[Ifeffit] Crytallites AND polycrystalline - Artemis handling?
Scott Calvin
SCalvin at slc.edu
Fri Oct 17 17:51:07 CDT 2008
Hi Joe,
Here's an in-progress Artemis file for a system with some broad
similarities to the one your describe. Perhaps it will help.
Disclaimer: This is not a final fit!
--Scott
On Oct 17, 2008, at 2:15 PM, Joseph Washington wrote:
> Hello all,
> I am working on analyzing Ge edge EXAFS data of an annealed sample
> which
> is likely to be Ge-Te crystallites with some amorphous material at the
> grain boundary (or perhaps, just Ge-N crystal material at the
> interface). I do not have any information about the grain size, only
> possible constituents for the grain and the boundary. Can anyone
> give me
> some examples of how Artemis might handle this?
>
> Thanks in advance,
>
> --
> Joseph Washington
> Research Assistant
> Department of Physics
> North Carolina State University
> 431 Riddick Hall
> Raleigh, NC 27695-8202
> email: jswashin at ncsu.edu
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20081017/0b8b5f50/attachment.htm>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: TXEExample.apj
Type: application/octet-stream
Size: 1640865 bytes
Desc: not available
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20081017/0b8b5f50/attachment-0002.obj>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20081017/0b8b5f50/attachment-0001.htm>
More information about the Ifeffit
mailing list