Hello Bruce,

Thank you for sharing your software. I found IFEFFIT in google and 
installed it recently in my MAC OSX computer. Trying to learn how to 
use it, I took a sample chi_k data (Al, k-edge) and played with the 
fitting in Artemis. One problem I can't solve by myself is that no 
matter how I chose the k range, r range, dr, dk, the fitting always 
stops at k~ 3 even though the data covers k= 1-8. So in the plot, the 
fit curve is much shorter than the data. Is this a plotting problem 
or a fitting problem? I've saved and attached the project to this 
email.

Thank you very much for your attention.
Yuan
-------------- next part --------------
A non-text attachment was scrubbed...
Name: %
Type: application/applefile
Size: 123 bytes
Desc: not available
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20070720/0f292a5d/attachment-0002.bin>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: Al-sample.apj
Type: application/octet-stream
Size: 147329 bytes
Desc: not available
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20070720/0f292a5d/attachment-0002.obj>


More information about the Ifeffit mailing list