 -2.344174194 2.340518188 1.84614563 1.957006836 520 9374.445375 -1.45E-11 2.45E-06 -2.46E-06 9.50E-12 1.83E-06 1.96E-06 1.27E-10 9.93E-11 -2.339971924 2.336080933 1.844113159 1.955175781 521 9375.639869 -6.95E-11 2.45E-06 -2.46E-06 4.80E-11 1.84E-06 1.96E-06 1.27E-10 9.92E-11 -2.339251709 2.334136963 1.844497681 1.955496216 522 9376.823293 7.50E-12 2.44E-06 -2.46E-06 5.90E-11 1.84E-06 1.97E-06 1.27E-10 9.94E-11 -2.340634155 2.336297607 1.846774292 1.957589722 523 9378.029791 -3.65E-11 2.45E-06 -2.46E-06 -1.80E-11 1.84E-06 1.97E-06 1.27E-10 9.94E-11 -2.342092896 2.338574219 1.849407959 1.960321045 524 9379.221424 5.15E-11 2.44E-06 -2.46E-06 3.15E-11 1.84E-06 1.97E-06 1.27E-10 9.95E-11 -2.338925171 2.334463501 1.848294067 1.959283447 525 9380.436146 -4.75E-11 2.45E-06 -2.46E-06 4.25E-11 1.84E-06 1.97E-06 1.27E-10 9.98E-11 -2.342669678 2.3381073 1.852807617 1.963909912 526 9381.624607 7.35E-11 2.44E-06 -2.46E-06 9.20E-11 1.84E-06 1.97E-06 1.27E-10 9.96E-11 -2.34317627 2.339709473 1.85475769 1.965911865 527 9382.824773 3.50E-11 2.45E-06 -2.46E-06 1.09E-10 1.84E-06 1.97E-06 1.27E-10 9.98E-11 -2.342907715 2.339312744 1.85640564 1.967849731 528 9384.03665 -1.08E-10 2.44E-06 -2.46E-06 6.45E-11 1.84E-06 1.97E-06 1.27E-10 9.99E-11 -2.340823364 2.336691284 1.856265259 1.967507935 529 9385.237447 -9.70E-11 2.45E-06 -2.46E-06 6.45E-11 1.85E-06 1.97E-06 1.27E-10 1.00E-10 -2.337225342 2.332443237 1.85531311 1.966461182 530 9386.438558 -3.50E-12 2.44E-06 -2.46E-06 7.00E-11 1.85E-06 1.98E-06 1.28E-10 1.00E-10 -2.340093994 2.336169434 1.859204102 1.970199585 531 9387.639984 -2.55E-11 2.44E-06 -2.46E-06 4.80E-11 1.85E-06 1.98E-06 1.28E-10 1.01E-10 -2.336920166 2.331677246 1.858157349 1.968862915 532 9388.841725 -1.08E-10 2.44E-06 -2.46E-06 3.15E-11 1.85E-06 1.98E-06 1.28E-10 1.01E-10 -2.337240601 2.333734131 1.860458374 1.971414185 533 9390.032367 -4.75E-11 2.44E-06 -2.45E-06 1.42E-10 1.85E-06 1.98E-06 1.28E-10 1.01E-10 -2.332772827 2.328771973 1.858779907 1.969274902 534 9391.242345 -3.10E-11 2.44E-06 -2.46E-06 4.80E-11 1.85E-06 1.98E-06 1.28E-10 1.01E-10 -2.338864136 2.33581543 1.865664673 1.976754761 535 9392.452643 2.40E-11 2.44E-06 -2.46E-06 5.90E-11 1.85E-06 1.98E-06 1.28E-10 1.01E-10 -2.340454102 2.336477661 1.868624878 1.979528809 536 9393.655645 -4.20E-11 2.45E-06 -2.46E-06 9.75E-11 1.85E-06 1.98E-06 1.29E-10 1.01E-10 -2.340359497 2.336117554 1.870257568 1.981500244 537 9394.86277 -1.91E-10 2.44E-06 -2.46E-06 1.69E-10 1.86E-06 1.99E-06 1.29E-10 1.01E-10 -2.33742981 2.332418823 1.869293213 1.980349731 538 9396.070213 -3.65E-11 2.44E-06 -2.46E-06 9.20E-11 1.86E-06 1.99E-06 1.29E-10 1.01E-10 -2.333877563 2.328201294 1.868218994 1.979394531 539 9397.266542 -1.85E-10 2.44E-06 -2.45E-06 7.00E-11 1.86E-06 1.99E-06 1.29E-10 1.01E-10 -2.337295532 2.333990479 1.873306274 1.984463501 540 9398.470806 -3.50E-12 2.44E-06 -2.45E-06 2.60E-11 1.86E-06 1.99E-06 1.29E-10 1.01E-10 -2.331756592 2.32678833 1.870523071 1.981539917 541 9399.679198 -4.75E-11 2.43E-06 -2.44E-06 1.31E-10 1.86E-06 1.99E-06 1.29E-10 1.02E-10 -2.321392822 2.317120361 1.864804077 1.974795532 542 9400.895536 -2.00E-11 2.41E-06 -2.42E-06 6.45E-11 1.86E-06 1.99E-06 1.29E-10 1.02E-10 -2.297061157 2.292495728 1.847192383 1.955639648 543 9402.093122 2.40E-11 2.39E-06 -2.41E-06 1.03E-10 1.85E-06 1.98E-06 1.29E-10 1.01E-10 -2.295233154 2.29107666 1.845983887 1.956259155 544 9403.306283 -4.75E-11 2.42E-06 -2.44E-06 1.14E-10 1.85E-06 1.97E-06 1.29E-10 1.01E-10 -2.327536011 2.323104858 1.873361206 1.985668945 545 9404.515948 2.00E-12 2.44E-06 -2.46E-06 7.00E-11 1.85E-06 1.98E-06 1.29E-10 1.02E-10 -2.336636353 2.33248291 1.883560181 1.995825195 546 9405.710662 2.40E-11 2.45E-06 -2.46E-06 4.80E-11 1.86E-06 1.99E-06 1.29E-10 1.02E-10 -2.338012695 2.333273315 1.886480713 1.998626709 547 9406.924778 -1.74E-10 2.44E-06 -2.46E-06 -7.00E-12 1.87E-06 2.00E-06 1.30E-10 1.02E-10 -2.341018677 2.33706665 1.89057312 2.003240967 548 9408.127757 2.95E-11 2.45E-06 -2.46E-06 8.65E-11 1.88E-06 2.01E-06 1.31E-10 1.03E-10 -2.338296509 2.333468628 1.88979187 2.002694702 549 9409.32723 1.29E-10 2.44E-06 -2.46E-06 5.35E-11 1.88E-06 2.01E-06 1.31E-10 1.03E-10 -2.3384552 2.334896851 1.892398071 2.00428772 550 9410.549944 -1.14E-10 2.44E-06 -2.46E-06 -4.00E-11 1.88E-06 2.01E-06 1.31E-10 1.03E-10 -2.336972046 2.332015991 1.892166138 2.004788208 551 9411.750049 -4.20E-11 2.45E-06 -2.46E-06 9.75E-11 1.88E-06 2.01E-06 1.31E-10 1.04E-10 -2.338909912 2.335775757 1.896176147 2.008877563 552 9412.958115 -1.47E-10 2.44E-06 -2.46E-06 1.03E-10 1.88E-06 2.01E-06 1.32E-10 1.04E-10 -2.340475464 2.336984253 1.89916687 2.012033081 553 9414.162673 -3.65E-11 2.44E-06 -2.46E-06 5.35E-11 1.89E-06 2.02E-06 1.32E-10 1.04E-10 -2.338989258 2.335534668 1.89977417 2.01277771 554 9415.379023 5.70E-11 2.45E-06 -2.46E-06 6.45E-11 1.89E-06 2.02E-06 1.32E-10 1.04E-10 -2.337268066 2.33420105 1.900674438 2.013641357 555 9416.588041 7.50E-12 2.44E-06 -2.45E-06 2.05E-11 1.89E-06 2.02E-06 1.32E-10 1.04E-10 -2.335855103 2.330264282 1.900091553 2.013153076 556 9417.797377 -5.30E-11 2.44E-06 -2.46E-06 8.65E-11 1.89E-06 2.02E-06 1.32E-10 1.04E-10 -2.340429688 2.336410522 1.905059814 2.018133545 557 9419.014688 -1.58E-10 2.44E-06 -2.45E-06 6.45E-11 1.89E-06 2.02E-06 1.32E-10 1.04E-10 -2.337594604 2.333398438 1.904727173 2.017730713 558 9420.220833 -2.07E-10 2.44E-06 -2.45E-06 7.55E-11 1.89E-06 2.03E-06 1.33E-10 1.05E-10 -2.33454895 2.329779053 1.904272461 2.017166138 559 9421.427293 -5.85E-11 2.44E-06 -2.45E-06 5.35E-11 1.90E-06 2.03E-06 1.33E-10 1.05E-10 -2.336999512 2.33269043 1.907907104 2.021258545 560 9422.637902 -3.10E-11 2.44E-06 -2.45E-06 1.03E-10 1.90E-06 2.03E-06 1.33E-10 1.05E-10 -2.33862915 2.334481812 1.910702515 2.023925781 561 9423.864159 -1.25E-10 2.44E-06 -2.46E-06 1.36E-10 1.90E-06 2.03E-06 1.33E-10 1.05E-10 -2.337200928 2.333432007 1.911813354 2.024932861 562 9425.06774 4.05E-11 2.44E-06 -2.45E-06 6.45E-11 1.90E-06 2.03E-06 1.33E-10 1.05E-10 -2.333856201 2.329656982 1.910900879 2.023757935 563 9426.294644 -9.70E-11 2.44E-06 -2.46E-06 4.25E-11 1.90E-06 2.03E-06 1.34E-10 1.05E-10 -2.336236572 2.33218689 1.914413452 2.028048706 564 9427.498862 -4.75E-11 2.44E-06 -2.45E-06 1.50E-11 1.90E-06 2.04E-06 1.34E-10 1.06E-10 -2.335467529 2.331262207 1.915859985 2.029177856 565 9428.70723 2.00E-12 2.44E-06 -2.45E-06 9.75E-11 1.91E-06 2.04E-06 1.34E-10 1.06E-10 -2.332827759 2.327661133 1.915667725 2.029031372 566 9429.919753 -2.55E-11 2.44E-06 -2.45E-06 4.80E-11 1.91E-06 2.04E-06 1.34E-10 1.06E-10 -2.336624146 2.332461548 1.920892334 2.034515381 567 9431.132595 -1.80E-10 2.44E-06 -2.45E-06 1.80E-10 1.91E-06 2.04E-06 1.35E-10 1.06E-10 -2.334265137 2.329147339 1.920928955 2.034344482 568 9432.349596 -1.30E-10 2.44E-06 -2.45E-06 6.45E-11 1.91E-06 2.04E-06 1.35E-10 1.06E-10 -2.336727905 2.33366394 1.924813843 2.038537598 569 9433.570759 -9.15E-11 2.44E-06 -2.45E-06 4.80E-11 1.91E-06 2.04E-06 1.35E-10 1.07E-10 -2.334786987 2.3302948 1.925390625 2.038735962 570 9434.780721 -1.19E-10 2.44E-06 -2.45E-06 5.35E-11 1.91E-06 2.05E-06 1.35E-10 1.07E-10 -2.336230469 2.333004761 1.928872681 2.042062378 571 9435.998685 9.55E-11 2.44E-06 -2.45E-06 1.20E-10 1.92E-06 2.05E-06 1.35E-10 1.07E-10 -2.331686401 2.326977539 1.926010132 2.039746094 572 9437.220815 -1.08E-10 2.44E-06 -2.46E-06 -1.25E-11 1.92E-06 2.05E-06 1.35E-10 1.07E-10 -2.336099243 2.332485962 1.931570435 2.04543457 573 9438.431735 8.45E-11 2.44E-06 -2.45E-06 8.65E-11 1.92E-06 2.05E-06 1.35E-10 1.07E-10 -2.334991455 2.330767822 1.932293701 2.046798706 574 9439.654509 -1.14E-10 2.44E-06 -2.45E-06 7.55E-11 1.92E-06 2.05E-06 1.36E-10 1.07E-10 -2.331799316 2.326513672 1.931280518 2.045272827 575 9440.869915 -4.75E-11 2.44E-06 -2.45E-06 5.35E-11 1.92E-06 2.05E-06 1.36E-10 1.08E-10 -2.333837891 2.330151367 1.935192871 2.049090576 576 9442.08564 -1.36E-10 2.44E-06 -2.45E-06 2.60E-11 1.92E-06 2.06E-06 1.36E-10 1.07E-10 -2.332467651 2.329446411 1.936026001 2.049996948 577 9443.309384 -8.60E-11 2.44E-06 -2.45E-06 8.65E-11 1.93E-06 2.06E-06 1.36E-10 1.07E-10 -2.33380127 2.329959106 1.938418579 2.052758789 578 9444.521902 -1.45E-11 2.44E-06 -2.45E-06 8.65E-11 1.93E-06 2.06E-06 1.36E-10 1.07E-10 -2.330963135 2.327059937 1.937600708 2.051763916 579 9445.746292 -3.10E-11 2.44E-06 -2.45E-06 1.03E-10 1.93E-06 2.06E-06 1.36E-10 1.08E-10 -2.332244873 2.329168701 1.94017334 2.05453186 580 9446.971006 -4.75E-11 2.44E-06 -2.45E-06 4.80E-11 1.93E-06 2.06E-06 1.37E-10 1.08E-10 -2.332037354 2.327938843 1.941659546 2.056231689 581 9448.180634 2.00E-12 2.43E-06 -2.45E-06 3.15E-11 1.93E-06 2.06E-06 1.37E-10 1.08E-10 -2.329803467 2.325445557 1.941375732 2.055877686 582 9449.398286 6.25E-11 2.44E-06 -2.45E-06 7.00E-11 1.93E-06 2.06E-06 1.37E-10 1.08E-10 -2.331817627 2.327017212 1.944458008 2.059060669 583 9450.60855 -3.50E-12 2.43E-06 -2.45E-06 1.25E-10 1.93E-06 2.07E-06 1.37E-10 1.09E-10 -2.326257324 2.321127319 1.941586304 2.055657959 584 9451.822987 -1.03E-10 2.42E-06 -2.43E-06 8.65E-11 1.93E-06 2.07E-06 1.37E-10 1.09E-10 -2.310339355 2.305130005 1.929174805 2.043148804 585 9453.037743 -4.20E-11 2.41E-06 -2.42E-06 2.05E-11 1.93E-06 2.06E-06 1.37E-10 1.09E-10 -2.307824707 2.305670166 1.929434204 2.043664551 586 9454.264392 -6.95E-11 2.40E-06 -2.42E-06 8.10E-11 1.92E-06 2.06E-06 1.37E-10 1.08E-10 -2.302023315 2.297631836 1.926660156 2.039892578 587 9455.47979 1.40E-10 2.40E-06 -2.41E-06 7.55E-11 1.92E-06 2.05E-06 1.37E-10 1.08E-10 -2.293865967 2.289672852 1.921029663 2.033407593 588 9456.703228 -3.10E-11 2.37E-06 -2.39E-06 4.80E-11 1.91E-06 2.04E-06 1.36E-10 1.08E-10 -2.270535278 2.266448975 1.903131104 2.014212036 589 9457.92699 9.00E-11 2.38E-06 -2.39E-06 6.45E-11 1.91E-06 2.04E-06 1.36E-10 1.08E-10 -2.283041382 2.279333496 1.916940308 2.028244019 590 9459.139489 -1.45E-11 2.40E-06 -2.42E-06 8.10E-11 1.91E-06 2.04E-06 1.36E-10 1.08E-10 -2.303234863 2.296612549 1.934729004 2.046960449 591 9460.352307 -3.50E-12 2.43E-06 -2.44E-06 1.25E-10 1.91E-06 2.04E-06 1.36E-10 1.08E-10 -2.325216675 2.320861816 1.954174805 2.068548584 592 9461.577035 2.00E-12 2.43E-06 -2.45E-06 2.05E-11 1.93E-06 2.06E-06 1.37E-10 1.09E-10 -2.33142395 2.327032471 1.961325073 2.076464844 593 9462.802087 7.50E-12 2.44E-06 -2.45E-06 8.65E-11 1.94E-06 2.07E-06 1.38E-10 1.10E-10 -2.331289673 2.32739563 1.962597656 2.077914429 594 9464.023598 1.85E-11 2.44E-06 -2.45E-06 2.60E-11 1.95E-06 2.08E-06 1.39E-10 1.10E-10 -2.335256958 2.331756592 1.96756897 2.083209229 595 9465.249298 -8.60E-11 2.44E-06 -2.45E-06 2.60E-11 1.95E-06 2.09E-06 1.39E-10 1.10E-10 -2.334146118 2.329867554 1.96711731 2.082644653 596 9466.475323 8.45E-11 2.44E-06 -2.45E-06 3.15E-11 1.95E-06 2.09E-06 1.39E-10 1.11E-10 -2.331359863 2.328173828 1.966699219 2.082150269 597 9467.701673 -9.70E-11 2.43E-06 -2.44E-06 6.45E-11 1.95E-06 2.09E-06 1.39E-10 1.11E-10 -2.325585938 2.320117188 1.962835693 2.078088379 598 9468.932218 -1.45E-11 2.44E-06 -2.45E-06 1.03E-10 1.96E-06 2.09E-06 1.39E-10 1.11E-10 -2.331610107 2.328137207 1.970620728 2.086260986 599 9470.151477 -4.75E-11 2.43E-06 -2.45E-06 1.03E-10 1.96E-06 2.09E-06 1.40E-10 1.11E-10 -2.328213501 2.323007202 1.969064331 2.084710693 600 9471.371057 -9.70E-11 2.43E-06 -2.45E-06 3.15E-11 1.96E-06 2.09E-06 1.40E-10 1.11E-10 -2.331658936 2.327536011 1.973739624 2.089346313 601 9472.606452 -6.40E-11 2.44E-06 -2.45E-06 8.10E-11 1.96E-06 2.10E-06 1.40E-10 1.11E-10 -2.328945923 2.324813843 1.972644043 2.088287354 602 9473.830553 7.50E-12 2.43E-06 -2.45E-06 1.03E-10 1.96E-06 2.10E-06 1.40E-10 1.11E-10 -2.330288696 2.325894165 1.97477417 2.090722656 603 9475.054978 -1.91E-10 2.44E-06 -2.45E-06 4.80E-11 1.96E-06 2.10E-06 1.40E-10 1.11E-10 -2.330368042 2.326309204 1.977139282 2.092706299 604 9476.279726 -1.25E-10 2.43E-06 -2.45E-06 7.00E-11 1.96E-06 2.10E-06 1.40E-10 1.11E-10 -2.333694458 2.330786133 1.981411743 2.097540283 605 9477.520308 -3.50E-12 2.43E-06 -2.45E-06 5.90E-11 1.97E-06 2.10E-06 1.40E-10 1.11E-10 -2.328863525 2.32406311 1.978686523 2.094451904 606 9478.74183 -2.55E-11 2.44E-06 -2.45E-06 7.00E-11 1.97E-06 2.10E-06 1.41E-10 1.12E-10 -2.331314087 2.327078247 1.982269287 2.097952271 607 9479.967554 -1.30E-10 2.43E-06 -2.45E-06 8.65E-11 1.97E-06 2.10E-06 1.41E-10 1.12E-10 -2.327966309 2.323312378 1.98135376 2.097070313 608 9481.197482 -1.45E-11 2.44E-06 -2.45E-06 7.55E-11 1.97E-06 2.11E-06 1.41E-10 1.12E-10 -2.330056763 2.325683594 1.985037231 2.100814819 609 9482.419974 -9.15E-11 2.43E-06 -2.45E-06 1.25E-10 1.97E-06 2.11E-06 1.41E-10 1.12E-10 -2.326538086 2.321569824 1.983462524 2.09932251 610 9483.642788 -8.05E-11 2.43E-06 -2.45E-06 5.90E-11 1.97E-06 2.11E-06 1.41E-10 1.12E-10 -2.327893066 2.32428894 1.987252808 2.102633667 611 9484.865925 7.35E-11 2.43E-06 -2.45E-06 2.60E-11 1.98E-06 2.11E-06 1.41E-10 1.12E-10 -2.328396606 2.323727417 1.988632202 2.104754639 612 9486.097154 4.60E-11 2.43E-06 -2.45E-06 9.50E-12 1.98E-06 2.11E-06 1.41E-10 1.12E-10 -2.330096436 2.32666626 1.992382813 2.108538818 613 9487.324824 7.35E-11 2.43E-06 -2.45E-06 1.03E-10 1.98E-06 2.11E-06 1.41E-10 1.13E-10 -2.33119812 2.326968384 1.99442749 2.110595703 614 9488.564478 1.23E-10 2.43E-06 -2.45E-06 9.75E-11 1.98E-06 2.12E-06 1.42E-10 1.13E-10 -2.326147461 2.321438599 1.991333008 2.107064819 615 9489.773364 -3.10E-11 2.43E-06 -2.44E-06 8.10E-11 1.98E-06 2.12E-06 1.42E-10 1.13E-10 -2.324273682 2.320474243 1.992449951 2.108074951 616 9491.002007 -5.30E-11 2.43E-06 -2.45E-06 1.03E-10 1.98E-06 2.12E-06 1.42E-10 1.13E-10 -2.325796509 2.322637939 1.995672607 2.111676025 617 9492.227086 -9.00E-12 2.43E-06 -2.44E-06 6.45E-11 1.98E-06 2.12E-06 1.42E-10 1.13E-10 -2.322268677 2.31647644 1.993191528 2.109310913 618 9493.46027 -9.00E-12 2.43E-06 -2.44E-06 9.20E-11 1.98E-06 2.12E-06 1.42E-10 1.13E-10 -2.323703003 2.318823242 1.996786499 2.112817383 619 9494.682107 -5.30E-11 2.43E-06 -2.44E-06 1.09E-10 1.99E-06 2.12E-06 1.42E-10 1.13E-10 -2.329873657 2.326397705 2.004095459 2.120556641 620 9495.931514 2.95E-11 2.43E-06 -2.45E-06 7.00E-11 1.99E-06 2.12E-06 1.42E-10 1.13E-10 -2.327334595 2.322494507 2.003015137 2.119232178 621 9497.138427 -5.30E-11 2.43E-06 -2.44E-06 1.42E-10 1.99E-06 2.13E-06 1.42E-10 1.13E-10 -2.327813721 2.325152588 2.005978394 2.122213745 622 9498.376811 -5.85E-11 2.43E-06 -2.45E-06 1.20E-10 1.99E-06 2.13E-06 1.43E-10 1.13E-10 -2.328842163 2.325390625 2.008840942 2.125085449 623 9499.615526 -2.55E-11 2.43E-06 -2.44E-06 9.75E-11 2.00E-06 2.13E-06 1.43E-10 1.14E-10 -2.323809814 2.319519043 2.005612183 2.122006226 624 9500.850674 9.55E-11 2.43E-06 -2.44E-06 1.03E-10 2.00E-06 2.13E-06 1.43E-10 1.14E-10 -2.324725342 2.320828247 2.008450317 2.12510376 625 9502.078355 -5.85E-11 2.43E-06 -2.44E-06 2.60E-11 2.00E-06 2.13E-06 1.43E-10 1.14E-10 -2.324081421 2.319421387 2.00854187 2.125045776 626 9503.310259 -8.05E-11 2.43E-06 -2.45E-06 8.10E-11 2.00E-06 2.13E-06 1.43E-10 1.14E-10 -2.324737549 2.320358276 2.011312866 2.127822876 627 9504.54249 -4.75E-11 2.43E-06 -2.44E-06 3.70E-11 2.00E-06 2.14E-06 1.43E-10 1.14E-10 -2.324804688 2.32024231 2.012979126 2.129559326 628 9505.775048 6.25E-11 2.43E-06 -2.45E-06 1.03E-10 2.00E-06 2.14E-06 1.43E-10 1.14E-10 -2.327676392 2.324301147 2.017147827 2.133874512 629 9507.000128 3.50E-11 2.43E-06 -2.44E-06 9.20E-11 2.00E-06 2.14E-06 1.44E-10 1.14E-10 -2.324981689 2.320657349 2.015991211 2.13260498 630 9508.245047 -1.45E-11 2.43E-06 -2.44E-06 6.45E-11 2.00E-06 2.14E-06 1.44E-10 1.15E-10 -2.32479248 2.320986938 2.017874146 2.134609985 631 9509.470779 -2.00E-11 2.43E-06 -2.44E-06 4.00E-12 2.01E-06 2.14E-06 1.44E-10 1.14E-10 -2.326220703 2.321984863 2.020584106 2.137341309 632 9510.712455 9.55E-11 2.43E-06 -2.44E-06 8.10E-11 2.01E-06 2.14E-06 1.44E-10 1.14E-10 -2.324230957 2.319891357 2.020785522 2.137521362 633 9511.94665 -1.19E-10 2.43E-06 -2.44E-06 3.15E-11 2.01E-06 2.14E-06 1.44E-10 1.14E-10 -2.323550415 2.319134521 2.0215271 2.138287354 634 9513.177265 -4.75E-11 2.43E-06 -2.44E-06 7.00E-11 2.01E-06 2.14E-06 1.44E-10 1.15E-10 -2.32192688 2.317367554 2.022521973 2.139489746 635 9514.408206 -8.05E-11 2.43E-06 -2.44E-06 4.80E-11 2.01E-06 2.15E-06 1.44E-10 1.15E-10 -2.323883057 2.319622803 2.025494385 2.142431641 636 9515.647291 1.01E-10 2.43E-06 -2.44E-06 8.10E-11 2.01E-06 2.15E-06 1.44E-10 1.15E-10 -2.323464966 2.318356323 2.026641846 2.14367981 637 9516.886707 5.70E-11 2.43E-06 -2.44E-06 9.20E-11 2.02E-06 2.15E-06 1.44E-10 1.15E-10 -2.32505188 2.320724487 2.030020142 2.14708252 638 9518.110807 -4.20E-11 2.43E-06 -2.44E-06 3.15E-11 2.02E-06 2.15E-06 1.45E-10 1.15E-10 -2.325906372 2.322903442 2.032778931 2.149871826 639 9519.354791 -6.95E-11 2.43E-06 -2.44E-06 9.20E-11 2.02E-06 2.15E-06 1.45E-10 1.16E-10 -2.323327637 2.318792725 2.031704712 2.148739624 640 9520.587367 2.00E-12 2.43E-06 -2.44E-06 1.14E-10 2.02E-06 2.16E-06 1.45E-10 1.16E-10 -2.325463867 2.321746826 2.035879517 2.153244019 641 9521.828099 -1.36E-10 2.43E-06 -2.44E-06 7.00E-11 2.02E-06 2.16E-06 1.45E-10 1.16E-10 -2.322775269 2.318261719 2.035308838 2.152548218 642 9523.065246 -3.50E-12 2.43E-06 -2.44E-06 7.55E-11 2.02E-06 2.16E-06 1.46E-10 1.16E-10 -2.322253418 2.318743896 2.037155151 2.154431152 643 9524.294888 1.40E-10 2.43E-06 -2.44E-06 3.70E-11 2.03E-06 2.16E-06 1.46E-10 1.17E-10 -2.318981934 2.313101196 2.035162354 2.152236938 644 9525.532691 -6.40E-11 2.43E-06 -2.44E-06 5.35E-11 2.03E-06 2.16E-06 1.46E-10 1.17E-10 -2.321438599 2.317407227 2.039962769 2.157424927 645 9526.778659 -1.41E-10 2.43E-06 -2.44E-06 -7.00E-12 2.03E-06 2.16E-06 1.46E-10 1.17E-10 -2.323535156 2.319717407 2.043701172 2.161270142 646 9528.009283 -1.69E-10 2.43E-06 -2.44E-06 7.00E-11 2.03E-06 2.16E-06 1.46E-10 1.17E-10 -2.320770264 2.315707397 2.042285156 2.15977478 647 9529.251993 5.70E-11 2.43E-06 -2.44E-06 1.42E-10 2.03E-06 2.17E-06 1.47E-10 1.17E-10 -2.323123169 2.319842529 2.047146606 2.16484375 648 9530.495036 -1.45E-11 2.43E-06 -2.44E-06 4.25E-11 2.03E-06 2.17E-06 1.47E-10 1.17E-10 -2.321890259 2.31819458 2.047250366 2.165167236 649 9531.730564 -1.45E-11 2.43E-06 -2.44E-06 5.90E-11 2.04E-06 2.17E-06 1.47E-10 1.18E-10 -2.320681763 2.316049194 2.047970581 2.165350342 650 9532.970343 2.95E-11 2.43E-06 -2.44E-06 -1.25E-11 2.04E-06 2.17E-06 1.47E-10 1.18E-10 -2.322195435 2.318258667 2.05128479 2.168859863 651 9534.210453 -1.36E-10 2.42E-06 -2.44E-06 6.45E-11 2.04E-06 2.17E-06 1.48E-10 1.18E-10 -2.320050049 2.315795898 2.050692749 2.168640137 652 9535.46267 -2.55E-11 2.43E-06 -2.44E-06 3.70E-11 2.04E-06 2.18E-06 1.48E-10 1.18E-10 -2.319998169 2.315255737 2.052114868 2.16986084 653 9536.695589 -9.00E-12 2.42E-06 -2.44E-06 9.75E-11 2.04E-06 2.18E-06 1.48E-10 1.18E-10 -2.32154541 2.317449951 2.05508728 2.172705078 654 9537.928833 -2.00E-11 2.43E-06 -2.44E-06 1.09E-10 2.04E-06 2.18E-06 1.48E-10 1.18E-10 -2.324328613 2.320840454 2.059335327 2.177310181 655 9539.174191 1.73E-10 2.42E-06 -2.44E-06 1.20E-10 2.04E-06 2.18E-06 1.48E-10 1.19E-10 -2.32003479 2.315887451 2.057376099 2.175250244 656 9540.431672 -9.15E-11 2.42E-06 -2.44E-06 8.65E-11 2.05E-06 2.18E-06 1.48E-10 1.19E-10 -2.320797729 2.316448975 2.059432983 2.177462769 657 9541.673767 -9.00E-12 2.43E-06 -2.44E-06 1.20E-10 2.05E-06 2.18E-06 1.48E-10 1.19E-10 -2.321948242 2.318835449 2.062609863 2.18109436 658 9542.935855 -3.65E-11 2.42E-06 -2.44E-06 1.20E-10 2.05E-06 2.18E-06 1.49E-10 1.19E-10 -2.31925354 2.313824463 2.061566162 2.179171753 659 9544.166817 4.60E-11 2.42E-06 -2.44E-06 7.55E-11 2.05E-06 2.19E-06 1.49E-10 1.19E-10 -2.318908691 2.313796997 2.063427734 2.181097412 660 9545.413841 -2.55E-11 2.42E-06 -2.43E-06 -1.50E-12 2.05E-06 2.19E-06 1.49E-10 1.19E-10 -2.313427734 2.309033203 2.05980835 2.17739563 661 9546.657263 2.95E-11 2.42E-06 -2.43E-06 9.20E-11 2.05E-06 2.19E-06 1.49E-10 1.19E-10 -2.31036377 2.305722046 2.059164429 2.176306152 662 9547.904953 4.60E-11 2.42E-06 -2.43E-06 9.75E-11 2.05E-06 2.19E-06 1.49E-10 1.19E-10 -2.313290405 2.309747314 2.064108276 2.181381226 663 9549.141163 -2.00E-11 2.41E-06 -2.43E-06 8.65E-11 2.05E-06 2.19E-06 1.49E-10 1.20E-10 -2.309506226 2.305447388 2.061932373 2.179086304 664 9550.405271 -9.70E-11 2.42E-06 -2.43E-06 4.80E-11 2.05E-06 2.19E-06 1.49E-10 1.20E-10 -2.316192627 2.312887573 2.069692993 2.187023926 665 9551.642144 9.00E-11 2.42E-06 -2.43E-06 8.65E-11 2.05E-06 2.19E-06 1.50E-10 1.20E-10 -2.317959595 2.313641357 2.072796631 2.190563965 666 9552.883285 -5.30E-11 2.42E-06 -2.44E-06 1.20E-10 2.06E-06 2.19E-06 1.50E-10 1.20E-10 -2.319107056 2.315380859 2.07583313 2.193435669 667 9554.132639 2.95E-11 2.42E-06 -2.44E-06 1.50E-11 2.06E-06 2.20E-06 1.50E-10 1.20E-10 -2.316342163 2.311624146 2.074645996 2.192367554 668 9555.378385 2.95E-11 2.42E-06 -2.43E-06 1.09E-10 2.06E-06 2.20E-06 1.50E-10 1.21E-10 -2.318722534 2.314273071 2.078530884 2.196292114 669 9556.624463 -6.40E-11 2.42E-06 -2.44E-06 1.31E-10 2.07E-06 2.20E-06 1.50E-10 1.21E-10 -2.318466187 2.314312744 2.080270386 2.198376465 670 9557.882707 -3.10E-11 2.42E-06 -2.43E-06 2.60E-11 2.07E-06 2.20E-06 1.51E-10 1.21E-10 -2.314862061 2.309362793 2.077670288 2.195974731 671 9559.129453 -8.05E-11 2.42E-06 -2.44E-06 8.10E-11 2.07E-06 2.20E-06 1.51E-10 1.21E-10 -2.319924927 2.317126465 2.084127808 2.203125 672 9560.372584 -6.95E-11 2.42E-06 -2.43E-06 -1.50E-12 2.07E-06 2.21E-06 1.51E-10 1.21E-10 -2.318054199 2.315063477 2.084957886 2.203469849 673 9561.619994 -8.05E-11 2.42E-06 -2.44E-06 3.70E-11 2.07E-06 2.21E-06 1.52E-10 1.21E-10 -2.316085815 2.312371826 2.084011841 2.202529907 674 9562.871686 -5.85E-11 2.42E-06 -2.43E-06 1.09E-10 2.07E-06 2.21E-06 1.51E-10 1.21E-10 -2.318832397 2.314968872 2.087969971 2.206732178 675 9564.119763 -3.65E-11 2.42E-06 -2.44E-06 1.53E-10 2.07E-06 2.21E-06 1.52E-10 1.21E-10 -2.317221069 2.312423706 2.08800354 2.206942749 676 9565.376075 -2.55E-11 2.42E-06 -2.43E-06 4.80E-11 2.08E-06 2.21E-06 1.52E-10 1.21E-10 -2.313970947 2.309188843 2.087451172 2.206103516 677 9566.620868 -2.00E-11 2.42E-06 -2.43E-06 -1.50E-12 2.08E-06 2.22E-06 1.52E-10 1.22E-10 -2.3146698 2.309606934 2.08949585 2.208389282 678 9567.862039 -6.95E-11 2.42E-06 -2.43E-06 1.03E-10 2.08E-06 2.22E-06 1.52E-10 1.22E-10 -2.319259644 2.315917969 2.096029663 2.215249634 679 9569.107493 -5.30E-11 2.42E-06 -2.43E-06 1.03E-10 2.08E-06 2.22E-06 1.52E-10 1.22E-10 -2.31519165 2.310577393 2.093695068 2.212460327 680 9570.365146 -1.45E-11 2.42E-06 -2.43E-06 1.50E-11 2.08E-06 2.22E-06 1.53E-10 1.22E-10 -2.31522522 2.311160278 2.095645142 2.214724731 681 9571.623136 -2.55E-11 2.42E-06 -2.43E-06 5.90E-11 2.08E-06 2.22E-06 1.53E-10 1.23E-10 -2.31451416 2.310513306 2.096734619 2.21590271 682 9572.861677 6.25E-11 2.41E-06 -2.43E-06 2.60E-11 2.08E-06 2.22E-06 1.53E-10 1.23E-10 -2.313830566 2.308566284 2.097164917 2.216357422 683 9574.124296 -6.40E-11 2.42E-06 -2.43E-06 9.75E-11 2.09E-06 2.22E-06 1.53E-10 1.23E-10 -2.318347168 2.315100098 2.103686523 2.222665405 684 9575.379338 -1.36E-10 2.42E-06 -2.43E-06 2.60E-11 2.09E-06 2.23E-06 1.53E-10 1.23E-10 -2.315228271 2.311407471 2.102172852 2.22130127 685 9576.618872 1.30E-11 2.42E-06 -2.43E-06 3.15E-11 2.09E-06 2.23E-06 1.53E-10 1.23E-10 -2.313427734 2.308251953 2.101843262 2.220724487 686 9577.870621 4.05E-11 2.42E-06 -2.43E-06 1.31E-10 2.09E-06 2.23E-06 1.53E-10 1.23E-10 -2.314630127 2.310281372 2.10456543 2.223898315 687 9579.11874 -1.14E-10 2.42E-06 -2.43E-06 9.20E-11 2.09E-06 2.23E-06 1.53E-10 1.23E-10 -2.314596558 2.310668945 2.106365967 2.22555542 688 9580.367193 7.50E-12 2.41E-06 -2.43E-06 1.31E-10 2.09E-06 2.23E-06 1.54E-10 1.23E-10 -2.312982178 2.309194946 2.107070923 2.226269531 689 9581.623908 -1.41E-10 2.41E-06 -2.43E-06 9.20E-11 2.09E-06 2.23E-06 1.54E-10 1.24E-10 -2.310266113 2.304592896 2.105706787 2.224890137 690 9582.876994 1.30E-11 2.42E-06 -2.43E-06 7.00E-11 2.10E-06 2.23E-06 1.54E-10 1.24E-10 -2.312341309 2.308535767 2.109661865 2.229025269 691 9584.138349 -1.45E-11 2.42E-06 -2.43E-06 -1.50E-12 2.10E-06 2.23E-06 1.54E-10 1.24E-10 -2.315063477 2.311889648 2.114193726 2.233905029 692 9585.380203 -2.55E-11 2.42E-06 -2.43E-06 8.10E-11 2.10E-06 2.24E-06 1.55E-10 1.24E-10 -2.31272583 2.308758545 2.113723755 2.233462524 693 9586.630325 -8.60E-11 2.41E-06 -2.43E-06 9.75E-11 2.10E-06 2.24E-06 1.55E-10 1.24E-10 -2.309213257 2.304504395 2.112698364 2.232110596 694 9587.88078 -1.25E-10 2.42E-06 -2.43E-06 9.50E-12 2.10E-06 2.24E-06 1.55E-10 1.25E-10 -2.313796997 2.309744263 2.117987061 2.237814331 695 9589.135539 -2.55E-11 2.41E-06 -2.43E-06 8.10E-11 2.10E-06 2.24E-06 1.55E-10 1.25E-10 -2.313180542 2.309210205 2.119967651 2.239266968 696 9590.39858 -6.95E-11 2.42E-06 -2.43E-06 4.25E-11 2.11E-06 2.24E-06 1.55E-10 1.25E-10 -2.308062744 2.302688599 2.117010498 2.236016846 697 9591.638119 -8.05E-11 2.41E-06 -2.43E-06 4.80E-11 2.11E-06 2.25E-06 1.56E-10 1.25E-10 -2.313708496 2.30994873 2.124435425 2.24375 698 9592.897859 -8.05E-11 2.41E-06 -2.43E-06 5.35E-11 2.11E-06 2.25E-06 1.56E-10 1.25E-10 -2.310317993 2.305709839 2.122900391 2.242364502 699 9594.14601 7.50E-12 2.41E-06 -2.43E-06 8.10E-11 2.11E-06 2.25E-06 1.56E-10 1.25E-10 -2.31489563 2.31237793 2.129888916 2.2496521 700 9595.406424 -1.96E-10 2.41E-06 -2.43E-06 8.10E-11 2.11E-06 2.25E-06 1.56E-10 1.26E-10 -2.309085083 2.303936768 2.125546265 2.245010376 701 9596.663198 1.23E-10 2.41E-06 -2.43E-06 1.03E-10 2.11E-06 2.25E-06 1.56E-10 1.26E-10 -2.311846924 2.308105469 2.129766846 2.249642944 702 9597.924287 -3.50E-12 2.41E-06 -2.42E-06 7.55E-11 2.12E-06 2.25E-06 1.56E-10 1.26E-10 -2.302462769 2.297894287 2.1230896 2.242385864 703 9599.177756 -1.36E-10 2.40E-06 -2.42E-06 8.10E-11 2.12E-06 2.25E-06 1.57E-10 1.26E-10 -2.298974609 2.293722534 2.12142334 2.240930176 704 9600.431559 5.70E-11 2.41E-06 -2.42E-06 4.25E-11 2.12E-06 2.25E-06 1.57E-10 1.26E-10 -2.301852417 2.297125244 2.125601196 2.245571899 705 9601.681715 -3.10E-11 2.41E-06 -2.42E-06 8.65E-11 2.12E-06 2.25E-06 1.57E-10 1.26E-10 -2.310220337 2.305862427 2.134899902 2.255184937 706 9602.936187 1.29E-10 2.41E-06 -2.43E-06 6.45E-11 2.12E-06 2.26E-06 1.57E-10 1.26E-10 -2.308984375 2.304055786 2.136032104 2.255740356 707 9604.202947 -7.50E-11 2.41E-06 -2.43E-06 3.70E-11 2.12E-06 2.26E-06 1.57E-10 1.27E-10 -2.308230591 2.305029297 2.137130737 2.257434082 708 9605.458092 -9.15E-11 2.41E-06 -2.42E-06 2.05E-11 2.12E-06 2.26E-06 1.58E-10 1.27E-10 -2.308544922 2.304443359 2.139031982 2.258920288 709 9606.717559 -1.80E-10 2.41E-06 -2.42E-06 1.31E-10 2.13E-06 2.27E-06 1.58E-10 1.27E-10 -2.309356689 2.305517578 2.141513062 2.261706543 710 9607.973377 -4.75E-11 2.41E-06 -2.42E-06 8.65E-11 2.13E-06 2.27E-06 1.58E-10 1.27E-10 -2.302404785 2.297640991 2.137210083 2.256988525 711 9609.22953 6.25E-11 2.41E-06 -2.43E-06 8.10E-11 2.13E-06 2.27E-06 1.59E-10 1.28E-10 -2.308752441 2.304772949 2.145059204 2.265393066 712 9610.47804 -3.50E-12 2.41E-06 -2.42E-06 8.65E-11 2.13E-06 2.27E-06 1.59E-10 1.28E-10 -2.310110474 2.305596924 2.147821045 2.268283081 713 9611.742844 -6.95E-11 2.42E-06 -2.43E-06 1.03E-10 2.13E-06 2.27E-06 1.59E-10 1.28E-10 -2.308303833 2.303051758 2.148114014 2.268701172 714 9613.003996 -1.45E-11 2.41E-06 -2.43E-06 8.65E-11 2.14E-06 2.28E-06 1.60E-10 1.29E-10 -2.309741211 2.305529785 2.151116943 2.271401978 715 9614.273472 -1.25E-10 2.41E-06 -2.43E-06 8.65E-11 2.14E-06 2.28E-06 1.60E-10 1.29E-10 -2.31244812 2.308633423 2.155517578 2.276303101 716 9615.519328 -1.52E-10 2.41E-06 -2.43E-06 9.20E-11 2.14E-06 2.28E-06 1.60E-10 1.29E-10 -2.309100342 2.30461731 2.153967285 2.274606323 717 9616.789483 -1.19E-10 2.41E-06 -2.43E-06 5.90E-11 2.14E-06 2.28E-06 1.60E-10 1.29E-10 -2.310620117 2.306732178 2.157208252 2.278082275 718 9618.05199 2.40E-11 2.41E-06 -2.42E-06 4.80E-11 2.14E-06 2.28E-06 1.61E-10 1.30E-10 -2.308831787 2.304916382 2.157824707 2.278201294 719 9619.314835 -2.00E-11 2.41E-06 -2.43E-06 7.00E-11 2.14E-06 2.28E-06 1.61E-10 1.30E-10 -2.306600952 2.302435303 2.157479858 2.277789307 720 9620.574021 -1.74E-10 2.41E-06 -2.43E-06 5.90E-11 2.14E-06 2.29E-06 1.61E-10 1.30E-10 -2.308554077 2.304058838 2.160345459 2.28104248 721 9621.833544 -1.45E-11 2.41E-06 -2.43E-06 7.55E-11 2.15E-06 2.29E-06 1.61E-10 1.30E-10 -2.308029175 2.303305054 2.161868286 2.2824646 722 9623.085405 -5.85E-11 2.41E-06 -2.42E-06 8.10E-11 2.15E-06 2.29E-06 1.61E-10 1.31E-10 -2.306445313 2.30302124 2.162515259 2.283041382 723 9624.341599 -9.70E-11 2.41E-06 -2.43E-06 9.50E-12 2.15E-06 2.29E-06 1.62E-10 1.31E-10 -2.306369019 2.302105713 2.164028931 2.284875488 724 9625.610135 -2.24E-10 2.40E-06 -2.41E-06 3.15E-11 2.15E-06 2.29E-06 1.61E-10 1.30E-10 -2.292385864 2.288903809 2.153512573 2.272924805 725 9626.891023 4.05E-11 2.37E-06 -2.39E-06 1.36E-10 2.14E-06 2.28E-06 1.61E-10 1.30E-10 -2.280557251 2.276486206 2.1431427 2.263186646 726 9628.144229 -1.25E-10 2.41E-06 -2.42E-06 9.75E-11 2.14E-06 2.28E-06 1.61E-10 1.30E-10 -2.306744385 2.302041626 2.169882202 2.291195679 727 9629.41379 2.00E-12 2.41E-06 -2.43E-06 9.20E-11 2.15E-06 2.29E-06 1.61E-10 1.30E-10 -2.308273315 2.304193115 2.173477173 2.294573975 728 9630.687699 1.01E-10 2.41E-06 -2.42E-06 4.25E-11 2.15E-06 2.29E-06 1.62E-10 1.31E-10 -2.305639648 2.300860596 2.172674561 2.293737793 729 9631.941916 9.55E-11 2.41E-06 -2.42E-06 7.55E-11 2.16E-06 2.30E-06 1.63E-10 1.32E-10 -2.30894165 2.305697632 2.178677368 2.299591064 730 9633.204483 -1.74E-10 2.41E-06 -2.42E-06 8.65E-11 2.16E-06 2.30E-06 1.63E-10 1.32E-10 -2.303109741 2.297662354 2.174530029 2.29553833 731 9634.479418 -4.75E-11 2.41E-06 -2.42E-06 8.10E-11 2.16E-06 2.31E-06 1.63E-10 1.32E-10 -2.306787109 2.302581787 2.179830933 2.30100708 732 9635.734644 -9.70E-11 2.41E-06 -2.42E-06 3.15E-11 2.16E-06 2.31E-06 1.63E-10 1.32E-10 -2.30569458 2.301925659 2.181130981 2.302304077 733 9637.00224 -2.55E-11 2.41E-06 -2.42E-06 7.00E-11 2.17E-06 2.31E-06 1.63E-10 1.32E-10 -2.305279541 2.301400757 2.182946777 2.303625488 734 9638.290241 -1.03E-10 2.41E-06 -2.42E-06 7.00E-11 2.17E-06 2.31E-06 1.63E-10 1.32E-10 -2.307168579 2.30322876 2.18583374 2.306799316 735 9639.550496 2.40E-11 2.41E-06 -2.42E-06 7.00E-11 2.17E-06 2.31E-06 1.63E-10 1.32E-10 -2.305374146 2.301269531 2.186297607 2.307043457 736 9640.827149 -1.74E-10 2.41E-06 -2.42E-06 4.80E-11 2.17E-06 2.31E-06 1.63E-10 1.32E-10 -2.304730225 2.300091553 2.187176514 2.308102417 737 9642.080049 2.40E-11 2.41E-06 -2.42E-06 5.35E-11 2.17E-06 2.32E-06 1.63E-10 1.32E-10 -2.303674316 2.299398804 2.18795166 2.30894165 738 9643.357386 6.25E-11 2.40E-06 -2.42E-06 9.20E-11 2.17E-06 2.32E-06 1.63E-10 1.32E-10 -2.298477173 2.292456055 2.184033203 2.304983521 739 9644.618996 -1.45E-11 2.41E-06 -2.42E-06 8.10E-11 2.18E-06 2.32E-06 1.63E-10 1.32E-10 -2.305709839 2.30234375 2.192922974 2.3146698 740 9645.897021 -1.25E-10 2.40E-06 -2.42E-06 9.75E-11 2.18E-06 2.32E-06 1.63E-10 1.32E-10 -2.300543213 2.295846558 2.189492798 2.310638428 741 9647.171371 7.50E-12 2.40E-06 -2.42E-06 1.31E-10 2.18E-06 2.32E-06 1.63E-10 1.32E-10 -2.295819092 2.291958618 2.187414551 2.308078003 742 9648.442044 -6.40E-11 2.37E-06 -2.39E-06 8.10E-11 2.18E-06 2.32E-06 1.63E-10 1.32E-10 -2.270095825 2.267053223 2.164193726 2.284112549 743 9649.709037 1.30E-11 2.39E-06 -2.41E-06 1.25E-10 2.17E-06 2.31E-06 1.63E-10 1.32E-10 -2.294882202 2.290429688 2.189550781 2.310296631 744 9651.000512 4.60E-11 2.41E-06 -2.42E-06 2.05E-11 2.17E-06 2.32E-06 1.63E-10 1.32E-10 -2.304089355 2.300143433 2.199734497 2.321783447 745 9652.260142 2.95E-11 2.41E-06 -2.42E-06 7.00E-11 2.18E-06 2.32E-06 1.63E-10 1.32E-10 -2.301498413 2.296975708 2.199102783 2.320819092 746 9653.540237 -6.40E-11 2.41E-06 -2.42E-06 3.15E-11 2.18E-06 2.32E-06 1.64E-10 1.33E-10 -2.302114868 2.298150635 2.201760864 2.323220825 747 9654.816652 -8.05E-11 2.41E-06 -2.42E-06 9.75E-11 2.19E-06 2.33E-06 1.64E-10 1.33E-10 -2.300527954 2.295175171 2.201483154 2.323339844 748 9656.089384 -2.55E-11 2.41E-06 -2.42E-06 1.03E-10 2.19E-06 2.33E-06 1.65E-10 1.33E-10 -2.306359863 2.302783203 2.208901978 2.330966187 749 9657.366489 -1.19E-10 2.41E-06 -2.42E-06 4.25E-11 2.19E-06 2.34E-06 1.65E-10 1.33E-10 -2.303344727 2.299533081 2.207806396 2.329870605 750 9658.635877 -8.05E-11 2.41E-06 -2.42E-06 3.15E-11 2.19E-06 2.34E-06 1.65E-10 1.33E-10 -2.301528931 2.29810791 2.207876587 2.329818726 751 9659.91367 1.30E-11 2.41E-06 -2.42E-06 4.25E-11 2.20E-06 2.34E-06 1.65E-10 1.33E-10 -2.301004028 2.296243286 2.208154297 2.330236816 752 9661.195841 5.70E-11 2.40E-06 -2.42E-06 1.25E-10 2.20E-06 2.34E-06 1.65E-10 1.33E-10 -2.301452637 2.297680664 2.210360718 2.332443237 753 9662.470292 -1.47E-10 2.40E-06 -2.41E-06 7.00E-11 2.20E-06 2.34E-06 1.65E-10 1.34E-10 -2.294458008 2.28899231 2.204830933 2.326565552 754 9663.737018 -9.15E-11 2.40E-06 -2.41E-06 1.03E-10 2.20E-06 2.34E-06 1.65E-10 1.34E-10 -2.297183228 2.293475342 2.21031189 2.3318573 755 9665.004083 1.51E-10 2.40E-06 -2.41E-06 5.90E-11 2.20E-06 2.34E-06 1.65E-10 1.34E-10 -2.293133545 2.28729248 2.207388306 2.32930603 756 9666.279561 7.90E-11 2.40E-06 -2.41E-06 1.36E-10 2.20E-06 2.34E-06 1.65E-10 1.34E-10 -2.298608398 2.295458984 2.215319824 2.337442017 757 9667.551346 2.95E-11 2.39E-06 -2.41E-06 5.35E-11 2.20E-06 2.34E-06 1.66E-10 1.34E-10 -2.292947388 2.288867188 2.210751343 2.332876587 758 9668.835589 -1.58E-10 2.39E-06 -2.41E-06 8.10E-11 2.20E-06 2.34E-06 1.66E-10 1.34E-10 -2.291751099 2.288534546 2.212347412 2.334283447 759 9670.108061 -5.85E-11 2.39E-06 -2.41E-06 3.70E-11 2.20E-06 2.34E-06 1.66E-10 1.34E-10 -2.288052368 2.283691406 2.210400391 2.331750488 760 9671.392999 7.50E-12 2.40E-06 -2.41E-06 6.45E-11 2.20E-06 2.34E-06 1.66E-10 1.34E-10 -2.29956665 2.296292114 2.223074341 2.345074463 761 9672.662117 6.25E-11 2.40E-06 -2.41E-06 7.55E-11 2.20E-06 2.35E-06 1.66E-10 1.34E-10 -2.295385742 2.290188599 2.219656372 2.342086792 762 9673.947748 7.90E-11 2.40E-06 -2.41E-06 8.10E-11 2.21E-06 2.35E-06 1.66E-10 1.34E-10 -2.296011353 2.291430664 2.223352051 2.345248413 763 9675.229685 -9.00E-12 2.40E-06 -2.41E-06 9.75E-11 2.21E-06 2.35E-06 1.67E-10 1.35E-10 -2.294360352 2.289505005 2.223501587 2.345629883 764 9676.503877 1.85E-11 2.40E-06 -2.41E-06 8.10E-11 2.21E-06 2.35E-06 1.67E-10 1.35E-10 -2.295547485 2.291259766 2.226358032 2.348526001 765 9677.790552 4.05E-11 2.40E-06 -2.41E-06 7.55E-11 2.21E-06 2.36E-06 1.67E-10 1.35E-10 -2.292922974 2.288296509 2.225717163 2.347668457 766 9679.069482 1.30E-11 2.40E-06 -2.41E-06 3.70E-11 2.21E-06 2.36E-06 1.67E-10 1.35E-10 -2.296118164 2.292129517 2.230792236 2.352975464 767 9680.348756 2.95E-11 2.39E-06 -2.41E-06 5.35E-11 2.21E-06 2.36E-06 1.67E-10 1.35E-10 -2.293988037 2.289251709 2.230099487 2.352230835 768 9681.636477 4.60E-11 2.40E-06 -2.41E-06 9.50E-12 2.22E-06 2.36E-06 1.67E-10 1.35E-10 -2.293670654 2.288934326 2.231555176 2.353970337 769 9682.928598 1.01E-10 2.40E-06 -2.41E-06 5.90E-11 2.22E-06 2.36E-06 1.68E-10 1.36E-10 -2.296206665 2.292575073 2.236022949 2.358712769 770 9684.204864 -2.00E-11 2.40E-06 -2.41E-06 8.65E-11 2.22E-06 2.36E-06 1.68E-10 1.36E-10 -2.292889404 2.288183594 2.235110474 2.357498169 771 9685.489579 -5.30E-11 2.40E-06 -2.41E-06 1.50E-11 2.22E-06 2.37E-06 1.68E-10 1.36E-10 -2.293481445 2.288790894 2.237216187 2.359597778 772 9686.778697 -1.52E-10 2.39E-06 -2.41E-06 1.09E-10 2.22E-06 2.37E-06 1.68E-10 1.36E-10 -2.290426636 2.285440063 2.236373901 2.358615112 773 9688.047889 -2.00E-11 2.40E-06 -2.41E-06 5.35E-11 2.23E-06 2.37E-06 1.69E-10 1.37E-10 -2.297540283 2.293795776 2.24487915 2.367694092 774 9689.337703 -3.10E-11 2.39E-06 -2.41E-06 1.20E-10 2.23E-06 2.37E-06 1.69E-10 1.37E-10 -2.291467285 2.286502075 2.240167236 2.362304688 775 9690.619753 -8.60E-11 2.40E-06 -2.41E-06 8.10E-11 2.23E-06 2.37E-06 1.69E-10 1.37E-10 -2.296630859 2.294168091 2.247808838 2.370370483 776 9691.914326 -1.14E-10 2.39E-06 -2.41E-06 4.80E-11 2.23E-06 2.37E-06 1.69E-10 1.37E-10 -2.294119263 2.289245605 2.246038818 2.36895752 777 9693.188953 -1.45E-11 2.40E-06 -2.41E-06 5.90E-11 2.23E-06 2.38E-06 1.69E-10 1.37E-10 -2.29614563 2.292626953 2.249911499 2.372790527 778 9694.488288 -2.55E-11 2.39E-06 -2.41E-06 3.15E-11 2.23E-06 2.38E-06 1.69E-10 1.37E-10 -2.293206787 2.289099121 2.248944092 2.371704102 779 9695.779855 -9.15E-11 2.39E-06 -2.41E-06 9.75E-11 2.24E-06 2.38E-06 1.70E-10 1.38E-10 -2.292004395 2.28717041 2.249539185 2.372006226 780 9697.055521 3.50E-11 2.39E-06 -2.41E-06 9.75E-11 2.24E-06 2.38E-06 1.70E-10 1.38E-10 -2.292626953 2.288772583 2.252780151 2.375906372 781 9698.335595 -2.55E-11 2.39E-06 -2.41E-06 1.25E-10 2.24E-06 2.38E-06 1.70E-10 1.38E-10 -2.289178467 2.283139038 2.250134277 2.372683716 782 9699.620079 4.05E-11 2.39E-06 -2.41E-06 3.70E-11 2.24E-06 2.38E-06 1.70E-10 1.38E-10 -2.29258728 2.287939453 2.255941772 2.378973389 783 9700.900844 3.50E-11 2.40E-06 -2.41E-06 5.35E-11 2.24E-06 2.39E-06 1.70E-10 1.38E-10 -2.293252563 2.289465332 2.258776855 2.38142395 784 9702.186022 -3.65E-11 2.39E-06 -2.41E-06 1.31E-10 2.24E-06 2.39E-06 1.71E-10 1.38E-10 -2.291033936 2.286114502 2.256869507 2.380029297 785 9703.483755 5.70E-11 2.40E-06 -2.41E-06 1.20E-10 2.24E-06 2.39E-06 1.71E-10 1.39E-10 -2.292367554 2.288259888 2.260916138 2.383987427 786 9704.765563 -9.00E-12 2.39E-06 -2.41E-06 1.20E-10 2.25E-06 2.39E-06 1.71E-10 1.38E-10 -2.29079895 2.286395264 2.260916138 2.384136963 787 9706.051788 -3.50E-12 2.39E-06 -2.41E-06 4.00E-12 2.25E-06 2.39E-06 1.71E-10 1.39E-10 -2.292163086 2.287356567 2.263510132 2.387088013 788 9707.334289 4.05E-11 2.39E-06 -2.40E-06 1.50E-11 2.25E-06 2.39E-06 1.71E-10 1.39E-10 -2.289804077 2.286386108 2.264151001 2.387387085 789 9708.617136 -5.30E-11 2.39E-06 -2.41E-06 1.03E-10 2.25E-06 2.40E-06 1.71E-10 1.39E-10 -2.286517334 2.280728149 2.261679077 2.384719849 790 9709.904404 7.50E-12 2.39E-06 -2.41E-06 1.97E-10 2.25E-06 2.40E-06 1.71E-10 1.39E-10 -2.291958618 2.288204956 2.268963623 2.392562866 791 9711.200172 7.50E-12 2.39E-06 -2.40E-06 9.20E-11 2.25E-06 2.40E-06 1.71E-10 1.39E-10 -2.280331421 2.275094604 2.259008789 2.381625366 792 9712.471835 -3.50E-12 2.38E-06 -2.39E-06 4.80E-11 2.25E-06 2.40E-06 1.71E-10 1.39E-10 -2.274761963 2.270993042 2.256039429 2.378494263 793 9713.75607 -1.96E-10 2.38E-06 -2.40E-06 1.47E-10 2.25E-06 2.39E-06 1.71E-10 1.39E-10 -2.285461426 2.281338501 2.26831665 2.391375732 794 9715.044731 -3.10E-11 2.39E-06 -2.40E-06 1.47E-10 2.25E-06 2.40E-06 1.71E-10 1.39E-10 -2.28913269 2.285528564 2.273989868 2.397122192 795 9716.34598 1.30E-11 2.39E-06 -2.40E-06 9.75E-11 2.25E-06 2.40E-06 1.72E-10 1.39E-10 -2.287091064 2.283688354 2.274563599 2.397964478 796 9717.627181 -5.30E-11 2.39E-06 -2.40E-06 3.70E-11 2.26E-06 2.40E-06 1.72E-10 1.39E-10 -2.285192871 2.280587769 2.274002075 2.397439575 797 9718.925056 -1.85E-10 2.39E-06 -2.40E-06 3.15E-11 2.26E-06 2.41E-06 1.72E-10 1.40E-10 -2.283071899 2.278811646 2.273483276 2.396673584 798 9720.202869 7.50E-12 2.39E-06 -2.40E-06 1.03E-10 2.26E-06 2.41E-06 1.72E-10 1.40E-10 -2.289096069 2.284939575 2.280682373 2.404092407 799 9721.489194 1.78E-10 2.39E-06 -2.41E-06 8.10E-11 2.27E-06 2.41E-06 1.72E-10 1.40E-10 -2.287445068 2.282351685 2.280462646 2.40401001 800 9722.784037 -3.65E-11 2.39E-06 -2.40E-06 1.20E-10 2.27E-06 2.41E-06 1.72E-10 1.40E-10 -2.286676025 2.282849121 2.282473755 2.40586853 801 9724.083319 -3.10E-11 2.39E-06 -2.40E-06 7.55E-11 2.27E-06 2.41E-06 1.73E-10 1.40E-10 -2.284884644 2.280517578 2.282983398 2.406286621 802 9725.378868 -3.65E-11 2.39E-06 -2.40E-06 1.09E-10 2.27E-06 2.41E-06 1.73E-10 1.40E-10 -2.285830688 2.282104492 2.285586548 2.408865356 803 9726.682948 1.30E-11 2.37E-06 -2.39E-06 1.14E-10 2.27E-06 2.41E-06 1.73E-10 1.40E-10 -2.270269775 2.265286255 2.271444702 2.393948364 804 9727.975115 -3.10E-11 2.37E-06 -2.39E-06 1.53E-10 2.27E-06 2.41E-06 1.73E-10 1.40E-10 -2.277102661 2.272827148 2.279858398 2.4027771 805 9729.263542 -3.50E-12 2.38E-06 -2.40E-06 2.05E-11 2.27E-06 2.41E-06 1.73E-10 1.41E-10 -2.282223511 2.277914429 2.286416626 2.41022644 806 9730.560502 -3.10E-11 2.37E-06 -2.39E-06 5.90E-11 2.27E-06 2.41E-06 1.73E-10 1.41E-10 -2.265167236 2.260812378 2.270620728 2.393365479 807 9731.849629 4.60E-11 2.37E-06 -2.39E-06 8.65E-11 2.27E-06 2.41E-06 1.73E-10 1.41E-10 -2.278134155 2.27303772 2.28581543 2.409555054 808 9733.147294 2.95E-11 2.39E-06 -2.40E-06 8.10E-11 2.27E-06 2.42E-06 1.73E-10 1.41E-10 -2.285800171 2.281924438 2.29621582 2.420336914 809 9734.437121 -1.45E-11 2.39E-06 -2.40E-06 1.20E-10 2.28E-06 2.42E-06 1.74E-10 1.41E-10 -2.281503296 2.276766968 2.293856812 2.417895508 810 9735.751876 1.30E-11 2.39E-06 -2.40E-06 1.09E-10 2.28E-06 2.42E-06 1.74E-10 1.41E-10 -2.28704834 2.283459473 2.301345825 2.425323486 811 9737.026019 -1.45E-11 2.38E-06 -2.40E-06 -1.25E-11 2.28E-06 2.43E-06 1.75E-10 1.42E-10 -2.283859253 2.279916382 2.299865723 2.42376709 812 9738.337389 1.12E-10 2.39E-06 -2.40E-06 2.05E-11 2.29E-06 2.43E-06 1.75E-10 1.42E-10 -2.286279297 2.282427979 2.303811646 2.428030396 813 9739.640922 -1.08E-10 2.38E-06 -2.40E-06 9.50E-12 2.29E-06 2.43E-06 1.75E-10 1.42E-10 -2.282608032 2.278182983 2.302197266 2.425964355 814 9740.940709 -6.40E-11 2.37E-06 -2.39E-06 1.14E-10 2.29E-06 2.43E-06 1.75E-10 1.42E-10 -2.263626099 2.258804321 2.284814453 2.407913208 815 9742.228546 3.50E-11 2.38E-06 -2.39E-06 1.25E-10 2.29E-06 2.43E-06 1.75E-10 1.42E-10 -2.279681396 2.275048828 2.30322876 2.427059937 816 9743.541349 -1.36E-10 2.38E-06 -2.40E-06 8.65E-11 2.29E-06 2.43E-06 1.75E-10 1.42E-10 -2.28109436 2.276202393 2.30617981 2.429910278 817 9744.829888 -4.20E-11 2.38E-06 -2.40E-06 7.00E-11 2.29E-06 2.43E-06 1.75E-10 1.43E-10 -2.285018921 2.280792236 2.312203979 2.436190796 818 9746.12288 -2.00E-11 2.39E-06 -2.40E-06 9.20E-11 2.29E-06 2.44E-06 1.75E-10 1.43E-10 -2.28543396 2.282330322 2.314981079 2.439215088 819 9747.424436 -9.70E-11 2.38E-06 -2.40E-06 8.10E-11 2.30E-06 2.44E-06 1.76E-10 1.43E-10 -2.281503296 2.27699585 2.312780762 2.436593628 820 9748.722239 2.00E-12 2.38E-06 -2.40E-06 7.00E-11 2.30E-06 2.45E-06 1.76E-10 1.43E-10 -2.281646729 2.278674316 2.316009521 2.440118408 821 9750.012179 -9.70E-11 2.38E-06 -2.39E-06 8.10E-11 2.30E-06 2.45E-06 1.76E-10 1.43E-10 -2.277767944 2.27258606 2.312661743 2.43687439 822 9751.310686 -1.14E-10 2.38E-06 -2.40E-06 3.15E-11 2.30E-06 2.45E-06 1.77E-10 1.44E-10 -2.283267212 2.279568481 2.32003479 2.444659424 823 9752.601325 -1.08E-10 2.38E-06 -2.39E-06 1.09E-10 2.30E-06 2.45E-06 1.77E-10 1.44E-10 -2.276351929 2.271340942 2.315060425 2.438656616 824 9753.904649 -6.95E-11 2.38E-06 -2.40E-06 -1.25E-11 2.30E-06 2.45E-06 1.77E-10 1.44E-10 -2.278890991 2.273825073 2.319619751 2.443673706 825 9755.200103 -7.50E-11 2.38E-06 -2.40E-06 4.80E-11 2.31E-06 2.45E-06 1.77E-10 1.44E-10 -2.280084229 2.275320435 2.322366333 2.446594238 826 9756.504136 -5.85E-11 2.38E-06 -2.39E-06 5.90E-11 2.31E-06 2.45E-06 1.77E-10 1.44E-10 -2.278872681 2.273690796 2.323190308 2.447460938 827 9757.800295 -9.15E-11 2.38E-06 -2.40E-06 1.03E-10 2.31E-06 2.46E-06 1.77E-10 1.44E-10 -2.281341553 2.277999878 2.327487183 2.452157593 828 9759.100923 1.95E-10 2.38E-06 -2.39E-06 4.80E-11 2.31E-06 2.46E-06 1.78E-10 1.45E-10 -2.279470825 2.276745605 2.328018188 2.452545166 829 9760.414257 -6.95E-11 2.38E-06 -2.39E-06 4.25E-11 2.31E-06 2.46E-06 1.78E-10 1.45E-10 -2.274029541 2.269180298 2.323596191 2.44798584 830 9761.699121 -2.00E-11 2.38E-06 -2.39E-06 8.10E-11 2.31E-06 2.46E-06 1.78E-10 1.45E-10 -2.278198242 2.274530029 2.329519653 2.454187012 831 9762.992571 -1.74E-10 2.37E-06 -2.39E-06 9.50E-12 2.31E-06 2.46E-06 1.78E-10 1.45E-10 -2.269625854 2.263754272 2.322259521 2.446292114 832 9764.294613 1.85E-11 2.37E-06 -2.39E-06 1.50E-11 2.31E-06 2.46E-06 1.78E-10 1.45E-10 -2.272167969 2.267739868 2.327639771 2.451516724 833 9765.605253 -6.40E-11 2.37E-06 -2.38E-06 7.55E-11 2.31E-06 2.46E-06 1.78E-10 1.45E-10 -2.26524353 2.261157227 2.322290039 2.445452881 834 9766.895637 7.50E-12 2.35E-06 -2.36E-06 6.45E-11 2.31E-06 2.46E-06 1.78E-10 1.45E-10 -2.242929077 2.238082886 2.302679443 2.423114014 835 9768.202867 -8.60E-11 2.32E-06 -2.34E-06 5.90E-11 2.30E-06 2.45E-06 1.78E-10 1.45E-10 -2.224893188 2.221472168 2.286706543 2.404751587 836 9769.518705 -5.85E-11 2.31E-06 -2.33E-06 9.20E-11 2.29E-06 2.43E-06 1.77E-10 1.44E-10 -2.21817627 2.21401062 2.281164551 2.399429321 837 9770.814272 -4.75E-11 2.32E-06 -2.33E-06 7.55E-11 2.28E-06 2.42E-06 1.77E-10 1.44E-10 -2.214266968 2.210388184 2.279434204 2.398364258 838 9772.122573 -3.65E-11 2.31E-06 -2.32E-06 1.36E-10 2.27E-06 2.41E-06 1.76E-10 1.43E-10 -2.209970093 2.205645752 2.275924683 2.395501709 839 9773.422974 4.05E-11 2.31E-06 -2.32E-06 1.36E-10 2.27E-06 2.41E-06 1.76E-10 1.43E-10 -2.211340332 2.207571411 2.27819519 2.399240112 840 9774.727859 -5.30E-11 2.31E-06 -2.32E-06 7.55E-11 2.27E-06 2.41E-06 1.76E-10 1.43E-10 -2.207824707 2.202789307 2.275061035 2.397344971 841 9776.037231 1.34E-10 2.30E-06 -2.32E-06 7.00E-11 2.26E-06 2.41E-06 1.76E-10 1.44E-10 -2.208410645 2.202374268 2.276226807 2.398907471 842 9777.342829 -1.69E-10 2.31E-06 -2.32E-06 3.70E-11 2.27E-06 2.41E-06 1.76E-10 1.44E-10 -2.211120605 2.206314087 2.280337524 2.404135132 843 9778.64465 -3.65E-11 2.31E-06 -2.33E-06 1.14E-10 2.27E-06 2.41E-06 1.76E-10 1.44E-10 -2.21774292 2.212680054 2.288000488 2.412817383 844 9779.95096 1.07E-10 2.33E-06 -2.34E-06 5.90E-11 2.27E-06 2.42E-06 1.77E-10 1.44E-10 -2.229867554 2.22507019 2.301620483 2.427630615 845 9781.265897 -3.65E-11 2.34E-06 -2.36E-06 9.75E-11 2.28E-06 2.43E-06 1.77E-10 1.45E-10 -2.252987671 2.24942627 2.328417969 2.455093384 846 9782.581195 -1.47E-10 2.37E-06 -2.38E-06 -1.25E-11 2.30E-06 2.44E-06 1.78E-10 1.46E-10 -2.271414185 2.266693115 2.350878906 2.476989746 847 9783.892717 -6.40E-11 2.38E-06 -2.39E-06 2.60E-11 2.32E-06 2.46E-06 1.80E-10 1.47E-10 -2.279351807 2.275845337 2.36277771 2.488391113 848 9785.204598 -6.95E-11 2.38E-06 -2.39E-06 1.14E-10 2.33E-06 2.48E-06 1.81E-10 1.48E-10 -2.275463867 2.269851685 2.360314941 2.485473633 849 9786.496138 -1.08E-10 2.38E-06 -2.39E-06 8.65E-11 2.34E-06 2.49E-06 1.82E-10 1.48E-10 -2.277807617 2.273312378 2.365585327 2.49112854 850 9787.800449 -1.41E-10 2.38E-06 -2.39E-06 5.90E-11 2.35E-06 2.50E-06 1.82E-10 1.49E-10 -2.274508667 2.269012451 2.364059448 2.489321899 851 9789.113401 5.70E-11 2.38E-06 -2.39E-06 4.80E-11 2.35E-06 2.50E-06 1.82E-10 1.49E-10 -2.279278564 2.275164795 2.371200562 2.496536255 852 9790.430856 -1.14E-10 2.38E-06 -2.39E-06 2.60E-11 2.35E-06 2.50E-06 1.83E-10 1.49E-10 -2.275491333 2.270822144 2.368914795 2.494195557 853 9791.72795 -8.05E-11 2.38E-06 -2.39E-06 2.60E-11 2.36E-06 2.50E-06 1.83E-10 1.49E-10 -2.279779053 2.276031494 2.37557373 2.501290894 854 9793.046123 -1.25E-10 2.38E-06 -2.39E-06 7.55E-11 2.36E-06 2.51E-06 1.83E-10 1.49E-10 -2.277383423 2.272756958 2.374090576 2.499694824 855 9794.343925 -1.47E-10 2.38E-06 -2.39E-06 1.31E-10 2.36E-06 2.51E-06 1.83E-10 1.49E-10 -2.279116821 2.275003052 2.3784729 2.504315186 856 9795.646226 1.85E-11 2.38E-06 -2.39E-06 2.05E-11 2.36E-06 2.51E-06 1.83E-10 1.49E-10 -2.275161743 2.26987915 2.375518799 2.501049805 857 9796.948881 -4.75E-11 2.38E-06 -2.39E-06 9.20E-11 2.36E-06 2.51E-06 1.83E-10 1.50E-10 -2.27633667 2.273098755 2.379602051 2.50519104 858 9798.26434 -1.30E-10 2.37E-06 -2.39E-06 5.90E-11 2.37E-06 2.51E-06 1.84E-10 1.50E-10 -2.274301147 2.269537354 2.378414917 2.503933716 859 9799.571857 9.00E-11 2.38E-06 -2.39E-06 8.10E-11 2.37E-06 2.51E-06 1.84E-10 1.50E-10 -2.275830078 2.271395874 2.3822052 2.507543945 860 9800.875579 -8.60E-11 2.37E-06 -2.39E-06 9.20E-11 2.37E-06 2.51E-06 1.84E-10 1.50E-10 -2.273529053 2.269204712 2.38142395 2.506784058 861 9802.192115 -1.08E-10 2.38E-06 -2.39E-06 5.90E-11 2.37E-06 2.52E-06 1.84E-10 1.50E-10 -2.274755859 2.270394897 2.384475708 2.510073853 862 9803.496549 1.30E-11 2.38E-06 -2.39E-06 2.05E-11 2.37E-06 2.52E-06 1.84E-10 1.50E-10 -2.275869751 2.271536255 2.387533569 2.513067627 863 9804.809649 -6.95E-11 2.38E-06 -2.39E-06 1.50E-11 2.37E-06 2.52E-06 1.84E-10 1.50E-10 -2.276626587 2.272351074 2.39012146 2.515869141 864 9806.114794 -1.08E-10 2.38E-06 -2.39E-06 2.05E-11 2.37E-06 2.52E-06 1.85E-10 1.51E-10 -2.274700928 2.270025635 2.389685059 2.515246582 865 9807.42861 -4.75E-11 2.37E-06 -2.39E-06 1.36E-10 2.38E-06 2.52E-06 1.85E-10 1.51E-10 -2.273681641 2.269503784 2.390762329 2.516690063 866 9808.738626 2.40E-11 2.37E-06 -2.39E-06 4.25E-11 2.38E-06 2.52E-06 1.85E-10 1.51E-10 -2.270751953 2.26595459 2.38913269 2.514807129 867 9810.053161 -3.65E-11 2.38E-06 -2.39E-06 1.14E-10 2.38E-06 2.53E-06 1.86E-10 1.52E-10 -2.275439453 2.2712677 2.396051025 2.522021484 868 9811.363893 9.55E-11 2.37E-06 -2.39E-06 7.00E-11 2.38E-06 2.53E-06 1.86E-10 1.52E-10 -2.270700073 2.265777588 2.392550659 2.518151855 869 9812.662495 -2.00E-11 2.37E-06 -2.39E-06 5.35E-11 2.38E-06 2.53E-06 1.86E-10 1.52E-10 -2.272613525 2.268600464 2.396957397 2.522839355 870 9813.978104 -1.08E-10 2.37E-06 -2.39E-06 1.31E-10 2.38E-06 2.53E-06 1.86E-10 1.52E-10 -2.273104858 2.269277954 2.399624634 2.525473022 871 9815.302403 -6.95E-11 2.37E-06 -2.39E-06 7.55E-11 2.38E-06 2.53E-06 1.86E-10 1.52E-10 -2.270913696 2.266351318 2.399301147 2.525097656 872 9816.606236 1.85E-11 2.37E-06 -2.39E-06 1.53E-10 2.39E-06 2.53E-06 1.86E-10 1.52E-10 -2.272598267 2.268811035 2.40307312 2.529165649 873 9817.93126 1.89E-10 2.37E-06 -2.39E-06 7.55E-11 2.39E-06 2.54E-06 1.86E-10 1.52E-10 -2.270141602 2.265093994 2.401345825 2.527389526 874 9819.244143 -2.02E-10 2.37E-06 -2.38E-06 6.45E-11 2.39E-06 2.54E-06 1.86E-10 1.53E-10 -2.270870972 2.267553711 2.405041504 2.530682373 875 9820.549046 -1.19E-10 2.37E-06 -2.39E-06 1.31E-10 2.39E-06 2.54E-06 1.86E-10 1.53E-10 -2.270748901 2.266168213 2.406231689 2.532415771 876 9821.866815 -6.40E-11 2.37E-06 -2.38E-06 4.80E-11 2.39E-06 2.54E-06 1.87E-10 1.53E-10 -2.26496582 2.259527588 2.40211792 2.527874756 877 9823.180774 -9.15E-11 2.37E-06 -2.38E-06 1.20E-10 2.39E-06 2.54E-06 1.87E-10 1.53E-10 -2.269787598 2.265826416 2.40874939 2.534912109 878 9824.495091 -9.00E-12 2.36E-06 -2.38E-06 7.00E-11 2.39E-06 2.54E-06 1.87E-10 1.53E-10 -2.264660645 2.260369873 2.40557251 2.531616211 879 9825.818116 3.50E-11 2.36E-06 -2.38E-06 4.80E-11 2.39E-06 2.54E-06 1.87E-10 1.53E-10 -2.263134766 2.259161377 2.405633545 2.531637573 880 9827.141505 -2.55E-11 2.36E-06 -2.38E-06 1.36E-10 2.39E-06 2.54E-06 1.87E-10 1.53E-10 -2.263827515 2.25960083 2.408361816 2.534194946 881 9828.452729 2.95E-11 2.36E-06 -2.37E-06 4.80E-11 2.39E-06 2.54E-06 1.87E-10 1.53E-10 -2.258639526 2.254760742 2.404983521 2.530853271 882 9829.76431 2.40E-11 2.36E-06 -2.37E-06 -7.00E-12 2.39E-06 2.54E-06 1.87E-10 1.53E-10 -2.25322876 2.248925781 2.401303101 2.526449585 883 9831.084605 -7.50E-11 2.35E-06 -2.37E-06 9.20E-11 2.39E-06 2.54E-06 1.87E-10 1.53E-10 -2.250454712 2.245480347 2.400369263 2.525552368 884 9832.401084 -1.74E-10 2.35E-06 -2.37E-06 7.55E-11 2.39E-06 2.54E-06 1.87E-10 1.53E-10 -2.253369141 2.249353027 2.405249023 2.530892944 885 9833.722103 7.50E-12 2.35E-06 -2.36E-06 8.65E-11 2.39E-06 2.54E-06 1.88E-10 1.54E-10 -2.250213623 2.245483398 2.402871704 2.528231812 886 9835.043485 4.60E-11 2.35E-06 -2.36E-06 1.14E-10 2.39E-06 2.54E-06 1.88E-10 1.54E-10 -2.247946167 2.243347168 2.403091431 2.528436279 887 9836.361046 -1.74E-10 2.35E-06 -2.36E-06 5.35E-11 2.39E-06 2.54E-06 1.88E-10 1.54E-10 -2.250634766 2.246902466 2.408584595 2.533630371 888 9837.678967 -4.75E-11 2.35E-06 -2.36E-06 5.35E-11 2.39E-06 2.54E-06 1.88E-10 1.54E-10 -2.246817017 2.24147644 2.405291748 2.530490112 889 9839.001435 -1.41E-10 2.35E-06 -2.36E-06 8.65E-11 2.39E-06 2.54E-06 1.88E-10 1.54E-10 -2.249716187 2.24576416 2.410824585 2.536282349 890 9840.328453 1.30E-11 2.34E-06 -2.36E-06 7.00E-11 2.39E-06 2.54E-06 1.88E-10 1.54E-10 -2.248138428 2.244064331 2.410745239 2.536050415 891 9841.655836 -3.50E-12 2.35E-06 -2.36E-06 2.60E-11 2.40E-06 2.54E-06 1.88E-10 1.54E-10 -2.24677124 2.242388916 2.411691284 2.536743164 892 9842.983585 1.30E-11 2.35E-06 -2.36E-06 3.70E-11 2.40E-06 2.55E-06 1.89E-10 1.54E-10 -2.248010254 2.243228149 2.414056396 2.539660645 893 9844.290749 -8.60E-11 2.35E-06 -2.36E-06 8.10E-11 2.40E-06 2.55E-06 1.89E-10 1.55E-10 -2.246646118 2.241412354 2.414459229 2.539648438 894 9845.615032 -1.19E-10 2.35E-06 -2.36E-06 1.53E-10 2.40E-06 2.55E-06 1.90E-10 1.55E-10 -2.249536133 2.245117188 2.420077515 2.54564209 895 9846.931295 -5.30E-11 2.35E-06 -2.36E-06 3.70E-11 2.40E-06 2.55E-06 1.90E-10 1.56E-10 -2.246340942 2.241668701 2.418789673 2.544302368 896 9848.256304 -5.30E-11 2.35E-06 -2.37E-06 3.70E-11 2.41E-06 2.55E-06 1.90E-10 1.56E-10 -2.251922607 2.247433472 2.426605225 2.551919556 897 9849.585872 -1.19E-10 2.35E-06 -2.36E-06 7.55E-11 2.41E-06 2.56E-06 1.90E-10 1.56E-10 -2.249389648 2.245700073 2.426019287 2.551434326 898 9850.920003 -5.30E-11 2.34E-06 -2.36E-06 8.10E-11 2.41E-06 2.56E-06 1.91E-10 1.56E-10 -2.249423218 2.245550537 2.427307129 2.552850342 899 9852.246108 7.50E-12 2.35E-06 -2.36E-06 4.80E-11 2.41E-06 2.56E-06 1.91E-10 1.56E-10 -2.248156738 2.24357605 2.428103638 2.553930664 900 9853.555785 -9.15E-11 2.35E-06 -2.36E-06 3.15E-11 2.41E-06 2.56E-06 1.91E-10 1.56E-10 -2.248739624 2.243927002 2.430368042 2.55642395 901 9854.886814 -3.10E-11 2.35E-06 -2.36E-06 4.80E-11 2.42E-06 2.56E-06 1.91E-10 1.57E-10 -2.24621582 2.241168213 2.429806519 2.555856323 902 9856.214011 -4.75E-11 2.35E-06 -2.36E-06 5.90E-11 2.42E-06 2.57E-06 1.91E-10 1.57E-10 -2.250201416 2.246328735 2.43666687 2.562875366 903 9857.541572 -8.05E-11 2.35E-06 -2.36E-06 1.09E-10 2.42E-06 2.57E-06 1.92E-10 1.57E-10 -2.246548462 2.240722656 2.43319397 2.559210205 904 9858.873701 2.95E-11 2.35E-06 -2.36E-06 3.70E-11 2.42E-06 2.57E-06 1.92E-10 1.58E-10 -2.250796509 2.247058105 2.439822388 2.566390991 905 9860.21881 3.50E-11 2.35E-06 -2.36E-06 -7.00E-12 2.42E-06 2.57E-06 1.92E-10 1.57E-10 -2.248883057 2.244628906 2.440188599 2.566372681 906 9861.539062 1.51E-10 2.35E-06 -2.36E-06 4.00E-12 2.43E-06 2.57E-06 1.92E-10 1.58E-10 -2.24916687 2.245401001 2.442236328 2.568740845 907 9862.868089 -8.05E-11 2.35E-06 -2.36E-06 4.80E-11 2.43E-06 2.58E-06 1.92E-10 1.58E-10 -2.247033691 2.242285156 2.441616821 2.567782593 908 9864.214311 2.00E-12 2.35E-06 -2.36E-06 -1.50E-12 2.43E-06 2.58E-06 1.92E-10 1.58E-10 -2.24864502 2.24520874 2.445510864 2.572167969 909 9865.531447 -1.91E-10 2.35E-06 -2.36E-06 4.80E-11 2.43E-06 2.58E-06 1.93E-10 1.58E-10 -2.247488403 2.242956543 2.445465088 2.572000122 910 9866.857362 -1.63E-10 2.35E-06 -2.36E-06 3.15E-11 2.43E-06 2.58E-06 1.93E-10 1.58E-10 -2.246746826 2.242373657 2.446936035 2.573678589 911 9868.187853 -6.95E-11 2.35E-06 -2.36E-06 6.45E-11 2.43E-06 2.58E-06 1.93E-10 1.58E-10 -2.243145752 2.237677002 2.445098877 2.570889282 912 9869.531346 -1.19E-10 2.34E-06 -2.36E-06 4.00E-12 2.44E-06 2.58E-06 1.93E-10 1.58E-10 -2.249407959 2.24498291 2.453552246 2.57989502 913 9870.841506 1.30E-11 2.35E-06 -2.36E-06 1.14E-10 2.44E-06 2.58E-06 1.93E-10 1.58E-10 -2.246084595 2.241281128 2.452084351 2.578433228 914 9872.181522 -3.50E-12 2.35E-06 -2.36E-06 3.15E-11 2.44E-06 2.59E-06 1.94E-10 1.59E-10 -2.24960022 2.245983887 2.458154297 2.584869385 915 9873.538772 -1.25E-10 2.35E-06 -2.36E-06 1.09E-10 2.44E-06 2.59E-06 1.94E-10 1.59E-10 -2.246850586 2.242953491 2.457067871 2.583584595 916 9874.854236 8.45E-11 2.35E-06 -2.36E-06 9.50E-12 2.44E-06 2.59E-06 1.94E-10 1.59E-10 -2.245690918 2.241464233 2.457128906 2.583609009 917 9876.199583 2.95E-11 2.34E-06 -2.36E-06 1.69E-10 2.44E-06 2.59E-06 1.94E-10 1.59E-10 -2.244787598 2.239849854 2.457809448 2.584109497 918 9877.545304 -1.47E-10 2.35E-06 -2.36E-06 3.15E-11 2.44E-06 2.59E-06 1.94E-10 1.59E-10 -2.245605469 2.241104126 2.460110474 2.587033081 919 9878.870298 -8.60E-11 2.35E-06 -2.36E-06 1.42E-10 2.45E-06 2.60E-06 1.94E-10 1.59E-10 -2.24720459 2.242114258 2.463812256 2.590664673 920 9880.204098 -5.85E-11 2.35E-06 -2.36E-06 1.09E-10 2.45E-06 2.60E-06 1.94E-10 1.59E-10 -2.244006348 2.239044189 2.462747192 2.58921814 921 9881.538265 -1.47E-10 2.34E-06 -2.36E-06 1.31E-10 2.45E-06 2.60E-06 1.94E-10 1.59E-10 -2.243664551 2.239071655 2.464871216 2.591473389 922 9882.885472 9.55E-11 2.35E-06 -2.36E-06 6.45E-11 2.45E-06 2.60E-06 1.94E-10 1.60E-10 -2.245172119 2.241986084 2.468762207 2.595410156 923 9884.22038 -1.03E-10 2.34E-06 -2.36E-06 1.03E-10 2.45E-06 2.60E-06 1.94E-10 1.59E-10 -2.243469238 2.237860107 2.46751709 2.594412231 924 9885.555655 -8.05E-11 2.34E-06 -2.36E-06 7.00E-11 2.46E-06 2.60E-06 1.94E-10 1.60E-10 -2.247314453 2.243756104 2.474093628 2.600756836 925 9886.891298 4.05E-11 2.34E-06 -2.36E-06 1.20E-10 2.46E-06 2.61E-06 1.94E-10 1.60E-10 -2.243856812 2.23991394 2.47265625 2.599206543 926 9888.235767 1.56E-10 2.34E-06 -2.36E-06 7.00E-11 2.46E-06 2.61E-06 1.95E-10 1.60E-10 -2.240301514 2.23425293 2.470516968 2.596630859 927 9889.559462 -1.41E-10 2.34E-06 -2.36E-06 9.20E-11 2.46E-06 2.61E-06 1.95E-10 1.60E-10 -2.244024658 2.239431763 2.476754761 2.603500366 928 9890.89621 -2.00E-11 2.34E-06 -2.36E-06 4.25E-11 2.46E-06 2.61E-06 1.95E-10 1.61E-10 -2.242883301 2.237487793 2.476989746 2.60406189 929 9892.229095 -4.20E-11 2.34E-06 -2.36E-06 8.10E-11 2.46E-06 2.61E-06 1.96E-10 1.61E-10 -2.244778442 2.240475464 2.481561279 2.608520508 930 9893.570814 4.60E-11 2.34E-06 -2.35E-06 3.70E-11 2.47E-06 2.62E-06 1.96E-10 1.61E-10 -2.239538574 2.233886719 2.477581787 2.604208374 931 9894.972184 -1.03E-10 2.34E-06 -2.36E-06 2.05E-11 2.47E-06 2.62E-06 1.96E-10 1.61E-10 -2.244827271 2.24196167 2.485406494 2.612997437 932 9896.272307 6.25E-11 2.34E-06 -2.36E-06 6.45E-11 2.47E-06 2.62E-06 1.96E-10 1.61E-10 -2.243045044 2.23901062 2.485147095 2.612481689 933 9897.632092 -2.55E-11 2.34E-06 -2.35E-06 9.75E-11 2.47E-06 2.62E-06 1.96E-10 1.61E-10 -2.241320801 2.236099243 2.484622192 2.611865234 934 9898.94988 -1.96E-10 2.34E-06 -2.36E-06 7.55E-11 2.47E-06 2.62E-06 1.96E-10 1.61E-10 -2.24317627 2.239483643 2.489407349 2.61661377 935 9900.272265 -7.50E-11 2.34E-06 -2.36E-06 7.00E-11 2.47E-06 2.62E-06 1.96E-10 1.61E-10 -2.241415405 2.236096191 2.488571167 2.615478516 936 9901.607732 -1.30E-10 2.34E-06 -2.36E-06 9.75E-11 2.48E-06 2.63E-06 1.97E-10 1.61E-10 -2.240670776 2.235247803 2.489520264 2.616503906 937 9902.952049 -1.14E-10 2.34E-06 -2.36E-06 9.75E-11 2.48E-06 2.63E-06 1.97E-10 1.62E-10 -2.243002319 2.238912964 2.49465332 2.62210083 938 9904.28401 -1.30E-10 2.34E-06 -2.36E-06 4.80E-11 2.48E-06 2.63E-06 1.97E-10 1.62E-10 -2.242800903 2.237689209 2.496426392 2.623739624 939 9905.612095 2.00E-12 2.34E-06 -2.36E-06 9.20E-11 2.48E-06 2.63E-06 1.97E-10 1.62E-10 -2.245141602 2.241558838 2.501315308 2.628591919 940 9906.944787 -5.30E-11 2.34E-06 -2.36E-06 4.25E-11 2.48E-06 2.63E-06 1.98E-10 1.63E-10 -2.241137695 2.236810303 2.498779297 2.625784302 941 9908.303322 -8.05E-11 2.34E-06 -2.36E-06 -4.00E-11 2.49E-06 2.64E-06 1.98E-10 1.63E-10 -2.243103027 2.239083862 2.502908325 2.630319214 942 9909.649495 -6.40E-11 2.34E-06 -2.35E-06 1.31E-10 2.49E-06 2.64E-06 1.98E-10 1.63E-10 -2.241497803 2.236489868 2.502209473 2.630102539 943 9910.996042 1.29E-10 2.34E-06 -2.35E-06 3.15E-11 2.49E-06 2.64E-06 1.98E-10 1.63E-10 -2.241491699 2.23710022 2.503973389 2.631378174 944 9912.308966 -9.70E-11 2.34E-06 -2.35E-06 2.05E-11 2.49E-06 2.64E-06 1.98E-10 1.63E-10 -2.238232422 2.233111572 2.501800537 2.629333496 945 9913.652 1.30E-11 2.34E-06 -2.36E-06 2.05E-11 2.49E-06 2.64E-06 1.98E-10 1.63E-10 -2.239648438 2.234765625 2.506030273 2.63347168 946 9914.995406 -8.05E-11 2.34E-06 -2.35E-06 1.50E-11 2.49E-06 2.64E-06 1.98E-10 1.63E-10 -2.240112305 2.235665894 2.508496094 2.635931396 947 9916.33493 -3.65E-11 2.34E-06 -2.35E-06 1.14E-10 2.49E-06 2.65E-06 1.98E-10 1.63E-10 -2.239138794 2.234262085 2.509127808 2.636935425 948 9917.679078 2.95E-11 2.34E-06 -2.36E-06 4.80E-11 2.50E-06 2.65E-06 1.99E-10 1.64E-10 -2.243154907 2.239489746 2.516442871 2.644335938 949 9919.027853 2.95E-11 2.34E-06 -2.35E-06 3.15E-11 2.50E-06 2.65E-06 1.99E-10 1.64E-10 -2.240359497 2.236169434 2.515158081 2.642694092 950 9920.36849 -4.75E-11 2.34E-06 -2.36E-06 -1.50E-12 2.50E-06 2.65E-06 1.99E-10 1.64E-10 -2.242672729 2.238876343 2.519692993 2.647454834 951 9921.700981 4.60E-11 2.34E-06 -2.35E-06 3.15E-11 2.50E-06 2.65E-06 2.00E-10 1.64E-10 -2.238092041 2.233096313 2.5159729 2.643725586 952 9923.059391 -5.85E-11 2.34E-06 -2.36E-06 7.00E-11 2.50E-06 2.66E-06 2.00E-10 1.65E-10 -2.24046936 2.236581421 2.5209198 2.648721313 953 9924.4054 -2.18E-10 2.34E-06 -2.35E-06 5.35E-11 2.51E-06 2.66E-06 2.00E-10 1.64E-10 -2.239447021 2.234606934 2.521511841 2.649038696 954 9925.730476 -4.75E-11 2.34E-06 -2.35E-06 7.55E-11 2.51E-06 2.66E-06 2.00E-10 1.65E-10 -2.238397217 2.233233643 2.521792603 2.649435425 955 9927.090012 -1.45E-11 2.34E-06 -2.35E-06 2.60E-11 2.51E-06 2.66E-06 2.00E-10 1.65E-10 -2.238528442 2.233883667 2.524169922 2.651651001 956 9928.437138 -6.95E-11 2.34E-06 -2.35E-06 9.20E-11 2.51E-06 2.66E-06 2.00E-10 1.65E-10 -2.239019775 2.235647583 2.526809692 2.654992676 957 9929.784637 -1.41E-10 2.34E-06 -2.35E-06 3.15E-11 2.51E-06 2.66E-06 2.01E-10 1.65E-10 -2.237527466 2.232098389 2.526074219 2.654086304 958 9931.141041 4.05E-11 2.34E-06 -2.35E-06 6.45E-11 2.51E-06 2.66E-06 2.01E-10 1.65E-10 -2.2431427 2.23934021 2.535021973 2.663571167 959 9932.506358 -5.85E-11 2.34E-06 -2.35E-06 4.80E-11 2.52E-06 2.67E-06 2.01E-10 1.66E-10 -2.236526489 2.231393433 2.529440308 2.657363892 960 9933.872059 -7.50E-11 2.34E-06 -2.35E-06 4.80E-11 2.52E-06 2.67E-06 2.01E-10 1.66E-10 -2.239953613 2.235787964 2.535681152 2.66355896 961 9935.225333 -4.20E-11 2.34E-06 -2.35E-06 1.09E-10 2.52E-06 2.67E-06 2.02E-10 1.66E-10 -2.237445068 2.232492065 2.534411621 2.662188721 962 9936.578985 1.85E-11 2.34E-06 -2.35E-06 1.03E-10 2.52E-06 2.67E-06 2.02E-10 1.66E-10 -2.238619995 2.234561157 2.537838745 2.665631104 963 9937.9501 -2.55E-11 2.33E-06 -2.35E-06 8.65E-11 2.52E-06 2.67E-06 2.02E-10 1.66E-10 -2.236917114 2.232388306 2.537692261 2.665679932 964 9939.29169 -4.75E-11 2.34E-06 -2.35E-06 4.25E-11 2.52E-06 2.68E-06 2.02E-10 1.67E-10 -2.238574219 2.233538818 2.540911865 2.669033813 965 9940.650747 -5.30E-11 2.34E-06 -2.35E-06 8.10E-11 2.53E-06 2.68E-06 2.02E-10 1.67E-10 -2.240524292 2.236712646 2.545602417 2.673922729 966 9942.027285 -1.36E-10 2.34E-06 -2.35E-06 4.80E-11 2.53E-06 2.68E-06 2.03E-10 1.67E-10 -2.238241577 2.233587646 2.544897461 2.672817993 967 9943.387105 -3.10E-11 2.33E-06 -2.35E-06 2.05E-11 2.53E-06 2.68E-06 2.03E-10 1.67E-10 -2.23777771 2.233041382 2.546557617 2.674969482 968 9944.755861 -8.05E-11 2.34E-06 -2.35E-06 7.55E-11 2.53E-06 2.68E-06 2.03E-10 1.67E-10 -2.239273071 2.235452271 2.550491333 2.678546143 969 9946.099327 -6.95E-11 2.33E-06 -2.35E-06 7.00E-11 2.53E-06 2.68E-06 2.03E-10 1.68E-10 -2.232888794 2.227093506 2.544503784 2.672232056 970 9947.447444 -1.08E-10 2.34E-06 -2.35E-06 2.60E-11 2.53E-06 2.69E-06 2.03E-10 1.67E-10 -2.237530518 2.2337677 2.55274353 2.680950928 971 9948.800215 -2.55E-11 2.33E-06 -2.35E-06 7.00E-11 2.54E-06 2.69E-06 2.03E-10 1.68E-10 -2.235562134 2.23163147 2.552227783 2.680636597 972 9950.157644 7.50E-12 2.34E-06 -2.35E-06 2.60E-11 2.54E-06 2.69E-06 2.03E-10 1.68E-10 -2.234429932 2.230099487 2.553289795 2.681237793 973 9951.519735 -4.20E-11 2.33E-06 -2.35E-06 1.36E-10 2.54E-06 2.69E-06 2.03E-10 1.68E-10 -2.234408569 2.229995728 2.55473938 2.683139038 974 9952.869352 1.51E-10 2.33E-06 -2.34E-06 4.80E-11 2.54E-06 2.69E-06 2.04E-10 1.68E-10 -2.229946899 2.224612427 2.551452637 2.679504395 975 9954.223629 -1.03E-10 2.33E-06 -2.35E-06 8.65E-11 2.54E-06 2.69E-06 2.04E-10 1.68E-10 -2.23505249 2.231835938 2.559863281 2.688226318 976 9955.582569 -8.60E-11 2.33E-06 -2.35E-06 6.45E-11 2.54E-06 2.69E-06 2.04E-10 1.69E-10 -2.233401489 2.229260254 2.559649658 2.68807373 977 9956.933311 -1.58E-10 2.33E-06 -2.35E-06 9.75E-11 2.54E-06 2.70E-06 2.05E-10 1.69E-10 -2.23270874 2.227740479 2.560784912 2.689144897 978 9958.288716 -8.60E-11 2.33E-06 -2.35E-06 3.15E-11 2.55E-06 2.70E-06 2.05E-10 1.69E-10 -2.235543823 2.230999756 2.565847778 2.694216919 979 9959.644498 2.95E-11 2.33E-06 -2.35E-06 9.75E-11 2.55E-06 2.70E-06 2.05E-10 1.69E-10 -2.231265259 2.22598877 2.562719727 2.690899658 980 9961.00495 -1.14E-10 2.33E-06 -2.35E-06 5.90E-11 2.55E-06 2.70E-06 2.05E-10 1.69E-10 -2.234686279 2.230026245 2.568588257 2.696829224 981 9962.36578 -4.75E-11 2.33E-06 -2.35E-06 2.60E-11 2.55E-06 2.71E-06 2.05E-10 1.69E-10 -2.234970093 2.230157471 2.570504761 2.699249268 982 9963.72699 -1.25E-10 2.33E-06 -2.35E-06 8.10E-11 2.55E-06 2.71E-06 2.06E-10 1.70E-10 -2.234332275 2.230386353 2.572659302 2.701467896 983 9965.08858 -1.03E-10 2.33E-06 -2.35E-06 5.35E-11 2.56E-06 2.71E-06 2.06E-10 1.70E-10 -2.233685303 2.228845215 2.573007202 2.702151489 984 9966.459144 -3.65E-11 2.33E-06 -2.35E-06 1.03E-10 2.56E-06 2.71E-06 2.06E-10 1.70E-10 -2.233773804 2.229858398 2.576156616 2.704812622 985 9967.817197 -1.58E-10 2.33E-06 -2.35E-06 7.00E-11 2.56E-06 2.71E-06 2.06E-10 1.70E-10 -2.23571167 2.232693481 2.58031311 2.709265137 986 9969.184228 -1.03E-10 2.33E-06 -2.34E-06 8.10E-11 2.56E-06 2.71E-06 2.07E-10 1.71E-10 -2.227111816 2.222161865 2.57227478 2.700689697 987 9970.551641 -1.08E-10 2.33E-06 -2.35E-06 8.65E-11 2.56E-06 2.71E-06 2.07E-10 1.71E-10 -2.230419922 2.225857544 2.577578735 2.706668091 988 9971.906531 -6.95E-11 2.33E-06 -2.34E-06 2.60E-11 2.56E-06 2.72E-06 2.07E-10 1.71E-10 -2.229537964 2.224685669 2.578665161 2.70723877 989 9973.257494 -7.50E-11 2.33E-06 -2.34E-06 8.65E-11 2.56E-06 2.72E-06 2.07E-10 1.71E-10 -2.228399658 2.223028564 2.579177856 2.707675171 990 9974.626048 -1.41E-10 2.32E-06 -2.34E-06 1.03E-10 2.57E-06 2.72E-06 2.07E-10 1.71E-10 -2.21986084 2.215979004 2.572262573 2.700018311 991 9975.986374 -9.15E-11 2.30E-06 -2.31E-06 9.20E-11 2.56E-06 2.71E-06 2.07E-10 1.71E-10 -2.206356812 2.202148438 2.557998657 2.685577393 992 9977.355692 9.55E-11 2.32E-06 -2.33E-06 7.00E-11 2.56E-06 2.71E-06 2.07E-10 1.71E-10 -2.225134277 2.22026062 2.581396484 2.710394287 993 9978.716778 9.55E-11 2.33E-06 -2.34E-06 8.65E-11 2.56E-06 2.71E-06 2.07E-10 1.71E-10 -2.230630493 2.226971436 2.590222168 2.719284058 994 9980.073934 7.50E-12 2.32E-06 -2.33E-06 7.55E-11 2.56E-06 2.71E-06 2.07E-10 1.71E-10 -2.222207642 2.217623901 2.582073975 2.710256958 995 9981.440087 -8.60E-11 2.32E-06 -2.33E-06 1.25E-10 2.57E-06 2.72E-06 2.08E-10 1.71E-10 -2.219168091 2.215319824 2.581103516 2.709362793 996 9982.80231 2.40E-11 2.31E-06 -2.32E-06 9.50E-12 2.57E-06 2.72E-06 2.08E-10 1.72E-10 -2.205627441 2.200567627 2.566885376 2.694073486 997 9984.164913 1.18E-10 2.32E-06 -2.33E-06 5.35E-11 2.57E-06 2.72E-06 2.08E-10 1.72E-10 -2.218603516 2.214260864 2.583966064 2.71265564 998 9985.53221 3.50E-11 2.32E-06 -2.33E-06 1.36E-10 2.57E-06 2.72E-06 2.08E-10 1.72E-10 -2.220004272 2.214901733 2.58706665 2.715911865 999 9986.891258 -6.40E-11 2.32E-06 -2.33E-06 9.20E-11 2.57E-06 2.72E-06 2.08E-10 1.72E-10 -2.221017456 2.216189575 2.589840698 2.718856812 #C Acquisition ended at Wed Feb 6 1:31:08 2013