Hi Carlo,
You seem to be right. I try to do the fit in my notebook, which has the same
Windows and Services Packs, and worked. I want to know why? Is it possible
to resolve this?
You right too assuming that there is an H2 adsorbed. In reality, this is a
sample catalyst of 1%Pt supported in Al2O3 that was treated in H2. The data
of EXAFS was colleted at 500ºC in an flux of H2. It is a catalysts prepared
by impregnation method. In the fit model I assuming that is possible to has
a oxigen neighbor to Pt, therefore, there is a PtO2 model atom to do the
fit. They work well with one path unless by the peak at 1A. I already
thought to assuming a H atom neighbor to Pt but, I not find a good model to
this. Do you have some idea if is possible to do that? Do you belives that I
should take more than one path for Pt-Pt distance?
2009/1/13 Carlo Segre <segre at iit.edu>
>
> Hi Kleper:
>
> There is a single Pt-Pt path in your fit. This is effectively a fcc Pt
> distance of 2.77. I see several problems:
>
> This spectrum has distances which are much shorter than 2.77 and so I
> would expect that this single path would not be a very good fit. I am not
> sure if the peak around 1.1A is real, but it could be given the hydrogen
> that you indicate is present in the file name. What is clear is that the
> bigger peaks are not Pt-Pt peaks at all. The Pt-Pt peak will usually
> appear around 2.5A in Chi(R).
>
> The second thing that I noticed, is that you must have a problem with your
> installation of the software because I just took your file and executed
> the fit and did not get the strange values for Chi^2 and reduced Chi^2
> that you have posted. The value for amp is negative, indicating that the
> path is not a good model, but the Chi^2 I got was around 1000.
>
> I can't tell much form the name of your file but I suspect that you have
> Pt-Al and possibly Pt-H distances in your sample. Do you have any other
> information about this sample?
>
> Carlo
>
>
> --
> Carlo U. Segre -- Professor of Physics
> Associate Dean for Special Projects, Graduate College
> Illinois Institute of Technology
> Voice: 312.567.3498 Fax: 312.567.3494
> segre at iit.edu http://www.iit.edu/~segre segre at debian.org
> _______________________________________________
> Ifeffit mailing list
> Ifeffit at millenia.cars.aps.anl.gov
> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
>
--
Kleper de Oliveira Rocha
Doutorando em Engenharia Química
Departamento de Engenharia Química/UFSCar
Tels. 55 016 3351-8694
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20090113/cec3e6a3/attachment.htm>
More information about the Ifeffit
mailing list