dear all,
I am interest in NiTi allow.and I done Total electron yield (TEY) method for NiTi .I would like to see together l3 and l2 edges peak versus theorical Ni L3 and L2 edges.I done it using FEFF8 for theorical calculation but it is not similar measured ones.how can I do for this?especially satellite peak does not seem like measured satellite one.
thanks for in advance