                    I also encountered the same problem you are facing now.
The basic problem is that when you save k chik or k2 chik in Athena and
then get it imported in Artemis then the data is already k weighted and when
you again try to weight it in Artemis, the data gets disturb. So, you have
to save simply chik of your data in Athena and then import it into
Artemis.Then in Artemis you can weight your data as you have done in Athena
and it will look same as Athena plot.
Also from Artemis you can select the groups of which you which you need chi
k or chir and then you can go for option save selected groups in Artemis.
You will get all the data in one file . then you cam import it in Origin or
any other software by import single ascii option.
 In your case you save chir data the real part, imaginary part also got
saved with magnitude, so if you need your fourier transform as seen in
Athena, you just plot the magnitude column with data.
 I think this will work
                                Abhijeet Gaur
                               School of Studies in Physics
                               Vikram University Ujjain ( India)


On 7/21/09, ifeffit-request at millenia.cars.aps.anl.gov <
ifeffit-request at millenia.cars.aps.anl.gov> wrote:
>
> Send Ifeffit mailing list submissions to
>        ifeffit at millenia.cars.aps.anl.gov
>
> To subscribe or unsubscribe via the World Wide Web, visit
>        http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
> or, via email, send a message with subject or body 'help' to
>        ifeffit-request at millenia.cars.aps.anl.gov
>
> You can reach the person managing the list at
>        ifeffit-owner at millenia.cars.aps.anl.gov
>
> When replying, please edit your Subject line so it is more specific
> than "Re: Contents of Ifeffit digest..."
>
>
> Today's Topics:
>
>   1. inquire (Makoto Matsuura)
>
>
> ----------------------------------------------------------------------
>
> Message: 1
> Date: Tue, 21 Jul 2009 15:28:34 +0900
> From: "Makoto Matsuura" <m_matsuura at imr.tohoku.ac.jp>
> Subject: [Ifeffit] inquire
> To: <ifeffit at millenia.cars.aps.anl.gov>
> Message-ID: <000601ca09cc$790f3aa0$6b2dafe0$@tohoku.ac.jp>
> Content-Type: text/plain; charset="us-ascii"
>
> Hi!
>
> I'm annoyed with the mismach of Fourier transform between Athena and
> Arthemis. The k-weighting (k^1), k-window( Kaiser Bessel) and k-range are
> kept same for both. The input chi-data and resultant Fourier transforms are
> attached.
>
> One more question  of Arthemis is that when I try to output data of chi(k)
> or chi(r) from menu of File, null data file comes out while right data can
> be obtained for the fitted data. How can I get data of chi(k) or chi(r) in
> ascii format for Arthemis? Thank you.
> ========================================================================
> Makoto Matsuura
>
> IMR Tohoku Univ. Sendai, Japan
>
> =========================================================================
>
> -------------- next part --------------
> An HTML attachment was scrubbed...
> URL:
> http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20090721/8d0a9582/attachment.html
> -------------- next part --------------
> A non-text attachment was scrubbed...
> Name: Artemis.JPG
> Type: image/jpeg
> Size: 18670 bytes
> Desc: not available
> Url :
> http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20090721/8d0a9582/attachment.jpe
> -------------- next part --------------
> A non-text attachment was scrubbed...
> Name: Athena.JPG
> Type: image/jpeg
> Size: 19927 bytes
> Desc: not available
> Url :
> http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20090721/8d0a9582/attachment-0001.jpe
> -------------- next part --------------
> A non-text attachment was scrubbed...
> Name: input_data.chi
> Type: application/octet-stream
> Size: 25901 bytes
> Desc: not available
> Url :
> http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20090721/8d0a9582/attachment.obj
> -------------- next part --------------
> A non-text attachment was scrubbed...
> Name: Athena.rsp
> Type: application/octet-stream
> Size: 32604 bytes
> Desc: not available
> Url :
> http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20090721/8d0a9582/attachment-0001.obj
>
> ------------------------------
>
> _______________________________________________
> Ifeffit mailing list
> Ifeffit at millenia.cars.aps.anl.gov
> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
>
>
> End of Ifeffit Digest, Vol 77, Issue 19
> ***************************************
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20090721/be18bec3/attachment.htm>


More information about the Ifeffit mailing list