Subject : Re: Titanium Oxide reference spectra 


Hello Carlo

If it is of use to  you, I have Ti K-edge spectra of in Ti1-xAlxN films 
nitrides, with the typical evolution of the prepeak from cubic 
(octahedral) to hexagonal (tetrahedral) Ti environment.

Marie-Hélène Tuilier


Université de Haute Alsace, 
Laboratoire Mécanique, Matériaux et Procédés de Fabrication
IUT de Mulhouse, 61 rue Albert Camus, 
F-68093 Mulhouse Cedex

Tel : 33 (0)3 89 33 75 16
Fax : 33 (0)3 89 33 75 05
http://www.mmpf.uha.fr/




ifeffit-request at millenia.cars.aps.anl.gov 
Envoyé par : ifeffit-bounces at millenia.cars.aps.anl.gov
10/06/08 17:42
Veuillez répondre à
ifeffit at millenia.cars.aps.anl.gov


A
ifeffit at millenia.cars.aps.anl.gov
cc

Objet
Ifeffit Digest, Vol 64, Issue 4






Send Ifeffit mailing list submissions to
                 ifeffit at millenia.cars.aps.anl.gov

To subscribe or unsubscribe via the World Wide Web, visit
                 http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
or, via email, send a message with subject or body 'help' to
                 ifeffit-request at millenia.cars.aps.anl.gov

You can reach the person managing the list at
                 ifeffit-owner at millenia.cars.aps.anl.gov

When replying, please edit your Subject line so it is more specific
than "Re: Contents of Ifeffit digest..."


Today's Topics:

   1. Titanium Oxide reference spectra (Carlo Segre)
   2. Re: Titanium Oxide reference spectra (Bruce Ravel)
   3. Re: Titanium Oxide reference spectra (Benjamin Marchetti)
   4. Re: Titanium Oxide reference spectra (Scott Calvin)
   5. Re: Titanium Oxide reference spectra (Benjamin Marchetti)


----------------------------------------------------------------------

Message: 1
Date: Tue, 10 Jun 2008 09:31:06 -0500 (CDT)
From: Carlo Segre <segre at iit.edu>
Subject: [Ifeffit] Titanium Oxide reference spectra
To: IFEFFIT Mailing List <ifeffit at millenia.cars.aps.anl.gov>
Message-ID: <alpine.DEB.1.10.0806100929490.11904 at oxide.phys.iit.edu>
Content-Type: TEXT/PLAIN; format=flowed; charset=US-ASCII


Hi All:

I am in need of various Ti-O reference spectra.  Does anyone have any such 

available?

Thanks,

Carlo

-- 
Carlo U. Segre -- Professor of Physics
Associate Dean for Special Projects, Graduate College
Illinois Institute of Technology
Voice: 312.567.3498            Fax: 312.567.3494
segre at iit.edu   http://www.iit.edu/~segre   segre at debian.org


------------------------------

Message: 2
Date: Tue, 10 Jun 2008 10:40:57 -0400
From: Bruce Ravel <bravel at bnl.gov>
Subject: Re: [Ifeffit] Titanium Oxide reference spectra
To: Carlo Segre <segre at iit.edu>,                 XAFS Analysis using 
Ifeffit
                 <ifeffit at millenia.cars.aps.anl.gov>
Message-ID: <200806101040.57281.bravel at bnl.gov>
Content-Type: text/plain;  charset="iso-8859-1"

On Tuesday 10 June 2008 10:31:06 Carlo Segre wrote:
> Hi All:
>
> I am in need of various Ti-O reference spectra.  Does anyone have any 
such
> available?

Hey Carlo,

I have various titante perovskites (Eu, Ba, Pb) if those help.

B


-- 
 Bruce Ravel  ------------------------------------ bravel at bnl.gov

 National Institute of Standards and Technology
 Synchrotron Methods Group at NSLS --- Beamlines U7A, X24A, X23A2
 Building 535A
 Upton NY, 11973

 My homepage:    http://xafs.org/BruceRavel
 EXAFS software: http://cars9.uchicago.edu/~ravel/software/exafs/



------------------------------

Message: 3
Date: Tue, 10 Jun 2008 16:52:30 +0200
From: Benjamin Marchetti <b.marchetti at ipc.uni-stuttgart.de>
Subject: Re: [Ifeffit] Titanium Oxide reference spectra
To: Bruce Ravel <bravel at bnl.gov>,                XAFS Analysis using 
Ifeffit
                 <ifeffit at millenia.cars.aps.anl.gov>
Message-ID: <484E952E.4000602 at ipc.uni-stuttgart.de>
Content-Type: text/plain; charset=ISO-8859-1; format=flowed

Bruce Ravel wrote:
> On Tuesday 10 June 2008 10:31:06 Carlo Segre wrote:
> 
>> Hi All:
>>
>> I am in need of various Ti-O reference spectra.  Does anyone have any 
such
>> available?
>> 
>
> Hey Carlo,
>
> I have various titante perovskites (Eu, Ba, Pb) if those help.
>
> B
>
>
> 
Hi

I have Anatase and Rutil Spektra.

benjamin

-- 
Benjamin Marchetti

Universit?t Stuttgart
Institut f?r Physikalische Chemie
Arbeitskreis Prof. Dr. H. Bertagnolli
Pfaffenwaldring 55
70569 Stuttgart (Vaihingen)

Telefon: (+49) 0711-685-64472
Fax: (+49) 0711-685-64443
E-Mail: b.marchetti at ipc.uni-stuttgart.de





------------------------------

Message: 4
Date: Tue, 10 Jun 2008 11:10:18 -0400
From: Scott Calvin <SCalvin at slc.edu>
Subject: Re: [Ifeffit] Titanium Oxide reference spectra
To: XAFS Analysis using Ifeffit <ifeffit at millenia.cars.aps.anl.gov>
Cc: Scott Calvin <SCalvin at slc.edu>
Message-ID: <FA824BA6-BADE-4E9D-BD21-7ECBB6B65F95 at slc.edu>
Content-Type: text/plain; charset=US-ASCII; format=flowed; delsp=yes

I also have anatase, although I haven't looked at it yet, so I can't 
vouch for it. If Benjamin knows his is good, go that route, but if 
you'd like a confirming spectrum, let me know.

--Scott Calvin
Sarah Lawrence College

On Jun 10, 2008, at 10:31 AM, Carlo Segre wrote:

>
> Hi All:
>
> I am in need of various Ti-O reference spectra.  Does anyone have 
> any such
> available?
>
> Thanks,
>
> Carlo



------------------------------

Message: 5
Date: Tue, 10 Jun 2008 17:41:26 +0200
From: Benjamin Marchetti <b.marchetti at ipc.uni-stuttgart.de>
Subject: Re: [Ifeffit] Titanium Oxide reference spectra
To: ifeffit at millenia.cars.aps.anl.gov
Message-ID: <484EA0A6.5020001 at ipc.uni-stuttgart.de>
Content-Type: text/plain; charset="iso-8859-1"

Sure .....
I used them for prepeak analysis, so the data should be fine.

benjamin

-- 
Benjamin Marchetti

Universit?t Stuttgart
Institut f?r Physikalische Chemie
Arbeitskreis Prof. Dr. H. Bertagnolli
Pfaffenwaldring 55
70569 Stuttgart (Vaihingen)

Telefon: (+49) 0711-685-64472
Fax: (+49) 0711-685-64443
E-Mail: b.marchetti at ipc.uni-stuttgart.de


-------------- next part --------------
An embedded and charset-unspecified text was scrubbed...
Name: rutil_ref
Url: 
http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20080610/2b273135/attachment.pl 

-------------- next part --------------
An embedded and charset-unspecified text was scrubbed...
Name: anatas_ref
Url: 
http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20080610/2b273135/attachment-0001.pl 


------------------------------

_______________________________________________
Ifeffit mailing list
Ifeffit at millenia.cars.aps.anl.gov
http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit


End of Ifeffit Digest, Vol 64, Issue 4
**************************************

-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20080611/8e8ad14d/attachment.htm>


More information about the Ifeffit mailing list