[Ifeffit] Atoms & Feff for Ferrihydrite Structure

Wayne Lukens wwlukens at lbl.gov
Thu Jan 10 14:58:57 CST 2008


Hi Andreas,

The problem was that for the atoms in position 6c, the sum
of x and y must be exactly 1. I have attached a corrected
atoms.inp file that seems to work.

Sincerely,

Wayne Lukens

Voegelin Andreas wrote:
> Dear all,
> 
> Using Atoms (latest version of Artemis), I tried to calculate a Feff
> input file based on a recently published structure for 6-Line
> Ferrihydrite (Michel et al, Science, 2007).
> 
> Attached: Atoms input file generated with Artemis.
> 
> For all three Fe sites as core (Fe1 and Fe2 octahedral, Fe3
> tetrahedral), running Atoms yields Feff files with "overlapping atoms"
> located close to each other. The Artemis error messages after running
> Feff suggests that a shift vector may be needed in order to obtain
> correct Feff input files. 
> 
> As a "non-crystallographer", I would be grateful for advice on how this
> problem can be solved.
> 
> Best regards,
> 
> Andreas
> 
> 
> ------------------------------------------------------------------------
> 
> _______________________________________________
> Ifeffit mailing list
> Ifeffit at millenia.cars.aps.anl.gov
> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit


-------------- next part --------------
An embedded and charset-unspecified text was scrubbed...
Name: atoms.inp
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20080110/b96a21c6/attachment.el>


More information about the Ifeffit mailing list