[Ifeffit] Mixed Multiple scattering shell

Joseph Washington breaditor2 at gmail.com
Wed Apr 1 12:55:53 CDT 2009


Hello all,
I was wondering if anyone can send any useful hints or tips
for parameterizing a mixed multiple scattering shell comprised of two NaCl
type strucutres, like the AgBr(1-x)Cl(x) example. Has anyone worked
on fitting the third shell in that example? I am looking for examples of
nacl rocksalt-like FEFF calculations that have successfully parametrized
multiple scattering path contributions. Right now, after running feff, I'm
using a different delr / ss term for each multiple scattering path I
include. Does anyone have any clever ways of representing these in terms of
the delr/ss in the first shell? Also, FEFF is telling me that the amp and
mixing terms are almost completely correlated and this cause the amp term to
blow up.

Thanks all, I really appreciate the assistance!

Joseph
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20090401/7125317d/attachment.htm>


More information about the Ifeffit mailing list