[Ifeffit] Fitting procedure

abhijeet gaur abhijeetgaur9 at gmail.com
Fri Apr 24 07:09:41 CDT 2009


Hello Matt Sir,
                      Thanks a lot for your valuable sugestions. I had
fitted the Cu foil spectra as you suggested. I had taken same SO2 value for
all the paths and after fitting the first shell , making its parameter fix
when fitting second shell I changed the fit R range 2.9- 3.7 in order to
make the contribution of first shell negligible. I got a nice fit.  The
values of different parameters I got are as follows :
E 0=2.90 eV   ,  SO2= 0.72
 1st shell  R = 2.54, delR= -0.011, SS2=0.0083
 2nd shell R= 3.69,   delR= 0.080,  SS2=0.0088
The experimental data is taken at room temperature.
Are these parameters within the experimental error limit. Please tell me
                                                  with regards
                                                  Abhijeet Gaur